Effect of additives on friction, wear, and iron fluoride formation under perfluoropolyether fluid lubrication in vacuum and various atmospheres containing oxygen (Unbekannt)
- Neue Suche nach: Nakayama, K.
- Neue Suche nach: Nakayama, K.
- Neue Suche nach: Dekura, T.
- Neue Suche nach: Kobayashi, T.
In:
Wear
;
192
, 1-2
; 178-185
;
1996
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:Effect of additives on friction, wear, and iron fluoride formation under perfluoropolyether fluid lubrication in vacuum and various atmospheres containing oxygen
-
Beteiligte:
-
Erschienen in:Wear ; 192, 1-2 ; 178-185
-
Verlag:
- Neue Suche nach: Elsevier
-
Erscheinungsort:Amsterdam [u.a.]
-
Erscheinungsdatum:1996
-
ISSN:
-
ZDBID:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Unbekannt
- Neue Suche nach: 535/5325
- Neue Suche nach: 52.12 / 52.12
- Weitere Informationen zu Basisklassifikation
-
Schlagwörter:
-
Klassifikation:
-
Datenquelle:
Inhaltsverzeichnis – Band 192, Ausgabe 1-2
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 1
-
Metallographic study on rolling contact fatigue of 0.44%C-1.71%Mn induction-hardened bearing steelsChoi, B.-Y. et al. | 1996
- 6
-
Study on tribological properties of the complex of rare earth dialkyldithiocarbamate and phenanthroline in lubricating greaseZhang, Z. et al. | 1996
- 11
-
Effect of slip amplitude on the fretting wear of silicon nitride against silicon nitrideVizintin, J. et al. | 1996
- 21
-
Hydrodynamic lubrication of journal bearings including micropolar lubricants and three-dimensional irregularitiesLin, T.-R. et al. | 1996
- 29
-
Correction of the roller generators in spherical roller bearingsKrzeminski-Freda, H. et al. | 1996
- 40
-
Calculation of the fractal dimensions of machined surface profilesHasegawa, M. et al. | 1996
- 46
-
Control of adhesion strength in metal-elastomer joints during elastomer crosslinkingLin, D.G. et al. | 1996
- 49
-
An evaluation of metallic coatings for erosive wear resistance in die casting applicationsShivpuri, R. et al. | 1996
- 56
-
Effect of interface layers formed during dry sliding of zirconia toughened alumina (ZTA) and monolithic alumina against steelRavikiran, A. et al. | 1996
- 66
-
An additive's influence on the pitting and wear of ball bearing steelTorrance, A.A. et al. | 1996
- 74
-
Antiwear and extreme pressure characteristics of 2-mercaptobenzothiazole derivative as the potential lubricating oil additiveWan, Y. et al. | 1996
- 78
-
Wear behaviours of laser-clad stellite alloy 6So, H. / Chen, C. T. / Chen, Y. A. et al. | 1996
- 78
-
Wear behaviours of laser-clad satellite alloy 6So, H. et al. | 1996
- 85
-
Magnetic fluid grinding of HIP-Si3N4 rollersUmehara, N. et al. | 1996
- 94
-
Rolling contact fatigue of three pearlitic rail steelsBeynon, J.H. et al. | 1996
- 112
-
Friction and wear properties of E-glass fiber reinforced epoxy composites under different sliding contact conditionsEl-Tayeb, N.S. et al. | 1996
- 118
-
Thermal effects on film thickness and traction in rolling-sliding EHL line contacts -- An accurate inlet zone analysisPandey, R.K. et al. | 1996
- 128
-
Si-modified ZA alloy for journal bearing applicationsHarmsen, M. et al. | 1996
- 134
-
Wear characteristics of sub-zero chilled cast ironSeah, K.H.W. et al. | 1996
- 141
-
Calibration procedures for frictional measurements with a lateral force microscopeLiu, E. et al. | 1996
- 151
-
Friction behaviour of a graphite-graphite dynamic electric contact in the presence of argonCsapo, E. et al. | 1996
- 157
-
An approximate model of surface ploughing by a rotating disc and other indentersAzarkhin, A. et al. | 1996
- 165
-
A study of wear resistance of a new brush-plated alloy FNi-Fe-W-SHui, W. / Liu, J. / Chaug, Y. / Dennis, J.K. et al. | 1996
- 165
-
A study of wear resistance of a new brush-plated alloy Ni-Fe-W-SHui, W. et al. | 1996
- 170
-
Abrasive wear resistance of aluminium alloy-ceramic particulate compositesGarcia-Cordovilla, C. et al. | 1996
- 170
-
Abrasive wear resistance of aluminium alloy/ceramic particulateGarcia-Cordovilla, C. / Narciso, J. / Louis, E. et al. | 1996
- 178
-
Effect of additives on friction, wear, and iron fluoride formation under perfluoropolyether fluid lubrication in vacuum and various atmospheres containing oxygenNakayama, K. et al. | 1996
- 186
-
Wear of aluminium matrix composites reinforced with nickel-coated carbon fibresChen, H. et al. | 1996
- 199
-
Effect of progressive wear on the friction characteristics of nickel LIGA processed rotorsMathieson, D. et al. | 1996
- 208
-
Influence of water vapor and oxygen on the tribology of carbon materials with sp2 valence configurationYen, B.K. et al. | 1996
- 216
-
Development of surface topography during cold rolling of twin-roll cast aluminiumGjønnes, L. et al. | 1996
- 228
-
Transitions in the mechanism of material removal in abrasive wear of aluminaXu, H.H.K. et al. | 1996
- 233
-
New bifunctionalised additives for cold rolling emulsionsHiver, P. et al. | 1996
- 237
-
Friction and wear of TiN coatings Contribution of CETRIB-INEGI to the TWA1-1993 VAMAS round-robinMonteiro Baptista, A.P. et al. | 1996
- 241
-
Dry sliding wear of NiAlJohnson, B.J. et al. | 1996
- 249
-
Author Index of Volume 192| 1996
- 251
-
Subject Index of Volume 192| 1996
- 424
-
Semiconductor Laser's Nonlinearity Compensation for DS-CDMA Optical Transmission System by Post Nonlinearity Recovery BlockPervez, R. / Nakagawa, M. et al. | 1996