Wear of die materials in full scale plastic injection moulding of glass fibre reinforced polycarbonate (Englisch)
- Neue Suche nach: Bergstrom, J.
- Neue Suche nach: Thuvander, F.
- Neue Suche nach: Devos, P.
- Neue Suche nach: Boher, C.
- Neue Suche nach: Bergstrom, J.
- Neue Suche nach: Thuvander, F.
- Neue Suche nach: Devos, P.
- Neue Suche nach: Boher, C.
In:
WEAR -LAUSANNE-
;
251
, 1-12
;
1511-1521
;
2001
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:Wear of die materials in full scale plastic injection moulding of glass fibre reinforced polycarbonate
-
Beteiligte:Bergstrom, J. ( Autor:in ) / Thuvander, F. ( Autor:in ) / Devos, P. ( Autor:in ) / Boher, C. ( Autor:in )
-
Erschienen in:WEAR -LAUSANNE- ; 251, 1-12 ; 1511-1521
-
Verlag:
- Neue Suche nach: ELSEVIER SEQUOIA SA
-
Erscheinungsdatum:01.01.2001
-
Format / Umfang:11 pages
-
ISSN:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Englisch
- Neue Suche nach: 620.11292
- Weitere Informationen zu Dewey Decimal Classification
-
Klassifikation:
DDC: 620.11292 -
Datenquelle:
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Inhaltsverzeichnis – Band 251, Ausgabe 1-12
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 827
-
Thermo-chemical erosion in gun barrelsLawton, B. et al. | 2001
- 839
-
The influence of water flow on the impact/sliding wear and oxidation of PWR control rods specimensLina, A. / Moinereau, D. / Delaune, X. / Phalippou, C. / Reynier, B. / Riberty, P. et al. | 2001
- 853
-
Experimental and numerical investigation of a new method for protecting bends from erosion in gas-particle flowsFan, J. / Yao, J. / Zhang, X. / Cen, K. et al. | 2001
- 861
-
Evaluation of wear resistance of thin hard coatings by a new solid particle impact testIwai, Y. / Honda, T. / Yamada, H. / Matsubara, T. / Larsson, M. / Hogmark, S. et al. | 2001
- 868
-
The influence of a heat treatment on the tribological performance of a high wear resistant high Si Al-Si alloy weld overlayOtt, R. D. / Blue, C. A. / Santella, M. L. / Blau, P. J. et al. | 2001
- 875
-
Wear of iron-aluminide intermetallic-based alloys and composites by hard particlesAlman, D. E. / Hawk, J. A. / Tylczak, J. H. / Dogan, C. P. / Wilson, R. D. et al. | 2001
- 885
-
Influences of graphite shapes on wear characteristics of austempered cast ironHatate, M. / Shiota, T. / Takahashi, N. / Shimizu, K. et al. | 2001
- 890
-
Abrasive wear behavior of a brittle matrix (MoSi2) composite reinforced with a ductile phase (Nb)Alman, D. E. / Hawk, J. A. et al. | 2001
- 901
-
Changes in microstructure, texture and residual stresses on the surface of a rail resulting from friction and wearPyzalla, A. / Wang, L. / Wild, E. / Wroblewski, T. et al. | 2001
- 908
-
Wear of tungsten carbide-cobalt hardmetals and hot isostatically pressed high speed steels under dry abrasive conditionsGant, A. J. / Gee, M. G. et al. | 2001
- 916
-
An analytical approach to study a special case of booted sleeper track rail corrugationGomez, I. / Vadillo, E. G. et al. | 2001
- 925
-
Analysis of heat partition and temperature distribution in sliding systemsKomanduri, R. / Hou, Z. B. et al. | 2001
- 939
-
Thermal compatibility of dry sliding tribo-specimensAbdel-Aal, H. A. et al. | 2001
- 949
-
Computer simulation of wear and rolling contact fatigueFranklin, F. J. / Widiyarta, I. / Kapoor, A. et al. | 2001
- 956
-
Modification of Archard`s equation by taking account of elastic/pseudoelastic properties of materialsLiu, R. / Li, D. Y. et al. | 2001
- 965
-
Friction and wear of rotating pivots in MEMS and other small scale devicesWilliams, J. A. et al. | 2001
- 973
-
The effect of lubricant selection on galling in a model wear testvan der Heide, E. / Huis in `t Veld, A. J. / Schipper, D. J. et al. | 2001
- 980
-
Effect of contact pressure and load on wear of aluminaRavikiran, A. / Jahanmir, S. et al. | 2001
- 985
-
The residual stresses on lubricated sliding surfaces during break-in and up to scuffingKim, J. W. / Lee, Y. Z. et al. | 2001
- 990
-
Friction and wear characteristics of hard coatingsStanford, M. K. / Jain, V. K. et al. | 2001
- 997
-
Tribological behaviour of multi-layered PVD nitride coatingsImbeni, V. / Martini, C. / Lanzoni, E. / Poli, G. / Hutchings, I. M. et al. | 2001
- 1003
-
Differential application of wear models to fractional thin filmsBlanchet, T. A. / Gregory Sawyer, W. et al. | 2001
- 1009
-
A comparison of the abrasive wear behaviour of HVOF sprayed titanium carbide- and titanium boride-based cermet coatingsJones, M. / Horlock, A. J. / Shipway, P. H. / McCartney, D. G. / Wood, J. V. et al. | 2001
- 1017
-
Sliding wear behaviour of plasma sprayed WC-NiCrBSi coatings at different temperaturesMartin, A. / Rodriguez, J. / Fernandez, J. E. / Vijande, R. et al. | 2001
- 1023
-
Wear of thermal spray deposited low carbon steel coatings on aluminum alloysEdrisy, A. / Perry, T. / Cheng, Y. T. / Alpas, A. T. et al. | 2001
- 1034
-
Investigation of surface treatments for galling protection of titanium alloysWiklund, U. / Hutchings, I. M. et al. | 2001
- 1042
-
Scale effects in abrasive wear of composite sol-gel alumina coated light alloysWilson, S. / Hawthorne, H. M. / Yang, Q. / Troczynski, T. et al. | 2001
- 1051
-
Characterization and wear behavior of pulsed electrode surfacing coatingsStaia, M. H. / Fragiel, A. / Cruz, M. / Carrasquero, E. / Campillo, B. / Perez, R. / Constantino, M. / Sudarshan, T. S. et al. | 2001
- 1061
-
Durability evaluation of selected solid lubricating filmsMiyoshi, K. et al. | 2001
- 1068
-
New solid lubricant coatingsTeer, D. G. et al. | 2001
- 1075
-
Tribological performance of thin organic permanent coatings deposited on 55%Al-Zn coated steel - influence of coating composition and thickness on friction and wearCarlsson, P. / Bexell, U. / Olsson, M. et al. | 2001
- 1085
-
The effect of lubricants in single point scratching and abrasive machining of alumina and silicon nitrideDesa, O. / Bahadur, S. et al. | 2001
- 1094
-
Lubrication behavior of Ni-Cr-based alloys containing MoS2 at high temperatureDangsheng, X. et al. | 2001
- 1100
-
Effect of carbon fibre reinforcement in the frictional behaviour of Peek in a water lubricated environmentDavim, J. P. / Marques, N. / Baptista, A. M. et al. | 2001
- 1105
-
Nano- to microscale wear and mechanical characterization using scanning probe microscopyBhushan, B. et al. | 2001
- 1124
-
Tribology challenges of modern magnetic hard disk drivesKhurshudov, A. / Waltman, R. J. et al. | 2001
- 1133
-
Application of single asperity abrasion process for surface micro-machiningLee, J. M. / Jin, W. H. / Kim, D. E. et al. | 2001
- 1144
-
Nanoindentation and microtribological behavior of Fe-N/Ti-N multilayers with different thickness of Ti-N layersLu, X. C. / Shi, B. / Li, L. K. / Luo, J. / Chang, X. / Tian, Z. / Mou, J. I. et al. | 2001
- 1150
-
Time-dependent mechanical properties and tribological behavior of magnetic tapesLi, X. / Bhushan, B. / Inoue, M. et al. | 2001
- 1159
-
The application of laser scanning confocal microscopy to tribological researchHanlon, D. N. / Todd, I. / Peekstok, E. / Rainforth, W. M. / van der Zwaag, S. et al. | 2001
- 1169
-
Investigation of the tribological behavior of octadecyltrichlorosilane deposited on siliconCha, K. H. / Kim, D. E. et al. | 2001
- 1177
-
Observations of the topography and friction properties of macromolecular thin films at the nanometer scaleShi, B. / Lu, X. / Zou, R. / Luo, J. / Chen, D. / Liang, H. / Huang, L. et al. | 2001
- 1183
-
Surface friction of polymer gelsGong, J. P. / Kagata, G. / Iwasaki, Y. / Osada, Y. et al. | 2001
- 1193
-
In situ evaluation of wear surface by ultrasoundAhn, H. S. / Kim, D. I. et al. | 2001
- 1202
-
Experimental and numerical evaluation of the mechanical properties of compacted wear debris layers formed between composite and steel surfaces in sliding contactFriedrich, K. / Flock, J. / Varadi, K. / Neder, Z. et al. | 2001
- 1213
-
Do current wear particle isolation procedures underestimate the number of particles generated by prosthetic bearing components?Scott, M. / Widding, K. / Jani, S. et al. | 2001
- 1218
-
The use of color in wear debris analysisMyshkin, N. K. / Kong, H. / Grigoriev, A. Y. / Yoon, E. S. et al. | 2001
- 1227
-
Fractal characterization of wear particle accumulation in the wear processShirong, G. / Guoan, C. / Xiaoyun, Z. et al. | 2001
- 1234
-
Effects of phase in stainless steels on corrosive wear behavior in sulfuric acidLu, X. C. / Li, S. / Jiang, X. et al. | 2001
- 1239
-
Corrosion response of surface engineered titanium alloys damaged by prior abrasionKomotori, J. / Lee, B. J. / Dong, H. / Dearnley, P. A. et al. | 2001
- 1250
-
Improvement in the resistance of aluminum with yttria particles to sliding wear in air and in a corrosive mediumZhang, T. / Li, D. Y. et al. | 2001
- 1257
-
Corrosion-erosion of nitrogen bearing martensitic stainless steels in seawater-quartz slurryToro, A. / Sinatora, A. / Tanaka, D. K. / Tschiptschin, A. P. et al. | 2001
- 1265
-
Finite element modelling of crack growth and wear particle formation in sliding contactKo, P. L. / Iyer, S. S. / Vaughan, H. / Gadala, M. et al. | 2001
- 1279
-
Service validation of corrosive wear synergySchumacher, W. et al. | 2001
- 1284
-
Mechanical and electrochemical interactions during liquid-solid impingement on high-alloy stainless steelsNeville, A. / Hu, X. et al. | 2001
- 1295
-
Influence of passivity on the tribocorrosion of carbon steel in aqueous solutionsMischler, S. / Spiegel, A. / Stemp, M. / Landolt, D. et al. | 2001
- 1308
-
Micro-scale abrasion and scratch response of PVD coatings at elevated temperaturesAllsopp, D. N. / Hutchings, I. M. et al. | 2001
- 1315
-
Evaluation of abrasive wear of ductile cast iron in a single pass pendulum deviceVelez, J. M. / Tanaka, D. K. / Sinatora, A. / Tschiptschin, A. P. et al. | 2001
- 1320
-
Shakedown analysis and fretting wear response under gross slip conditionFouvry, S. et al. | 2001
- 1332
-
Theoretical analysis of steady-state texture formation during wear of a bi-material surfaceFletcher, D. I. / Kapoor, A. / Steinhoff, K. / Schuleit, N. et al. | 2001
- 1337
-
Numerical and experimental study of the circular cracks observed at the contact edges of the indentations of coated systems with soft substratesSouza, R. M. / Sinatora, A. / Mustoe, G. G. / Moore, J. J. et al. | 2001
- 1347
-
Pitting of the rolling bodies contact surfaceDatsyshyn, O. P. / Panasyuk, V. V. et al. | 2001
- 1356
-
Computer simulation of two-body abrasion processesFang, L. / Xing, J. / Liu, W. / Xue, Q. / Wu, G. / Zhang, X. et al. | 2001
- 1361
-
Abrasive wear properties of Cr-Cr3Si compositesNewkirk, J. W. / Hawk, J. A. et al. | 2001
- 1372
-
Laser cladding of stainless steel with Ni-Cr3C2 for improved wear performanceZhang, D. W. / Lei, T. C. / Li, F. J. et al. | 2001
- 1377
-
Effect of thermal treatment and recycling on the tribological behaviour of an AlSiMg-SiCp compositeCeschini, L. / Bosi, C. / Casagrande, A. / Garagnani, G. L. et al. | 2001
- 1386
-
Development of an abrasion resistant steel composite with in situ TiC particlesBerns, H. / Wewers, B. et al. | 2001
- 1396
-
The role of tribo-layers on the sliding wear behavior of graphitic aluminum matrix compositesRiahi, A. R. / Alpas, A. T. et al. | 2001
- 1408
-
Dry sliding wear of garnet reinforced zinc/aluminium metal matrix compositesRanganath, G. / Sharma, S. C. / Krishna, M. et al. | 2001
- 1414
-
Tribological stability of Al2O3 short fiber reinforced high Cr cast ironsSakamoto, M. / Liu, H. N. / Nomura, M. / Ogi, K. et al. | 2001
- 1421
-
Dry wear behaviour and its relation to microstructure of novel 6092 aluminium alloy-Ni3Al powder metallurgy compositeWang, Y. / Rainforth, W. M. / Jones, H. / Lieblich, M. et al. | 2001
- 1433
-
Mapping erosion of Ni-Cr/WC-based composites at elevated temperatures: some recent advancesStack, M. M. / Pena, D. et al. | 2001
- 1444
-
Elevated temperature sliding wear behaviour of TiC-reinforced steel matrix compositesDegnan, C. C. / Shipway, P. H. / Wood, J. V. et al. | 2001
- 1452
-
Temperature effects on the tribological behavior of alumina reinforced with unidirectionally oriented SiC whiskersLim, D. S. / Park, D. S. / Han, B. D. / Kan, T. S. / Jang, H. et al. | 2001
- 1459
-
Wear resistance of a laser alloyed A-356 aluminum/WC compositeStaia, M. H. / Cruz, M. / Dahotre, N. B. et al. | 2001
- 1469
-
Chemical and microstructural changes induced by friction and wear of brakesOsterle, W. / Griepentrog, M. / Gross, T. / Urban, I. et al. | 2001
- 1477
-
Compositional effects of the brake friction material on creep groan phenomenaJang, H. / Lee, J. S. / Fash, J. W. et al. | 2001
- 1484
-
Synergistic effects of aramid pulp and potassium titanate whiskers in the automotive friction materialKim, S. J. / Cho, M. H. / Lim, D. S. / Jang, H. et al. | 2001
- 1492
-
A basic study of friction noise caused by frettingJibiki, T. / Shima, M. / Akita, H. / Tamura, M. et al. | 2001
- 1504
-
Tribological properties of ion-implanted polyphenylene oxide (PPO)San, J. / Liu, J. / Zhu, B. / Liu, Z. / Dong, C. / Zhang, Q. et al. | 2001
- 1511
-
Wear of die materials in full scale plastic injection moulding of glass fibre reinforced polycarbonateBergstrom, J. / Thuvander, F. / Devos, P. / Boher, C. et al. | 2001
- 1522
-
The effect of fillers on the wear resistance of thermoplastic polymeric coatingsXu, Y. M. / Mellor, B. G. et al. | 2001
- 1532
-
The role of filler deformability, filler-polymer bonding, and counterface material on the tribological behavior of polyphenylene sulfide (PPS)Schwartz, C. J. / Bahadur, S. et al. | 2001
- 1541
-
Experimental and numerical analysis of friction and wear behavior of polycarbonateLee, J. H. / Xu, G. H. / Liang, H. et al. | 2001
- 1557
-
A study of the tribological behaviour of polyamide 66 with varying injection-moulding parametersApichartpattanasiri, S. / Hay, J. N. / Kukureka, S. N. et al. | 2001
- 1567
-
Wear testing and measurement techniques for polymer composite gearsWright, N. A. / Kukureka, S. N. et al. | 2001
- 1579
-
An experimental study of the nano-scratch behaviour of poly(methyl methacrylate)Adams, M. J. / Allan, A. / Briscoe, B. J. / Doyle, P. J. / Gorman, D. M. / Johnson, S. A. et al. | 2001
- 1584
-
Fe micro-models to study contact states, stresses and failure mechanisms in a polymer composite subjected to a sliding steel asperityGoda, T. / Varadi, K. / Friedrich, K. et al. | 2001
- 1591
-
Wear experiments with selected engineering polymers and polymer composites under dry reciprocating sliding conditionsFranklin, S. E. et al. | 2001