Enhancement with Hirshfeld surface analysis of structural, electrical, dielectric and luminescent performance of two bioactive V-substituted polytungstates (Englisch)
- Neue Suche nach: Maalaoui, Ahlem
- Neue Suche nach: Maalaoui, Ahlem
- Neue Suche nach: Pérez, Olivier
- Neue Suche nach: Rzaigui, Mohamed
- Neue Suche nach: Akriche, Samah Toumi
In:
Journal of alloys and compounds
;
695
; 1061-1072
;
2017
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:Enhancement with Hirshfeld surface analysis of structural, electrical, dielectric and luminescent performance of two bioactive V-substituted polytungstates
-
Beteiligte:
-
Erschienen in:Journal of alloys and compounds ; 695 ; 1061-1072
-
Verlag:
- Neue Suche nach: Elsevier Sequoia
-
Erscheinungsort:Lausanne
-
Erscheinungsdatum:2017
-
ISSN:
-
ZDBID:
-
DOI:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Englisch
- Neue Suche nach: 51.54 / 33.61 / 35.90 / 51.10
- Weitere Informationen zu Basisklassifikation
-
Schlagwörter:
-
Klassifikation:
-
Datenquelle:
Inhaltsverzeichnis – Band 695
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 1
-
In situ synthesizing SiC particles and its strengthening effect on an Al–Si–Cu–Ni–Mg piston alloyDu, Xiaofan / Gao, Tong / Liu, Guiliang / Liu, Xiangfa et al. | 2016
- 9
-
Compressive and tensile deformation behaviour of TRIP steel-matrix composite materials with reinforcing additions of zirconia and/or aluminium titanateWeigelt, C. / Schmidt, G. / Aneziris, C.G. / Eckner, R. / Ehinger, D. / Krüger, L. / Ullrich, C. / Rafaja, D. et al. | 2016
- 21
-
Structural and optical studies of Eu3+ doped Na3Mg2P5O16 pentaphosphateGodlewska, P. / Pelczarska, A.J. / Watras, A. / Macalik, L. / Ptak, M. / Szczygieł, I. / Hanuza, J. et al. | 2016
- 27
-
Synthesis and structure of molybdenum diselenide nanosheets produced from MoO3 and Se powdersWang, B.B. / Zheng, K. / Zhong, X.X. / Gao, D. / Gao, B. et al. | 2016
- 35
-
Structural stability and mechanical properties of Ti2AlX (X = Hf, Re) intermetallics: A DFT studyPathak, Ashish et al. | 2016
- 45
-
Preparation of pure α″-phase titanium alloys with low moduli via high pressure solution treatmentZhang, Yang / Liu, Zhongyuan / Zhao, Zhisheng / Ma, Mingzhen / Shu, Yu / Hu, Wentao / Liu, Riping / Tian, Yongjun / Yu, Dongli et al. | 2016
- 52
-
Sintering of HDH Ti powder in a solar furnace at Plataforma Solar de AlmeriaKováčik, J. / Emmer, Š. / Rodríguez, J. / Cañadas, I. et al. | 2016
- 60
-
A novel Au-loaded Na2Ta2O6 multifunctional catalyst: Thermocatalytic and photocatalytic elimination of the poisonous nitrobenzene derivatives from wastewater under natural conditionLiu, Xiaoqing / Su, Yiguo / Lang, Junyu / Chai, Zhanli / Wang, Xiaojing et al. | 2016
- 70
-
Preparation of the gradient Mo layers on diamond grits by spark plasma sintering and their effect on Fe-based matrix diamond compositesChang, Rui / Zang, Jianbing / Wang, Yanhui / Yu, Yiqing / Lu, Jing / Xu, Xipeng et al. | 2016
- 76
-
Effect of Sn and Zr addition on the martensitic transformation behavior of Ti-Mo shape memory alloysEndoh, Kazuki / Tahara, Masaki / Inamura, Tomonari / Hosoda, Hideki et al. | 2016
- 83
-
Swift heavy ions induced nano-grain fragmentation in fluoride thin filmsKumar, Manvendra / Pandey, Ratnesh K. / Rajput, Parasmani / Khan, S.A. / Singh, Fouran / Avasthi, D.K. / Pandey, Avinash C. et al. | 2016
- 91
-
Enhanced compacting density and cycling performance of Ni-riched electrode via building mono dispersed micron scaled morphologyDuan, Jianguo / Wu, Ceng / Cao, Yanbing / Huang, Dianhua / Du, Ke / Peng, Zhongdong / Hu, Guorong et al. | 2016
- 100
-
Industrial waste silica preparation of silicon carbide composites and their applications in lithium-ion battery anodeXiang, Kaixiong / Wang, Xianyou / Chen, Manfang / Shen, Yongqiang / Shu, Hongbo / Yang, Xiukang et al. | 2016
- 106
-
Cerium-based modification treatment of Mg-Al hydrotalcite film on AZ91D Mg alloy assisted with alternating electric fieldBa, Zhixin / Dong, Qiangsheng / Zhang, Xiaobo / Qiang, Xinfa / Cai, Zhengyang / Luo, Xian et al. | 2016
- 114
-
A flexible mechanochemical route for the synthesis of copper oxide nanorods/nanoparticles/nanowires for supercapacitor applications: The effect of morphology on the charge storage abilityAmeri, Bahareh / Davarani, Saied Saeed Hosseiny / Roshani, Reza / Moazami, Hamid Reza / Tadjarodi, Azadeh et al. | 2016
- 124
-
Characterization and device applications of p-type ZnO films prepared by thermal oxidation of sputter-deposited zinc oxynitrideRakhshani, A.E. et al. | 2016
- 133
-
Experimental and multi-scale analyses of open-celled aluminum foam with hole under compressive quasi-static loadingHamidi Ghaleh Jigh, Behrang / Hosseini Toudeshky, Hossein / Farsi, Mohammad Ali et al. | 2016
- 142
-
Nano-structure evolution of secondary Al3(Sc1−xZrx) particles during superplastic deformation and their effects on deformation mechanism in Al-Zn-Mg alloysDeng, Ying / Yin, Zhimin / Pan, Qinlin / Xu, Guofu / Duan, Yulu / Wang, Yingjun et al. | 2016
- 154
-
Electrochemical synthesis of a ternary transition metal sulfide nanosheets on nickel foam and energy storage applicationSahoo, Surjit / Naik, Kusha Kumar / Late, Dattatray J. / Rout, Chandra Sekhar et al. | 2016
- 162
-
Distribution control of AlN particles in Mg-Al/AlN compositesChen, Jie / Bao, Chonggao / Ma, Yana / Chen, Zihan et al. | 2016
- 171
-
N(1)-pentyl isatin-N(4)-methyl-N(4)-phenyl thiosemicarbazone (PITSc) as a corrosion inhibitor on mild steel in HClMuralisankar, Mathiyan / Sreedharan, Ramdas / Sujith, Surendran / Bhuvanesh, Nattamai S.P. / Sreekanth, Anandaram et al. | 2016
- 183
-
Unexpected magnetic properties explained by the homogeneity of mixed ferritesSaidani, M. / Belkacem, W. / Bardeau, J.F. / Bezergheanu, A. / Patout, L. / Mliki, N. et al. | 2016
- 194
-
Pressure induced structural and optical properties of cubic phase SnSe: An investigation for the infrared/mid-infrared optoelectronic devicesRehman, Sajid ur / Butt, Faheem K. / Tariq, Zeeshan / Hayat, Fateh / Gilani, Rabilah / Aleem, F. et al. | 2016
- 202
-
Multifunctional luminescent nanofibres from Eu3+-doped La2O2SO4 with enhanced oxygen storage capabilityYang, Mei / Shi, Haiyan / Ma, Liwei / Gui, Qingyuan / Ma, Jinlei / Lin, Mimi / Sunna, Anwar / Zhang, Wenjing / Dai, Liming / Qu, Jia et al. | 2016
- 208
-
Enhanced electrochemical properties of Ti1.4V0.6Ni with Mo2C or WC coating as negative electrodes for Ni-MH batteryLin, Jing / Cao, Zhanyi / Sun, Lianshan / Liang, Fei / Wu, Yaoming / Wang, Limin et al. | 2016
- 215
-
Spectroscopic properties and continuous-wave laser operation of Er3+:Yb3+:LaMgB5O10 crystalHuang, Yisheng / Sun, Shijia / Yuan, Feifei / Zhang, Lizhen / Lin, Zhoubin et al. | 2016
- 221
-
Temperature dependence of photoluminescence spectra and dynamics of the red-emitting K2SiF6:Mn4+ phosphorShao, Qiyue / Wang, Lin / Song, Li / Dong, Yan / Liang, Chao / He, Jinhua / Jiang, Jianqing et al. | 2016
- 227
-
High rate capability of 5 V LiNi0.5Mn1.5O4 cathode material synthesized via a microwave assist methodFeng, Xu-Yong / Shen, Chen / Xiang, Hong-Fa / Liu, Han-Kang / Wu, Yu-Cheng / Chen, Chun-Hua et al. | 2016
- 233
-
Enhanced ferromagnetism in graphite-like carbon layer-coated ZnO crystalsTu, N. / Dung, N.H. / Lan, N.T. / Nguyen, K.T. / Dung, N.D. / Viet, D.X. / Tuan, N.T. / Bui, H.V. / Nam, D.V. / Huy, P.T. et al. | 2016
- 238
-
Controllable synthesis of {001} facet dependent foursquare BiOCl nanosheets: A high efficiency photocatalyst for degradation of methyl orangeLi, Kai / Liang, Yujun / Yang, Jian / Gao, Qiang / Zhu, Yingli / Liu, Shiqi / Xu, Rui / Wu, Xingya et al. | 2016
- 250
-
Spinodal decomposition in ternary Fe-Cr-Co systemMukhamedov, B.O. / Ponomareva, A.V. / Abrikosov, I.A. et al. | 2016
- 257
-
Orientation dependence of structural, electrical and magnetic properties of La0.9Sr0.1MnO3 thin filmsYin, Lu / Wang, Chuanbin / Shen, Qiang / Zhang, Lianmeng et al. | 2016
- 263
-
Synthesis of Cu-CuO nanocomposite in microreactor and its application to photocatalytic degradationXu, Lei / Srinivasakannan, C. / Peng, Jinhui / Zhang, Libo / Zhang, Di et al. | 2016
- 270
-
Study on photocatalyst Zinc Oxide annealed at different temperatures for photodegradation of Eosin Y dyeSharma, Nandini / Jha, Ranjana / Baghel, Sarita / Sharma, Darshan et al. | 2016
- 280
-
Synthesis and characterization of Na(Gd0.5Lu0.5)F4: Nd3+,a core-shell free multifunctional contrast agentMimun, L. Christopher / Ajithkumar, G. / Rightsell, Chris / Langloss, Brian W. / Therien, Michael J. / Sardar, Dhiraj K. et al. | 2016
- 286
-
Commensurate-incommensurate magnetic phase transition in the new Yb1−xLuxMn6Sn6 compoundsEichenberger, L. / Venturini, G. / Malaman, B. / Nataf, L. / Baudelet, F. / Mazet, T. et al. | 2016
- 294
-
In situ unipolar pulse electrodeposition of nickel hexacyanoferrate nanocubes on flexible carbon fibers for supercapacitor working in neutral electrolyteMa, Xuli / Du, Xiao / Li, Xiumin / Hao, Xiaogang / Jagadale, Ajay D. / Abudula, Abuliti / Guan, Guoqing et al. | 2016
- 302
-
Effect of Bi2O3 in borate-tellurite-silicate glass system for development of gamma-rays shielding materialsIssa, Shams A.M. / Mostafa, A.M.A. et al. | 2016
- 311
-
Red-emitting CaLa4(SiO4)3O:Eu3+ phosphor with superior thermal stability and high quantum efficiency for warm w-LEDsZhong, Jiasong / Chen, Daqin / Xu, Haoxiang / Zhao, Wenguang / Sun, Jie / Ji, Zhengguo et al. | 2016
- 319
-
New electrolytic bath for electrodeposition of protective binary FeMo and ternary FeMoP filmsBarbano, E.P. / Da Silva, F.S. / Carlos, I.A. / Vallés, E. et al. | 2016
- 329
-
Self-assembled Co3O4 nanoplatelets into micro-spheres via a simple solvothermal route: Structural and electrochemical propertiesDar, M.A. / Nam, S.H. / Abdo, H.S. / Almajid, A.A. / Kim, D.W. / Qurashi, A. / Kim, W.B. et al. | 2016
- 337
-
On the photophysics and speciation of actinide ion in MgAl2O4 spinel using photoluminescence spectroscopy and first principle calculation: A case study with uraniumGupta, Santosh K. / Pathak, Nimai / Ghosh, P.S. / Kadam, R.M. et al. | 2016
- 344
-
Microstructure and texture variation with Gd addition in extruded magnesiumKim, Sang-Hoon / Jung, Jae-Gil / You, Bong Sun / Park, Sung Hyuk et al. | 2016
- 351
-
Envisioning the attachment of CdS nanoparticles on the surface of MFe2O4 (M = Zn, Co and Ni) nanocubes: Analysis of structural, optical, magnetic and photocatalytic propertiesSingh, Charanjit / Goyal, Ankita / Malik, Rupal / Bansal, S. / Singhal, Sonal et al. | 2016
- 364
-
MWCNT reinforced τ-Mn-Al nanocomposite magnets through spark plasma sinteringSaravanan, P. / Hsu, Jen-Hwa / Vinod, V.T.P. / Černík, Miroslav / Kamat, S.V. et al. | 2016
- 372
-
Thermodynamic evaluation of the Mo-rich corner of the Mo-Hf-C system including O impuritiesLang, D. / Povoden-Karadeniz, E. / Schatte, J. / Knabl, W. / Clemens, H. / Primig, S. et al. | 2016
- 382
-
A comparative study on the structural, optical, electrochemical and photocatalytic properties of ZrO2 nanooxide synthesized by different routesRenuka, L. / Anantharaju, K.S. / Sharma, S.C. / Nagabhushana, H. / Vidya, Y.S. / Nagaswarupa, H.P. / Prashantha, S.C. et al. | 2016
- 396
-
The role of Al content on deformation behavior and related texture evolution during hot rolling of Mg-Al-Zn alloysGuo, Fei / Zhang, Dingfei / Wu, Huayi / Jiang, Luyao / Pan, Fusheng et al. | 2016
- 404
-
Effect of thermal annealing and nitrogen composition on quantum transport in GaInNAs alloy based modulation doped quantum well structuresNutku, Ferhat / Donmez, Omer / Cokduygulular, Erman / Sarcan, Fahrettin / Kuruoglu, Furkan / Mutlu, Selman / Yildirim, Saffettin / Erol, Ayse et al. | 2016
- 410
-
Nickel cobaltite nanoflakes grown around nickel foam-supported expanded mesocarbon microbeads for battery-like electrochemical capacitorsWu, Mao-Sung / Chen, Wei-Ann / Chen, Fang-Yi / Chuang, Farn-Yih et al. | 2016
- 418
-
Kinetic arrest of the ferrimagnetic state in indium-doped Mn1.82Co0.18SbTekgül, A. / Acet, M. / Farle, M. / Ünal, N. et al. | 2016
- 426
-
Impurity effects in the microscopic elastic properties of polycrystalline Mg-Zn-Y alloys with a synchronized long-period stacking ordered phaseHosokawa, S. / Kimura, K. / Yamasaki, M. / Kawamura, Y. / Yoshida, K. / Inui, M. / Tsutsui, S. / Baron, A.Q.R. / Kawakita, Y. / Itoh, S. et al. | 2016
- 433
-
Tribological performance of CrN and CrN/GLC coated components for automotive engine applicationsWan, Shanhong / Pu, Jibin / Li, Dongshan / Zhang, Guang'an / Zhang, Bo / Tieu, Anh Kiet et al. | 2016
- 443
-
Effect of Sr addition on microstructure evolution and mechanical properties of Zn4%Al hypoeutectic alloyLiu, Yang / Geng, Cong / Zhu, Yunke / Chen, Xu et al. | 2016
- 452
-
Precipitated Al2O3 phase characterization in internally oxidized Cu–Al alloy sheetsRen, Fengzhang / Li, Xin / Ren, Jiangzhuo / Xiong, Yi / Volinsky, Alex A. / Tian, Baohong et al. | 2016
- 458
-
Pattern transfer of hexagonal packed structure via ultrathin metal nanomesh masks for formation of Si nanopore arraysLi, Zeping / Xu, Zhimou / Qu, Xiaopeng / Wang, Shuangbao / Peng, Jing et al. | 2016
- 462
-
Processing, microstructure and properties of Ni1.5CoCuFeCr0.5−xVx high entropy alloys with carbon introduced from process control agentWang, Pei / Cai, Hongnian / Zhou, Shimeng / Xu, Lingyu et al. | 2016
- 476
-
TEM characterization of a TiN-MgAl2O4 epitaxial interfacePark, J.S. / Kim, D.H. / Park, J.H. et al. | 2016
- 482
-
Cation substitution induced structural transition, band gap engineering and grain growth of Cu2CdxZn1−xSnS4 thin filmsZhang, Qiao / Deng, Hongmei / Chen, Leilei / Yu, Lu / Tao, Jiahua / Sun, Lin / Yang, Pingxiong / Chu, Junhao et al. | 2016
- 489
-
In situ thermal decomposition for preparation of Nb3O7F/Nb2O5 hybrid nanomaterials with enhanced photocatalytic performanceHuang, Fei / Zhao, Hui / Yan, Aihua / Li, Zhen / Liang, Huagen / Gao, Qingyu / Qiang, Yinghuai et al. | 2016
- 496
-
Using one-step facile and solvent-free mechanochemical process to synthesize photoactive Fe2O3-TiO2 for treating industrial wastewaterSubramonian, Wennie / Wu, Ta Yeong / Chai, Siang-Piao et al. | 2016
- 508
-
Synthesis of flake shaped carbonyl iron/reduced graphene oxide/polyvinyl pyrrolidone ternary nanocomposites and their microwave absorbing propertiesWeng, Xiaodi / Li, Bingzhen / Zhang, Yang / Lv, Xuliang / Gu, Guangxin et al. | 2016
- 520
-
High performance humidity sensor based on metal organic framework MIL-101(Cr) nanoparticlesZhang, Jingjing / Sun, Liang / Chen, Chuan / Liu, Man / Dong, Wei / Guo, Wenbin / Ruan, Shengping et al. | 2016
- 526
-
The relationship between microstructure, crystallographic orientation, and fracture behavior in a high strength ferrous alloyYuan, G. / Hu, W. / Wang, X. / Kang, J. / Zhao, J. / Di, H. / Misra, R.D.K. / Wang, G. et al. | 2016
- 540
-
Tight-binding description of the silicon carbide nanotubesChegel, Raad et al. | 2016
- 549
-
Enhancement of short-circuit current density in Cu2O/ZnO heterojunction solar cellsPerng, Dung-Ching / Hong, Min-Hao / Chen, Kuan-Hung / Chen, Kuan-Hua et al. | 2016
- 555
-
Bi3+-doped CH3NH3PbI3: Red-shifting absorption edge and longer charge carrier lifetimeWang, Ruiqi / Zhang, Xian / He, Jianqiao / Ma, Cheng / Xu, Li / Sheng, Peng / Huang, Fuqiang et al. | 2016
- 561
-
Cu2PO4OH: Controlled synthesis of various architectures and morphology-dependent 808 nm laser-driven photothermal performanceHu, Xia / Zheng, Xiao-Jie / Li, Yan / Zhang, Jing / Ma, De-Kun et al. | 2016
- 567
-
Photoluminescence and charge compensation effects in Lu3MgyAl5−x−ySixO12:Ce3+ phosphors for white LEDsQiao, Jun / Shen, Leijun / Xiao, Wenge / Qiao, Xin / Wang, Zhongzhi / Gao, Lele / Li, Bo / Zhou, Yongbo / Zhang, Xia / Zhang, Xiyan et al. | 2016
- 574
-
Effect of nano Al2O3 additions on the interfacial behavior and mechanical properties of eutectic Sn-9Zn solder on low temperature wetting and soldering of 6061 aluminum alloysXing, Wen-qing / Yu, Xin-ye / Li, Heng / Ma, Le / Zuo, Wei / Dong, Peng / Wang, Wen-xian / Ding, Min et al. | 2016
- 583
-
Composite cathodes for electrolyte-supported solid oxide fuel cells with thin YbSZ electrolyteMiao, He / Xue, Yejian / He, Changrong / Wang, Jianxin / Sun, Shanshan / Liu, Man / Wang, Weiguo et al. | 2016
- 590
-
Spectroscopic investigations of Nd3+ doped gadolinium calcium silica borate glasses for the NIR emission at 1059 nmKesavulu, C.R. / Kim, H.J. / Lee, S.W. / Kaewkhao, J. / Wantana, N. / Kaewnuam, E. / Kothan, S. / Kaewjaeng, S. et al. | 2016
- 599
-
Scale synthesized cubic NaNbO3 nanoparticles with recoverable adsorption and photodegradation for prompt removal of methylene blueWang, Lin / Gu, Haoshuang / He, Jian / Zhao, Tingting / Zhang, Xuewen / Xiao, Chuan / Liu, Hui / Zhang, Xianghui / Li, Yuebin et al. | 2016
- 607
-
Enhanced VIS and NIR emissions of Pr3+ ions in TZYN glasses containing silver ions and nanoparticlesRajesh, Dagupati / Amjad, Raja J. / Reza Dousti, M. / de Camargo, A.S.S. et al. | 2016
- 613
-
Mechanical properties optimization of a Cu–Be–Co–Ni alloy by precipitation designTang, Yanchuan / Kang, Yonglin / Yue, Lijuan / Jiao, Xiaoliang et al. | 2016
- 626
-
Microstructure and impedance properties of La, Ce multi-rare earth ions doped Na0.5Bi2.5Nb2O9 Aurivillius type ceramicsPeng, Zhihang / Zeng, Xiangxiong / Cao, Feng / Yang, Xiang et al. | 2016
- 632
-
Rape seed shuck derived-lamellar hard carbon as anodes for sodium-ion batteriesCao, Liyun / Hui, Wenle / Xu, Zhanwei / Huang, Jianfeng / Zheng, Peng / Li, Jiayin / Sun, Qianqian et al. | 2016
- 638
-
Protective ability of graphene prepared by γ-irradiation and impregnated with organic inhibitor applied on AISI 316 stainless steelGalal, Ahmed / Amin, Khaled M. / Atta, Nada F. / Abd El-Rehim, Hassan A. et al. | 2016
- 648
-
Synthesis strategy, phase-chemical structure and microwave dielectric properties of paraelectric Sr(1−3x/2)CexTiO3 ceramicsUllah, Burhan / Lei, Wen / Zou, Zheng-Yu / Wang, Xiao-Hong / Lu, Wen-Zhong et al. | 2016
- 656
-
Modelling the sulfate capacity of simulated radioactive waste borosilicate glassesBingham, P.A. / Vaishnav, S. / Forder, S.D. / Scrimshire, A. / Jaganathan, B. / Rohini, J. / Marra, J.C. / Fox, K.M. / Pierce, E.M. / Workman, P. et al. | 2016
- 668
-
Influence of red lead on the intensity of green and orange emissions of Sm3+ and Ho3+ co-doped ZnO–SrO–P2O5 glass systemRavi Kumar, Valluri / Giridhar, G. / Sudarsan, V. / Veeraiah, N. et al. | 2016
- 682
-
Attempts to further enhance ZT in skutterudites via nano-compositesRogl, Gerda / Grytsiv, Andriy / Failamani, Fainan / Hochenhofer, Markus / Bauer, Ernst / Rogl, Peter et al. | 2016
- 697
-
Influence of thickness on the structural, optical and electrical properties of Ga-doped ZnO thin films deposited by sputtering magnetronMahdhi, H. / Alaya, S. / Gauffier, J.L. / Djessas, K. / Ben Ayadi, Z. et al. | 2016
- 704
-
Magnetic clusters on the verge of long range ferromagnetism in Lu(Fe0.75Al0.25)2 and Lu(Fe0.50Al0.50)2 alloysPiquer, C. / Fernández Barquín, L. / Chaboy, J. / Alba-Venero, D. / Laguna-Marco, M.A. / Boada, R. / Sánchez-Marcos, J. / Puente-Orench, I. et al. | 2016
- 715
-
Morphological, microstructural, and photoluminescence characterization of heterogeneous/homogeneous TeO2 nanostructures based on effect of different N2 gas flow ratesNa, Han Gil / Jung, Taek-Kyun / Ryou, Min / Lee, Ji-Woon / Beck, Jihyun / Hyun, Soong-Keun / Choi, Myung Sik / Mirzaei, Ali / Choe, Kyeonghwan / Kim, Hyoun Woo et al. | 2016
- 721
-
In situ consolidation of ball milled metalsHegedűs, Zoltán / Meka, Sai Ramudu / Mittemeijer, Eric J. et al. | 2016
- 726
-
Facile route to produce spherical and highly luminescent Tb3+ doped Y2O3 nanophosphorsKumar, Deepak / Sharma, Manoj / Haranath, D. / Pandey, O.P. et al. | 2016
- 737
-
Incommensurately modulated structure and spectroscopic properties of CaGd2(MoO4)4:Ho3+/Yb3+ phosphors for up-conversion applicationsLim, Chang Sung / Atuchin, Victor V. / Aleksandrovsky, Aleksandr S. / Molokeev, Maxim S. / Oreshonkov, Aleksandr S. et al. | 2016
- 747
-
Functional finishing of medical fabrics using CeO2/allicin nanocomposite for wound dressingsThanka Rajan, S. / Karthika, M. / Balaji, U. / Muthappan, A. / Subramanian, B. et al. | 2016
- 753
-
Novel type II InGaAs/GaAsBi quantum well for longer wavelength emissionYue, Li / Song, Yuxin / Chen, Xiren / Chen, Qimiao / Pan, Wenwu / Wu, Xiaoyan / Liu, Juanjuan / Zhang, Liyao / Shao, Jun / Wang, Shumin et al. | 2016
- 760
-
Enhanced pyroelectric properties and application of tetragonal Mn-doped 0.29Pb(In1/2Nb1/2)O3-0.31Pb(Mg1/3Nb2/3)O3-0.40PbTiO3 ternary single crystalsYang, Linrong / Li, Long / Zhao, Xiangyong / Xu, Qing / Ma, Jiashuai / Wang, Sheng / Li, Xiaobing / Di, Wenning / Xu, Haiqing / Luo, Haosu et al. | 2016
- 765
-
Oxygen-controlled structures and properties of transparent conductive SnO2:F filmsWu, Fayu / Tong, Xinru / Zhao, Zhuo / Gao, Jianbo / Zhou, Yanwen / Kelly, Peter et al. | 2016
- 771
-
Porous manganese oxide nanospheres for pseudocapacitor applicationsSingu, B.S. / Yoon, K.R. et al. | 2016
- 779
-
Physical properties of highly crystalline CIS layer prepared using single phase electrodeposition and low temperature RTP annealingSaidi, H. / Boujmil, M.F. / Durand, B. / Bouaïcha, M. et al. | 2016
- 787
-
High performance and balancing of cylindrical hybrid supercapacitor using hydrogen titanates/activated carbonLee, Jeong Hyun / Kim, Hong-Ki / Lee, Seung-Hwan et al. | 2016
- 792
-
Investigation on structural and microwave absorption property of Co2+ and Y3+ substituted M-type Ba-Sr hexagonal ferrites prepared by a ceramic methodSingh, Jasbir / Singh, Charanjeet / Kaur, Dalveer / Bindra Narang, S. / Jotania, Rajshree / Joshi, Rajat et al. | 2016
- 799
-
Sol-gel assisted hydrothermal synthesis and characterization of hybrid ZnS-RGO nanocomposite for efficient photodegradation of dyesKashinath, Lellala / Namratha, K. / Byrappa, K. et al. | 2016
- 810
-
Structure and magnetic properties of Sm(Fe,Si)9C/α-Fe nanocomposite magnetsBez, Riadh / Zehani, Karim / Batuk, Maria / Van Tendeloo, Gustaaf / Mliki, Najeh / Bessais, Lotfi et al. | 2016
- 818
-
Synthesis of two-dimensional Ti3C2Tx MXene using HCl+LiF etchant: Enhanced exfoliation and delaminationZhang, Tian / Pan, Limei / Tang, Huan / Du, Fei / Guo, Yanhua / Qiu, Tai / Yang, Jian et al. | 2016
- 827
-
Effect of cryorolling on microstructure and mechanical properties of a peak-aged AA6082 extrusionXu, Zebing / Liu, Manping / Jia, Zhihong / Roven, Hans J. et al. | 2016
- 841
-
Preparation and characterization of bismuth germanium oxide (BGO) polymer compositesBrajovic, Ljiljana M. / Stojanovic, Dusica B. / Mihailovic, Pedja / Markovic, Smilja B. / Romcevic, Maja / Mitric, Miodrag / Lazovic, Vladimir / Dramlic, Dragan / Petricevic, Slobodan / Romcevic, Nebojsa et al. | 2016
- 850
-
Gel-combustion synthesized vanadium pentoxide nanowire clusters for rechargeable lithium batteriesRamasami, Alamelu K. / Reddy, M.V. / Nithyadharseni, P. / Chowdari, B.V.R. / Balakrishna, Geetha R. et al. | 2016
- 859
-
Synthesis of cylindrically-concaved PMN–PT thick films by pad printing processLi, Jiapu / Yan, Xinxin / Zhu, Benpeng / Xu, Jiong / Ou-Yang, Jun / Yang, Xiaofei et al. | 2016
- 863
-
The influence of mechanical activation on structural evolution of nanocrystalline SrTiO3 powdersŽivojinović, Jelena / Pavlović, Vera P. / Kosanović, Darko / Marković, Smilja / Krstić, Jugoslav / Blagojević, Vladimir A. / Pavlović, Vladimir B. et al. | 2016
- 871
-
Synthesis and properties of gadolinium doped ceria electrolyte for IT-SOFCs by EDTA-citrate complexing methodAnjaneya, K.C. / Singh, Mahander Pratap et al. | 2016
- 877
-
Formation, magnetic properties and bending deformation of Fe-based amorphous alloy without metalloidsXie, Chunxiao / Yang, Yuanzheng / Zhong, Shouyan / Li, Sheng / Deng, Shichun et al. | 2016
- 881
-
Copper doped manganese ferrites nanoparticles anchored on graphene nano-sheets for high performance energy storage applicationsBashir, Bushra / Shaheen, Wajeeha / Asghar, Muhammad / Warsi, Muhammad Farooq / Khan, Muhammad Azhar / Haider, Sajjad / Shakir, Imran / Shahid, Muhammad et al. | 2016
- 888
-
Morphology dependent thermal conductivity of ZnO nanostructures prepared via a green approachVeluswamy, Pandiyarasan / Sathiyamoorthy, Suhasini / Chowdary, Kalari Hanuman / Muthusamy, Omprakash / Krishnamoorthy, Karthikeyan / Takeuchi, Tsunehiro / Ikeda, Hiroya et al. | 2016
- 895
-
Experimental investigation on microstructure and mechanical properties of gravity-die-cast magnesium alloysPoddar, Palash / Bagui, Sumanta / Ashok, K. / Murugesan, A.P. et al. | 2016
- 909
-
Structural and magnetic properties of Co2+-W4+ ions doped M-type Ba-Sr hexaferrites synthesized by a ceramic methodJoshi, Rajat / Singh, Charanjeet / Kaur, Dalveer / Zaki, Hesham / Bindra Narang, S. / Jotania, Rajshree / Mishra, Sanjay R. / Singh, Jasbir / Dhruv, Preksha / Ghimire, Madhav et al. | 2016
- 915
-
Synthesis and comparison of photocatalytic properties for Bi2WO6 nanofibers and hierarchical microspheresYang, Ai-Min / Han, Yang / Li, Shan-Shan / Xing, Hong-Wei / Pan, Yu-Hang / Liu, Wei-Xing et al. | 2016
- 922
-
Improved photocatalytic activity of few-layer Bi4O5I2 nanosheets induced by efficient charge separation and lower valence positionXia, Jiexiang / Ji, Mengxia / Di, Jun / Wang, Bin / Yin, Sheng / He, Minqiang / Zhang, Qi / Li, Huaming et al. | 2016
- 931
-
Polycrystalline Bi substituted YIG ferrite processed via low temperature sinteringJia, Ning / Huaiwu, Zhang / Li, Jie / Liao, Yulong / Jin, Lichuan / Liu, Cheng / Harris, Vincent G. et al. | 2016
- 937
-
Study on the effect of cuprite content on the electrical and CO2 sensing properties of cuprite-copper ferrite nanopowder compositesSumangala, T.P. / Thimont, Yohann / Baco-Carles, Valérie / Presmanes, Lionel / Bonningue, Corine / Pasquet, Isabelle / Tailhades, Philippe / Barnabé, Antoine et al. | 2016
- 944
-
Evaluation of thermophysical properties of (Np,Pu)O2 using molecular dynamics simulationsBellino, P.A. / Mosca, H.O. / Jaroszewicz, S. et al. | 2016
- 952
-
Effect of plunge depth on microstructure and mechanical properties of FSW lap joint between aluminum alloy and nickel-base alloyZheng, Qixian / Feng, Xiaomei / Shen, Yifu / Huang, Guoqiang / Zhao, Pengcheng et al. | 2016
- 962
-
Effect of Pd, temperature and time on wetting and interfacial microstructure of bulk metallic glasses TiCuZrPd on Ti-6Al-4V substrateSypien, Anna / Badura, Kamil / Fima, Przemyslaw / Miernik, Krzysztof et al. | 2016
- 971
-
The grain refinement potency of bismuth in magnesiumJoshi, Utsavi / Hari Babu, N. et al. | 2016
- 976
-
GMR effect and Kondo-like behaviour in Co-Cu microwiresZhukov, A. / Mino, J. / del Val, J.J. / Varga, R. / Martinez, G. / Baibich, M.N. / Ipatov, M. / Churyukanova, M. / Zhukova, V. et al. | 2016
- 981
-
Interfacial reaction, ball shear strength and fracture surface analysis of lead-free solder joints prepared using cobalt nanoparticle doped fluxSujan, G.K. / Haseeb, A.S.M.A. / Nishikawa, Hiroshi / Amalina, M.A. et al. | 2016
- 991
-
Enhanced room temperature magnetoelectric properties in Bi4−xPrxTi3−xCoxO12±d ceramics synthesized by the microwave sintering methodYang, Haibo / Sun, Yujia / Lin, Ying / Zhang, Xiaojie / Liu, Xiao / Wang, Tong / Wang, Fen et al. | 2016
- 998
-
Characterization and formation of bioactive hydroxyapatite coating on commercially pure zirconium by micro arc oxidationAktug, Salim Levent / Kutbay, Isil / Usta, Metin et al. | 2016
- 1005
-
Effect of Cu content on precipitation and age-hardening behavior in Al-Mg-Si-xCu alloysXiao, Qiao / Liu, Huiqun / Yi, Danqing / Yin, Deyan / Chen, Yuqiang / Zhang, Ying / Wang, Bin et al. | 2016
- 1014
-
Exchange hardening in FePt/Fe3Pt dual exchange spring magnet: Monte Carlo modelingGoyal, Rajan / Arora, Nishta / Kapoor, Akanksha / Lamba, S. / Annapoorni, S. et al. | 2016
- 1020
-
Investigations on the effect of substrate temperature on the properties of reactively sputtered zirconium carbide thin filmsKumar, S. Sathish / Sharma, Amit / Rao, G. Mohan / Suwas, Satyam et al. | 2016
- 1029
-
Carbon-doped ZnO aided by carboxymethyl cellulose: Fabrication, photoluminescence and photocatalytic applicationsZhao, Si-Wei / Zuo, Hong-Fen / Guo, Yuan-Ru / Pan, Qing-Jiang et al. | 2016
- 1038
-
Hot deformation behavior and microstructural evolution of Ti22Al25Nb1.0B alloy prepared by elemental powder metallurgyYang, Jianlei / Wang, Guofeng / Jiao, Xueyan / Li, Xiao / Yang, Chao et al. | 2016
- 1045
-
Shape recovery increase in a Co-Al-W alloy realized by stress-induced hcp martensitic transformation after strengthening matrixYang, X. / Wu, B.J. / Peng, H.B. / Wen, Y.H. et al. | 2016
- 1052
-
The Li-Sb phase diagram part I: New experimental resultsBeutl, A. / Cupid, D. / Flandorfer, H. et al. | 2016
- 1061
-
Enhancement with Hirshfeld surface analysis of structural, electrical, dielectric and luminescent performance of two bioactive V-substituted polytungstatesMaalaoui, Ahlem / Pérez, Olivier / Rzaigui, Mohamed / Akriche, Samah Toumi et al. | 2016
- 1073
-
A one step electrospinning process for the preparation of polyaniline modified TiO2/polyacrylonitile nanocomposite with enhanced photocatalytic activitySedghi, Roya / Moazzami, Hamid Reza / Hosseiny Davarani, Saied Saeed / Nabid, Mohammad Reza / Keshtkar, Ali Reza et al. | 2016
- 1080
-
The role of crystalline TiO2 nanoparticle in enhancing the photocatalytic and photoelectrocatalytic properties of CdS nanorodsShen, Qianqian / Xue, Jinbo / Zhao, Haocheng / Shao, Mingzhe / Liu, Xuguang / Jia, Husheng et al. | 2016
- 1088
-
The influences of extrusion-shear process on microstructures evolution and mechanical properties of AZ31 magnesium alloyHu, Hongjun / Liu, Yang / Zhang, Dingfei / Ou, Zhongwen et al. | 2016
- 1096
-
Structural aspect of chemical reaction between components of mechanically alloyed Al-MoO2 and Al-MoO3 compositesBlaz, Ludwik / Wloch, Grzegorz / Lobry, Patrycja / Sobota, Jakub / Dymek, Stanislaw et al. | 2016
- 1104
-
Ag-encapsulated Single-Crystalline Anatase TiO2 Nanoparticle photoanodes for enhanced dye-sensitized solar cell performanceXu, Yuanmei / Zhang, Haiyan / Li, Xueshi / Wang, Wenguang / Li, Jinlun et al. | 2016
- 1112
-
Elucidation of phase evolution, microstructural, Mössbauer and magnetic properties of Co2+Al3+ doped M-type BaSr hexaferrites synthesized by a ceramic methodSingh, Jasbir / Singh, Charanjeet / Kaur, Dalveer / Zaki, Hesham / Abdel-Latif, I.A. / Narang, S. Bindra / Jotania, Rajshree / Mishra, Sanjay R. / Joshi, Rajat / Dhruv, Preksha et al. | 2016
- 1122
-
High sensitive and fast formaldehyde gas sensor based on Ag-doped LaFeO3 nanofibersWei, Wei / Guo, Sijia / Chen, Chuan / Sun, Liang / Chen, Yu / Guo, Wenbin / Ruan, Shengping et al. | 2016
- 1128
-
Absence of the stripe antiferromagnetic order in the new 30 K superconductor ThFeAsNAlbedah, Mohammed A. / Nejadsattari, Farshad / Stadnik, Zbigniew M. / Wang, Zhi-Cheng / Wang, Cao / Cao, Guang-Han et al. | 2016
- 1137
-
Synthesis of flower-like Ta3N5-Au heterojunction with enhanced visible light photocatalytic activityLi, Shijie / Zhang, Junlei / Hu, Shiwei / Xu, Kaibing / Jiang, Wei / Liu, Jianshe et al. | 2016
- 1145
-
Fabrication of Ag/ZnO/reduced graphene oxide nanocomposite for SERS detection and multiway killing of bacteriaKo, Ya Chi / Fang, Hong Yi / Chen, Dong Hwang et al. | 2016
- 1154
-
Single-band near-infrared quantum cutting of Ho3+-Yb3+ codoped KLu2F7 phosphors by energy clusteringYu, T. / Yu, D.C. / Lin, H.H. / Zhang, Q.Y. et al. | 2016
- 1160
-
Luminescence study of Eu3+-doped garnet phosphors: Relating structure to emissionPasiński, Damian / Sokolnicki, Jerzy et al. | 2016
- 1166
-
Effect of Mn addition on corrosion properties of biodegradable Mg-4Zn-0.5Ca-xMn alloysCho, Dae Hyun / Lee, Byoung Woo / Park, Jin Young / Cho, Kyung Mox / Park, Ik Min et al. | 2016
- 1175
-
Microstructure, phase structure, and electrical properties in lead-free (1−x)(K0.40Na0.60)(Nb0.96Sb0.04)O3−x(Bi0.5Na0.5)0.9Cu0.1ZrO3 ceramicsWu, Wenjuan / Chen, Min / Wu, Bo / Ding, Yingchun / Liu, Chuanqi et al. | 2016
- 1180
-
Pressure-induced polyamorphism by quantitative structure factor and pair distribution function analysis in two Ce-based metallic glassesZhang, Linji / Sun, Fei / Hong, Xinguo / Wang, Junlong / Liu, Gang / Kong, Lingping / Yang, Hongwang / Liu, Xiuru / Zhao, Yong / Yang, Wenge et al. | 2016
- 1185
-
Effects of CeZn co-substitution on structure, magnetic and microwave absorption properties of nickel ferrite nanoparticlesYan, Zhu / Luo, Juhua et al. | 2016
- 1196
-
The synthesis, characterization and ZnS surface passivation of polycrystalline ZnO films obtained by the spin-coating methodBaranowska-Korczyc, Anna / Reszka, Anna / Sobczak, Kamil / Wojciechowski, Tomasz / Fronc, Krzysztof et al. | 2016
- 1205
-
Effect of pH on the synthesis of CuO films by SILAR methodGençyılmaz, O. / Taşköprü, T. et al. | 2016
- 1213
-
Effect of local environment on moment formation in iron silicidesZamkova, N.G. / Zhandun, V.S. / Ovchinnikov, S.G. / Sandalov, I.S. et al. | 2016
- 1223
-
A high-performance anode material based on FeMnO3/graphene compositeBin, Heng / Yao, Zhenpeng / Zhu, Shenmin / Zhu, Chengling / Pan, Hui / Chen, Zhixin / Wolverton, Chris / Zhang, Di et al. | 2016
- 1231
-
Effect of surface treated MWCNTs and BaTiO3 nanoparticles on the dielectric properties of a P(VDF-TrFE) matrixYaqoob, Usman / Chung, Gwiy-Sang et al. | 2016
- 1237
-
Mid-infrared luminescence of Dy3+ ions in modified Ga-Sb-S chalcogenide glasses and fibersYang, Anping / Qiu, Jiahua / Zhang, Mingjie / Ren, He / Zhai, Chengcheng / Qi, Sisheng / Zhang, Bin / Tang, Dingyuan / Yang, Zhiyong et al. | 2016
- 1243
-
Effect of annealing temperature on the microstructure and mechanical properties of Ni-Mn-Ga-Gd thin filmYao, Jian / Zheng, XiaoHang / Cai, Wei / Sui, Jiehe et al. | 2016
- 1248
-
Two-step approach of fabrication of interconnected nanoporous 3D reduced graphene oxide-carbon nanotube-polyaniline hybrid as a binder-free supercapacitor electrodeXiong, Chuanyin / Li, Tiehu / Zhu, Yechuan / Zhao, Tingkai / Dang, Alei / Li, Hao / Ji, Xianglin / Shang, Yudong / Khan, Muhammad et al. | 2016
- 1260
-
Removal of oxygen related defects from chemically synthesized In2O3 thin film doped with Er by spin-on techniqueGhosh, Anupam / Mondal, Aniruddha / Das, Avishek / Chattopadhyay, Sanatan / Chattopadhyay, Kalyan Kumar et al. | 2016
- 1266
-
Thermal dependence of structural and magnetic properties in an amorphous Fe-Si-B-Cu alloyDai, J. / Wang, Y.G. / Yang, L. / Xia, G.T. / Zeng, Q.S. / Lou, H.B. et al. | 2016
- 1271
-
The investigation of carbides evolution in a cobalt-base superalloy at elevated temperatureGui, Weimin / Zhang, Hongyu / Yang, Min / Jin, Tao / Sun, Xiaofeng / Zheng, Qi et al. | 2016
- 1279
-
Photocatalytic degradation of herbicides under visible light using Ni-Pr2O3 nanocompositesSobahi, T. et al. | 2016
- 1285
-
Local-ordering MoO2 nanostructures within porous N-doped carbon nanotubes for high-rate reversible lithium storageWang, Shuo / Zhao, Yang / Li, Chunyan / Zhang, Xitian / Chen, Yujin et al. | 2016
- 1294
-
Enhanced cycling performance of Se-doped SnS carbon nanofibers as negative electrode for lithium-ion batteriesLu, Lei / Zhang, Long / Zeng, Hong / Xu, Bo / Wang, Limin / Li, Yueming et al. | 2016
- 1301
-
The experiment and theory studies of silver substituting cadmium in CdS quantum dotsYin, Jianbo / Lu, Xuefeng / Dong, Qizheng et al. | 2016
- 1307
-
Reaction chemistry of group IV containing copper chalcogenide semiconductors Cu2MX3 (M = Sn, Ge and X = S, Se)Robert, Erika V.C. / de Wild, Jessica / Dale, Phillip J. et al. | 2016
- 1317
-
Lattice evolution and point defect chemistry in Ta-doped ceriaCharoonsuk, T. / Vittayakorn, N. / Kolodiazhnyi, T. et al. | 2016
- 1324
-
Influence of Cr layer thickness on the static and dynamic performances of Tb/Cr/Ni80Fe20 structureSun, Li / Yue, Jinjin / Jiang, Sheng / Xu, Yongjia / Li, Qiannan / Chen, Qian / Zhou, Xiaochao / Huang, Zhaocong / Yao, Zhongyu / Zhai, Ya et al. | 2016
- 1329
-
Effects of donor and acceptor doping on dielectric and ferroelectric properties of Ba0.7Ca0.3TiO3 lead-free ceramicsJaiban, Panupong / Watcharapasorn, Anucha / Yimnirun, Rattikorn / Guo, Ruyan / Bhalla, Amar S. et al. | 2016
- 1336
-
The effect of rare earth element doping on the microstructural evolution of sol-gel titania powdersYurtsever, Hüsnü Arda / Çiftçioğlu, Muhsin et al. | 2016
- 1354
-
Photophysical properties of a series of alloyed and non-alloyed water-soluble l-cysteine-capped core quantum dotsAdegoke, Oluwasesan / Nyokong, Tebello / Forbes, Patricia B.C. et al. | 2016