Probabilistic model for stress corrosion cracking of underground pipelines using Bayesian networks (Englisch)
- Neue Suche nach: Jain, Swati
- Neue Suche nach: Beavers, John A.
- Neue Suche nach: Ayello, Francois
- Neue Suche nach: Sridhar, Narasi
- Neue Suche nach: Jain, Swati
- Neue Suche nach: Beavers, John A.
- Neue Suche nach: Ayello, Francois
- Neue Suche nach: Sridhar, Narasi
In:
Corrosion Conference & Expo, NACE International, 2013
;
4281-4295
;
2013
-
ISBN:
- Aufsatz (Konferenz) / Print
-
Titel:Probabilistic model for stress corrosion cracking of underground pipelines using Bayesian networks
-
Weitere Titelangaben:Statistisches Modell für die Spannrisskorrosion von Untergrundrohrleitungen unter Anwendung des Bayes-Netzwerks
-
Beteiligte:Jain, Swati ( Autor:in ) / Beavers, John A. ( Autor:in ) / Ayello, Francois ( Autor:in ) / Sridhar, Narasi ( Autor:in )
-
Erschienen in:
-
Verlag:
- Neue Suche nach: Curran Associates
-
Erscheinungsort:Red Hook
-
Erscheinungsdatum:2013
-
Format / Umfang:15 Seiten, 11 Bilder, 1 Tabelle, 24 Quellen
-
ISBN:
-
Medientyp:Aufsatz (Konferenz)
-
Format:Print
-
Sprache:Englisch
-
Schlagwörter:
-
Datenquelle:
Inhaltsverzeichnis Konferenzband
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 42
-
Low cost real-time stray current monitoring system for seawater field studiesDrach, Andrew / Tsukrov, Igor et al. | 2013
- 62
-
Real-time AC/DC measurement technique for investigation of AC corrosion of pipelines and its effect on the cathodic protection effectivenessXu, Luyao / Cheng, Y. Frank et al. | 2013
- 103
-
Application of optical profilometric techniques to corrosion monitoringMenendez, Carlos M. et al. | 2013
- 119
-
New Corrosion Monitoring Probe Combines ER, LPR, HDA, Floating B-constant, Electrochemical Noise and Conductivity MeasurementsHeselmans, Jan / Hladky, Karel / Holdefer, Martin / Wessels, Roolf et al. | 2013
- 501
-
Welding, inspection and performance of joints in titaniumHolmes, Briony / Gittos, Michael / Bahrami, Amir / Maddox, Stephen et al. | 2013
- 595
-
Improving ph prediction for high pressure and high temperature applications in oil and gas productionPlennevaux, C. / Cassagne, T. / Bonis, M. / Ferrando, N. / Kittel, J. / Ropital, F. / Fregonese, M. / Normand, B. et al. | 2013
- 780
-
Laboratory corrosion assessment of post-tensioned tendons repaired with dissimilar groutLau, Kingley / Lasa, Ivan / Paredes, Mario / Rafols, Juan et al. | 2013
- 919
-
Evaluation of corrosion characteristics of aluminum alloys in the bio-ethanol gasoline blended fuel by using a 2-electrode electrochemical impedance spectroscopyPark, In-Jun / Kim, Jin-Ho / Nam, Tae-Heum / Kim, Jung-Gu et al. | 2013
- 1060
-
Materials selection and corrosion control for a CO2 transport and injection systemHuizinga, Sytze / Orzessek, Karin / Mul, Leo de / Koers, Ronald et al. | 2013
- 1233
-
Pitting in the water/hydrocarbon boundary region of pipelines - effect of corrosion inhibitors -Schmitt, Guenter / Karbasi, Gilda / Nesic, Srdjan / Hausler, Rudolf / Kinsella, Brian / Brown, Bruce et al. | 2013
- 1370
-
High temperature testing of corrosion inhibitor performancePalencsar, Attila / Gulbrandsen, Egil / Kosoru, Katenina et al. | 2013
- 1398
-
New water soluble high shear, high temperature corrosion inhibitorRamachandran, Sunder / Jovancicevic, Vladimir / Boyce, Greg / Zeadow, Christina et al. | 2013
- 1756
-
Characterization of silica precipitation kinetics under high temperature geothermal field conditions using ultrasonic techniquesAndhika, Muhamad / Regenspurg, Simona et al. | 2013
- 1777
-
Corrosion related tube failures in amine reboiler unitsSaithala, Janardhan Rao / Illson, Tim / Hachicha, Mohammed / Abdollah, Sabrina et al. | 2013
- 1868
-
Electrochemical studies of the effect of solution impurities on the onset of stress corrosion cracking of austenitic stainless steel in PWR primary waterBocher, Florent / Mintz, Todd et al. | 2013
- 1937
-
Hydrides formation from fuel cladding corrosion and influence of hydrides on mechanical behaviorHe, Xihua / Pan, Yiming / Chan, Kwai et al. | 2013
- 2122
-
Nuclear welding product 52MSS delivers improved tensile strength and maximum resistance to PWSCC and DDCKiser, Samuel / Zhang, Rengang / Caruso, Martin et al. | 2013
- 2247
-
Internal corrosion of CO2 pipelines for carbon capture and storageSim, S. / Corrigan, P. / Cole, I.S. / Birbilis, N. et al. | 2013
- 2314
-
Innovative approach for predicting galvanic corrosion effects on airframe systemsRose, Alan / Legg, Keith et al. | 2013
- 2364
-
Effects of surface modification conditions on hydrophobicity of silica-based coating additivesHillesheim, D.A. / Armstrong, B.L. / Pawel, S.J. / Haynes, J.A. / Hunter, S.R. et al. | 2013
- 2401
-
Modeling galvanic corrosion in multi-material aircraft structuresPeratta, Andres / Adey, Robert et al. | 2013
- 2502
-
Effect of bacteria on the corrosion resistance of structural metals in water sources and systemsEliezer, A. / Levak, O. / Baram, E. / Barri, K. / Koritny, A. / Schorr, M. / Valdez, B. / Shotland, Y. et al. | 2013
- 2525
-
Corrosion monitoring of a polymer coated subsea pipe with ultrasoundNerbo, Ingar Stian / Baltzersen, Oystein / Sleire, Harald / Karaga, Ibrahim / Fiksdal, Vegard / Haarberg, Sarbjyot / Guldstein, Malfrid et al. | 2013
- 2573
-
External cathodic protection of concrete-pad mounted aboveground storage tank - Necessity or choice?Khosravi, Javad et al. | 2013
- 2590
-
Improving the corrosion resistance of magnesium by vapor phase processingWolfe, Ryan C. / Shaw, Barbara A. et al. | 2013
- 2604
-
Mechanisms of inhibition of the chloride-induced crevice corrosion of alloy 22Rodriguez, Martin A. / Rebak, Raul B. / Carranza, Ricardo M. et al. | 2013
- 2702
-
Condensate in the muffler of automotive exhaust systemHashimoto, Reina / Mori, Gregor / Yasir, Muhammad / Tröger, Uwe / Wieser, Helmut et al. | 2013
- 2712
-
Crevice corrosion on super duplex stainless steel - effect of potential on critical crevice corrosion temperatureHoydal, Anne Britt / Hemmingsen, Tor / Skavas, Erling et al. | 2013
- 2794
-
Corrosion rate monitoring in pipeline casingsHilleary, Jamey / DeWitt, Jerry et al. | 2013
- 2803
-
Vehicle emission testing with corrosion sensorsYang, Andrew A. / Sun, Xiaodong et al. | 2013
- 2913
-
Dealing with severe corrosion on a recently installed pipelineSegall, S.M. / Gummow, R.A. / Fingas, D. / Shore, John et al. | 2013
- 2985
-
An approach to measurement of environmentally assisted small crack growthTurnbull, A. / Zhou, S. / McCormick, N. / Lukaszweicz, M. et al. | 2013
- 3066
-
Crack stability criteria and its implications on crack growth rates, mechanisms and crack geometryScott, Colin et al. | 2013
- 3153
-
Effect of flow on the mechanism and kinetics of some corrosion processesQuevedo, M.C. / Galicia, G. / Olalde, R. / Genesca, J. / Duran, R. / Mendoza, J. et al. | 2013
- 3182
-
Evaluating inhibitor performance in CO2-saturated, erosion-corrosion environmentsBarker, Richard / Hu, Xinming / Neville, Anne / Cushnaghan, Susan et al. | 2013
- 3304
-
The high-temperature corrosion resistance of spun-cast materials for steam-cracker furnaces - a comparative study of alumina- and chromia-forming alloysJakobi, Dietlinde / Karduck, Peter / Freiherr von Richthofen, Alexander et al. | 2013
- 3614
-
Acid corrosion mechanism and characterization of E-glass fibers with and without boronGu, Pu / Watson, James / Li, Hong / Richards, Cheryl et al. | 2013
- 3720
-
Why are some microbes corrosive and some not?Gu, Tingyue / Xu, Dake et al. | 2013
- 4043
-
Review of pipe line coating systems from an operators perspectiveThompson, Ian / Saithala, Janardhan Rao et al. | 2013
- 4071
-
New advancements in the abrasion resistance of internal plastic coatingsLauer, Robert S. et al. | 2013
- 4088
-
Compatibility between concrete coating, mainline coating, and CP systemPapavinasam, S. / Mtchim, M. et al. | 2013
- 4098
-
EMAT, pipe coatings, corrosion control and cathodic protection shieldingNorsworthy, Richard / Grillenberger, Jörg / Brockhaus, Stephan / Ginten, Markus et al. | 2013
- 4281
-
Probabilistic model for stress corrosion cracking of underground pipelines using Bayesian networksJain, Swati / Beavers, John A. / Ayello, Francois / Sridhar, Narasi et al. | 2013
- 4491
-
Hydrogen embrittlement in titanium and superferritic stainless steel steam surface condenser tubingSchumerth, Dennis J. / Demers, Thomas et al. | 2013
- 4521
-
New developed 6-Mo super-austenitic stainless steel with low sigma solvus temperature and high resistance to localised corrosionBehrens, R. / Alves, H. / Stenner, F. et al. | 2013
- 4549
-
Corrosion performance of nickel alloys in dilute hydrochloric and sulfuric acids near and above boiling pointDeodeshmukh, V.P. / Manning, P.E. / Crook, P. et al. | 2013
- 4574
-
Experience aids nickel alloy selection for CPI applicationsShoemaker, Lewis E. / Crum, James R. / Baker, Brian A. / McCoy, Steve / Hazeldine, Paul et al. | 2013
- 4641
-
Examination of a "green" corrosion inhibitor and corrosion resistant alloys for the overhead of the crude oil distillation unitGroysman, Alec / Penner, Joseph / Mizrahi, Liran / Brodsky, Naphtali et al. | 2013
- 4690
-
A novel approach for risk ranking, NDT priorities and damage mitigation of TIP units piping systems in high temperature hydrogen serviceMarco, Marco De / Mannello, Giuseppe et al. | 2013
- 4816
-
An electrochemical study of corrosion inhibition of carbon steel in sour glycol solutionsKvarekval, Jon / Pedersen, Anette et al. | 2013
- 4917
-
SSC resistance of 316Ti in brine under highly sour conditionsSiegmund, Gerit / Schmitt, Guenter / Noga, Josef et al. | 2013
- 4955
-
Evaluation of a novel top-of-the-line corrosion (TLC) mitigation method in a large scale flow loopJevremovic, I. / Miskovic-Stankovic, V. / Achour, M. / Singer, M. / Nesic, S. et al. | 2013
- 5189
-
Development of an accelerated weathering test to evaluate the corrosion protection of pipes by UV-curable varnishesRoche, V. / Schultes, F. / Millet, C. / Zeislmair, U. / Bonilla, F. et al. | 2013
- 5395
-
New corrosion inhibitors for evaporative cooling systemsWehlmann, Anika / Wolf, Florian / Hater, Wolfgang / Lunkenheimer, Rudolf / Foret, Christophe et al. | 2013