First results and surface analysis strategy for plasma-facing components after JET operation with the ITER-like wall (Deutsch)
- Neue Suche nach: Likonen, J
- Neue Suche nach: Likonen, J
- Neue Suche nach: Alves, E
- Neue Suche nach: Baron-Wiechec, A
- Neue Suche nach: Brezinsek, S
- Neue Suche nach: Coad, J P
- Neue Suche nach: Hakola, A
- Neue Suche nach: Heinola, K
- Neue Suche nach: Koivuranta, S
- Neue Suche nach: Matthews, G F
- Neue Suche nach: Petersson, P
- Neue Suche nach: Rubel, M
- Neue Suche nach: Stan-Sion, C
- Neue Suche nach: Widdowson, A
In:
Physica scripta
;
2014
, 159
; 14016-14016
;
2014
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:First results and surface analysis strategy for plasma-facing components after JET operation with the ITER-like wall
-
Beteiligte:Likonen, J ( Autor:in ) / Alves, E / Baron-Wiechec, A / Brezinsek, S / Coad, J P / Hakola, A / Heinola, K / Koivuranta, S / Matthews, G F / Petersson, P
-
Erschienen in:Physica scripta ; 2014, 159 ; 14016-14016
-
Verlag:
- Neue Suche nach: IoP Publ.
-
Erscheinungsort:Bristol
-
Erscheinungsdatum:2014
-
ISSN:
-
ZDBID:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Deutsch
- Neue Suche nach: 33.00
- Weitere Informationen zu Basisklassifikation
- Neue Suche nach: 640/3400
-
Schlagwörter:
-
Klassifikation:
-
Datenquelle:
Inhaltsverzeichnis – Band 2014, Ausgabe 159
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 10301
-
14th International Conference on Plasma-Facing Materials and Components for Fusion ApplicationsLoewenhoff, Thorsten et al. | 2014
- 14001
-
Plasma facing components for the Experimental Advanced Superconducting Tokamak and CFETRLi, Jiangang et al. | 2014
- 14002
-
Status of the ITER full-tungsten divertor shaping and heat load distribution analysisCarpentier-Chouchana, S et al. | 2014
- 14003
-
Experimental determination of the transient heat absorption of W divertor materialsGreuner, H et al. | 2014
- 14004
-
Removable samples for ITER—a feasibility and conceptual studyMertens, Ph et al. | 2014
- 14005
-
Investigation of the impact of transient heat loads applied by laser irradiation on ITER-grade tungstenHuber, A et al. | 2014
- 14006
-
ITER full tungsten divertor qualification program and progressHirai, T et al. | 2014
- 14007
-
Facility for high-heat flux testing of irradiated fusion materials and components using infrared plasma arc lampsSabau, Adrian S et al. | 2014
- 14008
-
Preliminary R&D on flat-type W/Cu plasma-facing materials and components for Experimental Advanced Superconducting TokamakXu, Y et al. | 2014
- 14009
-
Power handling of the JET ITER-like wallArnoux, G et al. | 2014
- 14010
-
Material migration patterns and overview of first surface analysis of the JET ITER-like wallWiddowson, A et al. | 2014
- 14011
-
An overview of the comprehensive First Mirror Test in JET with ITER-like wallIvanova, D et al. | 2014
- 14012
-
Surface analysis of tiles and samples exposed to the first JET campaigns with the ITER-like wallCoad, J P et al. | 2014
- 14013
-
Tile profiling analysis of samples from the JET ITER-like wall and carbon wallHeinola, K et al. | 2014
- 14014
-
Transient impurity events in JET with the new ITER-like wallSertoli, M et al. | 2014
- 14015
-
The second phase of JET operation with the ITER-like wallMatthews, G F et al. | 2014
- 14016
-
First results and surface analysis strategy for plasma-facing components after JET operation with the ITER-like wallLikonen, J et al. | 2014
- 14017
-
Impact of ion cyclotron wall conditioning on fuel removal from plasma-facing components at TEXTORCarrasco, A G et al. | 2014
- 14018
-
CuCrZr alloy microstructure and mechanical properties after hot isostatic pressing bonding cyclesFrayssines, P-E et al. | 2014
- 14019
-
Tungsten erosion under combined hydrogen/helium high heat flux loadingMaier, H et al. | 2014
- 14020
-
Irradiation resistance of grains near {0 0 1} on polycrystalline tungsten under 30 keV He+ bombardment at 1173 KGarrison, L M et al. | 2014
- 14021
-
The influence of nitrogen on deuterium permeation through tungstenLee, H T et al. | 2014
- 14022
-
ELM-induced melting: assessment of shallow melt layer damage and the power handling capability of tungsten in a linear plasma deviceMorgan, T W et al. | 2014
- 14023
-
Influence of nitrogen pre-implantation on deuterium retention in tungstenGao, L et al. | 2014
- 14024
-
Tungsten damage and melt losses under plasma accelerator exposure with ITER ELM relevant conditionsMakhlaj, V A et al. | 2014
- 14025
-
Tungsten coatings under high thermal loads in JET and Magnum-PSIRuset, C et al. | 2014
- 14026
-
Modification of arc emitted W particles in a model scrape-off layer plasmaLaux, M et al. | 2014
- 14027
-
Long-term erosion of plasma-facing materials with different surface roughness in ASDEX UpgradeHakola, A et al. | 2014
- 14028
-
In situ transmission electron microscope observation of the formation of fuzzy structures on tungstenMiyamoto, M et al. | 2014
- 14029
-
He-ion and self-atom induced damage and surface-morphology changes of a hot W targetMeyer, F W et al. | 2014
- 14030
-
Net versus gross erosion of high-Z materials in the divertor of DIII-DRudakov, D L et al. | 2014
- 14031
-
Enhanced toughness and stable crack propagation in a novel tungsten fibre-reinforced tungsten composite produced by chemical vapour infiltrationRiesch, J et al. | 2014
- 14032
-
Current status of nanostructured tungsten-based materials developmentKurishita, H et al. | 2014
- 14033
-
First results of flowing liquid lithium limiter in HT-7Ren, J et al. | 2014
- 14034
-
Spark plasma sintering of pure and doped tungsten as plasma facing materialAutissier, E et al. | 2014
- 14035
-
Performance of yttrium doped tungsten under ‘edge localized mode’-like loading conditionsLemahieu, N et al. | 2014
- 14036
-
ITER-relevant transient heat loads on tungsten exposed to plasma and berylliumYu, J H et al. | 2014
- 14037
-
Liquid metals as alternative solution for the power exhaust of future fusion devices: status and perspectiveCoenen, J W et al. | 2014
- 14038
-
Surface erosion and modification of toughened, fine-grained, recrystallized tungsten exposed to TEXTOR edge plasmaUeda, Y et al. | 2014
- 14039
-
Erosion, formation of deposited layers and fuel retention for beryllium under the influence of plasma impuritiesKreter, A et al. | 2014
- 14040
-
Impact of surface morphology on sputtering during high-fluence plasma exposureDoerner, R P et al. | 2014
- 14041
-
Movement of liquid beryllium during melt events in JET with ITER-like wallSergienko, G et al. | 2014
- 14042
-
Overview of nitrogen-15 application as a tracer gas for material migration and retention studies in tokamaksPetersson, P et al. | 2014
- 14043
-
Deuterium retention in tungsten used in ASDEX Upgrade: comparison of tokamak and laboratory studiesSugiyama, K et al. | 2014
- 14044
-
Review of hydrogen retention in tungstenTanabe, T et al. | 2014
- 14045
-
Influence of MeV helium implantation on deuterium retention in self-ion implanted tungstenMarkina, E et al. | 2014
- 14046
-
Deuterium retention in tungsten films deposited by magnetron sputteringWang, P et al. | 2014
- 14047
-
In situ nuclear reaction analysis of D retention in undamaged and self-damaged tungsten under atomic D exposureMarkelj, S et al. | 2014
- 14048
-
Deuterium retention in various toughened, fine-grained recrystallized tungsten materials under different irradiation conditionsOya, M et al. | 2014
- 14049
-
Surface modification and deuterium retention in reduced activation ferritic martensitic steels exposed to low-energy, high flux D plasma and D2 gasAlimov, V Kh et al. | 2014
- 14050
-
Deuterium retention in TiC and TaC doped tungsten under low-energy ion irradiationZibrov, M et al. | 2014
- 14051
-
Tritium trapping behavior in tungsten pre-irradiated with D, He, Ar and N plasmasHamaji, Y et al. | 2014
- 14052
-
Post-mortem measurements of fuel retention at JETKoivuranta, S et al. | 2014
- 14053
-
In situ measurement of deuterium retention in graphite under successive exposure to deuterium and hydrogen plasmasOhno, N et al. | 2014
- 14054
-
In situ deuterium inventory measurements of a-C:D layers on tungsten in TEXTOR by laser induced ablation spectroscopyGierse, N et al. | 2014
- 14055
-
Development of positron annihilation spectroscopy for characterizing neutron irradiated tungstenTaylor, C N et al. | 2014
- 14056
-
The micro-mechanical properties of ion irradiated tungstenGibson, James et al. | 2014
- 14057
-
Determination of Be sputtering yields from spectroscopic observations at the JET ITER-like wall based on three-dimensional ERO modellingBorodin, D et al. | 2014
- 14058
-
Modeling hydrogen transport in large disordered systemsToussaint, U von et al. | 2014
- 14059
-
Modelling of W–Be mixed material sputtering under D irradiationLasa, A et al. | 2014
- 14060
-
Hydrogen transport in solids with traps in the case of continuum distribution of detrapping energiesKrasheninnikov, S I et al. | 2014
- 14061
-
Experimental and numerical assessment of normal heat flux first wall qualification mock-ups under ITER relevant conditionsDu, J et al. | 2014
- 14062
-
Molecular dynamics simulation of a helium bubble bursting on tungsten surfacesIto, Atsushi M et al. | 2014
- 14063
-
Estimation of the contribution of gaps to tritium retention in the divertor of ITERMatveev, D et al. | 2014
- 14064
-
Divertor sheath power studies in DIII-D using fixed Langmuir probes and three-dimensional modeling of tile heat flowsDonovan, D et al. | 2014
- 14065
-
Thermo-chemical fuel removal from porous materials by oxygen and nitrogen dioxideMöller, S et al. | 2014
- 14066
-
Characterization of dust collected after plasma operation of all-tungsten ASDEX UpgradeFortuna-Zalesna, E et al. | 2014
- 14067
-
Development of laser-induced breakdown spectroscopy for analyzing deposited layers in ITERKarhunen, J et al. | 2014
- 14068
-
Gas analyses of the first complete JET cryopump regeneration with ITER-like wallGrünhagen Romanelli, S et al. | 2014
- 14069
-
Experimental Advanced Superconducting Tokamak/material and plasma evaluation system material migration experimentWampler, W R et al. | 2014
- 14070
-
Three-dimensional microscopy of deuterium in tungstenPeeper, K et al. | 2014