Hot deformation behavior of GH4169 superalloy associated with stick δ phase dissolution during isothermal compression process (Englisch)
- Neue Suche nach: Ning, Yongquan
- Neue Suche nach: Ning, Yongquan
- Neue Suche nach: Fu, M.W.
- Neue Suche nach: Chen, Xi
In:
Materials science and engineering / A
;
540
; 164-174
;
2012
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:Hot deformation behavior of GH4169 superalloy associated with stick δ phase dissolution during isothermal compression process
-
Beteiligte:
-
Erschienen in:Materials science and engineering / A ; 540 ; 164-174
-
Verlag:
- Neue Suche nach: Elsevier
-
Erscheinungsort:Amsterdam [u.a.]
-
Erscheinungsdatum:2012
-
ISSN:
-
ZDBID:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Englisch
- Neue Suche nach: 51.00
- Weitere Informationen zu Basisklassifikation
- Neue Suche nach: 535/5100
-
Schlagwörter:
-
Klassifikation:
-
Datenquelle:
Inhaltsverzeichnis – Band 540
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 1
-
Grain boundaries in ultrafine grained materials processed by severe plastic deformation and related phenomenaSauvage, X. / Wilde, G. / Divinski, S.V. / Horita, Z. / Valiev, R.Z. et al. | 2012
- 13
-
Effect of SiC particles on the microstructure evolution and mechanical properties of aluminum during ARB processAlizadeh, M. / Paydar, M.H. / Terada, D. / Tsuji, N. et al. | 2011
- 24
-
Influence of hot plastic deformation and cooling rate on martensite and bainite start temperatures in 22MnB5 steelNikravesh, M. / Naderi, M. / Akbari, G.H. et al. | 2012
- 30
-
Ratcheting phenomenon and post-ratcheting tensile behaviour of an aluminum alloyDutta, Krishna / Ray, K.K. et al. | 2012
- 38
-
Microstructure and high mechanical properties of Mg–9RY–4Zn (RY: Y-rich misch metal) alloy with long period stacking ordered phaseLeng, Zhe / Zhang, Jinghuai / Zhang, Milin / Liu, Xuhe / Zhan, Haibo / Wu, Ruizhi et al. | 2012
- 46
-
Recrystallization of 30Cr2Ni4MoV ultra-super-critical rotor steel during hot deformation. Part Ш: Metadynamic recrystallizationChen, Fei / Cui, Zhenshan / Sui, Dashan / Fu, Bo et al. | 2012
- 46
-
Recrystallization of 30Cr2Ni4MoV ultra-super-critical rotor steel during hot deformation. Part III: Metadynamic recrystallizationChen, Fei / Cui, Zhenshan / Sui, Dashan / Fu, Bo et al. | 2012
- 55
-
Effect of grain size in compression deformation on the microstructural evolution of an austenitic stainless steelRehrl, Christian / Kleber, Siegfried / Renk, Oliver / Pippan, Reinhard et al. | 2012
- 63
-
Determination of the growth restriction factor and grain size for aluminum alloys by a quasi-binary equivalent methodMitrašinović, A.M. / Robles Hernández, F.C. et al. | 2012
- 70
-
Load bearing capacity of API X65 pipe with dent defect under internal pressure and in-plane bendingBaek, Jong-hyun / Kim, Young-pyo / Kim, Woo-sik / Koo, Jae-min / Seok, Chang-sung et al. | 2012
- 83
-
Multiaxial creep of low density open-cell foamsFan, Z.G. / Chen, C.Q. / Lu, T.J. et al. | 2012
- 89
-
A comprehensive study on the damage tolerance of ultrafine-grained copperHohenwarter, A. / Pippan, R. et al. | 2012
- 97
-
The effects of changes in test temperature and loading conditions on fracture toughness of a β toughened Zr-based bulk metallic glass compositeHassan, Hala A. / El-Shabasy, Adel B. / Lewandowski, John J. et al. | 2012
- 97
-
The effects of changes in test temperature and loading conditions on fracture toughness of a b toughened Zr-based bulk metallic glass compositeHassan, H. A. / El-Shabasy, A. B. / Lewandowski, J. J. et al. | 2012
- 102
-
Microstructure and mechanical properties of h-BN–SiC ceramic composites prepared by in situ combustion synthesisZheng, Y.T. / Li, H.B. / Zhou, T. et al. | 2012
- 107
-
Processing and properties of silicon carbide and its composites containing MoSi2 and ZrB2Kumar, R. Suresh / Sivakumar, D. / Gandhi, Ashutosh S. et al. | 2012
- 115
-
Enhanced microstructure homogeneity and mechanical properties of AZ31 magnesium alloy by repetitive upsettingGuo, W. / Wang, Q.D. / Ye, B. / Liu, M.P. / Peng, T. / Liu, X.T. / Zhou, H. et al. | 2012
- 123
-
Development of SiCp/AZ91 magnesium matrix nanocomposites using ultrasonic vibrationNie, K.B. / Wang, X.J. / Wu, K. / Hu, X.S. / Zheng, M.Y. et al. | 2012
- 130
-
Mechanical properties and microscopic deformation mechanism of polycrystalline magnesium under high-strain-rate compressive loadingsLi, Qizhen et al. | 2012
- 135
-
Study on the mechanical heterogeneity of electron beam welded thick TC4-DT jointsLu, Wei / Li, Xiaoyan / Lei, Yongping / Shi, Yaowu et al. | 2012
- 142
-
Influence of minor addition of boron on tensile and fatigue properties of wrought Ti–6Al–4V alloySingh, Gaurav / Sen, Indrani / Gopinath, K. / Ramamurty, U. et al. | 2012
- 152
-
Microstructure and texture evolution during β extrusion of boron modified Ti–6Al–4V alloyRoy, Shibayan / Suwas, Satyam / Tamirisakandala, S. / Srinivasan, R. / Miracle, D.B. et al. | 2012
- 152
-
Microstructure and texture evolution during b extrusion of boron modified Ti-6Al-4V alloyRoy, S. / Suwas, S. / Tamirisakandala, S. / Srinivasan, R. / Miracle, D. B. et al. | 2012
- 164
-
Hot deformation behavior of GH4169 superalloy associated with stick δ phase dissolution during isothermal compression processNing, Yongquan / Fu, M.W. / Chen, Xi et al. | 2012
- 164
-
Hot deformation behavior of GH4169 superalloy associated with stick d phase dissolution during isothermal compression processNing, Y. / Fu, M. W. / Chen, X. et al. | 2012
- 174
-
Mechanical characterization and constitutive modeling of Mg alloy sheetsMekonen, M. Nebebe / Steglich, D. / Bohlen, J. / Letzig, D. / Mosler, J. et al. | 2012
- 187
-
Uniaxial, load-controlled cyclic deformation of recrystallized molybdenum sheetYu, X.J. / Kumar, K.S. et al. | 2012
- 198
-
Effects of lattice parameter changes on critical resolved shear stress and mechanical properties of magnesium binary single crystalsKim, Hyung Lae / Park, Jae Sin / Chang, Young Won et al. | 2012
- 207
-
Synthesis and properties of tungsten balls/Zr-base metallic glass compositeZhang, Bo / Fu, Huameng / Zhu, Zhengwang / Wang, Aimin / Li, Hong / Dong, Chuang / Hu, Zhuangqi / Zhang, Haifeng et al. | 2012
- 212
-
Modeling the deformation textures and microstructural evolutions of a Fe–Mn–C TWIP steel during tensile and shear testingBarbier, D. / Favier, V. / Bolle, B. et al. | 2012
- 226
-
Residual stress and deformation mechanism of friction stir welded aluminum alloys by nanoindentationCharitidis, C.A. / Dragatogiannis, D.A. / Koumoulos, E.P. / Kartsonakis, I.A. et al. | 2012
- 235
-
Effects of sintering processes on mechanical properties and microstructure of TiB2–TiC+8wt% nano-Ni composite ceramic cutting tool materialZou, Bin / Huang, Chuanzhen / Song, Jinpeng / Liu, Ziye / Liu, Lin / Zhao, Yan et al. | 2012
- 245
-
Microstructural features of TA15 titanium alloy under different temperature routes in isothermal local loading formingGao, P.F. / Yang, H. / Fan, X.G. / Yan, S.L. et al. | 2012
- 253
-
Author Index| 2012
- 255
-
Subject Index| 2012
- CO2
-
Editorial Board| 2012