Improving the quality of nanocrystalline MgAl2O4 spinel coating on graphite by a prior oxidation treatment on the graphite surface (Englisch)
- Neue Suche nach: Saberi, A.
- Neue Suche nach: Golestani-Fard, F.
- Neue Suche nach: Willert-Porada, M.
- Neue Suche nach: Simon, R.
- Neue Suche nach: Gerdes, T.
- Neue Suche nach: Sarpoolaky, H.
- Neue Suche nach: Saberi, A.
- Neue Suche nach: Golestani-Fard, F.
- Neue Suche nach: Willert-Porada, M.
- Neue Suche nach: Simon, R.
- Neue Suche nach: Gerdes, T.
- Neue Suche nach: Sarpoolaky, H.
In:
Journal of the European Ceramic Society
;
28
, 10
;
2011-2017
;
2008
-
ISSN:
- Aufsatz (Zeitschrift) / Elektronische Ressource
-
Titel:Improving the quality of nanocrystalline MgAl2O4 spinel coating on graphite by a prior oxidation treatment on the graphite surface
-
Beteiligte:Saberi, A. ( Autor:in ) / Golestani-Fard, F. ( Autor:in ) / Willert-Porada, M. ( Autor:in ) / Simon, R. ( Autor:in ) / Gerdes, T. ( Autor:in ) / Sarpoolaky, H. ( Autor:in )
-
Erschienen in:Journal of the European Ceramic Society ; 28, 10 ; 2011-2017
-
Verlag:
- Neue Suche nach: Elsevier Ltd
-
Erscheinungsdatum:04.01.2008
-
Format / Umfang:7 pages
-
ISSN:
-
DOI:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Elektronische Ressource
-
Sprache:Englisch
-
Schlagwörter:
-
Datenquelle:
Inhaltsverzeichnis – Band 28, Ausgabe 10
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 1923
-
Direct observation of mould cavity filling in ceramic injection mouldingDvorak, P. / Barriere, Th. / Gelin, J.C. et al. | 2008
- 1931
-
A further report on finite element analysis of sintering deformation using densification data—Error estimation and constrained sinteringHuang, Ruoyu / Pan, Jingzhe et al. | 2008
- 1941
-
Assessment of viscoelastic crack bridging toughening in refractory materialsBoccaccini, D.N. / Cannio, M. / Volkov-Husoviæ, T.D. / Dlouhy, I. / Romagnoli, M. / Veronesi, P. / Leonelli, C. et al. | 2008
- 1941
-
Assessment of viscoelestic crack bridging toughening in refractory materialsBoccaccini, D.N. / Cannio, M. / Volkov-Husoviae, T.D. / Dlouhy, I. / Romagnoli, M. / Veronesi, P. / Leonelli, C. et al. | 2008
- 1953
-
Microstructural changes and evolutions of elastic properties versus temperature of alumina and alumina–magnesia refractory castablesAuvray, Jean-Michel / Gault, Christian / Huger, Marc et al. | 2008
- 1961
-
Fracture behaviour of microcrack-free alumina–aluminium titanate ceramics with second phase nanoparticles at alumina grain boundariesBueno, S. / Berger, M.H. / Moreno, R. / Baudín, C. et al. | 2008
- 1973
-
Formation of Y3Al5O12–Al2O3 eutectic microstructure with off-eutectic compositionHarada, Yohei / Uekawa, Naofumi / Kojima, Takashi / Kakegawa, Kazuyuki et al. | 2008
- 1979
-
Failure of the plasma-sprayed coating of lanthanum hexaluminateCao, X.Q. / Zhang, Y.F. / Zhang, J.F. / Zhong, X.H. / Wang, Y. / Ma, H.M. / Xu, Z.H. / He, L.M. / Lu, F. et al. | 2008
- 1987
-
Synthesis of CoAl2O4 by double decomposition reaction between LiAlO2 and molten KCoCl3Ouahdi, N. / Guillemet, S. / B. Durand / Ouatib, R. El / Rakho, L. Er / Moussa, R. / Samdi, A. et al. | 2007
- 1995
-
Sintering of tricalcium phosphate–fluorapatite composites with zirconiaBen Ayed, Foued / Bouaziz, Jamel et al. | 2008
- 2003
-
Cracking of titania nanocrystalline coatingsMahé, Marie / Heintz, Jean-Marc / Rödel, Jürgen / Reynders, Peter et al. | 2008
- 2011
-
Improving the quality of nanocrystalline MgAl2O4 spinel coating on graphite by a prior oxidation treatment on the graphite surfaceSaberi, A. / Golestani-Fard, F. / Willert-Porada, M. / Simon, R. / Gerdes, T. / Sarpoolaky, H. et al. | 2008
- 2019
-
Dilatometer analysis of sintering behavior of nano-CeO2 particlesKinemuchi, Yoshiaki / Watari, Koji et al. | 2008
- 2025
-
A stabilization mechanism for the perovskite La2/3TiO3 compound with Fe2O3: A structural and electrical investigationŠkapin, Srečo Davor / Škapin, Andrijana Sever / Suvorov, Danilo / Gaberšček, Miran et al. | 2007
- 2025
-
A stabilization mechanism for the perovskite La(0.67)TiO3 compound with Fe2O3: A structural and electrical investigationSkapin, S.D. / Skapin, A.S. / Suvorov, D. / Gaberscek, M. et al. | 2008
- 2033
-
Brown pigment of the nanopowder spinel ferrite prepared by combustion reactionCosta, A.C.F.M. / Leite, A.M.D. / Ferreira, H.S. / Kiminami, R.H.G.A. / Cava, S. / Gama, L. et al. | 2007
- 2033
-
Brown pigment of nanopowder spinel ferrite prepared by combustion reactionCosta, A.C.F.M. / Leite, A.M.D. / Ferreira, H.S. / Kiminami, R.H.G.A. / Cava, S. / Gama, L. et al. | 2008
- 2039
-
Analyzing indentation behavior of LaGaO3 single crystals using sharp indentersPathak, Siddhartha / Kalidindi, Surya R. / Moser, Benedikt / Klemenz, Christine / Orlovskaya, Nina et al. | 2008
- 2049
-
Piezospectroscopic measurement of the stress field around an indentation crack tip in ruby using SEM cathodoluminescenceTodd, R.I. / Stowe, D. / Galloway, S. / Barnes, D. / Wilshaw, P.R. et al. | 2008
- 2057
-
A two-step synthesis of NiZn–W hexaferritesLisjak, Darja / Žnidaršič, Andrej / Sztanislav, Anna / Drofenik, Miha et al. | 2008
- 2063
-
Effect of different templates on microstructure of textured Na0.5Bi0.5TiO3–BaTiO3 ceramics with RTGG methodGao, Feng / Hong, Rong-zi / Liu, Jia-ji / Yao, Yong-hong / Tian, Chang-sheng et al. | 2008
- 2071
-
Electrical characterizations of PZT ceramics in large frequency and temperature rangesFasquelle, D. / Carru, J.C. et al. | 2008
- 2071
-
Electrical characterization of PZT ceramics in large frequency and temperature rangesFasquelle, D. / Carru, J.C. et al. | 2008
- 2075
-
Sintering and dielectric properties of Cu2Ta4O12 ceramicsSzwagierczak, D. / Kulawik, J. et al. | 2008
- 2075
-
Sintering and dielectric properties of Cu2Ta4O12 ceramcisSzwagierczak, D. / Kulawik, J. et al. | 2008
- 2085
-
New production of TiCxN1−x-based cermets by one step mechanically induced self-sustaining reaction: Powder synthesis and pressureless sinteringCórdoba, J.M. / Alcalá, M.D. / Avilés, M.A. / Sayagués, M.J. / Gotor, F.J. et al. | 2008
- 2099
-
Surface strengthening of Ti3SiC2 through magnetron sputtering Cu and subsequent annealingGuo, Haiping / Zhang, Jie / Li, Fangzhi / Liu, Yi / Yin, Jinjie / Zhou, Yanchun et al. | 2008
- CO2
-
Editorial Board| 2008