The mechanism of stress corrosion cracking of Alloy 690TT in a caustic solution containing lead (Englisch)
- Neue Suche nach: Hou, Qiang
- Neue Suche nach: Liu, Zhiyong
- Neue Suche nach: Li, Chengtao
- Neue Suche nach: Li, Xiaogang
- Neue Suche nach: Hou, Qiang
- Neue Suche nach: Liu, Zhiyong
- Neue Suche nach: Li, Chengtao
- Neue Suche nach: Li, Xiaogang
In:
Corrosion Science
;
128
;
154-163
;
2017
-
ISSN:
- Aufsatz (Zeitschrift) / Elektronische Ressource
-
Titel:The mechanism of stress corrosion cracking of Alloy 690TT in a caustic solution containing lead
-
Beteiligte:Hou, Qiang ( Autor:in ) / Liu, Zhiyong ( Autor:in ) / Li, Chengtao ( Autor:in ) / Li, Xiaogang ( Autor:in )
-
Erschienen in:Corrosion Science ; 128 ; 154-163
-
Erscheinungsdatum:12.09.2017
-
Format / Umfang:10 pages
-
ISSN:
-
DOI:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Elektronische Ressource
-
Sprache:Englisch
-
Schlagwörter:
-
Datenquelle:
Inhaltsverzeichnis – Band 128
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 1
-
A fast, low temperature zinc phosphate coating on steel accelerated by graphene oxideXie, Yuhui / Chen, Mingzhi / Xie, Delong / Zhong, Li / Zhang, Xinya et al. | 2017
- 9
-
The role of acetic acid or H+ in initiating crevice corrosion of N80 carbon steel in CO2-saturated NaCl solutionLi, Y.Z. / Xu, N. / Guo, X.P. / Zhang, G.A. et al. | 2017
- 23
-
Bio-corrosion behaviour of oxygen diffusion layer on Ti-6Al-4V during tribocorrosionYazdi, R. / Ghasemi, H.M. / Wang, C. / Neville, A. et al. | 2017
- 33
-
Effect of grain size on the resistance to hydrogen embrittlement of API 2W Grade 60 steels using in situ slow-strain-rate testingPark, Cheolho / Kang, Namhyun / Liu, Stephen et al. | 2017
- 42
-
Hot corrosion behavior and near-surface microstructure of a “low-temperature high-activity Cr-aluminide” coating on inconel 738LC exposed to Na2SO4, Na2SO4+V2O5 and Na2SO4+V2O5+NaCl at 900°CSalehi Doolabi, M. / Ghasemi, B. / Sadrnezhaad, S.K. / Habibollahzadeh, A. / Jafarzadeh, K. et al. | 2017
- 54
-
Synthesis, electrochemical and quantum chemical studies of some prepared surfactants based on azodye and Schiff base as corrosion inhibitors for steel in acid mediumBedair, M.A. / El-Sabbah, M.M.B. / Fouda, A.S. / Elaryian, H.M. et al. | 2017
- 73
-
Differences in pitting growth kinetics between Zr60Ni25Al15 and Zr60Cu25Al15 metallic glasses exposed to a 0.6M NaCl aqueous solutionLi, Yu / Xu, Jian et al. | 2017
- 85
-
Pyrophoric behaviour of ultrafine Mo powderWang, Lu / Zhang, Guo-Hua / Jiao, Shu-Qiang / Chou, Kuo-Chih et al. | 2017
- 94
-
Unexpected effect of citrate ions on the corrosion process of carbon steel in alkaline solutionsToujas, S. / Vázquez, M. / Valcarce, M.B. et al. | 2017
- 100
-
Effects of flow, Si inhibition, and concurrent corrosion of dissimilar metals on the corrosion of aluminium in the environment following a loss-of-coolant accidentGuo, Shaoqiang / Leavitt, Jeanette J / Zhou, Xinquan / Xie, Yi / Tietze, Sabrina / Zhu, Yakun / Lawver, Angela / Lahti, Erik / Zhang, Jinsuo et al. | 2017
- 110
-
Fabrication of non-wetting surfaces on zinc surface as corrosion barrierWang, Peng / Li, Tianping / Zhang, Dun et al. | 2017
- 120
-
Evaluation of multiple stress corrosion crack interactions by in-situ Digital Image CorrelationBolivar, J. / Frégonèse, M. / Réthoré, J. / Duret-Thual, C. / Combrade, P. et al. | 2017
- 130
-
Determination of the key parameters involved in the formation process of akaganeite in a laboratory-simulated wet-dry cyclic processXiao, Haigang / Ye, Wei / Song, Xiaoping / Wang, Yanmin / Ma, Yuantai / Li, Ying et al. | 2017
- 140
-
On the stress corrosion crack growth behaviour in high temperature water of 316L stainless steel made by laser powder bed fusion additive manufacturingLou, Xiaoyuan / Song, Miao / Emigh, Paul W. / Othon, Michelle A. / Andresen, Peter L. et al. | 2017
- 154
-
The mechanism of stress corrosion cracking of Alloy 690TT in a caustic solution containing leadHou, Qiang / Liu, Zhiyong / Li, Chengtao / Li, Xiaogang et al. | 2017
- 164
-
Cerium-loaded algae exoskeletons for active corrosion protection of coated AA2024-T3Denissen, Paul J. / Garcia, Santiago J. et al. | 2017
- 176
-
Fabrication of polydimethylsiloxane-derived superhydrophobic surface on aluminium via chemical vapour deposition technique for corrosion protectionSun, Wen / Wang, Lida / Yang, Zhengqing / Li, Sijia / Wu, Tingting / Liu, Guichang et al. | 2017
- 186
-
Surface recrystallization and its effect on oxidation of superalloy C263Sheng, Naicheng / Horke, Katharina / Meyer, Andreas / Gotterbarm, Martin R. / Rettig, Ralf / Singer, Robert F. et al. | 2017
- 198
-
Effect of heat treatment on hydrogen-assisted fracture behavior of PH13-8Mo steelLi, Xinfeng / Zhang, Jin / Akiyama, Eiji / Li, Qizhen / Wang, Yanfei et al. | 2017
- 213
-
The corrosion of Zr(Fe, Cr)2 and Zr2Fe secondary phase particles in Zircaloy-4 under 350°C pressurised water conditionsAnnand, Kirsty / Nord, Magnus / MacLaren, Ian / Gass, Mhairi et al. | 2017
- 224
-
Comprehensive screening of Mg corrosion inhibitorsLamaka, S.V. / Vaghefinazari, B. / Mei, Di / Petrauskas, R.P. / Höche, D. / Zheludkevich, M.L. et al. | 2017
- 241
-
Early oxidation mechanism of austenitic stainless steel TP347H in supercritical waterLi, Yanhui / Wang, Shuzhong / Sun, Panpan / Xu, Donghai / Ren, Mengmeng / Guo, Yang / Lin, Guike et al. | 2017
- 253
-
Microstructure of localized corrosion front on Mg alloys and the relationship with hydrogen evolutionChu, Peng-Wei / Le Mire, Etienne / Marquis, Emmanuelle A. et al. | 2017
- 265
-
Discussion on “Microstructural evolution and stress-corrosion-cracking behavior of thermally aged Ni–Cr–Fe alloy” by S.C. Yoo, K.J. Choi, T. Kim, S.H. Kim, J.Y. Kim, J.H. Kim [Corros. Sci. 111 (2016) 39]Kim, Young Suk / Kim, Sung Soo et al. | 2017
- 267
-
Reply to discussion on “Microstructural evolution and stress-corrosion-cracking behavior of thermally aged Ni-Cr-Fe alloy” by S.C. Yoo, K.J. Choi, T. Kim, S.H. Kim, J.Y. Kim, J.H. Kim [Corros. Sci. 111 (2016) 39]Yoo, Seung Chang / Choi, Kyoung Joon / Kim, Taeho / Kim, Si Hoon / Kim, Ju Young / Kim, Ji Hyun et al. | 2017
- IFC
-
IFC - Editorial Board| 2017