Dependence of inherent selective atomic layer deposition of FeOx on Pt nanoparticles on the coreactant and temperature (Englisch)
- Neue Suche nach: Cai, Jiaming
- Neue Suche nach: Merkx, Marc J. M.
- Neue Suche nach: Lan, Yuxiao
- Neue Suche nach: Jing, Yao
- Neue Suche nach: Cao, Kun
- Neue Suche nach: Wen, Yanwei
- Neue Suche nach: Kessels, Wilhelmus M. M.
- Neue Suche nach: Mackus, Adriaan J. M.
- Neue Suche nach: Chen, Rong
- Neue Suche nach: Cai, Jiaming
- Neue Suche nach: Merkx, Marc J. M.
- Neue Suche nach: Lan, Yuxiao
- Neue Suche nach: Jing, Yao
- Neue Suche nach: Cao, Kun
- Neue Suche nach: Wen, Yanwei
- Neue Suche nach: Kessels, Wilhelmus M. M.
- Neue Suche nach: Mackus, Adriaan J. M.
- Neue Suche nach: Chen, Rong
In:
Journal of Vacuum Science & Technology A
;
39
, 1
;
7
;
2021
- Aufsatz (Zeitschrift) / Elektronische Ressource
-
Titel:Dependence of inherent selective atomic layer deposition of FeOx on Pt nanoparticles on the coreactant and temperature
-
Beteiligte:Cai, Jiaming ( Autor:in ) / Merkx, Marc J. M. ( Autor:in ) / Lan, Yuxiao ( Autor:in ) / Jing, Yao ( Autor:in ) / Cao, Kun ( Autor:in ) / Wen, Yanwei ( Autor:in ) / Kessels, Wilhelmus M. M. ( Autor:in ) / Mackus, Adriaan J. M. ( Autor:in ) / Chen, Rong ( Autor:in )
-
Erschienen in:Journal of Vacuum Science & Technology A ; 39, 1 ; 7
-
Verlag:
- Neue Suche nach: American Vacuum Society
-
Erscheinungsdatum:01.01.2021
-
Format / Umfang:7 pages
-
ISSN:
-
DOI:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Elektronische Ressource
-
Sprache:Englisch
-
Schlagwörter:
-
Datenquelle:
Inhaltsverzeichnis – Band 39, Ausgabe 1
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
-
Review of key vertical-cavity laser and modulator advances enabled by advanced MBE technologyColdren, Larry A. et al. | 2021
-
Acquisition and analysis of scanning tunneling spectroscopy data—WSe2 monolayerFeenstra, Randall M. / Frazier, Grayson R. / Pan, Yi / Fölsch, Stefan / Lin, Yu-Chuan / Jariwala, Bhakti / Zhang, Kehao / Robinson, Joshua A. et al. | 2021
-
Characterization of vapor draw vessel performance for low-volatility solid precursor deliveryMaslar, James E. / Kimes, William A. / Sperling, Brent A. / Kanjolia, Ravindra K. et al. | 2021
-
Ultra-thin Al2O3 capped with SiNx enabling implied open-circuit voltage reaching 720 mV on industrial p-type Cz c-Si wafers for passivated emitter and rear solar cellsKökbudak, Gamze / Keçeci, Ahmet E. / Nasser, Hisham / Turan, Raşit et al. | 2021
-
Work function performance of a C12A7 electride surface exposed to low pressure low temperature hydrogen plasmasHeiler, A. / Waetzig, K. / Tajmar, M. / Friedl, R. / Nocentini, R. / Fantz, U. et al. | 2021
-
High temperature isotropic and anisotropic etching of silicon carbide using forming gasFrye, C. D. / Funaro, Devin / Conway, A. M. / Hall, D. L. / Grivickas, P. V. / Bora, M. / Voss, L. F. et al. | 2021
-
In-Cu alloy substrates for low-temperature chemical vapor deposition of Mo2CYoung, Katherine T. / Smith, Colter / Hitchcock, Dale A. / Vogel, Eric M. et al. | 2021
-
Assessment of the (010) β-Ga2O3 surface and substrate specificationMastro, Michael A. / Eddy, Charles R. / Tadjer, Marko J. / Hite, Jennifer K. / Kim, Jihyun / Pearton, Stephen J. et al. | 2021
-
Modeling atomic layer deposition process parameters to achieve dense nanocrystal-based nanocompositesCendejas, Austin / Moher, Dillon / Thimsen, Elijah et al. | 2021
-
Plasma enhanced atomic layer deposition of thin film Li1+xMn2−xO4 for realization of all solid-state 3D lithium-ion microbatteriesSheil, Ryan / Butts, Danielle / Jungjohann, Katherine / Yoo, Jinkyoung / Dunn, Bruce / Chang, Jane P. et al. | 2021
-
Control of ion energy during plasma enhanced atomic layer deposition: A new strategy for the modulation of TiN growth delay on SiO2Belahcen, Samia / Vallée, Christophe / Bsiesy, Ahmad / Chaker, Ahmad / Jaffal, Moustapha / Yeghoyan, Taguhi / Bonvalot, Marceline et al. | 2021
-
Origin of area selective plasma enhanced chemical vapor deposition of microcrystalline siliconAkiki, Ghewa / Frégnaux, Mathieu / Florea, Ileana / Bulkin, Pavel / Daineka, Dmitri / Filonovich, Sergej / Bouttemy, Muriel / Johnson, Erik V. et al. | 2021
-
Modification of copper and copper oxide surface states due to isopropyl alcohol treatment toward area-selective processesMawaki, Takezo / Teramoto, Akinobu / Ishii, Katsutoshi / Shiba, Yoshinobu / Kuroda, Rihito / Suwa, Tomoyuki / Azumo, Shuji / Shimizu, Akira / Umezawa, Kota / Shirai, Yasuyuki et al. | 2021
-
Physical vapor deposition of the halide perovskite CsBi2Br7Tran, Minh N. / Cleveland, Iver J. / Aydil, Eray S. et al. | 2021
-
Practical guide to the use of backgrounds in quantitative XPSTougaard, Sven et al. | 2021
-
Insight into the removal and reapplication of small inhibitor molecules during area-selective atomic layer deposition of SiO2Merkx, Marc J. M. / Jongen, Rick G. J. / Mameli, Alfredo / Lemaire, Paul C. / Sharma, Kashish / Hausmann, Dennis M. / Kessels, Wilhelmus M. M. / Mackus, Adriaan J. M. et al. | 2021
-
Selective atomic layer deposition on flexible polymeric substrates employing a polyimide adhesive as a physical maskForouzmehr, Matin / Zambou, Serges / Lahtonen, Kimmo / Honkanen, Mari / Nazmul Anam, Rafi Md / Ruhanen, Aleksi / Rokaya, Chakra / Lupo, Donald / Berger, Paul R. et al. | 2021
-
Influence of nitrogen gas flow ratio on gallium nitride film growth using high-density convergent plasma sputtering device at room temperatureMotomura, T. / Tabaru, T. / Fujio, Y. / Okuyama, T. et al. | 2021
-
Practical guides for x-ray photoelectron spectroscopy (XPS): Interpreting the carbon 1s spectrumGengenbach, Thomas R. / Major, George H. / Linford, Matthew R. / Easton, Christopher D. et al. | 2021
-
Area-selective aerosol jet fog deposition: Advancing large-area and sustainable fabricationMullapudi, Kamesh / Murari, Nishit M. / Mansergh, Ryan H. / Keszler, Douglas A. / Conley, John F. et al. | 2021
-
Errata: “Atomic layer etching of metals with anisotropy, specificity, and selectivity” [J. Vac. Sci. Technol. A 38, 043005 (2020)]Sang, Xia / Xia, Yantao / Sautet, Philippe / Chang, Jane P. et al. | 2021
-
Techniques for epitaxial site-selective growth of quantum dotsMcCabe, Lauren N. / Zide, Joshua M. O. et al. | 2021
-
Dependence of inherent selective atomic layer deposition of FeOx on Pt nanoparticles on the coreactant and temperatureCai, Jiaming / Merkx, Marc J. M. / Lan, Yuxiao / Jing, Yao / Cao, Kun / Wen, Yanwei / Kessels, Wilhelmus M. M. / Mackus, Adriaan J. M. / Chen, Rong et al. | 2021
-
Vacuum ultraviolet enhanced atomic layer etching of ruthenium filmsCoffey, Brennan M. / Nallan, Himamshu C. / Ekerdt, John G. et al. | 2021
-
Application of templated vapor-liquid-solid growth to heteroepitaxy of InP on SiSchneble, Olivia D. / Neumann, Anica N. / Mangum, John S. / Norman, Andrew G. / Warren, Emily L. / Zimmerman, Jeramy D. et al. | 2021
-
Rhombohedral boron nitride epitaxy on ZrB2Souqui, Laurent / Palisaitis, Justinas / Ghafoor, Naureen / Pedersen, Henrik / Högberg, Hans et al. | 2021
-
Errata: ‘‘Patterning nickel for extreme ultraviolet lithography mask application I. Atomic layer etch processing’’ [J. Vac. Sci. Technol. A 38, 042603 (2020)]Sang, Xia / Chen, Ernest / Chang, Jane P. et al. | 2021
-
Interface characteristics of β-Ga2O3/Al2O3/Pt capacitors after postmetallization annealingHirose, Masafumi / Nabatame, Toshihide / Irokawa, Yoshihiro / Maeda, Erika / Ohi, Akihiko / Ikeda, Naoki / Sang, Liwen / Koide, Yasuo / Kiyono, Hajime et al. | 2021
-
Erratum: “Practical guides for x-ray photoelectron spectroscopy: First steps in planning, conducting, and reporting XPS measurements” [J. Vac. Sci. Technol. A 37, 031401 (2019)]Baer, Donald R. / Artyushkova, Kateryna / Richard Brundle, Christopher / Castle, James E. / Engelhard, Mark H. / Gaskell, Karen J. / Grant, John T. / Haasch, Richard T. / Linford, Matthew R. / Powell, Cedric J. et al. | 2021
-
Mitigating residual stress of high temperature CVD diamond films on vanadium carbide coated steelMartins, Rômulo Luís / Damm, Djoille Denner / Corat, Evaldo José / Trava-Airoldi, Vladimir Jesus / Barquete, Danilo Maciel et al. | 2021
-
Superconformal growth and trench filling using a consumable inhibitor in chemical vapor deposition of Hf1−xVxByCanova, Kinsey L. / Zhang, Zhejun V. / Girolami, Gregory S. / Abelson, John R. et al. | 2021
-
Universal scaling relationship for atomic layer etchingKanarik, Keren J. / Tan, Samantha / Yang, Wenbing / Berry, Ivan L. / Pan, Yang / Gottscho, Richard A. et al. | 2021
-
Surface ligand removal in atomic layer deposition of GaN using triethylgalliumDeminskyi, Petro / Hsu, Chih-Wei / Bakhit, Babak / Rouf, Polla / Pedersen, Henrik et al. | 2021
-
Accuracy limitations for composition analysis by XPS using relative peak intensities: LiF as an exampleBrundle, Christopher Richard / Crist, Bruce Vincent / Bagus, Paul S. et al. | 2021
-
Plasma enhanced atomic layer deposition of titanium nitride-molybdenum nitride solid solutionsChowdhury, Md. Istiaque / Sowa, Mark / Kozen, Alexander C. / Krick, Brandon A. / Haik, Jewel / Babuska, Tomas F. / Strandwitz, Nicholas C. et al. | 2021
-
Effect of probe geometry during measurement of >100 A Ga2O3 vertical rectifiersSharma, Ribhu / Xian, Minghan / Fares, Chaker / Law, Mark E. / Tadjer, Marko / Hobart, Karl D. / Ren, Fan / Pearton, Stephen J. et al. | 2021