Deep Learning for fractographic classification in metallic materials (Englisch)
- Neue Suche nach: Bastidas-Rodriguez, María X.
- Neue Suche nach: Polania, Luisa
- Neue Suche nach: Gruson, Adrien
- Neue Suche nach: Prieto-Ortiz, Flavio
- Neue Suche nach: Bastidas-Rodriguez, María X.
- Neue Suche nach: Polania, Luisa
- Neue Suche nach: Gruson, Adrien
- Neue Suche nach: Prieto-Ortiz, Flavio
In:
Engineering Failure Analysis
;
113
;
2020
-
ISSN:
- Aufsatz (Zeitschrift) / Elektronische Ressource
-
Titel:Deep Learning for fractographic classification in metallic materials
-
Beteiligte:Bastidas-Rodriguez, María X. ( Autor:in ) / Polania, Luisa ( Autor:in ) / Gruson, Adrien ( Autor:in ) / Prieto-Ortiz, Flavio ( Autor:in )
-
Erschienen in:
-
Verlag:
- Neue Suche nach: Elsevier Ltd
-
Erscheinungsdatum:07.04.2020
-
ISSN:
-
DOI:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Elektronische Ressource
-
Sprache:Englisch
-
Schlagwörter:
-
Datenquelle:
Inhaltsverzeichnis – Band 113
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
-
Study of impact phenomena for the design of a mobile anti-terror barrier: Experiments and finite element analysesBaragetti, S. / Arcieri, E.V. et al. | 2020
-
Fracture failure analysis of steam generator channel heads with high carbon macro-segregationShi, Kaikai / Zhang, Yixiong / Yang, Yu / Zheng, Bin / Xie, Hai / Gao, Shiqing / Bai, Xiaoming / Fu, Xiaolong / Shao, Xuejiao et al. | 2020
-
Failure analysis and damage causes of a steam turbine blade of 410 martensitic stainless steel after 165,000 h of workingRivaz, A. / Mousavi Anijdan, S.H. / Moazami-Goudarzi, M. et al. | 2020
-
Deep Learning for fractographic classification in metallic materialsBastidas-Rodriguez, María X. / Polania, Luisa / Gruson, Adrien / Prieto-Ortiz, Flavio et al. | 2020
-
Fatigue life evaluation of web butt welding structure on boom of excavator by hot spot stress approachZhu, Qiuyan / Lu, Pengmin / Xiang, Qingyi et al. | 2020
-
Quantification of sub-surface railhead material damage due to composite endpost materials of insulated rail joints for cyclic wheel loadingsMandal, Nirmal Kumar / Lewis, Roger / Wen, Zefeng et al. | 2020
-
Investigation of the electrical rolling contact degradation based on fractal theoryNiu, Chunping / Chen, Junxingxu / Yang, Fei / Liu, Qi / Lei, Hang / Wu, Yifei / Wu, Yi / Rong, Mingzhe et al. | 2020
-
Failure analysis of cryogenically treated H13 specimen in rotating bending fatigueShinde, Tarang et al. | 2020
-
Failure investigation of buffer layers in high-voltage XLPE cablesChen, Yun / Hui, Baojun / Cheng, Yanting / Hao, Yanpeng / Fu, Mingli / Yang, Lin / Hou, Shuai / Li, Licheng et al. | 2020
-
Finite element modelling and fatigue life assessment of a cemented total hip prosthesis based on 3D scanningBabić, Milena / Verić, Ozren / Božić, Željko / Sušić, Aleksandar et al. | 2020
-
Mechanical behavior of secondary tunnel lining with longitudinal crackXu, Guowen / He, Chuan / Chen, Ziquan / Liu, Chuankun / Wang, Bo / Zou, Yulin et al. | 2020
-
Improving service life of magnesium reduction steel retorts against creep collapse by structural modificationShahheidari, Majid / Nazari-Onlaghi, Sina / Sadeghi, Alireza / Sadeghi, Mohammad Hossein et al. | 2020
-
Integrity assessment of the pipelines containing an isolated corrosion pitJin, Zhi-jiang / Qiu, Chang / Chen, Zhanfeng / Yan, Sun-ting / Shen, Xiao-li et al. | 2020
-
Predicting damage and failure under thermomechanical fatigue in hot forging toolsGhalehbandi, S.M. / Biglari, F. et al. | 2020
-
Study on reducing the risk of stress corrosion cracking of austenitic stainless steel hydraulically expanded jointsHong, Ying / Wang, Xuesheng / Wang, Yan / Zhang, Zhao et al. | 2020
-
Increase in wind load during assembly causes collapse of the hall structureIgnatowicz, Rajmund L. / Gierczak, Jan et al. | 2020
-
Investigation on leakage cause of oil pipeline in the west oilfield of ChinaLiu, Qiang / Yu, Haoyu / Zhu, Guo-chuan / Wang, Peng-bo / Song, Sheng-yin et al. | 2020
-
Evaluation of creep properties for aged Pb-free solder joints/(Ni-P/Au) UBM with small addition Cu using shear punch creep testing methodHai, Sophal / Oh, Sung-Hoon / Yu, Hyo-Sun et al. | 2020
-
Investigation of the effect of low temperature aging on the mechanical properties and susceptibility to sulfide stress corrosion cracking of 22%Cr duplex stainless steelTavares, S.S.M. / Batista, R.T. / Landim, R.V. / Velasco, J.A.C. / Senna, L.F. et al. | 2020
-
Hydrogen embrittlement induced fracture of 17-4 PH stainless steel valve stemJiang, Tao / Zhong, Jiru / Zhang, Xiaocheng / Wang, Wulin / Guan, Kaishu et al. | 2020
-
Analysis and interpretation of power auto-transformer winding axial displacement and radial deformation using frequency response analysisMahvi, Mojtaba / Behjat, Vahid / Mohseni, Hossein et al. | 2020
-
Fatigue failure analysis of dented pipeline and simulation calculationLuo, Jinheng / Zhang, Yani / Li, Lifeng / Zhu, Lixia / Wu, Gang et al. | 2020
-
Editorial Board| 2020
-
Failure analysis of fretting fracture in frame rails of heavy duty trucks – Case studyRao, Vinay N. / Eischen, Jeffrey W. et al. | 2020
-
Cracking mechanism in API 5L X65 steel in a CO2-saturated environment – Part II: A study under cathodic polarisationSilva, S.C. / Silva, A.B. / Folena, M.C. / Barker, R. / Neville, A. / Ponciano Gomes, J.A.C. et al. | 2020
-
Failure analysis and fatigue performance assessment of titanium diaphragms used in sonic soot blowersJavanmard, M. / Sarfaraz, R. / Dibajian, S.H. / Yadavar Nikravesh, S.M. et al. | 2020
-
Elastic limit load resource when reaming holes in turbine rotor discsPawlicki, Jakub / Głowacki, Dominik / Zwoliński, Janisław / Mościcki, Artur et al. | 2020
-
Influence of heat treatments on the susceptibility of 9%Ni low carbon steel to sulfide stress corrosion crackingCunha, R.P.C. / Barbosa, C. / Barrozo, R.F. / Velasco, J.A.C / Tavares, S.S.M. et al. | 2020
-
Analysis of the influence of soil moisture on the stability of a building based on a slopeŚlusarek, Jan / Łupieżowiec, Marian et al. | 2020
-
Structural integrity and life assessment of rotating equipmentMilovanović, N. / Sedmak, A. / Arsic, M. / Sedmak, S.A. / Božić, Ž. et al. | 2020
-
Fault prediction of drag system using artificial neural network for prevention of dragline failureSahu, Atma Ram / Palei, Sanjay Kumar et al. | 2020
-
Design research on forging mark of connecting rodJia, Dewen / Li, Yunpeng / Deng, Xiwen / Lei, Jilin / Deng, Wei et al. | 2020
-
Exploring factors controlling pre-corrosion fatigue of 316L austenitic stainless steel in hydrofluoric acidChen, Xu / Yang, Lin / Dai, Hailong / Shi, Shouwen et al. | 2020
-
Thermo-structural fatigue and lifetime analysis of a heat exchanger as a feedwater heater in power plantHoseinzadeh, Siamak / Heyns, P. Stephan et al. | 2020