Nano-scratch, nanoindentation and fretting tests of 5–80nm ta-C films on Si(100) (English)
- New search for: Beake, B.D.
- New search for: Davies, M.I.
- New search for: Liskiewicz, T.W.
- New search for: Vishnyakov, V.M.
- New search for: Goodes, S.R.
- New search for: Beake, B.D.
- New search for: Davies, M.I.
- New search for: Liskiewicz, T.W.
- New search for: Vishnyakov, V.M.
- New search for: Goodes, S.R.
In:
Wear
;
301
, 1-2
;
575-582
;
2013
-
ISSN:
- Article (Journal) / Electronic Resource
-
Title:Nano-scratch, nanoindentation and fretting tests of 5–80nm ta-C films on Si(100)
-
Contributors:Beake, B.D. ( author ) / Davies, M.I. ( author ) / Liskiewicz, T.W. ( author ) / Vishnyakov, V.M. ( author ) / Goodes, S.R. ( author )
-
Published in:Wear ; 301, 1-2 ; 575-582
-
Publisher:
- New search for: Elsevier B.V.
-
Publication date:2013-01-28
-
Size:8 pages
-
ISSN:
-
DOI:
-
Type of media:Article (Journal)
-
Type of material:Electronic Resource
-
Language:English
-
Keywords:
-
Source:
Table of contents – Volume 301, Issue 1-2
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 1
-
Editorial Chairman's MessageBlau, Peter J. et al. | 2013
- 2
-
19th International Conference on Wear of Materials, Portland, Oregon, USA, 14-18 April 2013| 2013
- 4
-
Analyzing pin-on-ball wear tests by means of the Greenwood–Williamson contact modelStickel, Daniel / Wimmer, Markus A. / Fischer, Alfons et al. | 2012
- 11
-
Study on effect of strain rate on 3D surface asperity flattening in uniaxial planar compression by crystal plasticity finite element modellingLi, H.J. / Jiang, Z.Y. / Wei, D.B. et al. | 2013
- 19
-
Experimental and numerical analysis of dry contact in the pin on disc testBortoleto, E.M. / Rovani, A.C. / Seriacopi, V. / Profito, F.J. / Zachariadis, D.C. / Machado, I.F. / Sinatora, A. / Souza, R.M. et al. | 2012
- 27
-
Thermal analysis of washer-on-disk wear test by micro-genetic algorithmChu, Hsiao-Yeh / Lin, Jen Fin / Hsieh, Hung-Tai / Chen, Guan-Lin / Li, Yi-Ting / Tsai, Ping-Hsueh et al. | 2013
- 34
-
Introduction of a power law formulation to quantify the contact size effects on friction and wear responses of dry oscillating sliding contacts: Application to a chromium steel interfaceFouvry, S. / Merhej, R. et al. | 2013
- 47
-
Dynamic transient analysis of squealing vibration of a reciprocating sliding systemQian, W.J. / Chen, G.X. / Zhou, Z.R. et al. | 2012
- 57
-
Analytical predictive modeling of scuffing initiation in metallic materials in sliding contactAjayi, O.O. / Lorenzo-Martin, C. / Erck, R.A. / Fenske, G.R. et al. | 2012
- 62
-
A molecular dynamics simulation of boundary lubrication: The effect of n-alkanes chain length and normal loadZheng, Xuan / Zhu, Hongtao / Kosasih, Buyung / Kiet Tieu, A. et al. | 2013
- 70
-
Understanding the influence of microstructure features on the erosion resistance of low-carbon pipeline steel through computational simulationLi, Lei / Li, D.Y. et al. | 2013
- 76
-
The influence of abrasive body dimensions on single asperity wearWoldman, M. / Van Der Heide, E. / Tinga, T. / Masen, M.A. et al. | 2012
- 82
-
Effect of particle hardness on mild–severe wear transition of hard second phase materialsCoronado, J.J. / Rodríguez, S.A. / Sinatora, A. et al. | 2012
- 89
-
Design of low hardness abrasion resistant steelsXu, Xiaojun / Xu, Wei / Ederveen, Fre Hipgrave / Zwaag, Sybrand van der et al. | 2013
- 94
-
Surface deformation of steels in impact-abrasion: The effect of sample angle and test durationRatia, Vilma / Miettunen, Ilkka / Kuokkala, Veli-Tapani et al. | 2013
- 102
-
Abrasive impact wear and surface fatigue wear behaviour of Fe–Cr–C PTA overlaysVeinthal, Renno / Sergejev, Fjodor / Zikin, Arkadi / Tarbe, Riho / Hornung, Johann et al. | 2013
- 109
-
On a wear test for rock drill insertsAngseryd, Jenny / From, Anna / Wallin, Johan / Jacobson, Staffan / Norgren, Susanne et al. | 2012
- 116
-
Modification of carbidic austempered ductile iron with nano ceria for improved mechanical properties and abrasive wear resistanceSun, Xiaoguang / Wang, You / Li, D.Y. / Wang, Guodong et al. | 2012
- 122
-
Friction and wear of fiber reinforced polyimide compositesZhao, Gai / Hussainova, Irina / Antonov, Maksim / Wang, Qihua / Wang, Tingmei et al. | 2012
- 130
-
Effect of load partition and particle distribution on micro-abrasive wear mapping of two-phase metal matrix compositesGava, G.H.S. / Souza, R.M. / de Mello, J.D.B. / de Macêdo, M.C.S. / Scandian, C. et al. | 2012
- 137
-
In-situ nanopolishing by nanolubricants for enhanced elastohydrodynamic lubricationMosleh, Mohsen / Shirvani, Khosro A. et al. | 2013
- 144
-
Tactile and visual perception during polishing: An ethnoarchaeological study in India (Mahabalipuram, Tamil Nadu)Procopiou, H. / Morero, E. / Vargiolu, R. / Suarez-Sanabria, M. / Zahouani, H. et al. | 2012
- 150
-
Carving techniques of Fatimid rock crystal ewers (10–12th cent. A.D.)Morero, E. / Procopiou, H. / Vargiolu, R. / Johns, J. / Zahouani, H. et al. | 2013
- 157
-
Wear of ultra-high molecular weight polyethylene moving along a circular path in a hip simulatorWang, Aiguo / Lee, Reginald / Herrera, Lizeth / Korduba, Laryssa et al. | 2012
- 162
-
Modeling and verification of ultra-high molecular weight polyethylene wear in multi-directional slidingWang, Aiguo / Lee, Reginald / Herrera, Lizeth / Korduba, Laryssa et al. | 2012
- 168
-
Cross-shear in metal-on-polyethylene articulation of orthopaedic implants and its relationship to wearSchwenke, T. / Wimmer, M.A. et al. | 2013
- 175
-
A study of the wear performance in a hip simulator of a metal–metal Co–Cr alloy with different boron additionsAlvarez-Vera, M. / Ortega-Saenz, J.A. / Hernandez-Rodríguez, M.A.L. et al. | 2013
- 182
-
Investigation of three-dimensional surface topographies and mechanical properties of hypothesized biological active wear particles from artificial jointsWu, Jingping / Peng, Zhongxiao / Tipper, Joanne et al. | 2012
- 188
-
Study of the nano-mechanical properties of human knee cartilage in different wear conditionsWang, M. / Peng, Z. / Price, J. / Ketheesan, N. et al. | 2012
- 192
-
Predicting the wear of hard-on-hard hip joint prosthesesUddin, M.S. / Zhang, L.C. et al. | 2013
- 201
-
Investigation of friction and surface degradation of innovative boundary lubricant functionalized hydrogel material for use as artificial articular cartilageBlum, Michelle M. / Ovaert, Timothy C. et al. | 2012
- 210
-
Three dimensional surface characterization of human cartilages at a micron and nanometre scalePeng, Zhongxiao / Wang, Meiling et al. | 2012
- 218
-
Tribological characterization of polyvinyl alcohol hydrogel as substitute of articular cartilageSardinha, V.M. / Lima, L.L. / Belangero, W.D. / Zavaglia, C.A / Bavaresco, V.P. / Gomes, J.R. et al. | 2012
- 226
-
Failure analysis of cemented metal-on-metal total hip replacements from a single centre cohortBryant, Michael / Ward, Michael / Farrar, Richard / Freeman, Robert / Brummitt, Ken / Nolan, John / Neville, Anne et al. | 2012
- 234
-
Biotribological study of multilayer coated metal-on-metal hip prostheses in a hip joint simulatorOrtega-Saenz, J.A. / Alvarez-Vera, M. / Hernandez-Rodriguez, M.A.L. et al. | 2013
- 243
-
Biotribological response of CoCr alloy with added boron under ball-on-disc testsAlvarez-Vera, M. / Juarez-Hernandez, A. / Gonzalez-Rivera, C.E. / Mercado-Solis, R.D. / Hernandez-Rodriguez, M.A.L. et al. | 2012
- 250
-
Pulsed electron beam surface melting of CoCrMo alloy for biomedical applicationsWalker, J.C. / Cook, R.B. / Murray, J.W. / Clare, A.T. et al. | 2013
- 257
-
Surface layer plastic deformation as a mechanism for UHMWPE wear, and its role in debris size.Plumlee, K.G. / Schwartz, C.J. et al. | 2012
- 264
-
The effect of bacterial contamination on friction and wear in metal/polyethylene bearings for total joint repair—A case reportWimmer, M.A. / Sah, R. / Laurent, M.P. / Virdi, A.S. et al. | 2012
- 271
-
Bulk metallic glasses (BMG) for biomedical applications—A tribocorrosion investigation of Zr55Cu30Ni5Al10 in simulated body fluidEspallargas, N. / Aune, R.E. / Torres, C. / Papageorgiou, N. / Muñoz, A.I. et al. | 2012
- 280
-
S-phase against S-phase tribopairs for biomedical applicationsBuhagiar, J. / Jung, A. / Gouriou, D. / Mallia, B. / Dong, H. et al. | 2012
- 290
-
Fretting corrosion of fully cemented polished collarless tapered stems: The influence of PMMA bone cementBryant, M. / Farrar, R. / Brummitt, K. / Freeman, R. / Neville, A. et al. | 2012
- 300
-
Effect of adsorption time on the lubricating properties of the salivary pellicle on human tooth enamelZhang, Y.F. / Zheng, J. / Zheng, L. / Shi, X.Y. / Qian, L.M. / Zhou, Z.R. et al. | 2012
- 308
-
A comparative study on the sliding wear behaviors of human tooth enamel, Cu–Zn alloy and Al2O3 ceramicZheng, L. / Li, Y. / Zheng, J. / Wen, M. / Zhang, Y.F. / Qian, L.M. / Zhou, Z.R. et al. | 2012
- 316
-
Effect of water content on the nanomechanical properties and microtribological behaviour of human tooth enamelZheng, J. / Weng, L.Q. / Shi, M.Y. / Zhou, J. / Hua, L.C. / Qian, L.M. / Zhou, Z.R. et al. | 2012
- 324
-
Stick–slip phenomena in the friction of human skinDerler, S. / Rotaru, G.-M. et al. | 2012
- 330
-
Human finger friction in contacts with ridged surfacesTomlinson, S.E. / Lewis, R. / Carré, M.J. / Franklin, S.E. et al. | 2012
- 338
-
The friction measurement between finger skin and material surfacesKim, Min-Seob / Kim, Il-Young / Park, Yon-Kyu / Lee, Young-Ze et al. | 2012
- 343
-
Effect of roughness on vibration of human finger during a friction testZahouani, H. / Mezghani, S. / Vargiolu, R. / Hoc, T. / EL Mansori, M. et al. | 2012
- 353
-
Influence of exfoliating facial cleanser on the bio-tribological properties of human skinLi, W. / Zhai, Z.H. / Pang, Q. / Kong, L. / Zhou, Z.R. et al. | 2012
- 362
-
Biomimetic touch perception of edge finish of ophthalmic lensEl Mansori, M. / Mezghani, S. / Zahouani, H. / Divo, F. et al. | 2013
- 370
-
Exploring the erosive wear of X65 carbon steel by acoustic emission methodUkpai, Jonathan I. / Barker, Richard / Hu, Xinming / Neville, Anne et al. | 2012
- 383
-
Study of solid particle erosion on AISI 420 stainless steel using angular silicon carbide and steel round grit particlesVite-Torres, M. / Laguna-Camacho, J.R. / Baldenebro-Castillo, R.E. / Gallardo-Hernández, E.A. / Vera-Cárdenas, E.E. / Vite-Torres, J. et al. | 2013
- 390
-
Performances of hybrid high-entropy high-Cr cast irons during sliding wear and air-jet solid-particle erosionWang, Y.P. / Li, D.Y. / Parent, L. / Tian, H. et al. | 2012
- 398
-
Solid particle erosion of AISI 304, 316 and 420 stainless steelsLaguna-Camacho, J.R. / Marquina-Chávez, A. / Méndez-Méndez, J.V. / Vite-Torres, M. / Gallardo-Hernández, E.A. et al. | 2012
- 406
-
Mechanical properties and erosion resistance of ceria nano-particle-doped ultrafine WC–12Co composite prepared by spark plasma sinteringSun, Xiaoguang / Wang, You / Li, D.Y. et al. | 2013
- 415
-
Cavitation erosion of Cr60Ni40 coatings generated by friction surfacingHanke, S. / Beyer, M. / Silvonen, Aulis / dos Santos, J.F. / Fischer, A. et al. | 2012
- 424
-
Understanding Liquid Impingement erosion behaviour of nickel–alumina based thermal spray coatingsGrewal, H.S. / Singh, H. / Agrawal, Anupam et al. | 2013
- 434
-
Erosive wear of plasma electrolytic oxidation layers on aluminium alloy 6061Treviño, M. / Mercado-Solis, R.D. / Colás, R. / Pérez, A. / Talamantes, J. / Velasco, A. et al. | 2012
- 442
-
Water droplet erosion mechanisms in rolled Ti–6Al–4VKamkar, N. / Bridier, F. / Bocher, P. / Jedrzejowski, P. et al. | 2013
- 449
-
Cavitation erosion resistance of low temperature plasma nitrided martensitic stainless steelEspitia, L.A. / Varela, L. / Pinedo, C.E. / Tschiptschin, A.P. et al. | 2012
- 457
-
Cavitation erosion resistance of high interstitial CrMnCN austenitic stainless steelsNiederhofer, P. / Huth, S. et al. | 2012
- 467
-
A study of cavitation erosion on engineering materialsLaguna-Camacho, J.R. / Lewis, R. / Vite-Torres, M. / Méndez-Méndez, J.V. et al. | 2012
- 477
-
Wear of hydrotransport lines in Athabasca oil sandsParent, L.L. / Li, D.Y. et al. | 2013
- 483
-
A multilayer nodes update method in FEM simulation of large depth fretting wearTang, Lichen / Ding, Shurong / Xie, Yongcheng / Huo, Yongzhong et al. | 2012
- 491
-
The effect of contact geometry on fretting wear rates and mechanisms for a high strengthsteelWarmuth, A.R. / Pearson, S.R. / Shipway, P.H. / Sun, W. et al. | 2013
- 501
-
Effect of hardness differential on metal-to-metal fretting damageBudinski, Kenneth G. et al. | 2013
- 508
-
Application of plain fretting test to extract fatigue properties of materialsDuhart, J. / Fouvry, S. / Gourdet, S. et al. | 2013
- 517
-
A simple model for friction evolution infrettingHirsch, M.R. / Neu, R.W. et al. | 2013
- 524
-
Fretting studies on self-mated stainless steel and chromium carbide coated surfaces under controlled environment conditionsChaudhry, V. / Kailas, Satish V. et al. | 2013
- 540
-
Dual-rotary fretting wear of 7075 alloy in media of oil and waterShen, M.X. / Cai, Z.B. / Peng, J.F. / Song, C. / Mo, J.L. / Shen, H.M. / Zhu, M.H. et al. | 2013
- 551
-
An investigation of fretting wear behaviour of nickel coatings for electrical contacts application in dry and lubricated conditionsNoël, S. / Alamarguy, D. / Brézard-Oudot, A. / Gendre, P. et al. | 2013
- 562
-
Fretting wear characteristics of titanium matrix composites reinforced by titanium boride and titanium carbide particulatesKim, Jin-Seon / Lee, Kyung-Moo / Cho, Dae-Hyun / Lee, Young-Ze et al. | 2012
- 569
-
Fretting wear behavior of a nuclear fuel rod under a simulated primary coolant conditionLee, Young-Ho / Kim, Hyung-Kyu et al. | 2013
- 575
-
Nano-scratch, nanoindentation and fretting tests of 5–80nm ta-C films on Si(100)Beake, B.D. / Davies, M.I. / Liskiewicz, T.W. / Vishnyakov, V.M. / Goodes, S.R. et al. | 2013
- 583
-
The asymmetrical friction mechanism that puts the curl in the curling stoneNyberg, Harald / Alfredson, Sara / Hogmark, Sture / Jacobson, Staffan et al. | 2013
- 590
-
Sliding wear behavior of a high-Mn austenitic twinning induced plasticity (TWIP) steel microalloyed with NbMejía, I. / Bedolla-Jacuinde, A. / Pablo, J.R. et al. | 2013
- 598
-
Interface adhesion during sliding wear in cast iron after hot deformationZhang, Q. / Jiang, Z.Y. / Wei, D.B. / Zhu, H.T. / Chen, Z.X. / Han, J.T. / Xie, G.L. et al. | 2012
- 608
-
Dry sliding tribological properties and subsurface structure of nanostructured copper at liquid nitrogen temperatureYao, B. / Han, Z. / Lu, K. et al. | 2012
- 615
-
Dry sliding wear behavior of AM60B magnesium alloyTaltavull, C. / Torres, B. / López, A.J. / Rams, J. et al. | 2012
- 626
-
Sliding wear mechanisms of magnesium composites AM60 reinforced with Al2O3 fibres under ultra-mild wear conditionsBanerji, A. / Hu, H. / Alpas, A.T. et al. | 2013
- 636
-
The effect of magnetic field on the wear properties of a ferromagnetic steelYetim, A.F. / Kovacı, H. / Aslan, M. / Çelik, A. et al. | 2012
- 641
-
Microstructure and tribological properties of reactive hot pressed TiN–TiB2 composites incorporated with or without MoSi2 from room temperature to 800°CYang, Zhen-Lin / Ouyang, Jia-Hu / Liu, Zhan-Guo / Liang, Xue-Song / Wang, Yu-Jin et al. | 2013
- 648
-
Effect of the metallic matrix on the sliding wear of plasma assisted debinded and sintered MIM self-lubricating steelde Mello, José Daniel B. / Binder, Cristiano / Hammes, Gisele / Klein, Aloisio N. et al. | 2013
- 656
-
Effects of thermal and thermomechanical treatments on sliding wear of graphite crystallised white cast ironGao, X.J. / Zhang, Q. / Wei, D.B. / Jiao, S.H. / Jiang, Z.Y. et al. | 2012
- 663
-
Analysis of the high speed sliding interaction between titanium alloy and tantalumList, G. / Sutter, G. / Arnoux, J.J. et al. | 2012
- 671
-
The effect of groove-textured surface on friction and wear and friction-induced vibration and noiseMo, J.L. / Wang, Z.G. / Chen, G.X. / Shao, T.M. / Zhu, M.H. / Zhou, Z.R. et al. | 2013
- 682
-
Wear and dent resistance of superelastic TiNi alloyNeupane, Rabin / Farhat, Zoheir et al. | 2012
- 688
-
Dry sliding wear of gradient AlNi/SiC compositesLeón-Patiño, C.A. / Aguilar-Reyes, E.A. / Bedolla-Becerril, E. / Bedolla-Jacuinde, A. / Méndez-Díaz, S. et al. | 2012
- 695
-
Microstructure refinement of hypereutectic high Cr cast irons using hard carbide-forming elements for improved wear resistanceChung, R.J. / Tang, X. / Li, D.Y. / Hinckley, B. / Dolman, K. et al. | 2013
- 707
-
Role of sliding-induced tribofilms on fracture of particles in aluminium–silicon alloysBhattacharya, S. / Alpas, A.T. et al. | 2013
- 717
-
Failure mode in sliding wear of PEEK based compositesSchroeder, R. / Torres, F.W. / Binder, C. / Klein, A.N. / de Mello, J.D.B. et al. | 2012
- 727
-
Influence of linear reciprocating and multi-directional sliding on PEEK wear performance and transfer film formationLaux, K.A. / Schwartz, C.J. et al. | 2012
- 735
-
Strengthening of CF/PEEK interface to improve the tribological performance in low amplitude oscillating wear modeSharma, Mohit / Bijwe, Jayashree / Mäder, Edith / Kunze, Klaus et al. | 2012
- 740
-
A low-viscosity ionic liquid demonstrating superior lubricating performance from mixed to boundary lubricationMordukhovich, Gregory / Qu, Jun / Howe, Jane Y. / Bair, Scott / Yu, Bo / Luo, Huimin / Smolenski, Donald J. / Blau, Peter J. / Bunting, Bruce G. / Dai, Sheng et al. | 2012
- 747
-
Tribological and thermal characteristics of reduced phosphorus plain ZDDP oil in the presence of PTFE/FeF3/TiF3 under optimized extreme loading condition and a break in period using two different rotational speedsNehme, Gabi et al. | 2012
- 753
-
Sliding tribological properties of 0.45% carbon steel lubricated with Fe3O4 magnetic nano-particle additives in baseoilZhou, Guanghong / Zhu, Yufu / Wang, Xiangming / Xia, Mujian / Zhang, Yue / Ding, Hongyan et al. | 2013
- 758
-
Running-in due to material transfer of lubricated steel/PA46 (aliphatic polyamide) contactsScherge, Matthias / Kramlich, Jeanette / Böttcher, Roman / Hoppe, Tobias et al. | 2012
- 763
-
Tribological characteristics of paraffin liquid with nanodiamond based on the scuffing life and wear amountKim, Hyun-Soo / Park, Jin-Whak / Park, Se-Min / Lee, Jung-Suk / Lee, Young-Ze et al. | 2013
- 768
-
Wear of sintered HSS under combined squeeze–sliding lubricationMessaadi, Maha / Bouvard, Gaétan / Yang, Jiao / Kapsa, Philippe et al. | 2012
- 776
-
Tribological behavior of nano TiO2 as an additive in base oilIngole, Sudeep / Charanpahari, Archana / Kakade, Amol / Umare, S.S. / Bhatt, D.V. / Menghani, Jyoti et al. | 2013
- 786
-
Sliding wear and friction behavior of CrN-coating in ethanol and oil–ethanol mixtureBandeira, A.L. / Trentin, R. / Aguzzoli, C. / Maia da Costa, M.E.H. / Michels, A.F. / Baumvol, I.J.R. / Farias, M.C.M. / Figueroa, C.A. et al. | 2013
- 795
-
Reprint of Nanowear behaviour of monocrystalline silicon against SiO2 tip in waterWang, X.D. / Song, C.F. / Yu, B.J. / Chen, L. / Qian, L.M. et al. | 2012
- 802
-
Surface lubrication of graphite fabric reinforced epoxy composites with nano- and micro-sized hexagonal boron nitrideKadiyala, Ajay Kumar / Bijwe, Jayashree et al. | 2012
- 810
-
Exploration of potential of solid lubricants and short fibers in Polyetherketone (PEK) compositesBijwe, Jayashree / Sharma, Sanjeev / Sharma, Mohit / Parida, Tushar / Trivedi, Prakash et al. | 2013
- 820
-
Friction and wear properties of hot-pressed NiCr–BaCr2O4 high temperature self-lubricating compositesOuyang, Jia-Hu / Liang, Xue-Song / Liu, Zhan-Guo / Yang, Zhen-Lin / Wang, Yu-Jin et al. | 2013
- IFC
-
Editorial board| 2013