Effects of crystallinity of starting carbons on diamond formation in presence of nickel under high pressure and high temperature condition (Englisch)
- Neue Suche nach: Tsuzuki, Akihiro
- Neue Suche nach: Hirano, Shin-Ich
- Neue Suche nach: Naka, Shigeharu
- Neue Suche nach: Tsuzuki, Akihiro
- Neue Suche nach: Hirano, Shin-Ich
- Neue Suche nach: Naka, Shigeharu
In:
Journal of Materials Science
;
19
, 4
; 1153-1158
;
1984
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:Effects of crystallinity of starting carbons on diamond formation in presence of nickel under high pressure and high temperature condition
-
Beteiligte:
-
Erschienen in:Journal of Materials Science ; 19, 4 ; 1153-1158
-
Verlag:
- Neue Suche nach: Kluwer Academic Publishers
- Neue Suche nach: Springer Science + Business Media B.V.
-
Erscheinungsort:Norwell, Mass
-
Erscheinungsdatum:1984
-
ISSN:
-
ZDBID:
-
DOI:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Englisch
- Neue Suche nach: 51.00
- Weitere Informationen zu Basisklassifikation
- Neue Suche nach: 275/5010
-
Schlagwörter:
-
Klassifikation:
-
Datenquelle:
Inhaltsverzeichnis – Band 19, Ausgabe 4
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 1043
-
The status of rapid solidification of alloys in research and applicationJones, H. et al. | 1984
- 1077
-
The preparation and characterization of alumina membranes with ultra-fine poresLeenaars, A. F. M. / Keizer, K. / Burggraaf, A. J. et al. | 1984
- 1089
-
Nitrocarburizing of low-carbon unalloyed steelDannefaer, S. / Dreyer, E. et al. | 1984
- 1089
-
Nitrocarburizing of low-carbon unalloyed steel. IDannefaer, S. / Dreyer, E. et al. | 1984
- 1099
-
Nitrocarburizing of low-carbon unalloyed steel. IIDannefaer, S. / Hogg, B. / Kerr, D. et al. | 1984
- 1109
-
Alkali resistant non-silicate porous glass-like materialWhite, R. W. / Res, M. A. / Hart, S. et al. | 1984
- 1116
-
Craze development and breakdown in PVC during cyclic loadingRimnac, C. M. / Hertzberg, R. W. / Manson, J. A. et al. | 1984
- 1125
-
The fracture of particulate-filled epoxide resinsMoloney, A. C. / Kausch, H. H. / Stieger, H. R. et al. | 1984
- 1131
-
Influence of impurities on the etching of NaCl crystalsSangwal, K. / Zaniewska, G. et al. | 1984
- 1145
-
Mechanism of fracture of short glass fibre-reinforced polyamide thermoplasticSato, Norio / Kurauchi, Toshio / Sato, Shigeyuki / Kamigaito, Osami et al. | 1984
- 1153
-
Effects of crystallinity of starting carbons on diamond formation in presence of nickel under high pressure and high temperature conditionTsuzuki, Akihiro / Hirano, Shin-Ich / Naka, Shigeharu et al. | 1984
- 1159
-
Microhardness and brittle fracture of garnet single crystalsPardavi-Horváth, M. et al. | 1984
- 1171
-
The detailed structure of delamination fracture surfaces in graphite/epoxy laminatesJohannesson, T. / Sjöblom, P. / Seldén, R. et al. | 1984
- 1178
-
Phase equilibria and ordering in the system $ HfO_{2} $-$ Yb_{2} $$ O_{3} $Duran, P. / Pascual, C. et al. | 1984
- 1185
-
Semiconducting behaviour of thin bismuth films vacuum-deposited at different substrate temperaturesDas, V. Damodara / Vaidehi, S. et al. | 1984
- 1191
-
Thermal stability of SiC fibres (Nicalon®)Mah, T. / Hecht, N. L. / McCullum, D. E. / Hoenigman, J. R. / Kim, H. M. / Katz, A. P. / Lipsitt, H. A. et al. | 1984
- 1202
-
Sintering of submicron metallic particlesBlachere, J. R. / Sedehi, A. / Meiksin, Z. H. et al. | 1984
- 1207
-
A study on the photoconductivity of a set of horizontal Bridgman semi-insulating GaAs ingotsJimenez, J. / Gonzalez, M. A. / De Saja, J. A. / Bonnafe, J. et al. | 1984
- 1220
-
Effects of boron addition on a melt-spun Ni-base superalloyHuang, S. C. / Chang, K. M. et al. | 1984
- 1229
-
Reactive processing of titanium carbide with titaniumQuinn, Candace Jo / Kohlstedt, David L. et al. | 1984
- 1251
-
Effect of cold rolling on the superconducting and electronic properties of two amorphous alloys; $ Nb_{50} $$ Zr_{35} $$ Si_{15} $ and $ Nb_{70} $$ Zr_{15} $$ Si_{15} $Inoue, A. / Okamoto, S. / Masumoto, T. / Chen, H. S. et al. | 1984
- 1261
-
Magnetic domain structure of isotropic MnAlC permanent magnet alloysWysłocki, J. J. / Szymura, S. et al. | 1984
- 1261
-
Magnetic domain structure of isotropic MnAIC permanent magnet alloysWysLocki, J.J. / Szymura, S. et al. | 1984
- 1267
-
Elastic anisotropy and the grain size dependence of ceramic fracture energiesRice, R. W. et al. | 1984
- 1272
-
The corrosion resistance of high $ ZrO_{2} $ fusion-cast $ Al_{2} $$ O_{3} $-$ ZrO_{2} $-$ SiO_{2} $ glass refractories in soda lime glassManfredo, L. J. / McNally, R. N. et al. | 1984
- 1277
-
The effects of magnetic quenching on glassy barium ferriteGallacher, D. G. / Richardson, R. T. / Willey, R. J. et al. | 1984
- 1283
-
Oxidation mechanism of porous silicon nitridePorz, F. / Thümmler, F. et al. | 1984
- 1296
-
A surface dislocation model of wearMarcinkowski, M. J. et al. | 1984
- 1307
-
Sinterability, strength and oxidation of alpha silicon carbide powdersDutta, Sunil et al. | 1984
- 1314
-
Kinetics of dissolution of silicon in $ CrO_{3} $-HF-$ H_{2} $O solutionsHeimann, Robert B. et al. | 1984
- 1321
-
Effect of strain, strain rate and temperature on cavity size distribution in a superplastic copper-base alloyRidley, N. / Livesey, D. W. / Mukherjee, A. K. et al. | 1984
- 1333
-
Switching in polystyrene and polymethyl methacrylate thin films: effect of preparation conditions of the polymersSakai, Y. / Sadaoka, Y. / Okada, G. et al. | 1984
- 1339
-
Reaction of Al/Mo thin filmsKitada, Masahiro / Shimizu, Noboru et al. | 1984
- 1343
-
The effect of titanium additions on Ms of beta-CuZnEucken, S. / Hornborgen, E. et al. | 1984
- 1343
-
The effect of titanium additions onMs of β-CuZnEucken, S. / Hornbogen, E. et al. | 1984
- 1349
-
Neutron and X-ray diffraction studies on pure and magnesia-doped zirconia gels decomposed in vacuoBrett, N. H. / Gonzalez, M. / Bouillot, J. / Niepce, J. C. et al. | 1984
- 1359
-
The fracture process of ultra-high strength polyethylene fibresSmook, Jan / Hamersma, Wim / Pennings, Albert J. et al. | 1984
- 1374
-
An investigation of the influence of cold-rolling on the structure factor of a metallic glassGuoan, Wu / Cowlam, N. / Gibbs, M. R. J. et al. | 1984
- 1385
-
Sintering $ LiTaO_{3} $ and $ KTaO_{3} $ with the aid of manganese oxideShimada, Shiro / Kodaira, Kohei / Matsushita, Toru et al. | 1984
- 1385
-
Sintering LiTaO3 und KTaO3 with the aid of manganese oxideShimada, S. / Kodaira, K. / Matsushita, T. et al. | 1984