Effect of weld metal chemistry on stress corrosion cracking behavior of AISI 444 ferritic stainless steel weldments in boiling chloride solution (Deutsch, Englisch)
- Neue Suche nach: Antunes, P. D.
- Neue Suche nach: Antunes, P. D.
- Neue Suche nach: Correa, E. O.
- Neue Suche nach: Barbosa, R. P.
- Neue Suche nach: Silva, E. M.
- Neue Suche nach: Padilha, A. F.
- Neue Suche nach: Guimaraes, P. M.
In:
Materials and corrosion
;
64
, 5
; 415-421
;
2013
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:Effect of weld metal chemistry on stress corrosion cracking behavior of AISI 444 ferritic stainless steel weldments in boiling chloride solution
-
Beteiligte:Antunes, P. D. ( Autor:in ) / Correa, E. O. / Barbosa, R. P. / Silva, E. M. / Padilha, A. F. / Guimaraes, P. M.
-
Erschienen in:Materials and corrosion ; 64, 5 ; 415-421
-
Verlag:
- Neue Suche nach: Wiley-VCH
-
Erscheinungsort:Weinheim [u.a.]
-
Erscheinungsdatum:2013
-
ISSN:
-
ZDBID:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Deutsch, Englisch
- Neue Suche nach: 51.00 / 51.24
- Weitere Informationen zu Basisklassifikation
-
Schlagwörter:
-
Klassifikation:
-
Datenquelle:
Inhaltsverzeichnis – Band 64, Ausgabe 5
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 367
-
Materials and Corrosion 5/2013| 2013
- 372
-
Corrosion rate and corrosion product characterisation using Raman spectroscopy for steel embedded in chloride polluted fly ash mortarCriado, M. / Martínez‐Ramirez, S. / Fajardo, S. / Gómez, P. P. / Bastidas, J. M. et al. | 2013
- 381
-
Effect of exposure time on the morphology of corrosion on high chromium white cast iron in high temperature caustic solutionsMcLeod, A. J. / Clegg, R. E. et al. | 2013
- 388
-
Corrosion of steel by carbonate‐bicarbonate solution for CO2 captureZhang, J. / Martin, F. J. et al. | 2013
- 394
-
Assessing the tribocorrosion performance of Ti–6Al–4V, 316 stainless steel and Monel K500 alloys in artificial seawaterChen, J. / Yan, F. Y. / Chen, B. B. / Wang, J. Z. et al. | 2013
- 402
-
Effects of the Zr and Mo contents on the electrochemical corrosion behavior of Ti–22Nb alloyYang, S. / Zhang, D. C. / Wei, M. / Su, H. X. / Wu, W. / Lin, J. G. et al. | 2013
- 408
-
Electrochemical studies on the corrosion inhibition of AA2024 aluminium alloy by rare earth ammonium nitrates in 3.5% NaCl solutionsMatter, E. A. / Kozhukharov, S. / Machkova, M. / Kozhukharov, V. et al. | 2013
- 415
-
Effect of weld metal chemistry on stress corrosion cracking behavior of AISI 444 ferritic stainless steel weldments in boiling chloride solutionAntunes, P. D. / Correa, E. O. / Barbosa, R. P. / Silva, E. M. / Padilha, A. F. / Guimaraes, P. M. et al. | 2013
- 422
-
The corrosion inhibitory property of N,N‐bis(2‐benzimidazolylmethyl)amine for Q235 steelQian, J. H. / Zhang, Y. / Yin, X. Y. / Liu, L. et al. | 2013
- 426
-
Corrosion characterization of microarc oxidation coatings formed on Mg–7Li alloyLi, J. G. / Lv, Y. / Wang, H. W. / Zhu, Z. J. / Wei, Z. J. / Meng, X. C. et al. | 2013
- 433
-
Corrosion behavior of ZnNiAl2O3 nanocomposite coatings obtained by electrodeposition from alkaline electrolytesBlejan, D. / Muresan, L. M. et al. | 2013
- 439
-
Poly(3‐octylthiophene) thermally treated as coating for corrosion protection of SS304 in sulfuric acid mediaLeón‐Silva, U. / Nicho, M. E. / González‐Rodríguez, J. G. / Chacón‐Nava, J. G. / Salinas‐Bravo, V. M. et al. | 2013
- 446
-
Ageing resistance and corrosion resistance of silicone‐epoxy and polyurethane topcoats used in sea splash zoneWang, Z. Y. / Liu, F. C. / Han, E. H. / Ke, W. et al. | 2013
- 454
-
Corrosion News| 2013
-
Korrosionsnachrichten| 2013