Materials Science & Engineering A: Structural Materials: Properties, Microstructure and Processing
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
Table of contents
- 6
-
Production and properties of light-metal-based amorphous alloysInoue, A. / Masumoto, T. et al. | 1991
- 10
-
Interrelations between electronic and ionic structures in metallic glassesHäussler, P. et al. | 1991
- 16
-
Grain refinement in rapidly solidified alloysGreer, A.L. et al. | 1991
- 22
-
Recent studies of chemical properties of amorphous alloysHashimoto, K. / Kumagai, N. / Yoshioka, H. et al. | 1991
- 26
-
The structure of amorphous and nanocrystalline metals and alloysWagner, C.N.J. / Boldrick, M.S. et al. | 1991
- 33
-
Modelling of growth and microstructure selection in rapid solidification: a progress reportJones, H. et al. | 1991
- 40
-
Atomic dynamics of metallic glasses and icosahedral alloys (quasicrystals)Suck, J.B. et al. | 1991
- 45
-
Influence of conduction electrons on tunneling states in amorphous metalsWeiss, G. et al. | 1991
- 51
-
Thermal properties of amorphous metalsLöhneysen, H. v. et al. | 1991
- 59
-
Electron transport properties of pseudo-binary amorphous transition metal-simple metal (Al) alloysStephens, T.A. / Rathnayaka, D. / Naugle, D.G. et al. | 1991
- 63
-
Electronic transport properties of Ni-Ta metallic glassesRichmond, T. / Rohr, L. / Reimann, P. et al. | 1991
- 67
-
Evidende for failure of the Faber-Ziman theory and application of Edwards' self-consistent Green function theory to the electron transport in sp-electron amorphous and quasicrystalline metalsItoh, M. / Ishida, A. / Nagata, T. et al. | 1991
- 72
-
The Faber-Ziman resistivity of amorphous Mg(x)Zn(1-x)From, M. / Muir, W.B. et al. | 1991
- 76
-
Hall effect in Ni-based amorphous alloysIvkov, J. / Babic, E. / Liebermann, H.H. et al. | 1991
- 80
-
Effect of the broadening of the spectral distribution on the hall coefficient of amorphous metalsItoh, M. / Ishida, A. / Nagata, T. et al. | 1991
- 85
-
Strong depression of Tc insuperconducting disordererd Cu50Zr50 with dilute magnetic impuritiesNordström, A. / Hedman, L. / Rapp, Ö. et al. | 1991
- 90
-
Limits to weak localization in Ca70Mg(30-x)Al(x)Baxter, D.V. / Fadnis, A.N. / Sahnoune, A. et al. | 1991
- 94
-
Electrical resistivities of stable quasicrystalsKimura, K. / Kishi, K. / Hashimoto, T. et al. | 1991
- 98
-
Temperature dependence of magnetoresistive of amorphous Fe80-(x)V(x)B14Si6Jen, S.U. / Lin, S.T. et al. | 1991
- 101
-
On the resistivity minimum in metallic glassesGupta, A. / Gupta, R. / Lal, S. et al. | 1991
- 104
-
D-wave phase shift of Cu-Zr metallic glass system under pressureHan, S.H. / Jin, R.Y. / Shen, B.G. et al. | 1991
- 107
-
Systematics in the electronic structure of amorphous transition metal/tin alloysBoyen, H.G. / Indlekofer, G. / Oelhafen, P. et al. | 1991
- 111
-
Electronic structure and transport properties of sp-electron quasicrystals in comparison with the Frank-Kasper crystals and amorphous alloysMizutani, U. / Kamiya, A. / Matsuda, T. et al. | 1991
- 115
-
Electronic structure of Mg(x)Zn100-(x), Zn(x)Ca100-(x), and Ca13Mg87 metallic glasses (x about 30, 50, 70)Häussler, P. / Zehringer, R. / Oelhafen, P. et al. | 1991
- 120
-
Electronic structure of disordered bismuth allyos: a comparison of the amorphous with the liquid stateHäussler, P. / Indlekofer, G. / Boyen, H.G. et al. | 1991
- 124
-
Comparison between electrical resistivity and magnetic anisotropy in a partially crystallited Fe78B13Si9 amorphous alloyAllia, P. / Baricco, M. / Vinai, F. et al. | 1991
- 127
-
High Tc superconductors prepared by rapid quenching and directional annealingYamamoto, T. / Stubicar, M. / Chan, S.K. et al. | 1991
- 132
-
Induced anisotropy and magnetostriction in Co70.4Fe4.6Si15B10Severino, A.M. / Santos, A.D. / Missell, F.P. et al. | 1991
- 136
-
Correlation between domain structure and permeability under stress in metallic glasses with induced anisotropySiemko, A. / Fink-Finowicki, J. / Slawska-Waniewska, A. et al. | 1991
- 140
-
Reversible and irreversible domain wall movement in Metglas amorphous ribbonsIrvine, J.T.S. / Amano, E. / Valenzuela, R. et al. | 1991
- 143
-
High coercivities in mechanically alloyed Sm-Fe-X magnetsSchultz, L. / Schnitzke, K. / Wecker, J. et al. | 1991
- 147
-
High coercivity in Sm-Fe-Ti alloys by rapid solidificationWecker, J. / Katter, M. / Schultz, L. et al. | 1991
- 151
-
Comparison of melt-spin Nd4Fe77B19 with neodymium-rich isotropic permanent magnetsMüller, K.H. / Schneider, J. / Handstein, A. et al. | 1991
- 154
-
Magnetic properties of melt-spin (Y(1-x)Sm(x))0.6Zr0.4Fe2.9Katter, M. / Wecker, J. / Schultz, L. et al. | 1991
- 158
-
The fabrication of fine metallic fibers by continuous melt-extraction and their magnetic and mechanical propertiesRudkowski, P. / Rudkowska, G. / Strom-Olsen, J.O. et al. | 1991
- 162
-
Magnetic moment, Curie temperature, and coercive field for amorphous (Fe(1-x)Nd(x)81.5B18.5 alloysShen Bao-gen / Zhang Jun-xian / Yang Lin-yuan et al. | 1991
- 165
-
Magnetic properties and crystallization of amorphous Co(100-x-y)B(x)Zr(y) alloysShen Bao-gen / Guo Hui-qun / Yang Lin-yuan et al. | 1991
- 169
-
Evidence for the reversible structural transformation in amorphous Fe18Co72Zr10Xu Ru-feng / Guo Hui-qun / Shen Bao-gen et al. | 1991
- 172
-
Magnetic properties and grain structure of nanocrystalline Fe73.5Cu1Nb3Si13.5B9 alloyGawior, W. / Kolano, R. / Wojcik, N. et al. | 1991
- 176
-
Magnetic properties of Fe-Cr-M-Si-B (M = Cr, V, Mo, Nb, Ta, W) alloysYoshizawa, Y. / Yamauchi, K. et al. | 1991
- 180
-
Displaced hysteresis loops of cobalt-based amorphous alloysYamauchi, K. / Yoshizawa, Y. et al. | 1991
- 184
-
Saturation magnetostriction of amorphous tapes with lambda s > 0 and lambda s about 0 after relaxation by conventional and rapid dynamic current annealingEscobar, M.A. / Yavari, A.R. / Lacheisserie, E.T. de et al. | 1991
- 188
-
Effects of crystallization on magnetic domain structure of amorphous Fe78B13Si9 alloyBhatti, A.R. et al. | 1991
- 192
-
Distinction of different types of pinning centers in metallic glassesHorvat, J. / Babic, E. / Marohnic, Z. et al. | 1991
- 196
-
Magnetic susceptibility and DSC study of the crystallization of melt-quenched Ni-P amorphous alloysWachtel, E. / Bakonyi, I. / Bahle, J. et al. | 1991
- 200
-
Effect of antiferromagnetically coupled species on Curie temperature during relaxation of metallic glassesTarnoczi, T. et al. | 1991
- 204
-
Effect of thickness on texture and magnetic properties of meltspun Fe6.5wt.%Si ribbonsPott-Langemeyer, M. / Riehemann, W. / Heye, W. et al. | 1991
- 209
-
High frequency magnetic properties of an amorphous Fe78B13Si9 ribbon improved by a.c. Joule heatingDer-Ray Huang / Li, J.C.M. et al. | 1991
- 213
-
Magnetic properties of planar flow cast amorphous Fe78B13(Si,Cr,Mo)9 and Fe82B12(Si,Cr)6 alloysBudurov, S. / Kovatchev, P. / Toncheva, S. et al. | 1991
- 216
-
Magnetic properties of amorphous (Fe(1-x)Ni(x))75Si10B15 alloysKyeong-Sup Kim / Joo-II Lee / Seong-Cho Yu et al. | 1991
- 220
-
Influence of magnetothermal treatment of magnetomechanical coupling in Fe79Cr6.6B14.4 metallic glassKaczkowski, Z. / Kisdi-Koszo, E. / Potocky, L. et al. | 1991
- 223
-
Magnetomechanical coupling and Delta E effect in Fe80.2Cr2Si3.8B14 metallic glassDuhaj, P. / Kaczkowski, Z. et al. | 1991
- 226
-
Magnetic clusters in melt-spun La-Fe alloysKondo, S. / Kita, E. / Siratori, K. et al. | 1991
- 229
-
Magnetic properties of amorphous (Fe(x)Ni100-(x))100-(y)(Si30B70)y alloysIlonca, G. / Botezan, N. et al. | 1991
- 232
-
Effect of flash- and furnace annealing on the magnetic and mechanical properties of metallic glassesKulik, T. / Matyja, H. et al. | 1991
- 236
-
Effect of ribbon dimensions on the magnetic properties of metallic glassesKulik, T. / Latuszkiewicz, J. / Matyja, H. et al. | 1991
- 241
-
Structural and magnetic properties of rapidly quenched Bi-Mn alloysLakshmi, C.S. / Smith, R.W. et al. | 1991
- 245
-
Magnetic properties of Co-Y amorphous alloys prepared by millingFukamichi, K. / Goto, T. / Fukunaga, T. et al. | 1991
- 248
-
Clustering in TM-M-B metallic glassesLovas, A. / Kisdi-Koszo, E. / Zsoldos, E. et al. | 1991
- 252
-
Correlation between the structure and the magnetic properties of Gd4Me3 metallic glasses (Me = Al, Cu)Petkov, V. / Skumryev, V. / Apostolov, A. et al. | 1991
- 256
-
Processing, structure and performance of RS 'classical' silver-base brazing alloysRabinkin, A. / Reidinger, F. / Marti, J. et al. | 1991
- 261
-
Calculation of the shear modulus properties of amorphous alloysKnuyt, G. / Stals, L.M. / De Schepper, L. et al. | 1991
- 265
-
The microstructure and properties of water atomized and extruded Cu-Cr alloy powdersCorreia, J.B. / Davies, H.A. / Sellars, C.M. et al. | 1991
- 270
-
Extrusion and swaging of rapidly quenched aluminium powders: microstructure and mechanical propertiesHodiamont, S. / Peters, M. / Bunk, W. et al. | 1991
- 274
-
The effects of aging on the properties of a rapidly solidified Al-Li-Mg-Zr alloysYu Gui-fu / Zhang Shao-qing / Feng Yu-shu et al. | 1991
- 279
-
Microstructure and mechanical properties of melt atomized and rapidly solidified ultrahigh boron alloy steelsFrommeyer, G. / Giegel, U. / Speis, H.J. et al. | 1991
- 284
-
Property enhancement in Type 316L stainless steel by spray formingIbrahim Ücok / Teiichi Ando / Grant, N.J. et al. | 1991
- 288
-
New heat resistant tool materials produced from devitrified amorphous Fe-Cr-Mo-C-B and Fe-Cr-Mo-C-V powdersArnberg, L. / Larsson, E. / Savage, S. et al. | 1991
- 292
-
Mechanical properties of Fe-4.5-6.5wt.%Si double roller ribbonsSeifert, H. / Jurisch, M. / Tobisch, J. et al. | 1991
- 297
-
Structural and mechanical properties of spray formed cast-ironEbalard, S. / Cohen, M. et al. | 1991
- 301
-
Effect of preparation technique and atmosphere on the mechanical properties of bulk amorphous alloy compactesTakagi, M. / Kawamura, Y. / Saka, H. et al. | 1991
- 307
-
Characterization and properties of new shape memory alloys in the Ni-Fe-Al systemWallin, M. / Johansson, P. / Savage, S. et al. | 1991
- 312
-
Hydrogen in titanium-based metallic glassesMenzel, D. / Niklas, A. / Köster, U. et al. | 1991
- 316
-
Amorphization of intermetallic compounds by hydrogen absorptionAoki, K. / Li.X.G. / Aihara, T. et al. | 1991
- 321
-
Elastic properties of nickel-based metallic glassesKursumovic, A. / Babic, E. / Liebermann, H.H. et al. | 1991
- 326
-
Mechanical and magnetic relaxation in ferromagnetic amorphous ribbonsBeatrice, C. / Vinai, F. / Allia, P. et al. | 1991
- 328
-
Thermally induced restoration of the ductility of brittle amorphous alloysSchimansky, F.P. / Gerling, R. / Wagner, R. et al. | 1991
- 332
-
Cyclic deformation and tribological behavior of an amorphous iron-based alloy filmImura, T. / Hasegawa, K. / Moori, M. et al. | 1991
- 337
-
Determination of the attempt frequency for relaxation phenomena in amorphous metalsDe Ceuninck, W. / Knuyt, G. / Stulens, H. et al. | 1991
- 342
-
How to use calorimetry to distinguish a microcrystalline structure from an amorphous structureChen, L.C. / Spaepen, F. et al. | 1991
- 346
-
Crystallization in amorphous NiZr2, studied by HRTEMBeeli, C. / Nissen, H.U. / Jiang, Q. et al. | 1991
- 353
-
Comparison dependence of thermal stability and crystallization behavior of Ni24(Zr-M)76 amorphous alloysGhosh, G. / Delaey, L. et al. | 1991
- 359
-
Crystallization kinetics of amorphous Cu-Ni-P alloysAdlwarth-Dieball, R. / Ryder, P.L. et al. | 1991
- 363
-
The effect of hydrostatic pressure on the surface crystallization of amorphous ribbonsSlawska-Waniewska, A. / Witek, A. / Reich, A. et al. | 1991
- 367
-
Crystallization of amorphous Al85Ni10Ce5 alloyCochrane, R.F. / Schumacher, P. / Greer, A.L. et al. | 1991
- 371
-
Crystallization of hydrogen-containing Co33Zr67: an internal friction studySinning, H.R. / Nicolaus, M.M. / Haessner, F. et al. | 1991
- 375
-
Kinetics of surface crystallization in the metallic glass Fe78Si9B13Gupta, A. / Habibi, S. et al. | 1991
- 379
-
Crystallization and stability of pseudo-binary amorphous transition metal-simple metal alloysPan, R. / Hays, C.C. / Naugle, D.G. et al. | 1991
- 383
-
About the Al-Cu-Fe isosahedral phase formationFaudot, F. / Quivy, A. / Calvayrac, Y. et al. | 1991
- 388
-
Decomposition of the isosahedral phase in Al-Cu-Fe alloysWei Liu / Köster, U. et al. | 1991
- 393
-
Quasicrystal formation and phase transitions by ball millingEckert, J. / Schultz, L. / Urban, K. et al. | 1991
- 398
-
The study of phase transformations in nanocrystalline materialsDuhaj, P. / Svec, P. / Janickovic, D. et al. | 1991
- 401
-
Diffusion and structural-relaxation mechanisms in metallic glassesKronmüller, H. / Frank, W. / Hörner, A. et al. | 1991
- 403
-
Structural relaxation and the glass transition in a metallic glassStröm-Olsen, J.O. / Ryan, D.H. / Altounian, Z. et al. | 1991
- 415
-
Indiffusion of cobalt in amorphous Co-ZrAaen Andersen, L.U. / Bottiger, J. / Janting, J. et al. | 1991
- 418
-
Glass transition and viscous flow behaviour of amorphous Fe-M-P (M = Cr, V or Mo) alloysWha-Nam Myung / Sun-Joo Yang / Hyun-Goo Kim et al. | 1991
- 423
-
Molecular-dynamics study of the glass transition in Ni80P20Lewis, L.J. et al. | 1991
- 427
-
Comparison between the melting and the crystal-to-glass transitionFecht, H.J. / Johnson, W.L. et al. | 1991
- 431
-
Chemical ordering in undercooled Cr40Ti60 beta-phasesBlatter, A. / Bührer, W. et al. | 1991
- 434
-
Thermodynamic properties of supercooled compound forming liquid alloysSommer, F. et al. | 1991
- 438
-
Thermodynamic constraints on non-equilibrium solidification of ordered intermetallic compoundsBoettinger, W.J. et al. | 1991
- 443
-
Free energy functions of undercooled liquid glas-forming Au-Pb-Sb alloysFecht, H.J. et al. | 1991
- 448
-
Influence of planar flow casting conditions on the thermal stability and Curie points of amorphous Fe79B14Si7 alloysBudurov, S. / Lazarova, M. / Stephani, G. et al. | 1991
- 452
-
The glass-forming region in the Ni-P system and thermal stability of the glasses obtainedBudurov, S. / Fotty, V. / Toncheva, S. et al. | 1991
- 455
-
The glass-forming ability in the ternary Ni-Co-P and Ni-Cu-P systemsBudurov, S. / Fotty, V. / Toncheva, S. et al. | 1991
- 458
-
Crystallization of amorphous Cu-Ni-Si-B alloysSchaefer, F. / Ryder, P.L. et al. | 1991
- 462
-
Investigation of the thermal stability and crystallization process of amorphous Hf0.67T0.33-(x)M(x) alloys, with T = Co or Ni, M = P or Si, by DSC, DTA and X-ray diffraction techniquesJansson, K. / Nygren, M. et al. | 1991
- 468
-
A metastable b.c.c. phase and its decomposition behavior in rapidly solidified Ni-10at.10%Zr and Ni-8at.%Zr-1at.%X alloysGhosh, G. / Chen, F.R. / Chandrasekaran, M. et al. | 1991
- 475
-
Effect of cobalt on the crystallization of Ni50Zr50 amorphous alloysCziraki, A. / Kastovszky, Z. / Gerös, I. et al. | 1991
- 479
-
Isothermal crystallization of amorphous Fe78B13Si9Jen, S.U. et al. | 1991
- 482
-
X-ray study of the crystallization processes in amorphous (Zr0.64Ni0.36)(1-x)Al(x) alloysBruton, W.D. / Callaway, T.O. / Langley, R.H. et al. | 1991
- 486
-
Influence of germanium-clustering on the precipitation behaviour of rapidly solidified Al-Ge solid solutionsSchmücker, M. / Köster, U. et al. | 1991
- 490
-
Thermal and structural investigation of the devitrification of the melt-spun Fe-Nd-B alloysAnimesh Jha / Buckley, R.A. / Davies, H.A. et al. | 1991
- 495
-
The role of X on the properties of Fe-X-B-Si metallic glassesRamanan, V.R.V. et al. | 1991
- 500
-
Activation energies for crystal nucleation and growth in amorphous alloysLu, K. / Wang, J.T. et al. | 1991
- 504
-
A new crystallization micromechanism for amorphous alloysLu, K. / Wang, J.T. et al. | 1991
- 509
-
Electron microscope studies of phase transformations in rapidly solidified MnBi alloysGuo, Y. / Zaluska, A. / Altounian, Z. et al. | 1991
- 513
-
Crystallization characteristics and viscous flow behavior of WC/amorphous Ni73Si10B17 metal matrix compositesWha-Nam Myung / Sun-Joo Yang / Hyun-Goo Kim et al. | 1991
- 518
-
Direct evidence of two different structural relaxation processes in amorphous FeNiCrPBSietsma, J. / Baricco.M. et al. | 1991
- 523
-
Structural relaxation of Pd82Si18 and Cu53.5Zr44.3Nb2.2 glassy systemsKubicar, L. / Spisiak, J. / Duhaj, P. et al. | 1991
- 526
-
Glass and Curie temperatures of metallic glassesTsai, C.L. et al. | 1991
- 529
-
Study of the structural relaxation of Pd82Si18) metallix glass by thermal expansion and viscous flow measurementsStojanova, L. / Russew, K. / Illekova, E. et al. | 1991
- 532
-
Viscous flow, thermal expansion and phase separation of Fe40Ni40Si6B14 amorphous alloyRussew, K. / Stojanova, L. / Lovas, A. et al. | 1991
- 535
-
The influence of quenching temperature on the structure and properties of amorphous alloysManov, V.P. / Popel, S.I. / Buler, P.I. et al. | 1991
- 541
-
The measurement of very early low-temperature relaxation in the amorphous system Fe(40)Ni(40)Si(14)B(6)Girt, E. / Knezevic, G. / Baltic, R. et al. | 1991
- 544
-
Relaxation in amorphous materials: A new approachPocsik, I. et al. | 1991
- 547
-
Anisotropic (CoFeNi)78(SiB)22 glasses: rheology and relaxation analysisKuhnast, F.A. / Aharoune, A. / Cunat, C. et al. | 1991
- 551
-
Solid state amorphization of RE-TM (RE = Ce, Er and Tm = Fe, Co) multilayersMatsuura, M. / Petkie, R. / Singco, G. et al. | 1991
- 555
-
Thermal properties of nanocrystalline and amorphous Fe-B alloys made by mechanical alloyingCalka, A. / Radlinski, A.P. / Shanks, R. et al. | 1991
- 560
-
Some peculiarities of the atomic structure of metallic phases formed during liquid quenching and solid state reactionsSkakov, Y.A. / Djakonova, N.P. / Edneral, N.V. et al. | 1991
- 565
-
Differential thermal analysis of hydrogen-induced amorphization in C15 Laves compounds GdM2 (M = Fe, Co, Ni)Aoki, K. / Li, X.G. / Masumoto, T. et al. | 1991
- 569
-
Undercooling experiments on quasicrystal-forming meltsEbalard, S. / Spaepen, F. / Cochrane, R.F. et al. | 1991
- 574
-
Rapid solidification of Ag-Cu and Ag-Pb alloysJacobson, N. et al. | 1991
- 577
-
Solid-liquid interfacial free energyGranasy, L. / Tegze, M. / Ludwig, A. et al. | 1991
- 581
-
Test of the adiabatic nucleation model in metallic glassesBarros Brasil, V. de / Meyer, E. et al. | 1991
- 584
-
An experimental study of thermodynamic properties in a ZBLAN glass-forming systemBattezzati, L. / Baricco, M. et al. | 1991
- 588
-
Effect of molybdenum substitution on B2 antiphase domain formation in rapidly solidified Fe-Al-Mo alloysPrakash, U. / Buckley, R.A. / Jones, H. et al. | 1991
- 592
-
Disorder trapping in Ni2TiAlBoettinger, W.J. / Bendersky, L.A. / Cline, J. et al. | 1991
- 596
-
Microstructural investigation of a rapidly solidified Fe-Si-C alloyChen, Y.C. / Chen, C.M. / Su, K.C. et al. | 1991
- 601
-
Nanostructure determination of a splat-cooled and laser-quenched Nb40Ni60 alloyby scanning tunneling microscopyScandella, L. / Staufer, U. / Brodbeck, D. et al. | 1991
- 602
-
The study of phase transitions in amorphous bilayers prepared by rapid quenchingDuhaj, P. / Svec, P. / Majkova, E. et al. | 1991
- 606
-
Electron microscopic study of Cr-Ti alloysPrasad, R. / Somekh, R.E. / Greer, A.L. et al. | 1991
- 611
-
Nanocrystalline materials by crystallization of metal-metalloid glassesKöster, U. / Schünemann, U. / Blank-Bewersdorff, M. et al. | 1991
- 616
-
Solidification mechanism of Cr-Ni steel with 8 % MoShahani, H. / Fredriksson, H. et al. | 1991
- 620
-
A TEM study of the microstructure of Fe-6.25wt.%Si ribbons prepared by twin roller quenchingLonhardt, M. / Jurisch, M. / Böttcher, U. et al. | 1991
- 624
-
Influence of an oxygen atmosphere and surface treatments on surface crystallization of (Co,Ni)-B glassesSteinbrink, G. / Punge-Witteler, B. / Köster, U. et al. | 1991
- 630
-
Surface crystallization of Fe80B20 metallic glass ribbonsOleszak, D. / Glijer, P. / Matyja, J. et al. | 1991
- 636
-
Evidence for amorphization in Ni-Ti multilayers from electrical resistivity changesGraaf, A. von der / Hollanders, M.A. / Thijsse, B.J. et al. | 1991
- 640
-
New metastable carbides produced by crystallization of amorphous Cr-C alloysBouzy, E. / Caer, G. le / Bauer-Grosse, E. et al. | 1991
- 644
-
Stability of rapidly solidified Cu-Y and Cu-Y-B alloysBatawi, E. / Morris, D.G. et al. | 1991
- 649
-
Determining the parameters of the Fulcher-Vogel equation from equilibrium viscosity dataDuine, P.A. / Sietsma, J. / Beukel, A. van den et al. | 1991
- 653
-
Numerical analysis of the casting wheels of foil strip casting machinesVogt, E. / Schenk, H. / Gellenbeck, H. et al. | 1991
- 657
-
Influence of CO2 gas flow around the melt puddle on the surface roughness of Fe-B-Si ribbonsFiedler, H. / Illgen, L. / Barth, M. et al. | 1991
- 667
-
Direct casting of continuous fibres and wires by in-rotating-liquid spinningHeyder, B. / Frommeyer, G. et al. | 1991
- 671
-
Thin strip casting by a twin roller pilot plantFiedler, H. / Jurisch, M. / Preiss, P. et al. | 1991
- 676
-
Melt overflow process for direct cast fiber, ribbon and stripGaspar, T.A. / Hackmann, L.E. et al. | 1991
- 680
-
Fundamentals of fibre formation during melt extractionLotze, G. / Stephani, G. / Löser, W. et al. | 1991
- 684
-
Production of sputtering target by powder metallurgy processing using Fe-Al-Si gas-atomized powderYanagitani, A. / Murakami, M. / Yanagimoto, K. et al. | 1991
- 688
-
Flaky amorphous powders in Fe-, Co- and Al-based systems prepared by a two-stage quenching techniqueOguchi, M. / Inoue, A. / Masumoto, T. et al. | 1991
- 692
-
Characterization of Ni-Cu alloy powders produced by the atomization processSalgado, L. / Ambrozio Filho, F. / Neves, M.D.M. das et al. | 1991
- 698
-
Dendrite growth velocities in undercooled Ni-Si alloysCochrane, R.F. / Greer, A.L. / Eckler, K. et al. | 1991
- 702
-
Non-equilibrium solidification in undercooled Ni-B alloysEckler, K. / Cochrane, R.F. / Herlach, D.M. et al. | 1991
- 706
-
Grain refinement in drop-tube-processed nickel-based alloysCochrane, R.F. / Herlach, D.M. / Feuerbacher, B. et al. | 1991
- 711
-
Quenching and supercooling of tungsten and tantalum dropletsSoares, V. / Rinderer, L. / Meyer, R. et al. | 1991
- 715
-
Refractory metallic glassesRohr, L. / Reimann, P. / Richmond, T. et al. | 1991
- 718
-
Measurements of surface tension on levitated oscillating metallic dropsEckler, K. / Egry, I. / Herlach, D.M. et al. | 1991
- 722
-
Modelling of dendritic growth during ribbon formation in planar flow castingLudwig, A. / Frommeyer, G. / Granasy, L. et al. | 1991
- 726
-
Thermobaric quenching - A new method for producing metastable statesPonyatovsky, E.G. / Barkalv, O.I. et al. | 1991
- 730
-
Dendrite growth velocities in highly undercooled, dilute Ni-C meltsEckler, K. / Herlach, D.M. / Hamerton, R.G. et al. | 1991
- 734
-
Pressure-quenched phases in binary B-metal alloysDegtyareva, V.F. / Ponyatovsky, E.G. et al. | 1991
- 738
-
Preparation of ductile Al-Ge soldering foils by PFC techniqueIllgen, L. / Mühlbach, H. / Löser, W. et al. | 1991
- 742
-
Production of rapid quenched copper-based solder using the melt-extraction techniqueVasiliev, V.A. / Mitin, B.S. / Pashkov, I.N. et al. | 1991
- 746
-
A plant for production of powders, fibres, wires and wire tape at a rate of 106 K s-1Mitin, B.S. / Vasiliev, V.A. / Scuridin, A.A. et al. | 1991
- 751
-
Heat transfer in the single roller quenching methodsGranasy, L. / Ludwig, A. et al. | 1991
- 755
-
Analysis of heat transfer in the splat cooling techniqueKubicar, L. et al. | 1991
- 758
-
Morphological variations in melt-spun Al-Cu alloysTaha, M.A. / El-Mahallawy, N.A. / Abdel-Ghaffar, M.A. et al. | 1991
- 764
-
Preparation and characterization of rapidly quenched BaO-B2O3-Fe2O3 glassSchubert, T. / Sellger, R. / Hurisch, M. et al. | 1991
- 767
-
The distribution of heterogeneous nucleants in Al-Cr alloy powdersAdkins, N.J.E. / Tsakiropoulos, P. et al. | 1991
- 771
-
Preparation of ultra-fine amorphous powders by the chemical reduction method and the properties of their sintered productsSaida, J. / Inoue, A. / Masumoto, T. et al. | 1991
- 775
-
Preparation of ultra-fine metallic powders. A study of the structural transformations and of the sintering behaviourZhou, Y.H. / Harmelin, M. / Bigot, J. et al. | 1991
- 780
-
A microstructural study of a Nd15Fe77B8 magnetic alloy produced by liquid dyamic compaction (LDC)Harada, T. / Ando, T. / O'Handley, R.C.O. et al. | 1991
- 785
-
Formation of glassy spheres of Fe-Ni-P-B by containerless processingDunst, A. / Herlach, D.M. / Gillessen, F. et al. | 1991
- 790
-
Rapid crystal growth in undercooled Fe-Ni meltsBarth, M. / Eckler, K. / Herlach, D.M. et al. | 1991
- 795
-
Phase seeding in the solidification of an undercooled meltHerlach, D.M. / Feuerbacher, B. / Schleip, E. et al. | 1991
- 799
-
Solidification of Fe40Ni40B20 at high undercoolingVitta, S. / Proctor, C.S. / Cochrane, R.F. et al. | 1991
- 803
-
A competitive growth analysis of phase formation in Al-8wt.%FeCochrane, R.F. / Evans, P.V. / Greer, A.L. et al. | 1991
- 807
-
Effect of the quencing conditions on the crystallization kinetics and morphology of Fe65Co18B16Si1Baro, M.D. / Surinach, S. / Diego, J.A. et al. | 1991
- 811
-
Solidification structure of FeAl25 and FeAl25B(0.05-1) (wt.%) ribbons produced by the planar-flow-casting processTaravel, C. / Camel, D. et al. | 1991
- 819
-
Effects of quench rate on the texture in melt-spun Nd-Fe-B alloysZaluska, A. / Yan Xu / Altonian, Z. et al. | 1991
- 823
-
Kinetic aspects of eutectic Fe.Fe3C solidificationLundbäck, E. / Östlund, A. et al. | 1991
- 827
-
Modelling of crystal growth during rapid solidificationJönsson, B. et al. | 1991
- 832
-
Theoretical investigation of the processes and the microcrystalline ribbon formation by rapid quenching from the meltAnestiev, L.A. et al. | 1991
- 836
-
Microstructure of melt-spin Fe(1-x)Si(x) alloys (0 less or equal x less or equal 0.5)Monstadt, H. / Hornbogen, E. et al. | 1991
- 842
-
Effect of secondary cooling on a rapidly solidified stainless steel stripYukumoto, M. / Miyake, S. / Yamane, H. et al. | 1991
- 846
-
Influence of superheat and hammer speed on the formation of metallic glassesBrower, W.E. jun. / Megli, S.C. et al. | 1991
- 850
-
Protection of amorphizing alloy Fe-B-Si from oxidation by means of refinery slagsKopit, V.Z. / Klimov, A.V. / Nikhiforov, V.V. et al. | 1991
- 854
-
Equiaxed microstructure by rapid solidificationRieker, C. / Morris, D.G. et al. | 1991