Optical characterization and differential scanning calorimetry studies of carboxymethyl cellulose–nickel chloride composite system (Englisch)
- Neue Suche nach: Abdel‐Rahim, Farid M.
- Neue Suche nach: Abdel‐Rahim, Farid M.
- Neue Suche nach: Mahmoud, K. H.
- Neue Suche nach: Aly, K. A.
In:
Journal of applied polymer science
;
127
, 6
; 4334-4339
;
2013
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:Optical characterization and differential scanning calorimetry studies of carboxymethyl cellulose–nickel chloride composite system
-
Beteiligte:
-
Erschienen in:Journal of applied polymer science ; 127, 6 ; 4334-4339
-
Verlag:
- Neue Suche nach: Wiley InterScience
-
Erscheinungsort:Hoboken, NJ [u.a.]
-
Erscheinungsdatum:2013
-
ISSN:
-
ZDBID:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Englisch
- Neue Suche nach: 51.70 / 51.70 / 35.80 / 35.80
- Weitere Informationen zu Basisklassifikation
- Neue Suche nach: 770/3675/5750
-
Schlagwörter:
-
Klassifikation:
BKL: 51.70 / 51.70 Polymerwerkstoffe, Kunststoffe / 35.80 Makromolekulare Chemie / 35.80 Lokalklassifikation TIB: 770/3675/5750 -
Datenquelle:
Inhaltsverzeichnis – Band 127, Ausgabe 6
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 4195
-
Utilization of waste polystyrene and starch for superabsorbent composite preparationIsmail, Hanafi / Irani, Maryam / Ahmad, Zulkifli et al. | 2013
- 4203
-
The use of poly(amidoamine) dendrimer in modification of jute for improving dyeing properties of reactive dyesZolriasatein, Ali Akbar / Yazdanshenas, Mohammad Esmail / Khajavi, Ramin / Rashidi, Abosaeed / Najafi, Farhood et al. | 2013
- 4211
-
Effect of processing techniques on the performance of Epoxy/MWCNT nanocompositesHosur, Mahesh / Barua, Rajib / Zainuddin, Shaik / Kumar, Ashok / Trovillion, Jonathan / Jeelani, Shaik et al. | 2013
- 4225
-
Effect of fiber structure on the properties of the electrospun hybrid membranes composed of poly(ε‐caprolactone) and gelatinChen, Zhengjian / Cao, Lihua / Wang, Liqun / Zhu, Huiyong / Jiang, Hongliang et al. | 2013
- 4233
-
Influence of nanoclays on electrical and morphological properties of thermoplastic polyurethane/multiwalled carbon nanotube/clay nanocompositesLee, Minho / Kim, Wantae / Ku, Jahun / Kim, Young Doo / Min, Byong Hun / Kim, Jeong Ho et al. | 2013
- 4241
-
A comparative study on curing characteristics and thermomechanical properties of elastomeric nanocomposites: The effects of eggshell and calcium carbonate nanofillersSaeb, Mohammad Reza / Ramezani‐Dakhel, Hadi / Khonakdar, Hossein Ali / Heinrich, Gert / Wagenknecht, Udo et al. | 2013
- 4251
-
Immobilization of Candida lipolytica lipase on macroporous beaded terpolymers with epoxy groupsLiu, Wentao / Duan, Hongdong / Meng, Xia / Qin, Dawei / Wang, Xingjian / Zhang, Juan et al. | 2013
- 4256
-
Self‐assembly of bovine serum albumin and poly(acrylic acid) induced by noncovalent bondsDu, Weiping / Wang, Yansong et al. | 2013
- 4262
-
Influence of laminate thickness reduction on the deformation mechanism of coextrudecl multilayered PC/PMMA filmsScholtyssek, Stefanie / Seydewitz, Volker / Adhikari, Rameshwar / Pfeifer, Frank / Michler, Goerg Hannes / Siesler, Heinz Wilhelm et al. | 2013
- 4262
-
Influence of laminate thickness reduction on the deformation mechanism of coextruded multilayered PC/PMMA filmsScholtyssek, Stefanie / Seydewitz, Volker / Adhikari, Rameshwar / Pfeifer, Frank / Michler, Goerg Hannes / Siesler, Heinz Wilhelm et al. | 2013
- 4273
-
Electrical and microwave absorbing properties of polypyrrole synthesized by optimum strategyHao, Bin / Li, Liangchao / Wang, Yuping / Qian, Haisheng / Tong, Guoxiu / Chen, Haifeng / Chen, Keyu et al. | 2013
- 4280
-
Effect of intermolecular and intramolecular forces on hydrodynamic diameters of poly(N‐isopropylacrylamide) copolymers in aqueous solutionsYang, Lei / Liu, Tianqing / Song, Kedong / Wu, Shuang / Fan, Xin et al. | 2013
- 4288
-
Electrospun magnetic carbon composite fibers: Synthesis and electromagnetic wave absorption characteristicsYang, Ying / Guo, Zhen / Zhang, Huan / Huang, Daqing / Gu, Jialin / Huang, Zhenghong / Kang, Feiyu / Alan Hatton, T. / Rutledge, Gregory C. et al. | 2013
- 4296
-
Laser scanning confocal microscopy versus scanning electron microscopy for characterization of polymer morphology: Sample preparation drastically distorts morphologies of poly(2‐hydroxyethyl methacrylate)‐based hydrogelsPaterson, Stefan M. / Casadio, Ylenia S. / Brown, David H. / Shaw, Jeremy A. / Chirila, Traian V. / Baker, Murray V. et al. | 2013
- 4305
-
Synthesis of alkyne‐terminated xanthate RAFT agents and their uses for the controlled radical polymerization of N‐vinylpyrrolidone and the synthesis of its block copolymer using click chemistryPatel, Vijay Kumar / Vishwakarma, Niraj Kumar / Mishra, Avnish Kumar / Biswas, Chandra Sekhar / Maiti, Pralay / Ray, Biswajit et al. | 2013
- 4318
-
Study of viscoelastic properties of nanocomposites of SiO2–acrylonitrile–butadiene–styreneHaghtalab, Ali / Rahimi, Sedighe et al. | 2013
- 4328
-
Development of high Tg epoxy resin and mechanical properties of its fiber‐reinforced compositesYi, Jin‐Woo / Um, Moon‐Kwang / Byun, Joon‐Hyung / Lee, Sang‐Bok / Lee, Sang‐Kwan et al. | 2013
- 4334
-
Optical characterization and differential scanning calorimetry studies of carboxymethyl cellulose–nickel chloride composite systemAbdel‐Rahim, Farid M. / Mahmoud, K. H. / Aly, K. A. et al. | 2013
- 4340
-
Sorption of remazol brilliant blue R onto polyurethane‐type foam prepared from peanut shellBilir, M. Hilal / Şakalar, Neslihan / Acemioğlu, Bilal / Baran, Evrim / Alma, M. Hakki et al. | 2013
- 4352
-
Development of a DOPO‐containing melamine epoxy hardeners and its thermal and flame‐retardant properties of cured productsXiong, Yuanqin / Jiang, Zhuojuan / Xie, Yanyan / Zhang, Xuyong / Xu, Weijian et al. | 2013
- 4359
-
Fabrication and characterization of HCl‐treated clinoptilolite filled ethylene vinyl acetate composite filmsMishra, Ajay K. / Mishra, Shivani B. / Mamba, Bhekie B. / Dlamini, Derrick S. / Mthombo, Thabo S. et al. | 2013
- 4366
-
High‐contrast, high‐sensitivity aqueous base‐developable polynorbornene dielectricRaeis‐Zadeh, Mehrsa / Kohl, Paul A. et al. | 2013
- 4374
-
Investigation of temperature sensitivity behaviors of water soluble polyacrylamidesUğuzdoğan, Erdal / Denkbaş, Emir Baki / Kabasakal, Osman Sermet et al. | 2013
- 4385
-
Synthesis and characterization of copolymeric aliphatic–aromatic esters derived from terephthalic acid, 1,4‐butanediol, and ε‐caprolactone by physical, thermal, and mechanical properties and NMR measurementsWang, Ching‐Huang / Tsai, Ping‐Hsun / Kan, Lou‐Sing / Chen, C. Will et al. | 2013
- 4395
-
Thermally induced crystallization and enzymatic degradation studies of poly (L‐lactic acid) filmsVasanthan, Nadarajah / Gezer, Hande et al. | 2013
- 4402
-
The effect of freeze‐drying parameters on the cure characteristics of freeze‐dried BSA‐loaded silicone elastomerMcConville, Christopher / Woolfson, Andrew David / Malcolm, Robert Karl et al. | 2013
- 4409
-
Evaluation of a functionalized copolymer as adsorbent on direct dyes removal process: Kinetics and equilibrium studiesMuntean, Simona Gabriela / Paska, Oana / Coseri, Sergiu / Simu, Georgeta Maria / Grad, Maria Elena / Ilia, Gheorghe et al. | 2013
- 4422
-
Kinetics of thermodegradation of palm kernel oil derived medium‐chain‐length polyhydroxyalkanoatesSin, Mei Chan / Tan, Irene Kit Ping / Annuar, Mohd Suffian Mohd / Gan, Seng Neon et al. | 2013
- 4426
-
Hybrid polyaniline/nanomagnetic particles composites: High performance materials for EMI shieldingKamchi, Noureddine El / Belaabed, Belkacem / Wojkiewicz, Jean‐Luc / Lamouri, Saad / Lasri, Tuami et al. | 2013
- 4433
-
Optimization and characteristics of preparing chitosan microspheres using response surface methodologyZhou, Xuan / Cheng, Xiao Jie / Liu, Wei Fang / Li, Jing / Ren, Li Hong / Dang, Qi Feng / Feng, Chao / Chen, Xi Guang et al. | 2013
- 4440
-
Composition dependence of dielectric properties, elastic modulus, and electroactivity in (carbon black‐BaTiO3)/silicone rubber nanocompositesZhao, Hang / Xia, Yu‐Juan / Dang, Zhi‐Min / Zha, Jun‐Wei / Hu, Guo‐Hua et al. | 2013
- 4446
-
Enhancing water resistance of paper by graft copolymerization reactionSayyah, S. M. / Khaliel, A. B. / Mohamed, E. H. et al. | 2013
- 4456
-
The effect of soft bake on adhesion property between SU‐8 photoresist and Ni substrate by molecular dynamics simulationZhang, Xiaolei / Du, Liqun / Xu, Zheng et al. | 2013
- 4463
-
Study of the effect of rutile/anatase TiO2 nanoparticles synthesized by hydrothermal route in electrospun PVA/TiO2 nanocompositesCosta, Rodrigo G. F. / Ribeiro, Caue / Mattoso, Luiz H. C. et al. | 2013
- 4470
-
Phase behaviors of diblock copolymer/nanorod composites under oscillatory shear flowHe, Linli / Li, Shiben / Zhang, Linxi et al. | 2013
- 4483
-
Generalizing solubility parameter theory to apply to one‐ and two‐dimensional solutes and to incorporate dipolar interactionsHughes, J. Marguerite / Aherne, Damian / Coleman, Jonathan N. et al. | 2013
- 4492
-
Structure–property correlation of polyurethane nanocomposites: Influence of loading and nature of nanosilica and microstructure of hyperbranched polyolMaji, Pradip K. / Bhowmick, Anil K. et al. | 2013
- 4505
-
Upgrading the adhesion properties of a fast‐curing epoxy using hydrophilic/hydrophobic hyperbranched poly(amidoamine)sEssawy, Hisham A. / Mohamed, Heba A. / Elsayed, Nadia H. et al. | 2013
- 4515
-
Preparation of melting‐free poly(lactic acid) by amorphous and crystal crosslinking under UV irradiationKoo, Gwang‐Hoe / Jang, Jinho et al. | 2013
- 4524
-
Synthesis of sulfonated polynaphthalene, polyanthracene, and polypyrene as strong solid acids via oxidative coupling polymerizationTanemura, Kiyoshi / Suzuki, Tsuneo / Horaguchi, Takaaki et al. | 2013
- 4537
-
Determination of crosslinking density of hydrogels prepared from microcrystalline celluloseXia, Zhiyong / Patchan, Marcia / Maranchi, Jeffrey / Elisseeff, Jennifer / Trexler, Morgana et al. | 2013
- 4542
-
Wet spinning of cellulose from ionic liquid solutions–viscometry and mechanical performanceOlsson, Carina / Westman, Gunnar et al. | 2013
- 4549
-
Synthesis and characterization of poly(HPMA)‐APMA‐DTPA‐99mTc for imaging‐guided drug delivery in hepatocellular carcinomaYuan, Jianchao / Miao, Chengping / Peng, Fangyu / Zeng, Xianwu / Guo, Hongyun / Wang, Xiaoqi / Liao, Shiqi / Xie, Xiaoli et al. | 2013
- 4557
-
Effect of noncovalent chemical modification on the electrical conductivity and tensile properties of poly(methyl methacrylate)/carbon nanotube compositesKoysuren, Ozcan / Karaman, Mustafa / Ozyurt, Demet et al. | 2013
- 4564
-
Modified poly(vinylidene fluoride) hollow fiber composite membranes reinforced by hydroxyapatite nanocrystal whiskersLang, Wan‐Zhong / Ji, Qin / Shen, Jian‐Ping / Guo, Ya‐Jun / Chu, Lian‐Feng et al. | 2013
- 4573
-
Preparation and characterization of porous chitosan–tripolyphosphate beads for copper(II) ion adsorptionWu, Shao‐Jung / Liou, Tzong‐Horng / Yeh, Chao‐Hsien / Mi, Fwu‐Long / Lin, Tsung‐Kuan et al. | 2013
- 4581
-
Effect of chemical structure and preparation process on the aggregation structure and properties of polyimide filmWang, Ying / Yang, Yang / Jia, Zhenxing / Qin, Jiaqiang / Gu, Yi et al. | 2013
- 4588
-
Preparation and characterization of novel polyamide paraffin MEPCM by interfacial polymerization techniqueWei, Ju / Li, Zhenzhong / Liu, Ling / Liu, Xiang et al. | 2013
- 4594
-
Polymerization of 1,3‐butadiene with VO(P204)2 activated by methylaluminoxane, purified methylaluminoxane, and trimethylaluminumWang, Haiying / Cao, Lihui / Zhang, Xuequan et al. | 2013
- 4601
-
Effect of copolymerization on crystallization kinetics of semicrystalline polyimidesWang, Wei / Wang, Daming / Jia, He / Liu, Changwei / Zhao, Xiaogang / Chen, Chunhai et al. | 2013
- 4610
-
Studies on the preparation of Parinari polyandra benth seed oil alkyd resinsOdetoye, T. E. / Ogunniyi, D. S. / Olatunji, G. A. et al. | 2013
- 4617
-
Cold‐crystallization behavior of poly(L‐lactide)/ACR blend films investigated by in situ FTIR spectroscopyWu, Ningjing / Wang, Honghao / Ding, Meichun / Man, Liu / Zhang, Jianming et al. | 2013
- 4624
-
Elastomeric skin selection for a fluid‐filled artificial fingertipRoy, Dipayon / Wettels, Nicholas / Loeb, Gerald E. et al. | 2013
- 4634
-
Differential microemulsion polymerization as a new root for entrapment of drugsMoustafa, A. B. / Sobh, R. A. / Rabie, A. M. / Nasr, H. E. / Ayoub, M. M. H. et al. | 2013
- 4644
-
Mechanical modeling of a three‐phase nanocomposite polymeric materialMeng, Qingkai / Kee, Daniel De et al. | 2013
- 4653
-
Positive‐tone, aqueous‐developable, polynorbornene dielectric: Lithographic, and dissolution propertiesMueller, Brennen K. / Elce, Edmund / Grillo, Angelica M. / Kohl, Paul A. et al. | 2013
- 4662
-
Modified MCM‐41 silica spheres filled polydimethylsiloxane membrane for dimethylcarbonate/methanol separation via pervaporationWang, Lei / Han, Xiaolong / Li, Jiding / Zheng, Dongju / Qin, Lin et al. | 2013
- 4672
-
Preparation and electrochemical properties of poly‐2,5‐dihydroxyaniline/activated carbon composite electrode in organic electrolyteSun, Miao / Wang, Wei / He, Benlin / Sun, Mingliang / Liu, Wei / Ge, Honglun / Zhang, Qinjie / Sun, Fan et al. | 2013
- 4681
-
Development and characterization of plasticized starch‐based biocomposites with soy pulp as reinforcement fillerBehera, Ajaya Kumar / Avancha, Sridevi / Sen, Ramkrishna / Adhikari, Basudam et al. | 2013
- 4688
-
Synergistic effect of plasma‐modified halloysite nanotubes and carbon black in natural rubber—butadiene rubber blendPoikelispää, Minna / Das, Amit / Dierkes, Wilma / Vuorinen, Jyrki et al. | 2013
- 4697
-
Preparation and characterization of melt‐blended graphene nanosheets–poly(vinylidene fluoride) nanocomposites with enhanced propertiesEl Achaby, M. / Arrakhiz, F. Z. / Vaudreuil, S. / Essassi, E. M. / Qaiss, A. / Bousmina, M. et al. | 2013
- 4708
-
Mechanical and UV‐shielding properties of in situ synthesized poly(acrylonitrile‐butadiene‐styrene)/zinc oxide nanocompositesRodríguez‐Tobías, Heriberto / Morales, Graciela / Rodríguez‐Fernández, Oliverio / Acuña, Pablo et al. | 2013
- 4719
-
Catalytic oxidation of thioanisole using oxovanadium(IV)‐functionalized electrospun polybenzimidazole nanofibersWalmsley, Ryan S. / Hlangothi, Percy / Litwinski, Christian / Nyokong, Tebello / Torto, Nelson / Tshentu, Zenixole R. et al. | 2013
- 4726
-
Biodegradation study on poly(ε‐caprolactone) with bimodal molecular weight distributionHermanová, Soňa / Bálková, Radka / Voběrková, Stanislava / Chamradová, Ivana / Omelková, Jiřina / Richtera, Lukáš / Mravcová, Ludmila / Jančář, Josef et al. | 2013
- 4736
-
Synthesis, characterization, and antifungal activity of nystatin—gum arabic conjugatesStefanovic, Jovana / Jakovljevic, Dragica / Gojgic‐Cvijovic, Gordana / Lazic, Miodrag / Vrvic, Miroslav et al. | 2013
- 4744
-
Presentation of a novel sensor based on acoustic emission in injection moldingMüller, Florian / Rath, Gerhard / Lucyshyn, Thomas / Kukla, Christian / Burgsteiner, Martin / Holzer, Clemens et al. | 2013
- 4750
-
Preparation and characterization of dual sensitive carboxylated methyl cellulose/poly(vinyl alcohol) physical composite hydrogelXiao, Congming / Xia, Cunping / Ma, Yue / He, Xuelei et al. | 2013
- 4756
-
Surface modification of multiwalled carbon nanotubes via gliding arc plasma for the reinforcement of polypropyleneLuo, Z. / Cai, X. / Hong, R. Y. / Li, J. H. / Wei, D. G. / Luo, G. H. / Li, H. Z. et al. | 2013
- 4764
-
New method for hydrogenating NBR latexWang, Xunzhang / Zhang, Liqun / Han, Yang / Shi, Xiangke / Wang, Weimin / Yue, Dongmei et al. | 2013
- 4769
-
The effects of gas counter pressure and mold temperature variation on the surface quality and morphology of the microcellular polystyrene foamsChen, Shia‐Chung / Hsu, Ping‐Shun / Hwang, Shyh‐Shin et al. | 2013
- 4777
-
Evaluation of cure state of vinylester resinsAcha, Betiana A. / Carlsson, Leif A. et al. | 2013
- 4785
-
α‐cyclodextrin assisted self‐assembly of poly(ethylene glycol)‐block‐poly(N‐isopropylacrylamide) in aqueous mediaYuen, Fanny / Tam, Kam Chiu et al. | 2013
- 4795
-
Deinked and acetylated fiber of newspapersNedjma, Samira / Djidjelli, Hocine / Boukerrou, Amar / Benachour, Djafer / Chibani, Nacera et al. | 2013
- 4802
-
All‐wood biocomposites by partial dissolution of wood flour in 1‐butyl‐3‐methylimidazolium chlorideShibata, Mitsuhiro / Yamazoe, Kentaro / Kuribayashi, Masaya / Okuyama, Yuto et al. | 2013
- 4809
-
Relations between structure and property of polyamide 11 nanocomposites based on raw clays elaborated by water‐assisted extrusionStoclet, Gregory / Sclavons, Michel / Devaux, Jacques et al. | 2013
- 4825
-
Hemocompatibility of electrospun halloysite nanotube‐ and carbon nanotube‐doped composite poly(lactic‐co‐glycolic acid) nanofibersZhao, Yili / Wang, Shige / Guo, Qingshan / Shen, Mingwu / Shi, Xiangyang et al. | 2013
- 4833
-
Rheology and polymer flooding characteristics of partially hydrolyzed polyacrylamide for enhanced heavy oil recoveryJung, Jae Chul / Zhang, Ke / Chon, Bo Hyun / Choi, Hyoung Jin et al. | 2013
- 4840
-
RAFT synthesis of cellulose‐g‐polymethylmethacrylate copolymer in an ionic liquidLin, Chunxiang / Zhan, Huaiyu / Liu, Minghua / Habibi, Youssef / Fu, Shiyu / Lucia, Lucian A. et al. | 2013
- 4850
-
Synthesis and characterization of N‐methyl‐2,6‐dinitrodiphenylamine‐4‐diazonium salt and its diazoresinWang, Jianguo / Zou, Yingquan et al. | 2013
- 4858
-
Application of a new unimolecular initiator in the synthesis of (α,ω) ketone functionalized polystyrene in nitroxide mediated polymerizationMegiel, Elżbieta et al. | 2013
- 4865
-
Synthesis, characterization, and anticoagulant activity of carboxymethyl starch sulfatesFan, Lihong / Gong, Yugui / Cao, Mi / Gao, Song / Sun, Yi / Chen, Lingyun / Zheng, Hua / Xie, Weiguo et al. | 2013
- 4873
-
Effect of polyarylene ether nitriles on processing and mechanical behaviors of phthalonitrile‐epoxy copolymers and glass fiber laminated compositesZhao, Xin / Guo, Heng / Lei, Yajie / Zhao, Rui / Zhong, Jiachun / Liu, Xiaobo et al. | 2013
- 4879
-
Reactive blend of epoxy‐novolac resin and epoxide‐terminated low‐molecular‐weight poly(phenylene oxide)Mo, Jingzhao / Xia, Lei / Pan, Pengju / Shentu, Baoqing / Weng, Zhixue et al. | 2013
- 4889
-
Preparation and sorption properties of tunable polyester copolymers containing β‐cyclodextrinPoon, Louis / Wilson, Lee D. / Headley, John V. et al. | 2013
- 4899
-
In‐line near‐infrared spectroscopy: A tool to monitor the preparation of polymer‐clay nanocomposites in extrudersBarbas, Joana M. / Machado, Ana V. / Covas, José A. et al. | 2013
- 4910
-
Modulating the physical properties of sunflower oil and sorbitan monopalmitate‐based organogelsBehera, Beauty / Sagiri, Sai S. / Pal, Kunal / Srivastava, Anand et al. | 2013
- 4918
-
Synthesis of amino acid‐based polymers having metronidazole moiety and study of their controlled release in vitroEl‐Newehy, Mohamed H. / Elsherbiny, Abeer S. / Mori, Hideharu et al. | 2013
- 4927
-
Syntheses, characterization, and antibacterial activity of chitosan grafted hydrogels and associated mica‐containing nanocomposite hydrogelsNoppakundilograt, Supaporn / Sonjaipanich, Kittichai / Thongchul, Nuttha / Kiatkamjornwong, Suda et al. | 2013
- 4939
-
Polymer nanocomposite‐based shielding against diagnostic X‐raysNambiar, Shruti / Osei, Ernest K. / Yeow, John T. W. et al. | 2013
- 4947
-
Plasticized and nanofilled poly(lactic acid)‐based cast films: Effect of plasticizer and organoclay on processability and final propertiesScatto, Marco / Salmini, Elena / Castiello, Stefania / Coltelli, Maria‐Beatrice / Conzatti, Lucia / Stagnaro, Paola / Andreotti, Leonardo / Bronco, Simona et al. | 2013
- 4957
-
Synthesis of urethane acrylate based electromagnetic interference shielding materialsYanılmaz, Meltem / Erbay, Betül Türel / Serhatli, Ersin / Sarac, Abdulkadir Sezai et al. | 2013
- 4967
-
The effect of different organic modified montmorillonites (OMMTs) on the thermal properties and flammability of PLA/MCAPP/lignin systemsZhang, Rui / Xiao, Xifu / Tai, Qilong / Huang, Hua / Yang, Jian / Hu, Yuan et al. | 2013
- 4974
-
A polyurethane‐based nanocomposite biocompatible bone adhesiveSchreader, Kevin J. / Bayer, Ilker S. / Milner, Derek J. / Loth, Eric / Jasiuk, Iwona et al. | 2013
- 4983
-
Fundamental studies on a new series of SPSEBS‐PVA‐QPSEBS bipolar membrane: Membrane preparation and characterizationVenugopal, Krishnaveni / Dharmalingam, Sangeetha et al. | 2013
- 4991
-
A novel approach to prepare etoposide‐loaded poly(N‐vinyl caprolactam‐co‐methylmethacrylate) copolymeric nanoparticles and their controlled release studiesShah, Sunil / Pal, Angshuman / Gude, Rajiv / Devi, Surekha et al. | 2013
- 5000
-
Probe dependency of flory–huggins interaction parameters between solvents: Cases of hydrocarbons and isosteric derivativesHuang, Jan‐Chan et al. | 2013
- 5007
-
Compatible blends of polypropylene with an amorphous polyamideAranburu, N. / Eguiazabal, J. I. et al. | 2013
- 5014
-
Development of a chitosan‐based adhesive. Application to wood bondingPatel, Anil K. / Michaud, Philippe / Petit, Emmanuel / de Baynast, Hélène / Grédiac, Michel / Mathias, Jean‐Denis et al. | 2013
- 5022
-
Effect of anionic/siloxy groups on the release of ofloxacin from soft contact lensesYamazaki, Y. / Matsunaga, T. / Syohji, K. / Arakawa, T. / Sato, T. et al. | 2013
- 5028
-
Poly(ethylene oxide)‐multiwall carbon nanotube composites: Effect of dicarboxylic acid salt‐based modifiersJagtap, S. B. / Kushwaha, R. K. / Ratna, D. et al. | 2013
- 5037
-
Ketimine substituted polyphenol: Synthesis, characterization and investigation of its thermal and electrochemical propertiesDemir, Hacı Ökkeş et al. | 2013
- 5045
-
Simultaneous polymerization and quaternization of 4‐vinyl pyridineMondal, P. / Saha, S. K. / Chowdhury, P. et al. | 2013
- 5051
-
Preparation and characterization of a bioadhesive with poly (vinyl alcohol) crosslinking agentXue, Jie / Wang, Tao / Nie, Jun / Yang, Dongzhi et al. | 2013
- 5059
-
Thermal storage nanocapsules by miniemulsion polymerizationde Cortazar, Maider García / Rodríguez, Raquel et al. | 2013
- 5065
-
Sulfur‐containing copolyimides for the membrane‐based separation of aromatic/aliphatic mixturesSuding, M. T. H. / Staudt, C. et al. | 2013
- 5075
-
Preparation and properties of rigid polyimide foams derived from dianhydride and isocyanateYu, Fei / Wang, Kai / Liu, Xiao‐Yan / Zhan, Mao‐Sheng et al. | 2013
- 5082
-
Structure, thermal, and mechanical properties of DDM‐hardened epoxy/benzoxazine hybrids: Effects of epoxy resin functionality and ETBN tougheningGrishchuk, Sergiy / Sorochynska, Liubov / Vorster, Olof C. / Karger‐Kocsis, József et al. | 2013
- 5094
-
Reinforcement of biodegradable poly(butylene succinate) with low loadings of graphene oxideWan, Chaoying / Chen, Biqiong et al. | 2013
- 5100
-
Effect of PES on the morphology and properties of proton conducting blends with sulfonated poly(ether ether ketone)Arigonda, Mahesh / Deshpande, Abhijit P. / Varughese, Susy et al. | 2013
- i
-
Cover Image, Volume 127, Issue 6| 2013
- ii
-
Inside Cover, Volume 127, Issue 6| 2013