Dependence of tribological properties on deposition parameters for non hydrogenated amorphous carbon films produced by magnetron sputtering (English)
- New search for: Mounier, E.
- New search for: Juliet, P.
- New search for: Quesnel, E.
- New search for: Pauleau, Y.
- New search for: Mounier, E.
- New search for: Juliet, P.
- New search for: Quesnel, E.
- New search for: Pauleau, Y.
In:
SURFACE AND COATINGS TECHNOLOGY
;
76/77
, 1/3
;
548-552
;
1995
-
ISSN:
- Article (Journal) / Print
-
Title:Dependence of tribological properties on deposition parameters for non hydrogenated amorphous carbon films produced by magnetron sputtering
-
Contributors:
-
Published in:SURFACE AND COATINGS TECHNOLOGY ; 76/77, 1/3 ; 548-552
-
Publisher:
- New search for: ELSEVIER SEQUOIA SA
-
Publication date:1995-01-01
-
Size:5 pages
-
ISSN:
-
Type of media:Article (Journal)
-
Type of material:Print
-
Language:English
- New search for: 671.73
- Further information on Dewey Decimal Classification
-
Classification:
DDC: 671.73 -
Source:
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Table of contents – Volume 76/77, Issue 1/3
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 1
-
Influence of plasma-sprayed Mo coating on sulphidation behaviour of Inconel 600 and Nimonic PE11 alloysDu, H. L. / Datta, P. K. / Burnell-Gray, J. S. / Guo, X. et al. | 1995
- 7
-
Synthesis of molybdenum disilicide on molybdenum substratesGovindarajan, S. / Mishra, B. / Olson, D. L. / Moore, J. J. / Disam, J. et al. | 1995
- 14
-
Blanching resistant Cu-Cr coating by vacuum plasma sprayChiang, K. T. / Krotz, P. D. / Yuen, J. L. et al. | 1995
- 20
-
Growth and oxidation resistance of boron-modified and germanium-doped silicide diffusion coatings formed by the halide-activated pack cementation methodCockeram, B. V. et al. | 1995
- 28
-
Microstructural analysis of the role of rhenium in advanced MCrAlY coatingsCzech, N. / Schmitz, F. / Stamm, W. et al. | 1995
- 34
-
Dispersion-strengthened modified MCrAlY coatings produced by reactive depositionTaylor, T. A. / Knapp, J. K. et al. | 1995
- 41
-
Structure and properties of protective coatings produced by vacuum arc depositionLeontiev, S. A. / Kuznetsov, V. G. / Rybnikov, A. I. / Burov, I. V. et al. | 1995
- 47
-
Mechanical degradation of coating systems in high-temperature cyclic oxidationPennefather, R. C. / Boone, D. H. et al. | 1995
- 53
-
Surface modification of several steels after their exposure at high temperature to oxygen and sulfur mixturesOtero, E. / Pardo, A. / Perosanz, F. J. / Orts, J. / Maffiotte, C. A. / Perez Trujillo, F. J. et al. | 1995
- 61
-
Friction and wear behavior of titanium nitride, zirconium nitride and chromium nitride coatings at elevated temperaturesSue, J. A. / Chang, T. P. et al. | 1995
- 70
-
Oxidation resistance of (Ti,Al,Zr,Si)N coatings in airRebouta, L. / Vaz, F. / Andritschky, M. / Da Silva, M. F. et al. | 1995
- 75
-
Erosion rate testing at high temperature for turbomachinery useTabakoff, W. / Shanov, V. et al. | 1995
- 81
-
Application of advanced coatings to narrow neck press and blow plungers in the glass container industryPenlington, R. / Sarwar, M. / Lewis, D. B. et al. | 1995
- 86
-
Experience with metal/ceramic coating in stationary gas turbinesOsyka, A. S. / Rybnikov, A. I. / Leontiev, S. A. / Nikitin, N. V. / Malashenko, I. S. et al. | 1995
- 95
-
Surface roughening of metallic substrates by high pressure pure waterjetTaylor, T. A. et al. | 1995
- 101
-
Adherence of combined physically vapour-deposited and plasma-sprayed ceramic coatingsAndritschky, M. / Teixeira, V. / Rebouta, L. / Buchkremer, H. P. / Stoever, D. et al. | 1995
- 106
-
Influence of phase stability on the residual stress in partially stabilized zirconia TBC produced by plasma sprayScardi, P. / Leoni, M. / Bertamini, L. et al. | 1995
- 113
-
Thick ceramic coatings using a sol gel based ceramic-ceramic 0-3 compositeBarrow, D. A. / Petroff, T. E. / Sayer, M. et al. | 1995
- 119
-
Chemical vapor co-deposition of C and SiC at moderate temperature for the synthesis of compositionally modulated Si~xC~1~-~x, ceramic layersMaury, F. / Agullo, J. M. et al. | 1995
- 126
-
Reactive sputter deposition of yttria-stabilized zirconiaJankowski, A. F. / Hayes, J. P. et al. | 1995
- 132
-
In-situ failure analysis of a Ni coating deposited by electrolyte brushingGrigorescu, I. C. / Navas, G. et al. | 1995
- 135
-
Energy and mass spectra of ions in triode ion plating of Ti(C,N) coatingsWouters, S. / Kadlec, S. / Nesladek, M. / Quaeyhaegens, C. / Stals, L. M. et al. | 1995
- 142
-
Effect of substrate bias on sputter-deposited TiC~x, TiN~y and TiC~xN~y thin filmsAdjaottor, A. A. / Meletis, E. I. / Logothetidis, S. / Alexandrou, I. / Kokkou, S. et al. | 1995
- 149
-
Investigation of superlattice coatings deposited by a combined steered arc evaporation and unbalanced magnetron sputtering techniqueDonohue, L. A. / Cawley, J. / Lewis, D. B. / Brooks, J. S. / Muenz, W.-D. et al. | 1995
- 159
-
Multilayered titanium tungsten nitride coatings with a superlattice structure grown by unbalanced magnetron sputteringHurkmans, T. / Trinh, T. / Lewis, D. B. / Brooks, J. S. / Muenz, W.-D. et al. | 1995
- 167
-
Formation of metal oxides by cathodic arc depositionAnders, S. / Anders, A. / Rubin, M. / Wang, Z. / Raoux, S. / Kong, F. / Brown, I. G. et al. | 1995
- 174
-
Properties of TiN and CrN coatings deposited at low temperature using reactive arc-evaporationGaahlin, R. / Bromark, M. / Hedenqvist, P. / Hogmark, S. / Haakansson, G. et al. | 1995
- 181
-
Arc behaviour during filtered vacuum arc deposition of Sn-O thin filmsKaplan, L. / Zhitomirsky, V. N. / Goldsmith, S. / Boxman, R. L. / Rusman, I. et al. | 1995
- 190
-
Ion current distribution in a filtered vacuum arc deposition systemZhitomirsky, V. N. / Kaplan, L. / Boxman, R. L. / Goldsmith, S. et al. | 1995
- 197
-
Influence of transverse current during In-O vapor depositionParkansky, N. / Rosenbaum, R. / Rosenberg, Y. / Boxman, R. L. / Goldsmith, S. et al. | 1995
- 202
-
Deposition and mechanical properties of multilayered PVD Ti-TiN coatingsLarsson, M. / Bromark, M. / Hedenqvist, P. / Hogmark, S. et al. | 1995
- 206
-
Influence of Ar pressure on r.f. magnetron-sputtered Ca~5(PO~4)~3OH layersVan Dijk, K. / Schaeken, H. G. / Maree, C. H. M. / Verhoeven, J. / Wolke, J. C. G. / Habraken, F. H. P. M. / Jansen, J. A. et al. | 1995
- 211
-
Single cycle, combination layers with plasma assistanceHuchel, U. / Bramers, S. / Crummenauer, J. / Dressler, S. / Kinkel, S. et al. | 1995
- 218
-
Comparison of the corrosion resistance of different steel grades nitrided, coated and duplex treatedDingremont, N. / Bergmann, E. / Hans, M. / Collignon, P. et al. | 1995
- 225
-
Preparation and characterization of hard mono- and multilayer plasma-assisted chemically vapour deposited coatingsLeonhardt, A. / Bartsch, K. / Endler, I. et al. | 1995
- 231
-
Chemical vapour deposition of TiN on stainless steelStaia, M. H. / Lewis, B. / Cawley, J. / Hudson, T. et al. | 1995
- 237
-
Deposition of TiN thin films by organometallic chemical vapor deposition: thermodynamical predictions and experimental resultsJimenez, C. / Gilles, S. / Bernard, C. / Madar, R. et al. | 1995
- 244
-
Vanadium oxycarbide thin films prepared by conventional chemical vapour deposition from vanadium(III) acetylacetonateRamirez, J. / Berroteran, I. et al. | 1995
- 250
-
Comparison of WCl~6-CH~4-H~2 and WF~6-CH~4-H~2 systems for growth of WC coatingsFitzsimmons, M. / Sarin, V. K. et al. | 1995
- 256
-
Characterisation of the kappa-Al~2O~3 -> -Al~2O~3 transformation in different single layer coatings of CVD kappa-Al~2O~3Hansson, P. / Halvarsson, M. / Vuorinen, S. et al. | 1995
- 265
-
Residual stresses in PVD hard coatingsOettel, H. / Wiedemann, R. et al. | 1995
- 274
-
Production of Ti films with controlled textureMusil, J. / Vlcek, J. / Jezek, V. / Benda, M. / Kolega, M. / Boomsma, R. et al. | 1995
- 280
-
Complex characterisation of vacuum arc-deposited chromium nitride thin filmsEhrlich, A. / Kuehn, M. / Richter, F. / Hoyer, W. et al. | 1995
- 287
-
The influence of the nucleation surface on the growth of CVD -Al~2O~3 and kappa-Al~2O~3Halvarsson, M. / Vourinen, S. et al. | 1995
- 297
-
Examination of mechanical properties and failure mechanisms of TiN and Ti-TiN multilayer coatingsMa, K. J. / Bloyce, A. / Bell, T. et al. | 1995
- 303
-
Gas phase reactivity in chemical vapor depositionTeyssandier, F. / Wang, Y. B. et al. | 1995
- 311
-
A model for texture evolution in a growing filmKnuyt, G. / Quaeyhaegens, C. / D'Haen, J. / Stals, L. M. et al. | 1995
- 316
-
Cross-sectional structure of tetrahedral amorphous carbon thin filmsDavis, C. A. / Knowles, K. M. / Amaratunga, G. A. J. et al. | 1995
- 322
-
Plasma diagnostics of arc-enhanced glow dischargeVetter, J. / Wallendorf, T. et al. | 1995
- 328
-
Multilayer PVD coatings for wear protectionHolleck, H. / Schier, V. et al. | 1995
- 337
-
Effect of ion beam energy on the synthesis of oriented aluminium nitride thin filmsNakamura, Y. / Watanabe, Y. / Hirayama, S. / Naota, Y. et al. | 1995
- 341
-
Protection of aluminium by duplex coatingsMusil, J. / Vlcek, J. / Jezek, V. / Benda, M. et al. | 1995
- 348
-
X-ray characterization of epitaxial (Sr,Ba)TiO~3 films grown by pulsed laser depositionQadri, S. B. / Horwitz, J. S. / Chrisey, D. B. / Auyeung, R. C. Y. / Knauss, L. A. et al. | 1995
- 352
-
Corrosion resistance of Zn coatings produced by air arc depositionParkansky, N. / Boxman, R. L. / Goldsmith, S. / Rosenberg, Y. et al. | 1995
- 358
-
Determination of the thermal expansion of kappa-Al~2O~3 by high temperature XRDHalvarsson, M. / Langer, V. / Vuorinen, S. et al. | 1995
- 363
-
Deposition of (Ti,Al)N coatings by means of electron beam ion plating with evaporation of Ti and Al from two separate cruciblesPalmers, J. / Van Stappen, M. et al. | 1995
- 367
-
Temperature stability of fluorinated amorphous hydrogenated carbon filmsMueller, U. / Hauert, R. / Oral, B. / Tobler, M. et al. | 1995
- 372
-
Preparation of aluminum nitride films by low pressure organometallic chemical vapor depositionJimenez, C. / Gilles, S. / Doppelt, P. / Bernard, C. / Madar, R. et al. | 1995
- 377
-
Nitride nanophases in a plasma-assisted surface modified steelPalacios, M. / Salas, O. / Mu�oz, M. / Oseguera, J. / Schabes Retchkiman, P. et al. | 1995
- 382
-
Influence of magnetron sputtering process parameters on wear properties of steel Cr~3Si or Cr/MoS~xWeise, G. / Teresiak, A. / Baecher, I. / Markschlaeger, P. / Kampschulte, G. et al. | 1995
- 393
-
Nanostructure of Au-20%Pd layers in MoS~2 multilayer solid lubricant filmsJayaram, G. / Marks, L. D. / Hilton, M. R. et al. | 1995
- 400
-
Frriction properties of WS2/graphite fluoride thin films grown by pulsed laser depositionZabinski, J.S. / Florkey, J.E. / Walck, S.D. / Bultman, J.E. / McDevitt, N.T. et al. | 1995
- 400
-
Friction properties of WS~2/graphite fluoride thin films grown by pulsed laser depositionZabinski, J. S. / Florkey, J. E. / Walck, S. D. / Bultman, J. E. / McDevitt, N. T. et al. | 1995
- 407
-
Evaluation of PS 212 coatings under boundary lubrication conditions with an ester-based oil to 300 CSliney, H. E. / Loomis, W. R. / DellaCorte, C. et al. | 1995
- 407
-
Evaluation of PS212 coatings under boundary lubrication conditions with an ester-based oil to 300 deg CSliney, H.E. / Loomis, W.R. / DellaCorte, C. et al. | 1995
- 415
-
A study of the tribological and electrical properties of sputtered and burnished transition metal dichalcogenide filmsWaghray, H. / Lee, T.-S. / Tatarchuk, B. J. et al. | 1995
- 421
-
Influence of the electrical current on the graphite surface in an electrical sliding contactCsapo, E. / Zaidi, H. / Paulmier, D. / Kadiri, E. K. / Bouchoucha, A. / Robert, F. et al. | 1995
- 425
-
Plasma diffusion treatment and duplex treatment - recent development and new applicationsRie, K.-T. / Broszeit, E. et al. | 1995
- 437
-
Development and characterization of TiN coating by ion beam assisted deposition process for improved wear resistanceHan, Jeon-G. / Joo S. Yoon / Choi, Byung-H. / In S. Choi et al. | 1995
- 437
-
Development and characterization of TiN coatings by ion beam assisted deposition process for improved wear resistanceHan, J. G. / Yoon, J. S. / Choi, B. H. / Choi, I. S. et al. | 1995
- 443
-
Formation and self-lubricating mechanism of boric acid on borided steel surfaceErdemir, A. / Bindal, C. et al. | 1995
- 443
-
Formation and self-lubricating mechanisms of boric acid on borided steel surfacesErdemir, A. / Bindal, C. et al. | 1995
- 450
-
Carbide-reinforced coatings on AISI 316 L stainless steel by laser surface alloyingTassin, C. / Laroudie, F. / Pons, M. / Lelait, L. et al. | 1995
- 456
-
The galling wear resistance of new iron-base hardfacing alloys: a comparison with established cobalt- and nickel-base alloysOcken, H. et al. | 1995
- 462
-
Dry rolling wear of different materials induced by a non-uniform hertzian pressure distributionNeubrand, J. / Weiss, H. et al. | 1995
- 462
-
Dry rolling wear of different materials induced by non-uniform hertzian pressure distributionNeubrand, J. / Weiss, H. et al. | 1995
- 469
-
Microwear mechanisms of coatingsKato, K. et al. | 1995
- 475
-
Wear and friction properties of hard PVD coatingsBienk, E. J. / Reitz, H. / Mikkelsen, N. J. et al. | 1995
- 481
-
Influence of recoating on the mechanical and tribological performance of TiN-coated HSSBromark, M. / Gaahlin, R. / Hedenqvist, P. / Hogmark, S. / Haakansson, G. / Hansson, G. et al. | 1995
- 487
-
Friction and wear of metallic and non-metallic surfacesGarzino-Demo, G. A. / Lama, F. L. et al. | 1995
- 494
-
Phase characterization in Ni alloy-hard carbide composites for fused coatingsGrigorescu, I. C. / Di Rauso, C. / Drira-Halouani, R. / Lavelle, B. / Di Giampaolo, R. / Lira, J. et al. | 1995
- 499
-
Oxidation behavior of titanium-aluminium nitridesJoshi, A. / Hu, H. S. et al. | 1995
- 508
-
A study of the corrosion properties of PVD Zn-Ni coatingsBowden, C. / Matthews, A. et al. | 1995
- 516
-
Multilayer films of TiC, Ti and Cu for the Gravity Probe B Relativity Mission gyroscopesZhou, P. / Buchman, S. / Davis, K. / Gray, C. / Turneaure, J. P. et al. | 1995
- 521
-
Metal transfer and oxidation of copper-steel surfaces in electrical sliding contactBouchoucha, A. / Kadiri, E.K. / Robert, F. / Zaidi, H. / Paulmier, D. et al. | 1995
- 521
-
Metals transfer and oxidation of copper-steel surfaces in electrical sliding contactBouchoucha, A. / Kadiri, E. K. / Robert, F. / Zaidi, H. / Paulmier, D. et al. | 1995
- 528
-
Comparison of acoustic emission from pointed and spherical indentation of TiN films on silicon and sapphireSwain, M. V. / Wittling, M. et al. | 1995
- 534
-
Mechanical and tribological properties of diamond-like carbon coatings prepared by pulsed laser depositionVoevodin, A. A. / Donley, M. S. / Zabinski, J. S. / Bultman, J. E. et al. | 1995
- 540
-
Fundamentals of the tribological behaviour of diamond, diamond-like carbon and cubic boron nitride coatingsHabig, K.-H. et al. | 1995
- 548
-
Dependence of tribological properties on deposition parameters for non hydrogenated amorphous carbon films produced by magnetron sputteringMounier, E. / Juliet, P. / Quesnel, E. / Pauleau, Y. et al. | 1995
- 553
-
Deep-drawing of aluminium sheets without lubricant by use of diamond-like carbon coated diesMurakawa, M. / Koga, N. / Kumagai, T. et al. | 1995
- 553
-
Deep-drawing of aluminum sheets without lubricant by use of diamond-like carbon coated diesMurakawa, M. / Koga, N. / Kumagai, T. et al. | 1995
- 559
-
Characterization of transfer layers on steel surfaces sliding against diamond-like hydrocarbon films in dry nitrogenErdemir, A. / Bindal, C. / Pagan, J. / Wilbur, P. et al. | 1995
- 564
-
Influence of defects and morphology of diamond-like carbon coatings on their tribological behaviourZaidi, H. / Le Huu, T. / Robert, F. / Bedri, R. / Kadiri, E. K. / Paulmier, D. et al. | 1995
- 572
-
Tribological behaviour of smooth diamond filmsPimenov, S. M. / Smolin, A. A. / Obraztsova, E. D. / Konov, V. I. / Boegli, U. / Blatter, A. / Maillat, M. / Leijala, A. / Burger, J. / Hintermann, H. E. et al. | 1995
- 579
-
Application of metal-C:H low-friction layers for bearing materialsLunow, T. / Kocis, R. / Leonhardt, G. / Wilberg, R. et al. | 1995
- 583
-
Steel surface modifications in magnetised sliding contactPaulmier, D. / Zaidi, H. / Bedri, R. / Kadiri, E. K. / Pan, L. / Jiang, Q. et al. | 1995
- 589
-
Treatment of the surface layer of steel with high energy plasma pulsesSpoerer, J. / Igenbergs, E. et al. | 1995
- 595
-
Corrosion behavior of nitrogen-implanted ZircaloyKim, W. / Jung, K. S. / Choi, B. H. / Kwon, H. S. / Lee, S. J. / Han, J. G. / Guseva, M. I. / Atamanov, M. V. et al. | 1995
- 600
-
Friction behavior of amorphous-BN-cubic-BN dual-layered filmWatanabe, S. / Miyake, S. / Murakawa, M. et al. | 1995
- 604
-
Tribological behaviour of electrochemically deposited coatings for shaft restorationGrigorescu, I. C. / Gonzalez, Y. / Rodrigues, O. / De Vita, Y. et al. | 1995
- 609
-
Structur, mechanical and tribological properties of d.c. magnetron sputtered TiB2 and TiB2(N) thin filmsDeng, H. / Chen, J. / Inturi, R.B. / Barnard, J.A. et al. | 1995
- 609
-
Structure, mechanical and tribological properties of d.c. magnetron sputtered TiB~2 and TiB~2(N) thin filmsDeng, H. / Chen, J. / Inturi, R. B. / Barnard, J. A. et al. | 1995
- 615
-
Electrochemical impedance spectroscopy of PVD-TiN coatings on mild steel and AISI316 substratesLiu, C. / Leyland, A. / Lyon, S. / Matthews, A. et al. | 1995
- 623
-
An a.c. impedance study on PVD CrN-coated mild steel with different surface roughnessesLiu, C. / Leyland, A. / Lyon, S. / Matthews, A. et al. | 1995
- 632
-
PLATIT: e new industrial approach to cathodic arc coating technologyCurtins, H. et al. | 1995
- 632
-
PLATIT: a new industrial approach to cathodic arc coating technologyCurtins, H. et al. | 1995
- 640
-
Improved hollow cathode magnetron deposition for producing high thermal conductivity graphite-copper compositeStoessel, C. H. / Withers, J. C. / Pan, C. / Wallace, D. / Loutfy, R. O. et al. | 1995
- 645
-
Low energy universal cold cathode ion source (LE-UCCIS)Garzino-Demo, G. A. / Lama, F. L. et al. | 1995
- 655
-
Microscale mechanical and tribological characterization of hard amorphous carbon coatings as thin as 5 nm for magnetic disksBhushan, B. / Koinkar, V. N. et al. | 1995
- 670
-
In situ plasma monitoring of pulsed laser deposition of diamond-like carbon filmsVoevodin, A. A. / Laube, S. J. P. et al. | 1995
- 675
-
Diode laser absorption spectroscopy for process control - sensor system design methodologyBerzins, E. V. / Anklam, T. M. / Chambers, F. / Galanti, S. / Haynam, C. A. / Worden, E. F. et al. | 1995
- 681
-
Evaporation rate and composition monitoring of electron beam physical vapor deposition processesAnklam, T. M. / Berzins, L. V. / Braun, D. G. / Haynam, C. / Meier, T. / McClelland, M. A. et al. | 1995
- 687
-
Optical emission spectroscopy of active species in a TiCN PVD arc dischargeBaravian, G. / Sultan, G. / Damond, E. / Detour, H. / Hayaud, C. / Jacquot, P. et al. | 1995
- 694
-
The influence of process gas characteristics on the properties of plasma nitrided steelFancey, K. S. / Leyland, A. / Egerton, D. / Torres, D. / Matthews, A. et al. | 1995
- 700
-
Deposition of arc TiAlN coatings with pulsed biasLugscheider, E. / Knotek, O. / Loeffler, F. / Barimani, C. / Guerreiro, S. / Zimmermann, H. et al. | 1995
- 706
-
The efficiency of uncoated and coated tool systems in the machining of low carbon steel assessed through cutting force measurementsAudy, J. / Strafford, K. N. / Subramanian, C. et al. | 1995
- 712
-
Today's applications and future developments of coatings for drills and rotating cutting toolsCselle, T. / Barimani, A. et al. | 1995
- 719
-
Vacuum arc coatings for tools: potential and applicationVetter, J. et al. | 1995
- 725
-
Large-area pretreatment for physical vapor depositionSchiller, S. / Goedicke, K. / Milde, F. / Hoetzsch, G. et al. | 1995
- 731
-
Hydrogen plasma chemical cleaning of metallic substrates and silicon wafersKorner, N. / Beck, E. / Dommann, A. / Onda, N. / Ramm, J. et al. | 1995
- 738
-
Oil removal from metals by linear multi-orifice hollow cathodeBelkind, A. / Li, H. / Clow, H. / Jansen, F. et al. | 1995
- 744
-
Wide web coating of complex materialsLievens, H. et al. | 1995
- 754
-
Effect of Plasma Activation on the Phase Transformations of Aluminum OxideZywitzki, O. / Hoetzsch, G. et al. | 1995
- 763
-
The magnetron-activated deposition processReschke, J. / Goedicke, K. / Schiller, S. et al. | 1995
- 770
-
Multipolar magnetic field structures for the scaling-up of high density plasmas excited in the d.c. to microwave frequency range and applicable to sputtering and chemical processingPelletier, J. / Lagarde, T. / Arnal, Y. / Burke, R. / Cocagne, J. et al. | 1995
- 776
-
Progress in large-area glass coatings by high-rate sputteringBeister, G. / Dietrich, E. / Schaefer, C. / Scherer, M. / Szczyrbowski, J. et al. | 1995
- 786
-
Application of diamond-like carbon films for anti-abrasion and low friction properties of VCR head drumsLee, K.-R. / Kwang Yong Eun / Kim, K.-M. / Choi, K.-C. et al. | 1995
- 791
-
Diamond film synthesis in low pressure premixed flames of different fuel typesKim, J. S. / Cappelli, M. A. et al. | 1995
- 797
-
Hot filament scaling-up for CVD diamond burr manufacturingTrava-Airoldi, V. J. / Corat, E. J. / Del Bosco, E. / Leite, N. F. et al. | 1995
- 803
-
Substrate and barrier layer considerations in the growth and properties of diamond and diamond-like carbonOgale, S. B. / Karve, P. / Kulkarni, A. A. / Sharma, R. P. / Prabhjyot Pal, J. / Kanetkar, S. M. et al. | 1995
- 809
-
Hard coatings on magnesium alloys by sputter deposition using a pulsed d.c. bias voltageReiners, G. / Griepentrog, M. et al. | 1995
- 815
-
Low-temperature deposition of titanium nitridePerry, A. J. / Treglio, J. R. / Tian, A. F. et al. | 1995
- 821
-
Inorganic coatings on polymersBenmalek, M. / Dunlop, H. M. et al. | 1995
- 827
-
Protective coatings for LEO environments in spacecraft applicationsKleiman, J. I. / Iskanderova, Z. A. / Perez, F. J. / Tennyson, R. C. et al. | 1995
- 835
-
Application of fracture mechanics to the adhesion of metal coatings on CFRPMenninoen, M. / Weiss, H. et al. | 1995