Significantly changed intergranular corrosion and exfoliation corrosion behavior of the ultra‐fine grained Al–5 mass% Cu alloy fabricated by ECAP (Deutsch, Englisch)
- Neue Suche nach: Song, D.
- Neue Suche nach: Song, D.
- Neue Suche nach: Ma, A. B.
- Neue Suche nach: Jiang, J. H.
- Neue Suche nach: Lin, P. H.
- Neue Suche nach: Lu, F. M.
- Neue Suche nach: Zhang, L. Y.
In:
Materials and corrosion
;
64
, 11
; 1015-1023
;
2013
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:Significantly changed intergranular corrosion and exfoliation corrosion behavior of the ultra‐fine grained Al–5 mass% Cu alloy fabricated by ECAP
-
Beteiligte:
-
Erschienen in:Materials and corrosion ; 64, 11 ; 1015-1023
-
Verlag:
- Neue Suche nach: Wiley-VCH
-
Erscheinungsort:Weinheim [u.a.]
-
Erscheinungsdatum:2013
-
ISSN:
-
ZDBID:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Deutsch, Englisch
- Neue Suche nach: 51.00 / 51.24
- Weitere Informationen zu Basisklassifikation
-
Schlagwörter:
-
Klassifikation:
-
Datenquelle:
Inhaltsverzeichnis – Band 64, Ausgabe 11
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 953
-
Materials and Corrosion 11/2013| 2013
- 960
-
Comparison study on anticorrosion performances of the epoxy coatings with two different nano‐polyanilines for Q235 steelHou, W. P. / Liu, Y. / Ge, Z. Y. / Zhao, W. Y. et al. | 2013
- 969
-
Corrosion performance of Zn–Mg–Al coated steel in accelerated corrosion tests used in the automotive industry and field exposuresLeBozec, N. / Thierry, D. / Peltola, A. / Luxem, L. / Luckeneder, G. / Marchiaro, G. / Rohwerder, M. et al. | 2013
- 979
-
Fabrication of superhydrophobic surfaces on Mg alloy substrates via primary cell corrosion and fluoroalkylsilane modificationSong, J. L. / Xu, W. J. / Lu, Y. / Liu, X. / Sun, J. et al. | 2013
- 988
-
Corrosion of stainless steel grades in H2O/KOH 50% at 120 °C: AISI304 austenitic and 2205 duplexBozzini, B. / Bogani, F. / Giovannelli, G. / Natali, S. / Scarselli, G. / Boniardi, M. et al. | 2013
- 996
-
Photocathodic protection properties of TiO2–V2O5 composite coatingsZhou, M.‐J. / Zhang, N. / Zhang, L. / Yan, J.‐H. et al. | 2013
- 1001
-
Preparation of titanium dioxide nanotube arrays on titanium mesh by anodization in (NH4)2SO4/NH4F electrolyteZeng, Q.‐Y. / Xi, M. / Xu, W. / Li, X.‐J. et al. | 2013
- 1007
-
Effect of carbonation process on the passivating products of zinc in Ca(OH)2 saturated solutionRoventi, G. / Bellezze, T. / Barbaresi, E. / Fratesi, R. et al. | 2013
- 1015
-
Significantly changed intergranular corrosion and exfoliation corrosion behavior of the ultra‐fine grained Al–5 mass% Cu alloy fabricated by ECAPSong, D. / Ma, A. B. / Jiang, J. H. / Lin, P. H. / Lu, F. M. / Zhang, L. Y. et al. | 2013
- 1024
-
Dynamic electrochemical impedance spectroscopy and polarization studies to evaluate the inhibition effect of benzotriazole on copper‐manganese‐aluminium alloy in artificial seawaterGerengi, H. / Slepski, P. / Bereket, G. et al. | 2013
- 1032
-
A methodology to investigate the wear of blast furnace hearth carbon refractory liningSilva, S. N. / Vernilli, F. / Justus, S. M. / Longo, E. / Baldo, J. B. / Varela, J. A. / Lopes, J. M. G. et al. | 2013
- 1039
-
Corrosion News| 2013
-
Korrosionsnachrichten| 2013