High temperature acidic stress corrosion of glass fibre composites: Part I Effect of fibre type (Englisch)
- Neue Suche nach: SAPALIDIS, S. N
- Neue Suche nach: HOGG, P. J
- Neue Suche nach: YOUD, S. J
- Neue Suche nach: SAPALIDIS, S. N
- Neue Suche nach: HOGG, P. J
- Neue Suche nach: YOUD, S. J
In:
Journal of Materials Science
;
32
, 2
; 309-316
;
1997
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:High temperature acidic stress corrosion of glass fibre composites: Part I Effect of fibre type
-
Beteiligte:
-
Erschienen in:Journal of Materials Science ; 32, 2 ; 309-316
-
Verlag:
- Neue Suche nach: Kluwer Academic Publishers
- Neue Suche nach: Springer Science + Business Media B.V.
-
Erscheinungsort:Norwell, Mass
-
Erscheinungsdatum:1997
-
ISSN:
-
ZDBID:
-
DOI:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Englisch
- Neue Suche nach: 51.00
- Weitere Informationen zu Basisklassifikation
- Neue Suche nach: 275/5010
-
Schlagwörter:
-
Klassifikation:
-
Datenquelle:
Inhaltsverzeichnis – Band 32, Ausgabe 2
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 279
-
A high-temperature solid-state potentiometric sensor for nitrogen based on ceramic LaAl12O18NWARNER, T. E / FRAY, D. J / DAVIES, A et al. | 1997
- 283
-
A rolling-ball device for producing surface fatigue and its application to dental materialsMcCABE, J. F / ABU KASIM, N. H / CLEARY, S et al. | 1997
- 289
-
Effect of magnesium alloying additions on infiltration threshold pressure and structure of SiC powder compacts infiltrated by aluminium-based meltsCANDAN, E / ATKINSON, H. V / JONES, H et al. | 1997
- 295
-
Processing, microstructure and mechanical properties of hot-pressed SiC continuous fibre/SiC compositesPARK, K / VASILOS, T et al. | 1997
- 301
-
Diffusion of water within an amorphous carbohydrateALDOUS, B. J / FRANKS, F / GREER, A. L et al. | 1997
- 309
-
High temperature acidic stress corrosion of glass fibre composites: Part I Effect of fibre typeSAPALIDIS, S. N / HOGG, P. J / YOUD, S. J et al. | 1997
- 317
-
Thermal shock behaviour of unidirectional silicon carbide fibre reinforced calcium aluminosilicateBLISSETT, M. J / SMITH, P. A / YEOMANS, J. A et al. | 1997
- 327
-
Thermal stability of a PCS-derived SiC fibre with a low oxygen content (Hi-Nicalon)CHOLLON, G / PAILLER, R / NASLAIN, R / LAANANI, F / MONTHIOUX, M / OLRY, P et al. | 1997
- 349
-
Novel aqueous sol–gel preparation and characterization of barium M ferrite, BaFe12O19 fibresPULLAR, R. C / TAYLOR, M. D / BHATTACHARYA, A. K et al. | 1997
- 353
-
Environment sensitive impedance spectroscopy and dc conductivity measurements on NiWO4BHATTACHARYA, A. K / BISWAS, R. G / HARTRIDGE, A et al. | 1997
- 357
-
Microstructural development in copper-interlayer transient liquid phase bonds between martensitic NiAl and NiTiGALE, W. F / GUAN, Y et al. | 1997
- 365
-
Magnetic Co2Y ferrite, Ba2Co2Fe12O22 fibres produced by a blow spun processPULLAR, R. C / TAYLOR, M. D / BHATTACHARYA, A. K et al. | 1997
- 369
-
Extended X-ray absorption fine structure (EXAFS) study of secondary phases in Yb2O3-doped Si3N4 ceramicsKIZLER, P / KLEEBE, H. J / ALDINGER, F / RUHLE, M et al. | 1997
- 375
-
Influence of short-fibre reinforcement on the mechanical and fracture behaviour of polycarbonate/Acylonitrile Butadiene Styrene polymer blendDIN, K. J / HASHEMI, S et al. | 1997
- 389
-
Electrochemical Al2O3–ZrO2 composite coatings on non-oxide ceramic substratesCHAIM, R / ZHITOMIRSKY, I / GAL-OR, L / BESTGEN, H et al. | 1997
- 401
-
Carbon black/high density polyethylene conducting composite materials: Part I Structural modification of a carbon black by gasification in carbon dioxide and the effect on the electrical and mechanical properties of the compositeMATHER, P. J / THOMAS, K. M et al. | 1997
- 409
-
Influence of precursors and synthetic conditions on carbon trapping and related superconducting properties in bulk YBCOWANG, J / MONOT, I / DELAMARE, M. P / DESGARDIN, G et al. | 1997
- 415
-
Varistor properties and microstructure of ZnO–BaO ceramicsFAN, J / FREER, R et al. | 1997
- 421
-
Dynamic behaviour of domains during poling by acoustic emission measurements in La-modified PbTiO3 ferroelectric ceramicsCHOI, D. G / CHOI, S. K et al. | 1997
- 427
-
Fatigue crack growth behaviour of a Si–Mn steel with carbide-free lathy bainiteWENYAN, LIU / JINGXIN, QU / HESHENG, SHAO et al. | 1997
- 431
-
Controlled nucleation and crystallization in Fe2O3–CaO–SiO2 glassLEE, YONG-KEUN / CHOI, SE-YOUNG et al. | 1997
- 437
-
Effect of dynamic strain ageing on the tensile properties of a modified 9Cr–1Mo steelKISHORE, R / SINGH, R. N / SINHA, T. K / KASHYAP, B. P et al. | 1997
- 443
-
Preparation and properties of polypropylene composites reinforced with wheat and flax straw fibes. Part I. Fibre characterizationHornsby, P.R. / Hinrichsen, E. / Tarverdi, K. et al. | 1997
- 443
-
Preparation and properties of polypropylene composites reinforced with wheat and flax straw fibres: Part I Fibre characterizationHORNSBY, P. R / HINRICHSEN, E / TARVERDI, K et al. | 1997
- 451
-
The compressive behaviour of porous copper made by the GASAR processSIMONE, A. E / GIBSON, L. J et al. | 1997
- 459
-
Crystallization of a Bi–Pb–Fe–Cd–O glass under magnetic annealingHU, YI et al. | 1997
- 465
-
Synthesis of high-speed tool steel surfaces on mild steelTAUQIR, A / ZAIGHAM, H / HASHMI, F.H / KHAN, A.Q et al. | 1997
- 469
-
Low pressure injection moulding of SiC platelet reinforced reaction bonded silicon nitrideKOSMAC, T / JANSSEN, R et al. | 1997
- 475
-
Mechanical characterization by dynamical tensile loading of 2017 aluminium alloy joints welded by diffusion bonding. New results and SEM observations of the failure surfacesDEBBOUZ, O / NAVAI, F et al. | 1997
- 483
-
Fracture mechanics of single-fibre pull-out testWANG, CHI et al. | 1997
- 491
-
Properties of hydrogels synthesized by freezing and thawing aqueous polyvinyl alcohol solutions and their applicationsMORI, YOSHIHIRO / TOKURA, HITOSHI / YOSHIKAWA, MASANORI et al. | 1997
- 497
-
Synthesis and characterization of molybdenum disulphide formed from ammonium tetrathiomolybdateWANG, H.W / SKELDON, P / THOMPSON, G.E / WOOD, G.C et al. | 1997
- 503
-
Alumina–mullite–zirconia composites: Part II Microstructural development and tougheningJANG, H. M / CHO, S.M / KIM, K.T et al. | 1997
- 513
-
Tetragonal to monoclinic transformation and microstructural evolution in ZrO2–9.7 mol% MgO during cyclic heating and coolingABE, FUJIO / MUNEKI, SEIICHI / YAGI, KOICHI et al. | 1997
- 523
-
Chemical reactions in mullite matrix SiC whisker reinforced composites in RF plasmaPARK, Y. S / McNALLAN, M. J et al. | 1997
- 529
-
Dielectric properties of vanadium phosphate glasses in a combined electric fieldMIKLOS, P / DOUPOVEC, J et al. | 1997
- 533
-
Recycling effects on microstructure and mechanical behaviour of PEEK short carbon-fibre compositesSARASUA, J. R / POUYET, J et al. | 1997
- 537
-
Microstructure and mechanical properties of a Si3N4/Al2O3 nanocompositeZHU, W. Z / GAO, J. H / DING, Z. S et al. | 1997
- 543
-
Characterization of the whisker–matrix interfacial reactions in K2O·6TiO2 whisker-reinforced aluminium matrix compositesLI, J. H / NING, X. G / YE, H. Q / PAN, J / FUKUNAGA, H et al. | 1997
- 549
-
Double yield points in triblends of LDPE, LLDPE and EPDMPLAZA, A. R / RAMOS, E / MANZUR, A / OLAYO, R / ESCOBAR, A et al. | 1997