Corrosion behavior of nickel-based superalloys in thermal storage medium of molten eutectic NaCl-MgCl2 in atmosphere (Englisch)
- Neue Suche nach: Wang, Jun-wei
- Neue Suche nach: Wang, Jun-wei
- Neue Suche nach: Zhang, Cui-zhen
- Neue Suche nach: Li, Zhuo-hua
- Neue Suche nach: Zhou, Hong-xia
- Neue Suche nach: He, Jia-xin
- Neue Suche nach: Yu, Jing-chao
In:
Solar energy materials & solar cells
;
164
; 146-155
;
2017
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:Corrosion behavior of nickel-based superalloys in thermal storage medium of molten eutectic NaCl-MgCl2 in atmosphere
-
Beteiligte:Wang, Jun-wei ( Autor:in ) / Zhang, Cui-zhen / Li, Zhuo-hua / Zhou, Hong-xia / He, Jia-xin / Yu, Jing-chao
-
Erschienen in:Solar energy materials & solar cells ; 164 ; 146-155
-
Verlag:
- Neue Suche nach: NH, Elsevier
-
Erscheinungsort:Amsterdam [u.a.]
-
Erscheinungsdatum:2017
-
ISSN:
-
ZDBID:
-
DOI:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Englisch
- Neue Suche nach: 53.36 / 52.52 / 52.56 / 50.70
- Weitere Informationen zu Basisklassifikation
-
Schlagwörter:
-
Klassifikation:
-
Datenquelle:
Inhaltsverzeichnis – Band 164
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 1
-
Solution processable wurtzite CuInS2 inverted type solar cellGolobostanfard, Mohammad Reza / Abdizadeh, Hossein / Jannati, Ali et al. | 2017
- 7
-
Electrical and optical properties of Si microwire solar cellsKim, Hong-Sik / Patel, Dipal B. / Kim, Hyunyub / Patel, Malkeshkumar / Chauhan, Khushbu R. / Park, Wanghee / Kim, Joondong et al. | 2017
- 13
-
Thickness effects of thermally evaporated C60 thin films on regular-type CH3NH3PbI3 based solar cellsLee, Kun-Mu / Chen, Cheng-Chiang / Chen, Lung-Chien / Chang, Sheng Hsiung / Chen, Kai-Shiang / Yeh, Shih-Chieh / Chen, Chin-Ti / Wu, Chun-Guey et al. | 2017
- 19
-
CuSbS2 thin films by rapid thermal processing of Sb2S3-Cu stack layers for photovoltaic applicationVinayakumar, V. / Shaji, S. / Avellaneda, D. / Das Roy, T.K. / Castillo, G.A. / Martinez, J.A.A. / Krishnan, B. et al. | 2017
- 28
-
Absorption coefficients in AlGaInP lattice-matched to GaAsCheong, J.S. / Baharuddin, A.N.A.P. / Ng, J.S. / Krysa, A.B. / David, J.P.R. et al. | 2017
- 32
-
Experimental study of photothermal specifications and stability of graphene oxide nanoplatelets nanofluid as working fluid for low-temperature Direct Absorption Solar Collectors (DASCs)khosrojerdi, S. / Lavasani, A.M. / Vakili, M. et al. | 2017
- 40
-
Efficient nanostructured quasi-single crystalline silicon solar cells by metal-catalyzed chemical etchingWang, Qiang / Pan, Chengfeng / Chen, Kexun / Zou, Shuai / Shen, Mingrong / Su, Xiaodong et al. | 2017
- 47
-
Low-temperature electrodeposited crystalline SnO2 as an efficient electron-transporting layer for conventional perovskite solar cellsChen, Jung-Yao / Chueh, Chu-Chen / Zhu, Zonglong / Chen, Wen-Chang / Jen, Alex K.-Y. et al. | 2017
- 56
-
Fabrication of CH3NH3PbI3 perovskite-based solar cells: Developing various new solvents for CuSCN hole transport materialMurugadoss, Govindhasamy / Thangamuthu, Rangasamy / Senthil Kumar, Sakkarapalayam Murugesan et al. | 2017
- 63
-
Microstructure, chromaticity and thermal stability of SS/TiC-WC/Al2O3 spectrally selective solar absorbersGao, Xiang-Hu / Guo, Zhi-Ming / Geng, Qing-Fen / Ma, Peng-Jun / Wang, Ai-Qin / Liu, Gang et al. | 2017
- 70
-
Pathway for recovery of photo-degraded polymer solar cells by post degradation thermal annealBhattacharya, J. / Joshi, P.H. / Biswas, R. / Dalal, V.L. et al. | 2017
- 80
-
Study on snail trail formation in PV module through modeling and accelerated aging testsFan, Jing / Ju, Daliang / Yao, Xiaoqin / Pan, Zhen / Terry, Mason / Gambogi, William / Stika, Katherine / Liu, Junhui / Tao, Wusong / Liu, Zengsheng et al. | 2017
- 87
-
Low-temperature processed SnO2 compact layer by incorporating TiO2 layer toward efficient planar heterojunction perovskite solar cellsHuang, Xiaokun / Hu, Ziyang / Xu, Jie / Wang, Peng / Wang, Liming / Zhang, Jing / Zhu, Yuejin et al. | 2017
- 93
-
A reaction-diffusion formulation to simulate EVA polymer degradation in environmental and accelerated ageing conditionsGagliardi, M. / Lenarda, P. / Paggi, M. et al. | 2017
- 107
-
Enhancing the adsorption of CdSe quantum dots on TiO2 nanotubes by tuning the solvent polarityTorresan, María F. / Baruzzi, Ana M. / Iglesias, Rodrigo A. et al. | 2017
- 114
-
Novel low melting point binary nitrates for thermal energy storage applicationsWU, Yu-ting / LI, Ying / LU, Yuan-wei / Wang, Hui-fu / MA, Chong-fang et al. | 2017
- 122
-
Improved stability of depletion heterojunction solar cells employing cation-exchange PbS quantum dotsYao, Xudong / Song, Zihang / Mi, Longfei / Li, Guopeng / Wang, Xiaoyan / Wang, Xiaoming / Jiang, Yang et al. | 2017
- 128
-
Cd doping at PVD-CdS/CuInGaSe2 heterojunctionsHe, Xiaoqing / Paulauskas, Tadas / Ercius, Peter / Varley, Joel / Bailey, Jeff / Zapalac, Geordie / Poplavskyy, Dmitry / Mackie, Neil / Bayman, Atiye / Spaulding, David et al. | 2017
- 135
-
Temperature- and ligand-dependent carrier transport dynamics in photovoltaic PbS colloidal quantum dot thin films using diffusion-wave methodsHu, Lilei / Mandelis, Andreas / Yang, Zhenyu / Guo, Xinxin / Lan, Xinzheng / Liu, Mengxia / Walters, Grant / Melnikov, Alexander / Sargent, Edward H. et al. | 2017
- 146
-
Corrosion behavior of nickel-based superalloys in thermal storage medium of molten eutectic NaCl-MgCl2 in atmosphereWang, Jun-wei / Zhang, Cui-zhen / Li, Zhuo-hua / Zhou, Hong-xia / He, Jia-xin / Yu, Jing-chao et al. | 2017
- 156
-
Quantized interfacial properties at lead sulfide/Zn1−xMgxO energy harvesting assembly: Formation of nanocrystal solid solutionCho, Seongeun / Kim, Youngjun / Kim, Minkyoing / Kim, Jin-A. / Kim, Kihyun / Park, Yujin / Han, Soojin / Han, Chang-Yeol / Kim, Jong-Hoon / Hwang, Jun Yeon et al. | 2017
- 165
-
Plasmon hybridisation of self-assembled 3d multiphase nano-titanium oxide towards broadband photon absorptionThakur, Pooja / Tan, Bo / Venkatakrishnan, Krishnan et al. | 2017
- 175
-
A review on the use of SrBr2·6H2O as a potential material for low temperature energy storage systems and building applicationsFopah-Lele, Armand / Tamba, Jean Gaston et al. | 2017
- 188
-
Di-functional nanocomposite films for efficient conversion and storage of solar energyShang, Mengya / Zhang, Shudong / Li, Nian / Gu, Xiaomin / Li, Li / Wang, Zhenyang et al. | 2017
- IFC
-
Editorial Board| 2017