On localised corrosive attack, stress corrosion cracking and corrosion fatigue effects in a hardmetal cutting-tool material (Englisch)
- Neue Suche nach: Pugsley, Victoria
- Neue Suche nach: Korn, Gregor
- Neue Suche nach: Luyckx, Silvana
- Neue Suche nach: Sockel, Hans-Georg
- Neue Suche nach: Pugsley, Victoria
- Neue Suche nach: Korn, Gregor
- Neue Suche nach: Luyckx, Silvana
- Neue Suche nach: Sockel, Hans-Georg
In:
International Journal of Materials Research
;
93
, 7
;
745-749
;
2021
- Aufsatz (Zeitschrift) / Elektronische Ressource
-
Titel:On localised corrosive attack, stress corrosion cracking and corrosion fatigue effects in a hardmetal cutting-tool material
-
Beteiligte:Pugsley, Victoria ( Autor:in ) / Korn, Gregor ( Autor:in ) / Luyckx, Silvana ( Autor:in ) / Sockel, Hans-Georg ( Autor:in )
-
Erschienen in:International Journal of Materials Research ; 93, 7 ; 745-749
-
Verlag:
- Neue Suche nach: De Gruyter
-
Erscheinungsdatum:07.12.2021
-
Format / Umfang:5 pages
-
ISSN:
-
DOI:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Elektronische Ressource
-
Sprache:Englisch
-
Schlagwörter:
-
Datenquelle:
Inhaltsverzeichnis – Band 93, Ausgabe 7
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 1
-
Frontmatter| 2022
- 600
-
Editorial| 2022
- 602
-
A model for the work hardening of WC–Co “hard metals”ProfessorNabarro, F. R. N. / Bilby, B. A. et al. | 2022
- 605
-
On the dispersion strengthening mechanisms in ODS materialsProf. Dr.Reppich, Bernd et al. | 2022
- 614
-
Effect of hydrogen on the mechanical properties of the β titanium alloy Timetal® 21SSenemmar, Ali / Prof. Dr.-Ing.Christ, Hans-Jürgen et al. | 2021
- 620
-
Cyclic deformation behaviour of (α + β) titanium alloys under complex mechanical and physiological loading conditionsSchwilling, Berthold / Dr.-Ing.Fleck, Claudia / Eifler, Dietmar et al. | 2021
- 627
-
Assessment of the influence of interdendritic shrinkage cavities on the thermo-mechanical fatigue behaviour of the nickel-base superalloy MAR-M247LCBeck, Markus / Dr.-Ing.Lang, Karl-Heinz / Löhe, Detlef et al. | 2022
- 635
-
Effects of static strain aging on residual stress stability and alternating bending strength of shot peened AISI 4140Menig, Rainer / Dr.-Ing.Schulze, Volker / Vöhringer, Otmar et al. | 2022
- 641
-
On the possibilities to enhance the fatigue properties of ultrafine-grained metalsDr.Höppel, H. W. / Valiev, R. Z. et al. | 2022
- 649
-
New method of determining stress relaxation behavior in creep machines by controlled unloadingProf.Blum, Wolfgang / Breutinger, Falk et al. | 2022
- 654
-
Creep of binary Ni-rich NiTi shape memory alloys and the influence of pre-creep on martensitic transformationsEggeler, G. / Khalil-Allafi, J. / Neuking, K. / Dlouhý, A. et al. | 2022
- 661
-
Interaction of high-cycle fatigue with high-temperature creep in superalloy single crystalsAssoc. Prof. Dr.Lukáš, Petr / Kunz, Ludvík / Svoboda, Milan et al. | 2021
- 666
-
A unified description of creep in pure and dispersion-strengthened copperDr.Heilmaier, Martin / Kestler, Heinrich / Gibeling, Jeffery C. et al. | 2022
- 672
-
A new interpretation of flow-stress measurements of high-purity NiAl below room temperatureDr.Brunner, D. / Gumbsch, P. et al. | 2021
- 681
-
A mesoscopic plasticity model accounting for spatial fluctuations of plastic strains, internal stresses and dislocation densitiesAldazabal, J. / Prof.Sevillano, J. Gil et al. | 2022
- 689
-
Behavior of X-ray peak widths in the Wilkens model of a restrictedly random distribution of dislocationsDr.Borbély, András / Guiglionda, Gilles / Driver, Julian H. et al. | 2022
- 694
-
Dislocation structure and crystallite size distribution in hexagonal nanomaterials from X-ray peak profile analysisDr.Ungár, Tamás / Gubicza, Jenö et al. | 2022
- 699
-
Werden gewichtsoptimiert konstruierte Bauteile durch die Verwendung von Leichtmetallen wirklich leichter?*)Prof. Dr.Neumann, Peter et al. | 2022
- 706
-
Strain-induced martensite formation in metastable austenitic steels with varying carbon contentKrupp, Ulrich / West, Charles G. / Duan, Huiping / Prof. Dr.-Ing.Christ, Hans-Jürgen et al. | 2022
- 712
-
Isothermal bainitic transformation in low alloy steels: factors limiting prediction of the resulting material’s propertiesProf. Dr.-Ing.Maier, Hans Jürgen / Ahrens, Uwe et al. | 2022
- 719
-
Fatigue damage evolution in a particulate-reinforced metal matrix composite determined by acoustic emission and compliance methodProf. Dr.Biermann, Horst / Vinogradov, Alexei / Hartmann, Oliver et al. | 2021
- 724
-
Microstructure and modification mechanisms of Si phase in as-thixoformed alloy A356Wen, K. Y. / Gottstein, G. et al. | 2021
- 730
-
Influence of size effect on microstructural changes in cyclically deformed polycrystalline nickelDr.Thiele, Ellen / Holste, Carl / Klemm, Robert et al. | 2021
- 737
-
Self-diffusion of 71Ge and 31Si in Si –Ge alloysStrohm, Andreas / Voss, Thilo / Prof. Dr.Frank, Werner / Laitinen, Pauli / Räisänen, Jyrki et al. | 2021
- 745
-
On localised corrosive attack, stress corrosion cracking and corrosion fatigue effects in a hardmetal cutting-tool materialPugsley, Victoria / Korn, Gregor / Luyckx, Silvana / Sockel, Hans-Georg et al. | 2021
- 750
-
The internal stress during growth of SiC single crystalsProf. Dr.Strunk, Horst P. / Heindl, Jürgen et al. | 2022
- 754
-
Personal/Personelles| 2022
- 756
-
Books/Bücher| 2022
- 757
-
DGM Conferences/Training| 2022