Lateral and vertical size effects on nanoindented microstructures (English)
- New search for: Wang, Tong Hong
- New search for: Fang, Te-Hua
- New search for: Wang, Tong Hong
- New search for: Fang, Te-Hua
In:
Computational Materials Science
;
46
, 4
;
1007-1013
;
2009
-
ISSN:
- Article (Journal) / Electronic Resource
-
Title:Lateral and vertical size effects on nanoindented microstructures
-
Contributors:Wang, Tong Hong ( author ) / Fang, Te-Hua ( author )
-
Published in:Computational Materials Science ; 46, 4 ; 1007-1013
-
Publisher:
- New search for: Elsevier B.V.
-
Publication date:2009-05-07
-
Size:7 pages
-
ISSN:
-
DOI:
-
Type of media:Article (Journal)
-
Type of material:Electronic Resource
-
Language:English
-
Keywords:
-
Source:
Table of contents – Volume 46, Issue 4
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 777
-
Combined analytical/numerical modelling of nucleation and growth during equiaxed solidification under the influence of thermal convectionMirihanage, Wajira U. / Browne, David J. et al. | 2009
- 785
-
Investigation of integration algorithms for rate-dependent crystal plasticity using explicit finite element codesDumoulin, S. / Hopperstad, O.S. / Berstad, T. et al. | 2009
- 800
-
Prediction of cold rolling texture of steels using an Artificial Neural NetworkBrahme, Abhijit / Winning, Myrjam / Raabe, Dierk et al. | 2009
- 805
-
Prediction of relationships between hydrostatic coefficients and processing parameters of porous PZT ceramics by radial basis functionPraveenkumar, B. / Vijayakumar, C. / Kumar, H.H. / Kharat, D.K. et al. | 2009
- 810
-
Single fibre and multifibre unit cell analysis of strength and cracking of unidirectional compositesWang, H.W. / Zhou, H.W. / Mishnaevsky, L. Jr. / Brøndsted, P. / Wang, L.N. et al. | 2009
- 821
-
Analyzing Fe–Zn system using molecular dynamics, evolutionary neural nets and multi-objective genetic algorithmsBhattacharya, Baidurya / Dinesh Kumar, G.R. / Agarwal, Akash / Erkoç, Şakir / Singh, Arunima / Chakraborti, Nirupam et al. | 2009
- 828
-
Single and double plate impact welding: Experimental and numerical simulationChizari, M. / Barrett, L.M. et al. | 2009
- 834
-
Modelling of laser forming – An reviewShen, Hong / Vollertsen, Frank et al. | 2009
- 834
-
Modelling of laser forming - a reviewHong, Shen / Vollertsen, Frank et al. | 2009
- 841
-
Finite element analysis of combined heat and mass transfer in hydromagnetic micropolar flow along a stretching sheetKumar, Lokendra et al. | 2009
- 849
-
Structural and thermochemical properties, and energetics of C8(NO2)8 and C20(NO2)4n (n=0–4)Peköz, Rengin / Erkoç, Şakir et al. | 2009
- 854
-
Thermo-mechanical vibration of a single-walled carbon nanotube embedded in an elastic medium based on nonlocal elasticity theoryMurmu, T. / Pradhan, S.C. et al. | 2009
- 860
-
Two semi-empirical approaches for the prediction of oxide ionic conductivities in ABO3 perovskitesXu, Liu / Wencong, Lu / Chunrong, Peng / Qiang, Su / Jin, Guo et al. | 2009
- 869
-
A 3D fourth order fabric tensor approach of anisotropy in granular mediaRahmoun, Jamila / Kondo, Djimédo / Millet, Olivier et al. | 2009
- 881
-
Prediction study of the structural, elastic and electronic properties of ANSr3 (A=As, Sb and Bi)Haddadi, K. / Bouhemadou, A. / Louail, L. / Rahal, F. / Maabed, S. et al. | 2009
- 887
-
Optimization approach in variable-charge potential for metal/metal oxide systemsSoontrapa, C. / Chen, Y. et al. | 2009
- 893
-
Construction of a constitutive model in calculations of pressure-dependent materialHu, Weilong / Wang, Z.R. et al. | 2009
- 902
-
ETMB model investigation of flow softening during severe plastic deformationHosseini, E. / Kazeminezhad, M. et al. | 2009
- 906
-
Effect of thermomechanical loads on the propagation of crack near the interface brittle/ductileBoutabout, Benali / Chama, Mourad / Bouiadjra, Bel Abbes Bachir / Serier, Boualem / Lousdad, Abdelkader et al. | 2009
- 912
-
Loading path effect on the chemical expansion in substoichiometric LSF based perovskiteValentin, O. / Blond, E. / Julian, A. / Richet, N. et al. | 2009
- 921
-
Structural, elastic and electronic properties of intermetallics in the Pt–Sn system: A density functional investigationZhou, Wei / Liu, Lijuan / Li, Baoling / Wu, Ping / Song, Qinggong et al. | 2009
- 932
-
Modeling the effect of grain clustering on the intergranular crack-propagation behaviour in polycrystalline materialsArafin, M.A. / Szpunar, J.A. et al. | 2009
- 942
-
Interfacial interactions in clay-based nylon 6 nanocomposites: A density functional theory studyMrayed, S.M. / Zeng, Q.H. / Yu, A.B. et al. | 2009
- 950
-
Analysis of the plastic zone size ahead of repaired cracks with bonded composite patch of metallic aircraft structuresOudad, W. / Bachir Bouiadjra, B. / Belhouari, M. / Touzain, S. / Feaugas, X. et al. | 2009
- 955
-
Modelling of the break up mechanism in gas atomization of liquid metals Part II. The gas flow modelAntipas, G.S.E. et al. | 2009
- 960
-
Local and global instabilities in nanosize rectangular prismatic gold specimensBatra, R.C. / Pacheco, A.A. et al. | 2009
- 977
-
Modeling buckling distortion of DP600 overlap joints due to gas metal arc welding and the influence of the mesh densitySchenk, T. / Richardson, I.M. / Kraska, M. / Ohnimus, S. et al. | 2009
- 987
-
Influences of heat source model on welding residual stress and distortion in a multi-pass J-groove jointKiyoshima, Shoichi / Deng, Dean / Ogawa, Kazuo / Yanagida, Nobuyoshi / Saito, Koichi et al. | 2009
- 996
-
Experimental and numerical study of the Young’s modulus vs temperature for heterogeneous model materials with polygonal inclusionsQi, B. / Absi, J. / Tessier-Doyen, N. et al. | 2009
- 1002
-
Finite element simulation of the effects of process parameters on deposition uniformity of chemical-vapor-deposited silicon carbideSun, Guodong / Li, Hejun / Fu, Qiangang / Huang, Min / Cao, Wei / Wu, Heng et al. | 2009
- 1007
-
Lateral and vertical size effects on nanoindented microstructuresWang, Tong Hong / Fang, Te-Hua et al. | 2009
- 1014
-
Finite element simulation of the residual stresses in high strength carbon steel butt weld incorporating solid-state phase transformationLee, Chin-Hyung / Chang, Kyong-Ho et al. | 2009
- 1023
-
Analysis of the distribution of thermal residual stresses in bonded composite repair of metallic aircraft structuresAminallah, L. / Achour, T. / Bachir Bouiadjra, B. / Serier, B. / Amrouche, A. / Feaugas, X. / Benssediq, N. et al. | 2009
- 1028
-
Network numerical analysis of magneto-micropolar convection through a vertical circular non-Darcian porous medium conduitZueco, Joaquín / Bég, O. Anwar / Takhar, H.S. et al. | 2009
- 1038
-
Numerical modeling the bonding mechanism of HVOF sprayed particlesKamnis, S. / Gu, S. / Lu, T.J. / Chen, C. et al. | 2009
- 1044
-
Dependencies of grain refinement on processing route and die angle in equal channel angular extrusion of bcc materialsLi, Saiyi et al. | 2009
- 1051
-
Elastic, electronic and optical properties of cubic antiperovskites SbNCa3 and BiNCa3Moakafi, M. / Khenata, R. / Bouhemadou, A. / Semari, F. / Reshak, Ali H. / Rabah, M. et al. | 2009
- 1058
-
Numerical study on the deformation behaviors of the flexible die forming by using viscoplastic pressure-carrying mediumFu, M.W. / Li, H. / Lu, J. / Lu, S.Q. et al. | 2009
- 1069
-
Directional solidification of an Al–Pb alloy in a static magnetic fieldLi, Haili / Zhao, Jiuzhou et al. | 2009
- 1076
-
Structural and electronic properties of BiOX (X=F, Cl, Br, I) considering Bi 5f statesHuang, Wen Lai / Zhu, Qingshan et al. | 2009
- 1085
-
Adsorption of formaldehyde molecule on the intrinsic and Al-doped graphene: A first principle studyChi, Mei / Zhao, Ya-Pu et al. | 2009
- 1091
-
Stress orientation of second-phase in alloys: Hydrides in zirconium alloysMassih, A.R. / Jernkvist, L.O. et al. | 2009
- 1098
-
First principles investigation on the structural, mechanical and electronic properties of OsC2Cai, Jun / Zhao, Erjun / Wu, Zhijian et al. | 2009
- 1102
-
Analysis of the transverse cracking in hybrid cross-ply composite laminatesEl Meiche, N. / Tounsi, A. / Adda-Bedia, E.A. / Megueni, A. et al. | 2009
- 1109
-
Numerical analysis of multipoint CDW welding process on stainless AISI304 steel barsCavaliere, P. / Dattoma, V. / Panella, F.W. et al. | 2009
- 1119
-
Analysis of interfacial fracture in ceramic–metal assemblies under effect of thermal residual stressesDrai, A. / Bouiadjra, B. Bachir / Meddah, M. / Benguediab, M. et al. | 2009
- 1124
-
Strengthening mechanism in micro-polycrystals with penetrable grain boundaries by discrete dislocation dynamics simulation and Hall–Petch effectLi, Zhenhuan / Hou, Chuantao / Huang, Minsheng / Ouyang, Chaojun et al. | 2009
- 1135
-
A framework for stress computation in single-walled carbon nanotubes under uniaxial tensionRagab, Tarek / Basaran, Cemal et al. | 2009
- 1144
-
The joint effect of shape and size of reinforcement on progressive damage of random compositesAl-Ostaz, A. / Wu, W. / Alkhateb, H. / Alzebdeh, K.I. et al. | 2009
- 1152
-
A new constitutive model of austenitic stainless steel for cryogenic applicationsLee, Kyung Jun / Chun, Min Sung / Kim, Myung Hyun / Lee, Jae Myung et al. | 2009
- 1163
-
Development and validation of a 3D computational tool to describe concrete behaviour at mesoscale. Application to the alkali-silica reactionComby-Peyrot, Isabelle / Bernard, Fabrice / Bouchard, Pierre-Olivier / Bay, François / Garcia-Diaz, Eric et al. | 2009
- 1178
-
Mobility of small clusters of self-interstitial atoms in dilute Fe–Cr alloy studied by means of atomistic calculationsTerentyev, D. / Castin, N. et al. | 2009
- 1187
-
Rare earth elements in alpha-Ti: a first-principles investigationLu, Song / Hu, Qing-Miao / Yang, Rui / Johansson, B. / Vitos, Levente et al. | 2009
- 1187
-
Rare earth elements in α-Ti: A first-principles investigationLu, Song / Hu, Qing-Miao / Yang, Rui / Johansson, Börje / Vitos, Levente et al. | 2009
- 1187
-
Rare earth elements in a-Ti: A first-principles investigationLu, S. / Hu, Q. M. / Yang, R. / Johansson, B. / Vitos, L. et al. | 2009
- IFC
-
IFC| 2009