Dependence of room-temperature nanoindentation creep behavior and shear transformation zone on the glass transition temperature in bulk metallic glasses (English)
- New search for: Zhao, X.N.
- New search for: Cao, Q.P.
- New search for: Wang, C.
- New search for: Wang, X.D.
- New search for: Zhang, D.X.
- New search for: Qu, S.X.
- New search for: Jiang, J.Z.
- New search for: Zhao, X.N.
- New search for: Cao, Q.P.
- New search for: Wang, C.
- New search for: Wang, X.D.
- New search for: Zhang, D.X.
- New search for: Qu, S.X.
- New search for: Jiang, J.Z.
In:
Journal of Non-Crystalline Solids
;
445-446
;
19-29
;
2016
-
ISSN:
- Article (Journal) / Electronic Resource
-
Title:Dependence of room-temperature nanoindentation creep behavior and shear transformation zone on the glass transition temperature in bulk metallic glasses
-
Contributors:Zhao, X.N. ( author ) / Cao, Q.P. ( author ) / Wang, C. ( author ) / Wang, X.D. ( author ) / Zhang, D.X. ( author ) / Qu, S.X. ( author ) / Jiang, J.Z. ( author )
-
Published in:Journal of Non-Crystalline Solids ; 445-446 ; 19-29
-
Publisher:
- New search for: Elsevier B.V.
-
Publication date:2016-05-08
-
Size:11 pages
-
ISSN:
-
DOI:
-
Type of media:Article (Journal)
-
Type of material:Electronic Resource
-
Language:English
-
Keywords:
-
Source:
Table of contents – Volume 445-446
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 1
-
Detection of “free” oxide ions in low-silica Ca/Mg silicate glasses: Results from 17O→ 29Si HETCOR NMRHung, Ivan / Gan, Zhehong / Gor'kov, Peter L. / Kaseman, Derrick C. / Sen, Sabyasachi / LaComb, Michelle / Stebbins, Jonathan F. et al. | 2016
- 7
-
Correlation of structural, thermo-kinetic and thermo-mechanical properties of the Ge11Ga11Te78 glassSvoboda, Roman / Stříteský, Daniel / Zmrhalová, Zuzana / Brandová, Daniela / Málek, Jiří et al. | 2016
- 15
-
Hard-sphere behavior in the dynamics of all mono-atomic liquids at the de Gennes minimumMontfrooij, Wouter et al. | 2016
- 19
-
Dependence of room-temperature nanoindentation creep behavior and shear transformation zone on the glass transition temperature in bulk metallic glassesZhao, X.N. / Cao, Q.P. / Wang, C. / Wang, X.D. / Zhang, D.X. / Qu, S.X. / Jiang, J.Z. et al. | 2016
- 30
-
Transport properties of the sodium-yttrium-silicate glassesNechaev, G.V. / Vlasova, S.G. / Kovyazina, I.S. / Reznitskich, O.G. et al. | 2016
- 34
-
Thermal history dependence of indentation induced densification in an aluminosilicate glassStriepe, Simon / Deubener, Joachim / Potuzak, Marcel / Smedskjaer, Morten M. / Matthias, Anja et al. | 2016
- 40
-
Novel oxyfluorophosphate glasses and glass-ceramicsCui, S. / Massera, J. / Lastusaari, M. / Hupa, L. / Petit, L. et al. | 2016
- 45
-
Elasticity and viscosity of BaOTiO2 SiO2 glasses in the 0.9 to 1.2Tg temperature intervalMezeix, P. / Célarié, F. / Houizot, P. / Gueguen, Y. / Muñoz, F. / Rouxel, T. et al. | 2016
- 53
-
Effect of annealing on the devitrification behavior and mechanical properties of rapidly quenched Ce-based glassy alloysSingh, Dharmendra / Singh, Devinder / Mandal, R.K. / Srivastava, O.N. / Tiwari, R.S. et al. | 2016
- 61
-
Size distribution of shear transformation zones and their evolution towards the formation of shear bands in metallic glassesZhong, C. / Zhang, H. / Cao, Q.P. / Wang, X.D. / Zhang, D.X. / Ramamurty, U. / Jiang, J.Z. et al. | 2016
- 69
-
Design of air aging induced surface patterns on 45S5 Bioglass® compacted by spark plasma sinteringLi, Zhong / Hu, Huanlong / Khor, Khiam Aik et al. | 2016
- 77
-
Improved color rendering index and thermal stability of white LEDs with phosphor-in-glass using the SiO2-B2O3-ZnO-Na2O glass systemHan, Karam / Lee, Sang Hun / Choi, Yong Gyu / Im, Won Bin / Chung, Woon Jin et al. | 2016
- 81
-
Synthesis, characterization and in-vitro studies of strontium-zinc co-substituted fluorohydroxyapatite for biomedical applicationsSanyal, Vijayalakshmi / Raja, C. Ramachandra et al. | 2016
- 88
-
Role of niobium and oxygen concentration on glass forming ability and crystallization behavior of Zr-Ni-Al-Cu-Nb bulk metallic glasses with low copper concentrationCole, K.M. / Kirk, D.W. / Singh, C.V. / Thorpe, S.J. et al. | 2016
- 95
-
Water molecular dynamics of metakaolin and phosphoric acid-based geopolymers investigated by impedance spectroscopy and DSC/TGADouiri, H. / Kaddoussi, I. / Baklouti, S. / Arous, M. / Fakhfakh, Z. et al. | 2016
- 102
-
Mechanical properties of silica glass predicted by a pair-wise potential in molecular dynamics simulationsSundararaman, Siddharth / Ching, Wai-Yim / Huang, Liping et al. | 2016
- 110
-
Influence of the preparation conditions of erbium-doped bismuth germanate glasses on its optical responseCabello, F. / Sanchez-Cortes, S. / Jiménez de Castro, M. et al. | 2016
- 116
-
Non-isothermal crystallization kinetics of stoichiometric lithium disilicate-based glasses with Al2O3 additivesBai, Yang / Peng, Lian / Zhu, Qingshan / Hao, Zhigang et al. | 2016
- IFC
-
Editorial Board| 2016