A fractographic criterion for subcritical crack growth boundaries at internal fracture origins in hot pressed silicon nitride (Englisch)
- Neue Suche nach: Kirchner, H. P.
- Neue Suche nach: Gruver, R. M.
- Neue Suche nach: Richard, D. M.
- Neue Suche nach: Kirchner, H. P.
- Neue Suche nach: Gruver, R. M.
- Neue Suche nach: Richard, D. M.
In:
Journal of Materials Science
;
14
, 11
; 2713-2720
;
1979
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:A fractographic criterion for subcritical crack growth boundaries at internal fracture origins in hot pressed silicon nitride
-
Beteiligte:
-
Erschienen in:Journal of Materials Science ; 14, 11 ; 2713-2720
-
Verlag:
- Neue Suche nach: Kluwer Academic Publishers
- Neue Suche nach: Springer Science + Business Media B.V.
-
Erscheinungsort:Norwell, Mass
-
Erscheinungsdatum:1979
-
ISSN:
-
ZDBID:
-
DOI:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Englisch
- Neue Suche nach: 51.00
- Weitere Informationen zu Basisklassifikation
- Neue Suche nach: 275/5010
-
Schlagwörter:
-
Klassifikation:
-
Datenquelle:
Inhaltsverzeichnis – Band 14, Ausgabe 11
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 2529
-
Kinetics of crystallization of trans-1, 4-polyisoprene crystallized in thin filmsDavies, C. K. L. / Eng Long, Ong et al. | 1979
- 2537
-
Identification and properties of ultra-fine iron particles dispersed in a glass-like carbon matrixOmori, M. / Yajima, S. et al. | 1979
- 2543
-
Crystal structure of $ Si_{3} $$ N_{4} $·$ Y_{2} $$ O_{3} $ examined by a 1 MV high-resolution electron microscopeHoriuchi, S. / Mitomo, M. et al. | 1979
- 2547
-
The activation energy for superplastic flow in Al-6Cu-0.4ZrBricknell, R. H. / Bentley, A. P. et al. | 1979
- 2555
-
Microstructure-property relationships of GRPGuild, Felicity J. / Ralph, Brian et al. | 1979
- 2563
-
The embrittling effects of hydrogen on a variety of inorganic materials as indicated by acoustic emissionCuthrell, R. E. / Randich, E. et al. | 1979
- 2567
-
On the scribing and subsequent fracturing of silicon semiconductor wafersMisra, A. / Fininie, I. et al. | 1979
- 2575
-
Statistical analysis of the brittle fracture of sintered tungstenMargetson, J. / Sherwood, P. J. et al. | 1979
- 2581
-
Glass workability study and correlation of melting history, microstructure, apparent liquidus temperature, and mechanical strengthHsich, Henry S. -Y. et al. | 1979
- 2589
-
The age hardening effect in Ti-6 Al-4 V due to ω and α precipitation in the β grainsLasalmonie, Alain / Loubradou, Marc et al. | 1979
- 2596
-
Crystallization of fusion cast ceramics and glass-ceramicsMcNally, R. N. / Beall, G. H. et al. | 1979
- 2605
-
The temperature dependence of the fracture toughness and acoustic emission of polycrystalline aluminaDalgleish, B. J. / Fakhr, A. / Pratt, P. L. / Rawlings, R. D. et al. | 1979
- 2616
-
Fatigue life-limiting parameters in fibreglass compositesKim, H. C. / Ebert, L. J. et al. | 1979
- 2625
-
Recovery of a creep-deformed Type 316 stainless steelMorris, D. G. / Harries, D. R. et al. | 1979
- 2637
-
High-temperature glass-ceramics of the BaO-$ Al_{2} $$ O_{3} $-$ SiO_{2} $-$ Ta_{2} $$ O_{5} $ system and molybdenum metal compositesBahat, D. / Chu, G. P. K. et al. | 1979
- 2642
-
The metallography of cuboid-shaped inclusions in commercial Cu-Be-Co alloyNourbakhsh, S. / Nutting, J. et al. | 1979
- 2645
-
On the equation of state of crystalline polyvinylidene fluorideJain, R. K. / Simha, Robert et al. | 1979
- 2650
-
An electrostatic technique for revealing internal structure in diamondsDeVries, R. C. / Tuft, R. E. et al. | 1979
- 2659
-
Influence of surface potential on the kinetics of glass reactions with aqueous solutionsMularie, W. M. / Furth, W. F. / Westwood, A. R. C. et al. | 1979
- 2665
-
A critical examination of a cryochemical method for the preparation of high surface area semiconducting powdersHibbert, D. B. / Tseung, A. C. C. et al. | 1979
- 2672
-
The chemical interaction of metals with polytetrafluoroethyleneCadman, P. / Gossedge, G. M. et al. | 1979
- 2679
-
Compliances and failure modes of oriented chain-extended polyethyleneAttenburrow, G. E. / Bassett, D. C. et al. | 1979
- 2688
-
The development of fine structure superplasticity in cast ultrahigh carbon steels through thermal cyclingKayali, E. S. / Sunada, H. / Oyama, T. / Wadsworth, J. / Sherby, O. D. et al. | 1979
- 2693
-
Solid phase compaction of polymersCrawford, R. J. / Paul, D. et al. | 1979
- 2703
-
Kinetic aspects of slow crack growth in the gaseous hydrogen embrittlement of steelsSieradzki, K. / Ficalora, P. et al. | 1979
- 2709
-
The preparation of textured Te thin films with pronounced acicular morphology and concomitant high absorptivityPeterson, M. J. / Cocks, F. H. et al. | 1979
- 2713
-
A fractographic criterion for subcritical crack growth boundaries at internal fracture origins in hot pressed silicon nitrideKirchner, H. P. / Gruver, R. M. / Richard, D. M. et al. | 1979
- 2721
-
Effect of surface treatments on strength of PZT polycrystalline ceramicsBiswas, Dipak R. / Fulrath, Richard M. et al. | 1979
- 2726
-
The morphologies of boron fibres in the temperature range 1000 to 1500° C and the relationship between mechanical properties and morphologyCarlsson, Jan -Otto et al. | 1979
- 2726ff
-
Morphologies of boron fibres in the temperature range 1000 to 1500 c and the relationship between mechanical properties and morphology.Carlsson, J.O. et al. | 1979
- 2733
-
Analytical treatment of the role of surface oxide layers in the sintering of metalsMunir, Z. A. et al. | 1979
- 2741
-
TEM studies on $ Al_{4} $$ C_{3} $·3 $ Be_{2} $ CZangvil, A. / Gauckler, L. J. / Schneider, G. / Rühle, M. et al. | 1979
- 2747
-
On the guillotining of materialsAtkins, A. G. / Mai, Y. W. et al. | 1979
- 2755
-
Fracture toughness of ABSNusbaum, H. J. et al. | 1979
- 2757
-
High temperature interactions of metal oxides with rhenium in vacuoSu, Ching -Shen et al. | 1979
- 2760
-
Strain rates for three- and four-point flexure testsLand, Peter L. et al. | 1979
- 2761
-
Preparation and characterization of thin films of $ FeS_{2} $Seehra, S. S. / Montano, P. A. / Seehra, M. S. / Sen, S. K. et al. | 1979
- 2764
-
Oxidative stabilization of acrylic fibres: Part 4 Moisture sensitivityWarner, S. B. / Peebles, L. H. / Uhlmann, D. R. et al. | 1979
- 2764ff
-
Oxidative stabilization of acrylic fibres. Iv. Moisture sensitivityWarner, S.B. / Peebles, C.H. / Uhlmann, D.R. et al. | 1979
- 2765
-
Au thin films with nm-sized pores made from Au-Ge eutectic alloy filmsKitada, Masahiro et al. | 1979
- 2767
-
Comments on “Thermochemical effects on the formation of $ Ca_{3} $$ SiO_{5} $”Glasser, F. P. et al. | 1979
- 2768
-
Internal stress dependence of the hardness of crystallized glassesRice, R. W. / McMillan, P. W. / Stryjak, A. J. et al. | 1979
- 2773
-
Creep of hot-pressed silicon nitride ceramicsDixon-Stubbs, P. J. / Wilshire, B. et al. | 1979
- 2775
-
Superstructural ordering in oriented nylon 66 filmGarton, A. / Carlsson, D. J. / Stepaniak, R. F. / Sturgeon, P. Z. / Wiles, D. M. et al. | 1979
- 2778
-
Comments on “New compound in the system La-Si-O-N″′Morgan, P. E. D. / Mitomo, M. / Kuramoto, N. / Susuki, H. et al. | 1979