On the mechanism of intergranular stress corrosion cracking of sensitized stainless steel in tetrathionate solution (Englisch)
- Neue Suche nach: Yonezu, Akio
- Neue Suche nach: Kusano, Ryota
- Neue Suche nach: Chen, Xi
- Neue Suche nach: Yonezu, Akio
- Neue Suche nach: Kusano, Ryota
- Neue Suche nach: Chen, Xi
In:
Journal of Materials Science
;
48
, 6
; 2447-2453
;
2012
-
ISSN:
- Aufsatz (Zeitschrift) / Print
-
Titel:On the mechanism of intergranular stress corrosion cracking of sensitized stainless steel in tetrathionate solution
-
Beteiligte:
-
Erschienen in:Journal of Materials Science ; 48, 6 ; 2447-2453
-
Verlag:
- Neue Suche nach: Springer US
- Neue Suche nach: Springer Science + Business Media B.V.
-
Erscheinungsort:Norwell, Mass
-
Erscheinungsdatum:2012
-
ISSN:
-
ZDBID:
-
DOI:
-
Medientyp:Aufsatz (Zeitschrift)
-
Format:Print
-
Sprache:Englisch
- Neue Suche nach: 51.00
- Weitere Informationen zu Basisklassifikation
- Neue Suche nach: 275/5010
-
Schlagwörter:
-
Klassifikation:
-
Datenquelle:
Inhaltsverzeichnis – Band 48, Ausgabe 6
Zeige alle Jahrgänge und Ausgaben
Die Inhaltsverzeichnisse werden automatisch erzeugt und basieren auf den im Index des TIB-Portals verfügbaren Einzelnachweisen der enthaltenen Beiträge. Die Anzeige der Inhaltsverzeichnisse kann daher unvollständig oder lückenhaft sein.
- 2299
-
Magnetic properties of multicore magnetite nanoparticles prepared by glass crystallisationWorsch, Christian / Büttner, Markus / Schaaf, Peter / Harizanova, Ruzha / Rüssel, Christian / Schmidl, Frank / Seidel, Paul et al. | 2012
- 2308
-
Fabrication and characterizations of PCDTBT: PC71BM bulk heterojunction solar cell using air brush coating methodKannappan, Santhakumar / Palanisamy, Kumar / Tatsugi, Jiro / Shin, Paik-Kyun / Ochiai, Shizuyasu et al. | 2012
- 2318
-
The coupling effects of thermal cycling and high current density on Sn58Bi solder jointsZuo, Yong / Ma, Limin / Liu, Sihan / Wang, Ting / Guo, Fu / Wang, Xitao et al. | 2012
- 2326
-
β-Crystal in the iPP melt encapsulated by transcrystallinity and spherulites: effect of molecular weightLiang, Yanyan / Zheng, Guoqiang / Liu, Shuangyang / Dai, Kun / Liu, Chuntai / Chen, Jingbo / Shen, Changyu et al. | 2012
- 2334
-
Meso-scale deformation and damage in thermally bonded nonwovensFarukh, Farukh / Demirci, Emrah / Acar, Memiş / Pourdeyhimi, Behnam / Silberschmidt, Vadim V. et al. | 2012
- 2346
-
Albumin nanoparticle-coated carbon composite electrode for electrical double-layer biosupercapacitor applicationsSattarahmady, N. / Parsa, A. / Heli, H. et al. | 2012
- 2352
-
One-step synthesis of yellow-emitting carbogenic dots toward white light-emitting diodesChen, Qiao-Ling / Wang, Cai-Feng / Chen, Su et al. | 2012
- 2358
-
Morphological syntheses of ZnO nanostructures under microwave irradiationShen, Xiaoping / Sun, Jiquan / Zhu, Guoxing / Ji, Zhenyuan / Chen, Zhixin / Li, Niya et al. | 2012
- 2365
-
Facile synthesis of water-soluble and superparamagnetic Fe3O4 dots through a polyol-hydrolysis routeJiang, Pin / Yang, Xi / Xin, Ying / Qi, Yongxin / Ma, Xicheng / Li, Qian / Zhang, Zhaoliang et al. | 2012
- 2370
-
Hardness and density profile of surface densified and thermally modified Scots pine in relation to degree of densificationRautkari, Lauri / Laine, Kristiina / Kutnar, Andreja / Medved, Sergej / Hughes, Mark et al. | 2012
- 2376
-
Effect of annealing twins on crack initiation under high cycle fatigue conditionsCastelluccio, Gustavo M. / McDowell, David L. et al. | 2012
- 2388
-
Densification behavior and mechanical properties of spark plasma-sintered ZrC–TiC and ZrC–TiC–CNT compositesAcicbe, Ramazan Burak / Goller, Gultekin et al. | 2012
- 2394
-
Characterization of the cure shrinkage, reaction kinetics, bulk modulus and thermal conductivity of thermoset resin from a single experimentNawab, Yasir / Casari, Pascal / Boyard, Nicolas / Jacquemin, Frédéric et al. | 2012
- 2404
-
Effect of the size and dispersion of precipitates formed in hot rolling on recrystallization texture in ferritic stainless steelsGao, Fei / Liu, Zhen-Yu / Wang, Guo-Dong et al. | 2012
- 2416
-
Graphene-reinforced epoxy resin with enhanced atomic oxygen erosion resistanceZhang, Wen / Yi, Min / Shen, Zhigang / Zhao, Xiaohu / Zhang, Xiaojing / Ma, Shulin et al. | 2012
- 2424
-
Cystine-capped CdSe@ZnS nanocomposites: mechanochemical synthesis, properties, and the role of capping agentBaláž, Matej / Baláž, Peter / Tjuliev, Georgi / Zubrík, Anton / Sayagués, María Jesús / Zorkovská, Anna / Kostova, Nina et al. | 2012
- 2433
-
Investigations on photo and electrically switchable asymmetric bent-core liquid crystalsVijay Srinivasan, Murugesan / Kannan, Palaninathan / Roy, Arun et al. | 2012
- 2447
-
On the mechanism of intergranular stress corrosion cracking of sensitized stainless steel in tetrathionate solutionYonezu, Akio / Kusano, Ryota / Chen, Xi et al. | 2012
- 2454
-
Finite element analysis of plastic deformation in variable lead axisymmetric forward spiral extrusionFarhoumand, A. / Hodgson, P. D. / Khoddam, S. et al. | 2012
- 2462
-
Modelling the deformation of a confectionery wafer as a non-uniform sandwich structureMohammed, I. K. / Charalambides, M. N. / Williams, J. G. / Rasburn, J. et al. | 2012
- 2479
-
Analysing the growth of intermetallic compounds in lead-free solder joints by differential scanning calorimetry measurementsSchreck, Timo / Schnorpfeil, Anna / Kaloudis, Michael et al. | 2012
- 2485
-
The effect of ball-milling treatment of original powders on the sintering process and critical current density of graphite-doped MgB2 bulksJiang, Hua / Ma, Zongqing / Liu, Yongchang / Dong, Zhizhong / Yu, Liming / Cai, Qi / Wang, Rui et al. | 2012
- 2490
-
Electrochemical performance of steel in cement extract and bulk matrix properties of cement paste in the presence of Pluronic 123 micellesKoleva, D. A. / Denkova, A. G. / Boshkov, N. / Breugel, K. et al. | 2012
- 2504
-
Effect of nano-Calcium Carbonate on microcellular foaming of polypropyleneDing, Jie / Ma, Weihua / Song, Fujiao / Zhong, Qin et al. | 2012
- 2512
-
Different types of MnO2 recovered from spent LiMn2O4 batteries and their application in electrochemical capacitorsYang, Zeheng / Mei, Zhousheng / Xu, Feifei / Yao, Yunjin / Zhang, Weixin / Qi, Wencong / Song, Qiuli / Gao, Zhuwei / Zhao, Tuan et al. | 2012
- 2520
-
Synthesis, characterization, and biological activities of organosoluble and thermally stable xanthone-based polyamidesMansour lakouraj, Moslem / Rahpaima, Ghasem / Mohseni, Seyed Mojtaba et al. | 2012
- 2530
-
Preparation and characterization of in situ polymerized cyclic butylene terephthalate/graphene nanocompositesBalogh, Gábor / Hajba, Sándor / Karger-Kocsis, József / Czigány, Tibor et al. | 2012
- 2536
-
Infrared and microwave shielding of transparent Al-doped ZnO superlattice grown via atomic layer depositionFernandes, Gustavo E. / Lee, Do-Joong / Kim, Jin Ho / Kim, Ki-Bum / Xu, Jimmy et al. | 2012
- 2543
-
Large scale synthesis of single-crystal and polycrystalline boron nitride nanosheetsSajjad, Muhammad / Ahmadi, Majid / Guinel, Maxime J-F / Lin, Yi / Feng, Peter et al. | 2012
- 2550
-
Synthesis of silica-coated aqueous ferrofluids through ligand exchange with a new organosilica precursorArizaga, Ana / Millán, Angel / Schubert, Ulrich / Palacio, Fernando et al. | 2012
- 2557
-
Electrospinning preparation of LaOBr:Tb3+ nanostructures and their photoluminescence propertiesMa, Wenwen / Dong, Xiangting / Wang, Jinxian / Yu, Wensheng / Liu, Guixia et al. | 2012
- 2566
-
Electrodeposition of platinum nanoparticles on polypyrrole-functionalized grapheneZhao, Wengao / Zhou, Xibin / Xue, Zhonghua / Wu, Bowan / Liu, Xiuhui / Lu, Xiaoquan et al. | 2012
- 2574
-
Effect of solute interaction on interfacial segregation and grain boundary embrittlement in binary alloysLejček, Pavel et al. | 2012
- 2581
-
Reaction of tantalum oxide with calcium chloride–calcium oxide meltsBarnett, R. P. / Fray, D. J. et al. | 2012
- 2590
-
Pb2B5O9Cl: a chloride borate with second harmonic generation effectChen, Zhaohui / Pan, Shilie / Yang, Zhihua / Dong, Xiaoyu / Su, Xin / Yang, Yun et al. | 2012
- 2597
-
Thermomechanical environment characterisation in injection moulding and its relation to the mechanical properties of talc-filled polypropyleneBarbosa, Carlos N. / Simoes, Ricardo / Franzen, Markus / Viana, Júlio C. et al. | 2012
- 2608
-
Effect of peritectic reaction on the migration of secondary dendrite arms in the presence of tertiary dendrites: analysis of a directionally solidified Sn–36 at.%Ni peritectic alloyPeng, Peng / Li, Xinzhong / Su, Yanqing / Liu, Dongmei / Guo, Jingjie / Fu, Hengzhi et al. | 2012
- 2618
-
Structural, optical, and magnetic characterization of Co and N co-doped ZnO nanopowdersKumar, Sanjeev / Chen, C. L. / Dong, C. L. / Ho, Y. K. / Lee, J. F. / Chan, T. S. / Thangavel, R. / Chen, T. K. / Mok, B. H. / Rao, S. M. et al. | 2012
- 2624
-
Effects of tool positioning on joint interface microstructure and fracture strength of friction stir lap Al-to-steel weldsChen, Z. W. / Yazdanian, S. / Littlefair, G. et al. | 2012
- 2635
-
Superplastic behavior and microstructural stability of friction stir processed AZ91C alloyJain, Vipin / Mishra, Rajiv S. / Gouthama et al. | 2012
- 2647
-
Theoretical study on the structure and stability of aluminum hydride (Al n H3n ) clustersXu, Bo / Liu, Jiping / Zhao, Lili / Yan, Lili et al. | 2012
- 2659
-
Transient and steady state creep of age-hardenable Al–5 wt% Mg alloy during superimposed torsional oscillationsAbd El-Rehim, A. F. / Mahmoud, M. A. et al. | 2012
- 2670
-
Metal nanoparticle templating and electrocatalytic modification using functionalized graphene sheetsPonce, A. A. / Sims, C. M. / Liu, Z. / Gaskell, K. J. / Lai, L.-C. / Chiou, W.-A. / Eichhorn, B. W. et al. | 2012
- 2681
-
Interface characterization and thermal degradation of ferrite/poly(vinylidene fluoride) multiferroic nanocompositesMartins, P. / Costa, C. M. / Benelmekki, M. / Botelho, G. / Lanceros-Méndez, S. et al. | 2012
- 2690
-
Preparation and properties of nanofiber-coated composite membranes as battery separators via electrospinningAlcoutlabi, Mataz / Lee, Hun / Watson, Jill V. / Zhang, Xiangwu et al. | 2012
- 2701
-
Growth mechanism of one-dimensional zinc sulfide nanostructures through electrophoretic depositionVázquez, Alejandro / López, Israel A. / Gómez, Idalia et al. | 2012
- 2705
-
Effect of synthesis methods for mesoporous zirconia on its structural and textural propertiesMokhtar, Mohamed / Basahel, Sulaiman N. / Ali, Tarek T. et al. | 2012
- 2714
-
Microstructural characterization of Co-based coating deposited by low power pulse laser claddingFarnia, A. / Malek Ghaini, F. / Ocelík, V. / Hosson, J. Th. M. et al. | 2012
- 2724
-
Microstructural variation and high-speed impact responses of Sn–3.0Ag–0.5Cu/ENEPIG solder joints with ultra-thin Ni–P depositHo, Cheng-Ying / Duh, Jenq-Gong / Lin, Chih-Wei / Lin, Chun-Jen / Wu, Yu-Hui / Hong, Huei-Cheng / Wang, Te-Hui et al. | 2012
- 2733
-
Porous nanocrystalline TiO2 with high lithium-ion insertion performanceWang, Jie / Zhou, Yingke / Hu, Yuanyuan / O’Hayre, Ryan / Shao, Zongping et al. | 2012