Direct current electrical conductivity of gamma ferric oxide (Englisch)
- Neue Suche nach: Nikumbh, A. K.
- Neue Suche nach: Rane, K. S.
- Neue Suche nach: Mukhedkar, A. J.
- Neue Suche nach: Nikumbh, A. K.
- Neue Suche nach: Rane, K. S.
- Neue Suche nach: Mukhedkar, A. J.
In:
Journal of Materials Science
;
17
, 9
; 2503-2513
;
1982
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:Direct current electrical conductivity of gamma ferric oxide
-
Beteiligte:
-
Erschienen in:Journal of Materials Science ; 17, 9 ; 2503-2513
-
Verlag:
- Neue Suche nach: Kluwer Academic Publishers
- Neue Suche nach: Springer Science + Business Media B.V.
-
Erscheinungsort:Norwell, Mass
-
Erscheinungsdatum:1982
-
ISSN:
-
ZDBID:
-
DOI:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Englisch
- Neue Suche nach: 51.00
- Weitere Informationen zu Basisklassifikation
- Neue Suche nach: 275/5010
-
Schlagwörter:
-
Klassifikation:
-
Datenquelle:
Inhaltsverzeichnis – Band 17, Ausgabe 9
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 2463
-
Fatigue crack propagation in polymethylmethacrylate bone cementsWright, Timothy M. / Robinson, Raymond P. et al. | 1982
- 2469
-
Crack-front shape effects in the double torsion testLeevers, P. S. et al. | 1982
- 2481
-
Some geometrical observations on crack front profiles in PMMA double torsion specimensStalder, B. / Kausch, H. H. et al. | 1982
- 2486
-
Microstructures and subcritical crack growth in oxidized hot-pressed $ Si_{3} $$ N_{4} $Das, G. / Mendiratta, M. G. / Cornish, G. R. et al. | 1982
- 2495
-
Study of growth rate and failure mode of chemically vapour deposited TiN, $ TiC_{x} $$ N_{y} $ and TiC on cemented tungsten carbideCho, J. S. / Nam, S. W. / Chun, J. S. et al. | 1982
- 2503
-
Direct current electrical conductivity of gamma ferric oxideNikumbh, A. K. / Rane, K. S. / Mukhedkar, A. J. et al. | 1982
- 2514
-
Plastic deformation and fracture of notched specimens due to bending in glassy polymersKitagawa, M. et al. | 1982
- 2525
-
TEM investigation of crystallization phenomena in the metallic glass VitrovacR 0040 (Fe40Ni40B20)Mueller, K. / Heimendahl, M. von et al. | 1982
- 2525
-
TEM investigation of crystallization phenomena in the metallic glass $ Vitrovac^{®} $ 0040 ($ Fe_{40} $$ Ni_{40} $$ B_{20} $)Müller, K. / Von Heimendahl, M. et al. | 1982
- 2533
-
The electrical conductivity of fluorozirconate and chloro-fluorozirconate glassesAlmeida, Rui M. / MacKenzie, John D. et al. | 1982
- 2539
-
Creep behaviour of hot isostatically pressed niobium alloy powder compactsWadsworth, J. / Roberts, C. A. / Rennhack, E. H. et al. | 1982
- 2547
-
On a fatigue crack-front marking technique for polymersTakemori, M. T. et al. | 1982
- 2553
-
Observations on the characteristics of a fluidized bed for the thermal shock testing of brittle ceramicsNiihara, K. / Singh, J. P. / Hasselman, D. P. H. et al. | 1982
- 2560
-
Grain size effect of electro-plated tin coatings on whisker growthKakeshita, Tomoyuki / Shimizu, Ken'ichi / Kawanaka, Ryusuke / Hasegawa, Tomoharu et al. | 1982
- 2567
-
Compression fatigue behaviour of notched composite laminatesWalsh, R. M. / Pipes, R. B. et al. | 1982
- 2577
-
Electrical conduction of partially stabilized zirconia $ Zr_{0.94} $$ Ca_{0.06} $$ O_{1.94} $ as a function of temperature and oxygen partial pressurePyun, Su-Il / Ihm, Yeong-Eon et al. | 1982
- 2585
-
Thermoluminescent mechanisms involving transition metal ion impurities and V-type centres in MgO crystals exposed to ultraviolet radiationLas, W. C. / Stoebe, T. G. et al. | 1982
- 2594
-
Scanning electron microscopy studies on tensile rupture of rubberMathew, N. M. / Bhowmick, A. K. / Dhindaw, B. K. / De, S. K. et al. | 1982
- 2599
-
The use of scanning electron microscopy to study the ion beam sputter modification of the surface topography of biological implantsKowalski, Zbigniew W. et al. | 1982
- 2605
-
The effect of varying the polyethylene content and the co-polymer content on crazing in polystyrene—low-density polyethylene blendsSjoerdsma, S. D. / Dekkers, M. E. J. / Heikens, D. et al. | 1982
- 2613
-
Microstructure of vacuum-deposited tin thin filmsDas, V. Damodara et al. | 1982
- 2618
-
Crystallographic effects in metal cuttingWilliams, J. A. / Horne, J. G. et al. | 1982
- 2625
-
Liquid jet impact damage on zinc sulphideVan Der Zwaag, S. / Field, J. E. et al. | 1982
- 2637
-
Sub-eutectoid aged Mg-PSZ alloy with enhanced thermal up-shock resistanceHannink, R. H. J. / Garvie, R. C. et al. | 1982
- 2644
-
Solidification of undercooled cadmium-zinc eutectic meltsOjha, S. N. / Anantharaman, T. R. / Ramachandrarao, P. et al. | 1982
- 2649
-
Diffusion studies of porous materialsClark, J. D. / Robinson, P. J. et al. | 1982
- 2657
-
Single crystal elastic constants of tungsten monocarbideLee, M. / Gilmore, R. S. et al. | 1982
- 2661
-
Phase transformations in the thermotropic liquid crystal polymer: 60/40 PABA/PETViney, C. / Windle, A. H. et al. | 1982
- 2671
-
Microstructure and grain growth in $ Li_{2} $O-$ Al_{2} $$ O_{3} $-$ SiO_{2} $ glass ceramicsChen, Q. Q. / Gai, P. L. / Groves, G. W. et al. | 1982
- 2677
-
Crystallization kinetics of $ Fe_{40} $$ Ni_{38} $$ Mo_{4} $$ B_{18} $ and $ Fe_{80} $$ B_{20} $ metallic glassesCumbrera, F. L. / Miranda, H. / Conde, A. / Márquez, R. / Vigier, P. et al. | 1982
- 2687
-
Study of $ Na_{2} $O-$ SiO_{2} $-$ Fe_{2} $$ O_{2} $-$ Y_{2} $$ O_{3} $ glass by Mössbauer and EPR spectroscopyPrasad, Akhilesh / Bahadur, D. / Singru, R. M. / Chakravorty, D. et al. | 1982
- 2693
-
Discussion of the indentation hardness of a glass-ceramic with participate microstructureMiyata, N. / Jinno, H. et al. | 1982
- 2700
-
Strain softening in an epoxy resinThomson, K. W. / Broutman, L. J. et al. | 1982
- 2709
-
Thermal transformation of hydrated ferric oxide gel and preparation of ultrafine oxideRajendran, S. / Sitakara Rao, V. / Maiti, H. S. et al. | 1982
- 2715
-
Interaction of sodium with simple glassesLau, J. / McMillan, P. W. et al. | 1982
- 2727
-
The characterization of high-strength surface-crystallized glassesAdams, R. / McMillan, P. W. et al. | 1982
- 2736
-
Properties and composition of bredigite-structured phasesMoseley, David / Glasser, F. P. et al. | 1982
- 2741
-
Microstructure of a plasma-sprayed superalloy coating/substrateRitter, Ann M. / Henry, Michael F. et al. | 1982
- 2753
-
Consequence of electron scattering mechanisms on the conductivity of semi-metal filmsDeschacht, D. / Boyer, A. / Groubert, E. / Pichard, C. R. / Tosser, A. T. / Tellier, C. R. et al. | 1982
- 2757
-
Production of strontium-substituted lanthanum manganite perovskite powder by the amorphous citrate processBaythoun, M. S. G. / Sale, F. R. et al. | 1982