The application of self-healing concept in Ni superalloys: Theoretical design and experimental validation (English)
Free access
- New search for: Yu, Hao
- Further information on Yu, Hao:
-
https://orcid.org/0000-0002-9576-1077
- New search for: Shao, Jianfeng
- New search for: Shuai, Sansan
- Further information on Shuai, Sansan:
-
https://orcid.org/0000-0003-3801-0944
- New search for: Chen, Chaoyue
- Further information on Chen, Chaoyue:
-
https://orcid.org/0000-0003-3696-7769
- New search for: Wang, Lingyu
- Further information on Wang, Lingyu:
-
https://orcid.org/0000-0002-5790-6052
- New search for: San-Martín, David
- Further information on San-Martín, David:
-
https://orcid.org/0000-0001-6720-3599
- New search for: Xu, Wei
- Further information on Xu, Wei:
-
https://orcid.org/0000-0002-4615-545X
- New search for: Yu, Hao
- New search for: Shao, Jianfeng
- New search for: Shuai, Sansan
- New search for: Chen, Chaoyue
- New search for: Wang, Lingyu
- New search for: San-Martín, David
- New search for: Xu, Wei
In:
Materials and Design
;
237
;
2023
-
ISSN:
- Article (Journal) / Electronic Resource
-
Title:The application of self-healing concept in Ni superalloys: Theoretical design and experimental validation
-
Contributors:Yu, Hao ( author ) / Shao, Jianfeng ( author ) / Shuai, Sansan ( author ) / Chen, Chaoyue ( author ) / Wang, Lingyu ( author ) / San-Martín, David ( author ) / Xu, Wei ( author )
-
Published in:Materials and Design ; 237
-
Publisher:
- New search for: The Authors
-
Publication date:2023-12-15
-
ISSN:
-
DOI:
-
Type of media:Article (Journal)
-
Type of material:Electronic Resource
-
Language:English
-
Keywords:
-
Source:
Table of contents – Volume 237
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
-
Minimal-surface-based multiphase metamaterials with highly variable stiffnessZheng, Xiaoyang / Watanabe, Ikumu / Wang, Siqian / Chen, Ta-Te / Naito, Masanobu et al. | 2023
-
Endoplasmic reticulum and mitochondrial double-targeted NIR photosensitizer synergistically promote tumor cell deathYang, Hekai / Li, Fahui / Chen, Shuzhen / Jin, Shanshan / Chen, Weiwei / Sun, Wen / Wei, Liuya / Xu, Guangzhao / Song, Weiguo / Zhong, Wenda et al. | 2023
-
The overview of the formation mechanisms of topologically close-packed phases in Ni-based single crystal superalloysCheng, Yuan / Zhao, Xinbao / Xia, Wanshun / Yue, Quanzhao / Gu, Yuefeng / Zhang, Ze et al. | 2023
-
Temperature-dependent evolution mechanism of interface microstructure between gradient MCrAlY coatings and nickel-based superalloyKang, Jie / Liu, Yuan / Zhou, Jun / Zhuo, WeiWei / Zhang, Jie / Zeng, Jiamin / Zhang, Heng / Pei, Yanling / Li, Shusuo / Gong, Shengkai et al. | 2023
-
The application of self-healing concept in Ni superalloys: Theoretical design and experimental validationYu, Hao / Shao, Jianfeng / Shuai, Sansan / Chen, Chaoyue / Wang, Lingyu / San-Martín, David / Xu, Wei et al. | 2023
-
A novel 3D printed compliant ball-end grinding tool with crystal structure: Feasibility and performance analysisLi, Mingcong / Huang, Yun / Wang, Wenxi / Yan, Shengbo / Liu, Yingjie / Zou, Lai et al. | 2023
-
Interaction and evolution of phases at the coating/substrate interface in galvannealed 3rd Gen AHSS with high Si contentMinenkov, Alexey / Arndt, Martin / Knapp, Johannes / Hesser, Günter / Gierl-Mayer, Christian / Mörtlbauer, Thomas / Angeli, Gerhard / Groiss, Heiko et al. | 2023
-
Unraveling solid–liquid phase transition and microstructural coarsening of semi-solid Al0.8Co0.5Cr1.5CuFeNi HEA with dual globules for thixoforming applicationHuang, Minjie / Jiang, Jufu / Wang, Ying / Liu, Yingze / Zhang, Ying / Dong, Jian / Cui, Jingbo et al. | 2023
-
Framework for additive manufacturing of porous Inconel 718 for electrochemical applicationsZafari, Ahmad / Kiran, Kiran / Gimenez-Garcia, Inmaculada / Xia, Kenong / Gibson, Ian / Jafari, Davoud et al. | 2023
-
3D-printed porous PEI/TCP composite scaffolds loaded with graphdiyne oxide on the surface for bone defect repair and near-infrared light-responsive antibacterialWang, Hao / Xu, Xinyu / Mei, Xiaohan / Zeng, Dapeng / Ying, Boda / Yu, Zehao / Liu, Shibo / Li, Ruiyan / Qin, Yanguo et al. | 2023
-
Study on the effect of dynamic chemical polishing treatment on porous titanium alloy scaffolds fabricated using laser powder bed fusionHu, Jinwang / Xue, Jingbo / Liu, Lulu / Liu, Yami / Li, Minmin / Wang, Fengtao / Peng, Wen et al. | 2023
-
Insight into grain boundaries with reduced liquid metal embrittlement susceptibility in a boron-added 3rd generation advanced high strength steelAkbari, Elahe / Kürnsteiner, Philipp / Steineder, Katharina / Gruber, Martin / Arndt, Martin / Letofsky-Papst, Ilse / Sierlinger, Robert / Groiss, Heiko et al. | 2023
-
Laser polishing and simultaneous hardening of the electrical discharge machined Zr-based metallic glass surfaceHong, Jing / Huang, Hu / Zhang, Lin / Zhang, Zhiyu / Jiang, Minqiang / Yan, Jiwang et al. | 2023
-
Advancing the precision of thermal Hall measurements for novel materials researchKojda, Danny / Sigusch, Ida / Klemke, Bastian / Gerischer, Sebastian / Kiefer, Klaus / Fritsch, Katharina / Guguschev, Christo / Habicht, Klaus et al. | 2023
-
Biomimetic amniotic/silicone-based bilayer membrane for corneal tissue engineeringEsmaeili, Zahra / Nokhbedehghan, Zeinab / Alizadeh, Sanaz / majidi, Jila / Chahsetareh, Hadi / Daryabari, Seyed-Hashem / Nazm-Bojnourdi, Maryam / Kadkhodaie, Majid / Ghaffari, Maryam / Hashemi, Ali et al. | 2023
-
An optimized lozenge-chiral auxetic metamaterial with tunable auxeticity and stiffnessHou, Runsheng / Dong, Peng / Hu, Jiayi / Gong, Zhi / Sadeghzade, Sorour / Cao, Jinrui / Yuan, Hongyan et al. | 2023
-
Reinforcing melt electrowritten elements with entangled multifibrillar strands for thin hydrogels with potential in bone resurfacingNicolae, Carmen-Valentina / Olăreț, Elena / Bratu, Adriana-Elena / Lungu, Adriana / Stancu, Izabela-Cristina / Mastalier Manolescu, Bogdan Stelian et al. | 2023
-
Processing and microstructure of a Cu-Al-Fe-Mn alloy via droplet-on-demand additive manufacturingTraxel, Kellen D. / Elton, Eric S. / Petersen, Amelia M. / Silva, Chinthaka M. / Perron, Aurélien / Jeffries, Jason R. / Pascall, Andrew J. et al. | 2023
-
Structural engineering of two-dimensional black phosphorus towards advanced photonic integrated circuitsYuan, Jian / Li, Zhixuan / Yu, Wenzhi / Xue, Yunzhou / Long, Gen / Li, Yanyong / Mu, Haoran / Li, Dabing / Lin, Shenghuang et al. | 2023
-
The road to the ideal stent: A review of stent design optimisation methods, findings, and opportunitiesKapoor, A. / Jepson, N. / Bressloff, N.W. / Loh, P.H. / Ray, T. / Beier, S. et al. | 2023
-
A 3D pantographic metamaterial behaving as a mechanical shield: Experimental and numerical evidenceCiallella, Alessandro / Giorgio, Ivan / Barchiesi, Emilio / Alaimo, Gianluca / Cattenone, Alberto / Smaniotto, Benjamin / Vintache, Antoine / D'Annibale, Francesco / dell'Isola, Francesco / Hild, François et al. | 2023
-
Design and modelling of a reversible shape memory alloy torsion hinge actuatorLiu, Qiang / Ghodrat, Sepideh / Jansen, Kaspar M.B. et al. | 2023
-
Flexible self-supporting interconnected cobalt sulfide nanosheets enable high-loading and long-cycling Li-S batteries with high areal capacityTian, Xiaohui / Xue, Minghui / Cheng, Yunnian / Che, Lukang / Liu, Mengdie / Beolle Songwe Selabi, Naomie / Zhou, Yingke et al. | 2023
-
Surface disinfection change the mechanical, structural and biological properties of flexible materials used for additive manufacturing of medical devicesKardos, Kinga / Told, Roland / Pentek, Attila / Sahai, Nitin / Banfai, Krisztina / Vizi, Andras / Koltai, Arnold / Szabo, Peter / Gurdan, Zsuzsanna / Bovari-Biri, Judit et al. | 2023
-
Hollow porous PLA/PBAT composite microfibers with enhanced toughness and prolonged drug release for wound healingLiu, Yufei / Wei, Yuanzhi / Xiong, Qinqin / Xie, Chuan / An, Taofang / He, Min / Xia, Lu / Wei, Shinan / Yu, Jia / Cheng, Sha et al. | 2023
-
Microstructural and neutron residual stress characterization of 316L laser-powder bed fusion simplified end-use part: A modelling benchmarkSanchez-Poncela, Manuel / Cabeza, Sandra / Martinez, Juan M. / Cabrera, Analia / Rementeria, Rosalía et al. | 2023
-
A thermo-mechanical model for hot cracking susceptibility in electron beam powder bed fusion of Ni-base superalloysWahlmann, Benjamin / Markl, Matthias / Körner, Carolin et al. | 2023
-
Tensile strength and toughness of carbon nanotube-graphene foam composite materials and the corresponding microscopic influence mechanismWang, Shuai / Liang, Lihong / Chen, Shaohua et al. | 2023
-
Selective crack propagation in steel-nickel component printed by wire arc directed energy depositionWu, Bintao / Shi, Hanxiang / Liu, Ji / Zhang, Benshun / Zhou, Tianhao / Pan, Zengxi / Li, Huijun et al. | 2023
-
Simulation-driven-design of metal lattice structures for a target stress–strain curveMcDonnell, Brian / O'Hara, Eimear M. / Harrison, Noel M. et al. | 2023
-
Novel cellular coil design for improved temperature uniformity in inductive heating of carbon fibre compositesUzzell, James P.N. / Pickard, Laura R. / Hamerton, Ian / Ivanov, Dmitry S. et al. | 2023
-
A strategy for simultaneously enhancing mechanical strength and hydrogen embrittlement resistance: Exceptional performance of laminated metal composite in hydrogen environmentsLuo, Z.A. / Mao, L.Y. / Huang, C. / Zhou, H.Y. / Wang, M.K. et al. | 2023
-
3D printing in upcycling plastic and biomass waste to sustainable polymer blends and composites: A reviewHassan, Malik / Mohanty, Amar K. / Misra, Manjusri et al. | 2023
-
Nano-micelle formation and aggregation in SBS-Modified asphalt induced by π-π interaction using molecular dynamicsLiu, Zhiyang / Wang, Peng / Huang, Zhenfu / Ren, Ruibo / Liu, Kai et al. | 2023
-
Crosslinking and pyrolysis of a methyl-silsesquioxane: Effect of heating rate on fabrication of polymer derived mullite ceramics using thermoplastic shapingSarraf, Fateme / Hadian, Amir / Gfeller, Frank / Churakov, Sergey V. / Clemens, Frank et al. | 2023
-
Fabrication of breathable superhydrophobic composite fabric with moisture permeability and weak-electric-field bactericidal ability designed for protective clothing applicationsLiu, Yanbo / Wang, Qiang / Zhang, Tianyi / Hao, Ming / Hu, Xiaodong / Chen, Zhijun / Yang, Bo et al. | 2023
-
Cover_237| 2024
-
Genetic sampling for surrogate-assisted topology optimization in electromagnetic riveting device designSun, Hao / Cui, Junjia / Li, Guangyao / Jiang, Hao et al. | 2023
-
Defect-Engineered photothermal nanozyme with NIR-II absorption induces Cuproptosis-Apoptosis for synergized cancer immunotherapy and fast wound healingHu, Pengcheng / Li, Yongxin / Zhang, Luchen / Lan, Xiaopeng / Ren, Xiaochuan / Liang, Wenlong / Wang, Shen / Wang, Yizhen / Zhao, Yanhui / Zhang, Yanhui et al. | 2023
-
A double cross-linked anisotropic quaternized chitosan/sodium alginate-based wound dressing for rapid drainage of biofluidsJi, Maocheng / Li, Jianyong / Li, Fangyi / Wang, Yi / Man, Jia / Wang, Xiaojie / Qiu, Yinghua / Zhang, Chuanwei / Peng, Sixian / Li, Jianfeng et al. | 2023
-
A microstructure enhancement method for hard magnetic particle chains based on magnetic field oscillation sieveHu, Zhezai / Zhang, Chengqian / Sun, Haonan / Dai, Huangzhe / Tang, Daofan / Hu, Hao / Li, Tiefeng / Fu, Jianzhong / Zhao, Peng et al. | 2023
-
Editorial Board| 2024
-
Bioactive electrospun nanoyarn-constructed textile dressing patches delivering Chinese herbal compound for accelerated diabetic wound healingLi, Yiran / Zhao, Wenwen / Chen, Shaojuan / Zhai, Huiyuan / Wu, Shaohua et al. | 2023
-
Predicting meltpool depth and primary dendritic arm spacing in laser powder bed fusion additive manufacturing using physics-based machine learningRiensche, Alex R. / Bevans, Benjamin D. / King, Grant / Krishnan, Ajay / Cole, Kevin D. / Rao, Prahalada et al. | 2023
-
True active surface area as a key indicator of corrosion behavior in additively manufactured 316L stainless steelCho, Seongkoo / Buchsbaum, Steven F. / Biener, Monika / Jones, Justin / Melia, Michael A. / Stull, Jamie A. / Colon-Mercado, Hector R. / Dwyer, Jonathan / Roger Qiu, S. et al. | 2023
-
A sequential physical and chemical dual crosslinked multifunctional hydrogel with enhanced mechanical and osteogenic effects for vascularized bone tissue regenerationHe, Wenbao / Chen, Kai / Gao, Wei / Duan, Riquan / Li, Zhendong / Li, Bing / Xia, Jiang / Zhao, Youguang / Liu, Wei / Zhou, Haichao et al. | 2023
-
Interaction of Y and impurity P on the synergistic enhancement of elongation and electrical conductivity of single crystal copper rodGe, Chenyang / Li, Shaolin / Song, Kexing / Guo, Xiuhua / Zhou, Yanjun / Liu, Haitao / Zhang, Chaomin / Cao, Jun / Cao, Fei / Gao, Yan et al. | 2023
-
Long term curl of printing paper due to ink solvent migrationMaass, Alexander / Hirn, Ulrich et al. | 2023
-
Influence of secondary orientation on [111]-orientated high temperature creep properties of single crystal alloy with a thin-wall structureZhang, Shuangqi / Wang, Haibo / Ru, Yi / Hu, Bin / Shang, Yong / Zhao, Haigen / Ma, Guoquan / Li, Shusuo / Pei, Yanling / Gong, Shengkai et al. | 2023
-
Light-adaptable artificial iris with dynamically scalable pupil-aperture function by radially patterned photochromic transition controlNauman, Asad / Choi, Jun-Chan / Cho, Young-Min / Lee, Jae-Won / Na, Jun-Hee / Kim, Hak-Rin et al. | 2023
-
Triple conversion strategy to build anti-de-icing sheets for the leading edge of the rotor bladeHe, Qiang / Jia, Yangyang / Wang, Haoyu / He, Jiaqi / Wang, Jiwen / Xu, Yuan / Liu, Yujie / Li, Anling et al. | 2023
-
High-productivity, field-relevant assessment of relative fracture resistance for hard materials – The ball mill edge chipping test (BMECT)Gates, J.D. / Pourasiabi, Hamid / Keen, Laura M. / Dalton, Alexander / Bennet, P.J. / Ali, Yahia et al. | 2023
-
Self-charging protective layer for marine reinforced concrete based on arch-shaped triboelectric nanogeneratorGao, Ying / Dong, Biqin / Wang, Yanshuai / Hong, Shuxian / Fang, Guohao / Zhang, Yuanyuan et al. | 2023
-
Site-specifically tailored microstructures with enhanced strength and hardening through laser powder bed fusionSofras, C. / Čapek, J. / Li, X. / Roth, C.C. / Leinenbach, C. / Logé, R.E. / Strobl, M. / Polatidis, E. et al. | 2023
-
Heterogeneous effect of aging temperature on the fatigue life of additively manufactured thin-walled 18Ni300 maraging steel tubular specimenKarolczuk, Aleksander / Kurek, Andrzej / Böhm, Michał / Derda, Szymon / Prażmowski, Mariusz / Kluger, Krzysztof / Żak, Krzysztof / Pejkowski, Łukasz / Seyda, Jan et al. | 2023
-
Nanotextured and drug loaded Neovius Ti6Al4V ELI scaffolds with osteogenesis and anti-cancer potentialSingh, Sonu / Roy, Rahul / Kumar Meena, Vijay / Vashisth, Priya / Kalyanasundaram, Dinesh et al. | 2023
-
Auxetic cementitious composites (ACCs) with excellent compressive ductility: Experiments and modelingXu, Yading / Šavija, Branko et al. | 2023
-
Functional biomimetic design of 3D printed polyether-ether-ketone flexible chest wall reconstruction implants for restoration of the respirationSun, Changning / Dong, Enchun / Tian, Yucong / Kang, Jianfeng / Zheng, Jibao / Zhang, Qing / Wang, Lei / Liu, Chaozong / Wang, Ling / Li, Dichen et al. | 2023
-
Fracture and Toughening of Mycelium-based BiocompositesEtinosa, Precious O. / Salifu, Ali A. / Osafo, Sarah / Eluu, Stanley C. / Obayemi, John D. / Soboyejo, Winston O. et al. | 2023
-
A new efficient grain growth model using a random Gaussian-sampled mode filterMelville, Joseph / Yadav, Vishal / Yang, Lin / Krause, Amanda R. / Tonks, Michael R. / Harley, Joel B. et al. | 2023
-
Corrigendum to ‘Thermally stable piezoelectric sensors for quantitative pressure sensing based on linear piezoelectric zinc oxide thin films’ [Mater. Design 235 (2023) 112466]Li, Yongkuan / Lin, Hongsen / Lin, Jianrong / Zhou, Cheng / Luo, Aixin / Yang, Jiachen / Zhang, Jieyu / Hong, Zhixiang / Hou, Xueyan / Xiao, Peng et al. | 2023
-
Unprecedented electrical performance of friction-extruded copper-graphene compositesGwalani, Bharat / Li, Xiao / Nittala, Aditya / Choi, Woongjo / Reza-E-Rabby, Md. / Atehortua, Julian Escobar / Bhattacharjee, Arun / Pole, Mayur / Silverstein, Joshua / Song, Miao et al. | 2023
-
Multiscale characterization of an additively manufactured property graded Ni-base alloy for molten-salts\supercritical-CO2 heat exchangersRen, Qing-Qiang / Su, Yi-Feng / Feldhausen, Thomas A. / Kurfess, Rebecca A. / Fillingim, Kenton B. / Nag, Soumya / Pillai, Rishi R. et al. | 2023
-
Studying the effects of Nb on high-temperature deformation in TiAl alloys using atomistic simulationsChandran, Anju / Ganesan, Hariprasath / Cyron, Christian J. et al. | 2023
-
Multimodal and multiscale strengthening mechanisms in Al-Ni-Zr-Ti-Mn alloy processed by laser powder bed fusion additive manufacturingDhal, Abhijeet / Thapliyal, Saket / Agrawal, Priyanka / Roy, Ankita / Sharma, Aishani / Mishra, Rajiv S. / Faierson, Eric et al. | 2023
-
Tunable architectures in Al/Al2O3 composites for enhanced damage tolerance using zirconium acetate-mediated ice-templatingSun, Meng-Qi / Shen, Ping et al. | 2023
-
Corrigendum to “Investigation of the structure and ionic conductivity of a Li3InCl6 modified by dry room annealing for solid-state Li-ion battery applications” [Mater. Design 227 (2023) 111690]Molaiyan, Palanivel / Mailhiot, Sarah E. / Voges, Kevin / Kantola, Anu M. / Hu, Tao / Michalowski, Peter / Kwade, Arno / Telkki, Ville-Veikko / Lassi, Ulla et al. | 2023
-
Comments on Seo et al., Materials & Design 117 (2017) 131–138, https://doi.org/10.1016/j.matdes.2016.12.066Mangindaan, Dave et al. | 2023
-
Tensile behaviour of WAAM high strength steel material and membersWeber, Ben / Meng, Xin / Zhang, Ruizhi / Nitawaki, Masashi / Sagawa, Takayuki / Gardner, Leroy et al. | 2023
-
Flow-induced crystallization of piezoelectric poly(L-lactide) fibers by a one-step melt-spinning processSchönlein, Richard / Fernández, Mercedes / Calafel, Itxaso / Azkune, Mikel / Liu, Guoming / Müller, Alejandro J. / Ugartemendia, Jone M. / Aguirresarobe, Robert et al. | 2023
-
Microstructure and mechanical property comparison of Inconel alloys fabricated using micro and conventional laser powder bed fusionChen, Yixuan / Wang, Weihao / Ou, Yao / Chang, Hai / Wu, Yingna / Yang, Rui / Zhai, Zirong / Li, Kefei / Shen, Liyaowei et al. | 2023
-
High performance surface plasmon enhanced ZnO-Pt @ AlN core shell UV photodetector synthesized by magnetron sputteringLiu, Wei / Shi, Baolong / Li, Zhu Xin / Qiu, Hangkai / Wang, Bohan / Bi, Changwei / Shi, Zengliang / Wang, Chao / Dai, Chaoqing / Wang, Dalei et al. | 2023
-
Generative design of graded metamaterial arrays for dynamic response modulationWang, Weidi / Cheney, Willoughby / Amirkhizi, Alireza V. et al. | 2023
-
Effects of Y and Ho doping on microstructure evolution during oxidation of extraordinary stable Hf-B-Si-Y/Ho-C-N films up to 1500 °CJiang, J.C. / Shen, Y. / Zeman, P. / Procházka, M. / Vlček, J. / Meletis, E.I. et al. | 2023
-
PMD Core Ontology: Achieving semantic interoperability in materials scienceBayerlein, Bernd / Schilling, Markus / Birkholz, Henk / Jung, Matthias / Waitelonis, Jörg / Mädler, Lutz / Sack, Harald et al. | 2023
-
Active-oxygenating hollow Prussian blue nanosystems loaded with biomacromolecules for photodynamic/photothermal therapy of cancer and alleviating hypoxic tumorsZhu, Mingzhi / Wang, Pei / Chen, Biaoqi / Shi, Linrong / Long, Ruimin / Wang, Shibin / Liu, Yuangang et al. | 2023
-
A self-healing injectable hydrogel integrated with enzymatic and nonenzymatic antioxidants as artificial antioxidant defense system for diabetic wound healingWang, Ye / Chen, Chong / He, Changyuan / Dong, Wentao / Yang, Xuekun / Wu, Ye / Liu, Jialin / Kong, Qingquan / He, Jin / Yan, Bin et al. | 2023
-
Multiplexed terahertz multifocal metalens based on stretchable single-, dual-, and quad-axis synthetic rectangular optical sparse apertureLiu, Yuxin / Lin, Yu-Sheng et al. | 2024
-
Characterization of aluminum and boron carbide based additive manufactured material for thermal neutron shieldingStone, M.B. / Kolesnikov, A.I. / Fanelli, V.R. / May, A.F. / Bai, Shuang / Liu, J. et al. | 2023
-
Ultrasensitive and rapid detection of hydrogen sulfide by an upconversion nanosensor NaYF4:Yb3+, Tm3+@NaYF4@Ag2OZha, Shuai / Pan, Siyu / Jian, Yuehan / Peng, Yunhui / Jiang, Lijun et al. | 2023
-
Modelling and experimental study of laser-assisted milling of fibre reinforced SiC/Ti-6Al-4V metal matrix compositeMypati, Omkar / Panzer, Jeriel / Robles-Linares, Jose A. / Zan, Shusong / Liao, Zhirong / Axinte, Dragos et al. | 2023
-
Space deployable mechanics: A review of structures and smart drivingWang, Bing / Zhu, Juncheng / Zhong, Shuncong / Liang, Wei / Guan, Chenglong et al. | 2023
-
Decitabine/paclitaxel co-delivery systems modified with anti-PD-L1 antibodies mediate chemoimmunotherapy for Triple negative breast cancerHe, Yang / Hu, Qin / Wang, Liting / Chen, Chuanrong et al. | 2023
-
Cut/puncture resistance and mechanisms of protective composite textiles reinforced with inorganic powderMao, Lizhou / Yu, Hang / Yao, Lu / Shen, Yue / Yan, Xuefeng / Ma, Yan et al. | 2023
-
A review of diamond synthesis, modification technology, and cutting tool application in ultra-precision machiningZhang, Jiabao / Wang, Jianpeng / Zhang, Guoqing / Huo, Zexuan / Huang, Zejia / Wu, Linjia et al. | 2023
-
Metasurfaces and their intelligent advancesLv, Jiangtao / Zhang, Ruizhe / Gu, Qiongchan / Hemayet Uddin, Md / Jiang, Xiaoxiao / Qi, Junqiao / Si, Guangyuan / Ou, Qingdong et al. | 2023
-
Nanosystems-enabled regenerative strategies for spinal cord Injury: Recent advances and future prospectsJia, Zhiwei / Li, Wei et al. | 2023
-
Construction of methylene blue embedded core–shell-satellite structured Au@Ag nanorods@SiO2@Au nanocomposites for synergistic therapy of cancerZhang, Min / Zhu, Shunhua / Yi, Ge / Wang, Jingjing / Wang, Meng / Li, Shibao / Huang, Qingli et al. | 2023
-
Corrigendum to “Effect of cooling rate on microstructure and properties of SiCP/A359 composites” [Mater. Design 234 (2023) 112297]Jin, Zuheng / Jia, Lina / Wang, Wenbo / Liu, Yanyu / Qi, Yan / Zhang, Hu et al. | 2023
-
Enhancing compressive performance in 3D printed pyramidal lattice structures with geometrically tailored I-shaped strutsUddin, Mohammed Ayaz / Barsoum, Imad / Kumar, S. / Schiffer, Andreas et al. | 2023
-
Cu2Se-based injectable hydrogels for synergistic photothermal/gas therapy of oral squamous cell carcinomaZhong, Nanping / Xing, Jianghao / He, Jia / Zhao, Xinyu / Wang, Xianwen / Xue, Haowei et al. | 2023
-
The columnar to equiaxed transition of CoCrNi medium-entropy alloy fabricated by laser directed energy depositionZhao, Wenjie / Sun, Yonggang / Che, Pengcheng / Ning, Zhiliang / Fan, Hongbo / Yang, Haiyan / Sun, Jianfei / Liaw, Peter K. / Ngan, Alfonso H.W. / Huang, Yongjiang et al. | 2023
-
High-power-density sputtering of industrial-scale targets: Case study of (Al,Cr)NKlimashin, F.F. / Klusoň, J. / Učík, M. / Žemlička, R. / Jílek, M. / Lümkemann, A. / Michler, J. / Edwards, T.E.J. et al. | 2023
-
A novel octa-arginine-modified injectable self-assembling peptide hydrogel for multidrug-resistant cancer therapyWang, Ying / Hao, Zhuowen / Li, Bingshu / Tang, Jianming / Zhang, Zihui / Wang, Zhi / Yang, Lian / Peng, Jiaxin / Li, Jingfeng / Hong, Li et al. | 2023
-
Development of an integrated device utilizing exosome-hyaluronic acid-based hydrogel and investigation of its osteogenic and angiogenic characteristicsWan, Longbiao / He, Yan / Wang, Ao / Pan, Jiali / Xu, Chun / Fu, Dehao / Ye, Qingsong / Wu, Fei et al. | 2023
-
High-performance brazing of single crystal superalloys with Ni-Cr-Ta filler materialLang, Zhenqian / Zou, Taiyong / Ye, Zheng / Wu, Tao / Wang, Wanli / Yang, Jian / Huang, Jihua et al. | 2023
-
The synergistic and interactive effects of slip systems and dynamic recrystallization on the weakening basal texture of Mg-Y-Nd-Zr-Gd magnesium alloyHan, Luyi / Yu, Yanan / Wei, Dejin / Wang, Xin / Zhao, Guoqun / Wang, Guangchun et al. | 2023
-
Multi-objective design of 3D phononic crystal waveguide by design space trimmingValiya Valappil, Sabiju / Goosen, Johannes F.L. / Aragón, Alejandro M. et al. | 2023
-
Inhibition effect of covalent carbon nanosheets on mechanochemical wear of diamondChen, Ni / Zhao, Junyi / Wang, Runkai / Yan, Bo / Wu, Yang / Li, Liang / Yu, Nan / He, Ning et al. | 2023
-
Simultaneously enhancing strength-ductility synergy in the Ti2AlNb diffusion bonding joint via heterogeneous high-entropy interface designDu, Y.J. / Song, J.F. / Xiong, J.T. / Li, S.W. / Jin, F. / Li, J.L. / Wen, G.D. / Guo, W. et al. | 2023
-
Quantification of micro-damage evolution process in ceramics through extensive analysis of multi-source heterogeneous dataZhang, Jinshuo / Sui, Tianyi / Lin, Bin / Lv, Bingrui / Du, Haoxuan / Song, Nan et al. | 2023
-
Mechanical properties and rate-sensitive deformation of AA6063 aluminum alloys at 298 K, 78 K, and 4 KKula, A. / Niewczas, M. et al. | 2023