Long term integrity of overpack closure weld for HLW geological disposal Part 2 - corrosion properties under anaerobic conditions (Englisch)
- Neue Suche nach: Kobayashi, M
- Neue Suche nach: Kobayashi, M
- Neue Suche nach: Yokoyama, Y
- Neue Suche nach: Takahashi, R
- Neue Suche nach: Asano, H
- Neue Suche nach: Taniguchi, N
- Neue Suche nach: Naito, M
In:
Corrosion engineering, science and technology
;
46
, 2
; 212-217
;
2011
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:Long term integrity of overpack closure weld for HLW geological disposal Part 2 - corrosion properties under anaerobic conditions
-
Beteiligte:
-
Erschienen in:Corrosion engineering, science and technology ; 46, 2 ; 212-217
-
Verlag:
- Neue Suche nach: Maney Publishing
-
Erscheinungsort:London
-
Erscheinungsdatum:2011
-
ISSN:
-
ZDBID:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Englisch
- Neue Suche nach: 51.24 / 51.24
- Weitere Informationen zu Basisklassifikation
-
Klassifikation:
-
Datenquelle:
Inhaltsverzeichnis – Band 46, Ausgabe 2
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 81
-
Guest Editorial: Long term prediction of corrosion damage in nuclear waste systemsKursten, B. / Druyts, F. / Feron, D. et al. | 2011
- 81
-
Long term prediction of corrosion damage in nuclear waste systems| 2011
- 82
-
Review of the corrosion performance of selected canister materials for disposal of UK HLW and/or spent fuelKing, F et al. | 2011
- 91
-
Review of corrosion studies of metallic barrier in geological disposal conditions with respect to Belgian Supercontainer conceptKursten, B et al. | 2011
- 98
-
Some important issues in electrochemistry of carbon steel in simulated concrete pore water Part 1 - theoretical issuesMacdonald, D D et al. | 2011
- 104
-
Some important issues in electrochemistry of carbon steel in simulated concrete pore water Part 2 - ExperimentalSaleh, A et al. | 2011
- 111
-
Further studies on the effect of irradiation on the corrosion of carbon steel in alkaline mediaWinsley, R J et al. | 2011
- 117
-
Propagation behaviour of general and localised corrosion of carbon steel in simulated groundwater under aerobic conditionsTaniguchi, N et al. | 2011
- 124
-
Effect of chloride deposition on stress corrosion cracking of 316L stainless steel used for intermediate level radioactive waste containersAlbores-Silva, O E et al. | 2011
- 129
-
Crevice corrosion testing methods for measuring repassivation potential of alloy 22Giordano, C M et al. | 2011
- 134
-
Evidence for internal diffusion of sulphide from groundwater into grain boundaries ahead of crack tip in Cu OFP copperArilahti, E et al. | 2011
- 138
-
Rate controlling reactions for copper corrosion in anaerobic aqueous sulphide solutionsChen, J et al. | 2011
- 142
-
Further studies of in situ corrosion testing of miniature copper-cast iron nuclear waste canistersSmart, N et al. | 2011
- 148
-
Corrosion rate of pure copper in an oxic bentonite/saline groundwater environmentRosborg, B et al. | 2011
- 153
-
Scientific basis for corrosion of copper in water and implications for canister lifetimesKing, F et al. | 2011
- 159
-
Long term integrity against corrosion of titanium used for TRU waste containerNakayama, G et al. | 2011
- 165
-
Long term integrity of overpack closure weld for HLW geological disposal Part 1 - prediction and evaluation method for structural integrity of weld jointAsano, H et al. | 2011
- 171
-
Corrosion issues related to disposal of 316 SS-zirconium metal waste form under simulated repository conditionsNingshen, S et al. | 2011
- 177
-
Passive corrosion of steel in concrete in context of nuclear waste disposalL'Hostis, V et al. | 2011
- 182
-
Effect of temperature on corrosion parameters and apparent activation energy measured by embedded sensors in pilot container in El Cabril repositoryAndrade, C et al. | 2011
- 190
-
Electrochemical treatment to condition contaminated EAFD as addition to immobilisation mortar in low level waste concrete containersCastellote, M et al. | 2011
- 195
-
Effect of dissolved oxygen on corrosion properties of reinforcing steelJung, H et al. | 2011
- 199
-
Fluctuation of redox conditions in radioactive waste disposal cell: characterisation of corrosion layers formed on archaeological analoguesSaheb, M et al. | 2011
- 205
-
Pitting corrosion of stainless steel: measuring and modelling pit propagation in support of damage prediction for radioactive waste containersGhahari, S M et al. | 2011
- 212
-
Long term integrity of overpack closure weld for HLW geological disposal Part 2 - corrosion properties under anaerobic conditionsKobayashi, M et al. | 2011
- 217
-
Modelling long term corrosion behaviour of copper canisters in KBS-3 repositoryKing, F et al. | 2011
- 223
-
Cellular automata approach for morphological evolution of localised corrosionDi Caprio, D et al. | 2011