Thermal mechanical fatigue of single crystal superalloys: Achievements and challenges (English)
- New search for: Zhang, W. J.
- New search for: Zhang, W. J.
In:
MATERIALS SCIENCE AND ENGINEERING A
;
650
;
389-395
;
2016
-
ISSN:
- Article (Journal) / Print
-
Title:Thermal mechanical fatigue of single crystal superalloys: Achievements and challenges
-
Contributors:Zhang, W. J. ( author )
-
Published in:MATERIALS SCIENCE AND ENGINEERING A ; 650 ; 389-395
-
Publisher:
- New search for: Elsevier Science B.V., Amsterdam.
-
Publication date:2016-01-01
-
Size:7 pages
-
ISSN:
-
Type of media:Article (Journal)
-
Type of material:Print
-
Language:English
- New search for: 620.11
- Further information on Dewey Decimal Classification
-
Classification:
DDC: 620.11 -
Source:
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Table of contents – Volume 650
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 1
-
A study on the capability of equal channel forward extrusion processEbrahimi, M. / Gholipour, H. / Djavanroodi, F. et al. | 2015
- 8
-
Microstructural evolution, mechanical properties, and strain hardening behavior of ultrafine grained commercial pure copper during the accumulative roll bonding processFattah-alhosseini, A. / Imantalab, O. / Mazaheri, Y. / Keshavarz, M.K. et al. | 2015
- 15
-
Evaluation of high-temperature Vickers hardness using instrumented indentation systemPark, Chan-Pyoung / Lee, Jung-Jun / Kang, Seung-Kyun / Kim, Young-Cheon / Woo, Kwan-Sik / Jeon, Seung-Won / Kwon, Dongil et al. | 2015
- 20
-
Acoustic emission study on the activity of slip and twin mechanisms during compression testing of magnesium single crystalsDrozdenko, Daria / Bohlen, Jan / Chmelík, František / Lukáč, Pavel / Dobroň, Patrik et al. | 2015
- 28
-
Ordering and the micromechanics of Ti–7AlRadecka, Anna / Coakley, James / Jones, Ian P. / Rugg, David / Lindley, Trevor C. / Dye, David et al. | 2015
- 38
-
Depth-sensing indentation-based studies of surface mechanical behavior and fatigue damage evolution of an austenitic stainless steel subjected to cyclic strainingYe, Duyi / Xu, Haifeng / Feng, Xianfeng / Xu, Yuandong / Xiao, Lei et al. | 2015
- 52
-
Thermomechanical fatigue and damage mechanisms in Sanicro 25 steelPetráš, R. / Škorík, V. / Polák, J. et al. | 2015
- 63
-
Influence of microalloying with zirconium on the structure and properties of Cu–Cr alloy after high pressure torsionShangina, D.V. / Bochvar, N.R. / Gorshenkov, M.V. / Yanar, H. / Purcek, G. / Dobatkin, S.V. et al. | 2015
- 67
-
Enhancement of C/C-LAS joint using aligned carbon nanotubes prepared by injection chemical vapor depositionZhao, Feng-Ling / Fu, Qian-Gang / Feng, Lei / Shen, Qing-Liang et al. | 2015
- 75
-
Effect of phosphorus content on the mechanical, microstructure and corrosion properties of supermartensitic stainless steelRodrigues, C.A.D. / Bandeira, R.M. / Duarte, B.B. / Tremiliosi-Filho, G. / Jorge, A.M. Jr. et al. | 2015
- 84
-
Ordered phases and microhardness of Fe–6.5%Si steel sheet after hot rolling and annealingLi, Chang-Sheng / Yang, Cheng-Lin / Cai, Guo-Jun / Wang, Qi-Wen et al. | 2015
- 93
-
Comparative study of the SCC behavior of E690 steel and simulated HAZ microstructures in a SO2-polluted marine atmosphereMa, Hongchi / Liu, Zhiyong / Du, Cuiwei / Li, Xiaogang / Cui, Zhongyu et al. | 2015
- 102
-
Effects of dendrite size on dynamic tensile deformation behavior in Zr-based amorphous alloys containing ductile dendritesJeon, Changwoo / Kang, Minju / Paul Kim, Choongnyun / Seop Kim, Hyoung / Lee, Sunghak et al. | 2015
- 110
-
Investigation and microstructural analyses of massive LSP impacts with coverage area on crack initiation location and tensile properties of AM50 magnesium alloyLuo, K.Y. / Wang, C.Y. / Sun, G.F. / Cui, C.Y. / Sheng, J. / Lu, J.Z. et al. | 2015
- 119
-
Influence of prior cold rolling reduction on microstructure and mechanical properties of a reversion annealed high-Mn austenitic steelBehjati, P. / Kermanpur, A. / Karjalainen, L.P. / Järvenpää, A. / Jaskari, M. / Samaei Baghbadorani, H. / Najafizadeh, A. / Hamada, A. et al. | 2015
- 129
-
Spark plasma sintering and age hardening of an Al–Zn–Mg alloy powder blendRudinsky, S. / Hendrickx, P. / Bishop, D.P. / Brochu, M. et al. | 2015
- 139
-
Microstructures and mechanical properties of AA6061–SiC composites prepared through spark plasma sintering and hot rollingLi, X.P. / Liu, C.Y. / Ma, M.Z. / Liu, R.P. et al. | 2015
- 145
-
Development of nano-Y2O3 dispersed Zr alloys by mechanical alloying and spark plasma sinteringNuthalapati, Mohan / Karak, S.K. / Chakravarty, D. / Basu, A. et al. | 2015
- 154
-
Changing distribution and geometry of S′ in Al–Cu–Mg single crystals during stress aging by controlling the loading orientationChen, Jiqiang / Chen, Zhiguo / Guo, Xiaobin / Deng, Yunlai et al. | 2015
- 161
-
High temperature low cycle fatigue properties of alloy 625Mataveli Suave, Lorena / Cormier, Jonathan / Bertheau, Denis / Villechaise, Patrick / Soula, Aurélie / Hervier, Zéline / Hamon, Florence et al. | 2015
- 171
-
Equiaxed Ti-based composites with high strength and large plasticity prepared by sintering and crystallizing amorphous powderLiu, L.H. / Yang, C. / Kang, L.M. / Long, Y. / Xiao, Z.Y. / Li, P.J. / Zhang, L.C. et al. | 2015
- 183
-
Influence of loading path and precipitates on indentation creep behavior of wrought Mg–6wt% Al–1wt% Zn magnesium alloyNautiyal, Pranjal / Jain, Jayant / Agarwal, Arvind et al. | 2015
- 190
-
Creep behavior of high-pressure die-cast Mg-4Al-4La-0.4Mn alloy under medium stresses and at intermediate temperaturesYang, Qiang / Zheng, Tian / Zhang, Deping / Bu, Fanqiang / Qiu, Xin / Liu, Xiaojuan / Meng, Jian et al. | 2015
- 197
-
Evolution of activation energies for hot deformation of 7150 aluminum alloys with various Zr and V additionsShi, Cangji / Chen, X.-Grant et al. | 2015
- 210
-
Enhanced strength and electrical conductivity of Al–Mg–Si alloy by thermo-mechanical treatmentLin, Gaoyong / Zhang, Zongpeng / Wang, Hongyang / Zhou, Ke / Wei, Yuyong et al. | 2015
- 218
-
Enhanced mechanical properties of polycrystalline Cu–Al–Ni alloy through grain boundary orientation and composition controlFu, Huadong / Song, Shilei / Zhuo, Longchao / Zhang, Zhihao / Xie, Jianxin et al. | 2015
- 225
-
Texture and anisotropy in selective laser melting of NiTi alloyDadbakhsh, S. / Vrancken, B. / Kruth, J.-P. / Luyten, J. / Van Humbeeck, J. et al. | 2015
- 233
-
Forgeability, microstructure and mechanical properties of a free-forged Mg–8Gd–3Y–0.4Zr alloyLiu, Bin / Zhang, Zhenyan / Jin, Li / Gao, Jianliang / Dong, Jie et al. | 2015
- 240
-
Effect of Y content on microstructure and mechanical properties of as-cast Mg–8Li–3Al–2Zn alloy with duplex structureZhao, Jiong / Zhang, Jie / Liu, Wencai / Wu, Guohua / Zhang, Liang et al. | 2015
- 248
-
Aging behavior and precipitates analysis of the Cu–Cr–Zr–Ce alloyZhang, Yi / Volinsky, Alex A. / Tran, Hai T. / Chai, Zhe / Liu, Ping / Tian, Baohong / Liu, Yong et al. | 2015
- 254
-
Effects of re-ageing treatment on microstructure and tensile properties of solution treated and cold-rolled Al–Cu–Mg alloysLi, Hai / Xu, Wei / Wang, Zhixiu / Fang, Bijun / Song, Renguo / Zheng, Ziqiao et al. | 2015
- 264
-
On the microstructure and mechanical properties of severely cold shape rolled CuForouzanmehr, Nazanin / Nili-Ahmadabadi, Mahmoud / Samadi Khoshkhoo, Mohsen et al. | 2015
- 273
-
Fatigue behavior of variable-plane-rolled AZ31 magnesium alloyWu, Yanjun / Zhu, Rong / Cai, Xiaotian / Liu, Lingli et al. | 2015
- 281
-
Influence of multi-pass friction stir processing on the microstructure and mechanical properties of Al-5083 alloyChen, Yu / Ding, Hua / Li, Jizhong / Cai, Zhihui / Zhao, Jingwei / Yang, Wenjing et al. | 2015
- 290
-
Toughness evolution of 9Cr–3W–3Co martensitic heat resistant steel during long time agingYan, Peng / Liu, Zhengdong et al. | 2015
- 295
-
Anisotropy in the impact toughness of selective laser melted Ti–6Al–4V alloyWu, Ming-Wei / Lai, Pang-Hsin / Chen, Jhewn-Kuang et al. | 2015
- 300
-
Strengthening and toughening of extruded magnesium alloy rods by combining pre-torsion deformation with subsequent annealingSong, Bo / Guo, Ning / Xin, Renlong / Pan, Hucheng / Guo, Changfa et al. | 2015
- 305
-
Quasi-static and high-rate mechanical behavior of aluminum-based MMC reinforced with boron carbide of various length scalesBehm, Nathan / Yang, Hanry / Shen, Jianghua / Ma, Kaka / Kecskes, Laszlo J. / Lavernia, Enrique J. / Schoenung, Julie M. / Wei, Qiuming et al. | 2015
- 317
-
Portevin-Le Chatelier effect in a Ni–Cr–Mo alloy containing ordered phase with Pt2Mo-type structure at room temperatureYuan, Liang / Hu, Rui / Li, Jinshan / Zhang, Xiaoqing / Yang, Yan’an et al. | 2015
- 323
-
Numerical and theoretical modeling of the elasto-plastic response of aluminum–graphite composites during strainingHernández-Rivera, J.L. / Medellín-Castillo, H.I. / de Lange, D.F. et al. | 2015
- 335
-
Effect of the mode of deformation on activation volume of a materialKumari, Mamta / Ray, Kalyan Kumar et al. | 2015
- 345
-
Microstructure and property of Cu–2.7Ti–0.15Mg–0.1Ce–0.1Zr alloy treated with a combined aging processSi, Li / Zhou, Li / Zhu, Xiao / Sanhua, Li / Leinuo, Shen / Qiyi, Dong et al. | 2015
- 354
-
Traction–separation relationships for hydrogen induced grain boundary embrittlement in nickel via molecular dynamics simulationsBarrows, Wesley / Dingreville, Rémi / Spearot, Douglas et al. | 2015
- 365
-
The impact of melt conditioning on microstructure, texture and ductility of twin roll cast aluminium alloy stripsBarekar, N.S. / Das, S. / Yang, X. / Huang, Y. / Fakir, Omer El / Bhagurkar, A.G. / Zhou, L. / Fan, Z. et al. | 2015
- 374
-
Structure and properties of the Fe3Al-type intermetallic alloy fabricated by laser engineered net shaping (LENS)Durejko, Tomasz / Ziętala, Michał / Łazińska, Magda / Lipiński, Stanisław / Polkowski, Wojciech / Czujko, Tomasz / Varin, Robert A. et al. | 2015
- 382
-
Effect of cooling rate on damping capacity of Fe–Cr based ferromagnetic metal alloyWang, Hui / Wang, Fu / Xiao, Jun / Wang, Yuan / Ma, Ce / Dou, Zuoyong / Wang, Min / Zhang, Pengcheng et al. | 2015
- 389
-
Thermal mechanical fatigue of single crystal superalloys: Achievements and challengesZhang, Wei-Jun et al. | 2015
- 396
-
Effect of initial base metal temper on microstructure and mechanical properties of friction stir processed Al-7B04 alloyChen, Yu / Ding, Hua / Cai, Zhihui / Zhao, Jingwei / Li, Jizhong et al. | 2015
- 404
-
Enhanced mechanical response of an ultrafine grained Ti–6Al–4V alloy produced through warm symmetric and asymmetric rollingChao, Qi / Cizek, Pavel / Wang, Jiangting / Hodgson, Peter D. / Beladi, Hossein et al. | 2015
- 414
-
Low-temperature superplastic behavior of beta titanium alloyDu, Zhaoxin / Liu, Jingshun / Li, Guowei / Lv, Kai / Liu, Guolong / Yan, Liangming / Chen, Yuyong et al. | 2015
- 422
-
Deformation mechanisms of IN713C nickel based superalloy during Small Punch TestingColeman, M. / Alshehri, H. / Banik, R. / Harrison, W. / Birosca, S. et al. | 2015
- 432
-
Microstructure and mechanical properties of commercially pure titanium foam with varied cell size fabricated by replica impregnation methodManonukul, Anchalee / Srikudvien, Pathompoom / Tange, Makiko et al. | 2015
- 438
-
The potential significance of microalloying with niobium in governing very high cycle fatigue behavior of bainite/martensite multiphase steelsZhao, P. / Cheng, C. / Gao, G. / Hui, W. / Misra, R.D.K. / Bai, B. / Weng, Y. et al. | 2015
- 445
-
Plastic deformation in nanocrystalline TiN at ultra-low stress: An in situ nanoindentation studyJian, Jie / Lee, Joon Hwan / Liu, Yue / Khatkhatay, Fauzia / Yu, Kaiyuan / Su, Qing / Zhang, Xinghang / Jiao, Liang / Wang, Haiyan et al. | 2015
- 454
-
Influence of thickness reduction per pass on strain, microstructures and mechanical properties of 7050 Al alloy sheet processed by asymmetric rollingMa, Cunqiang / Hou, Longgang / Zhang, Jishan / Zhuang, Linzhong et al. | 2015
- 469
-
Microstructure and strengthening mechanism of Si3N4/Invar joint brazed with TiNp-doped fillerWang, Tianpeng / Liu, Chunfeng / Leinenbach, Christian / Zhang, Jie et al. | 2015
- 478
-
Microstructure and mechanical properties of (B4C+Al3Ti)/Al hybrid composites fabricated by a two-step stir casting processHu, Qiyao / Zhao, Haidong / Ge, Jilong et al. | 2015
- 483
-
Flow softening of 253 MA austenitic stainless steel during hot compression at higher strain ratesZhang, Jingqi / Di, Hongshuang / Wang, Xiaoyu et al. | 2015
- 492
-
Deformation and fracture characteristics of ultrafine-grained vanadiumHohenwarter, A. / Wurster, S. et al. | 2015
- 497
-
The effect of loading direction and Sn alloying on the deformation modes of Zr: An in-situ neutron diffraction studyMani Krishna, K.V. / Leo Prakash, D.G. / Timár, Gábor / Fitzner, Arnas / Srivastava, D. / Saibaba, N. / Quinta da Fonseca, J. / Dey, G.K. / Preuss, M. et al. | 2015
- 510
-
Extending an empirical and a fundamental bainite start model to a continuously cooled microalloyed steelKhodaie, Nasseh / Ivey, Douglas G. / Henein, Hani et al. | 2015
- 523
-
Enhanced mechanical behavior and reduced mechanical anisotropy of AZ31 Mg alloy sheet processed by ECAPSuh, Joungsik / Victoria-Hernández, José / Letzig, Dietmar / Golle, Roland / Volk, Wolfram et al. | 2015
- 530
-
Author Index| 2015
- 533
-
Subject Index| 2015
- IFC
-
Editorial Board| 2015