A nanoindentation technique for functional evaluation of cartilage repair tissue (English)
- New search for: Ebenstein, Donna M.
- New search for: Ebenstein, Donna M.
- New search for: Kuo, Alfred
- New search for: Rodrigo, Juan J.
- New search for: Reddi, A.Hari
- New search for: Ries, Michael
- New search for: Pruitt, Lisa
In:
Journal of materials research
;
19
, 1
; 273-281
;
2004
-
ISSN:
- Article (Journal) / Print
-
Title:A nanoindentation technique for functional evaluation of cartilage repair tissue
-
Contributors:Ebenstein, Donna M. ( author ) / Kuo, Alfred / Rodrigo, Juan J. / Reddi, A.Hari / Ries, Michael / Pruitt, Lisa
-
Published in:Journal of materials research ; 19, 1 ; 273-281
-
Publisher:
- New search for: Materials Research Society
-
Place of publication:Warrendale, Pa.
-
Publication date:2004
-
ISSN:
-
ZDBID:
-
Type of media:Article (Journal)
-
Type of material:Print
-
Language:English
- New search for: 770/5000
- New search for: 51.00 / 51.00
- Further information on Basic classification
-
Keywords:
-
Classification:
-
Source:
Table of contents – Volume 19, Issue 1
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 1
-
FUNDAMENTALS AND APPLICATIONS OF INSTRUMENTED INDENTATION IN MULTIDISCIPLINARY RESEARCH - IntroductionCheng, Yang-Tse et al. | 2004
-
Measurement of hardness and elastic modulus by instrumented indentation: Advances in understanding and refinements to methodologyOliver, W. C. / Pharr, G. M. et al. | 2004
- 3
-
REVIEWS - Measurement of hardness and elastic modulus by instrumented indentation: Advances in understanding and refinements to methodologyOliver, W.C. et al. | 2004
- 22
-
REVIEWS - Fracture and deformation in brittle solids: A perspective on the issue of scaleLawn, Brian R. et al. | 2004
-
Fracture and deformation in brittle solids: A perspective on the issue of scaleLawn, Brian R. et al. | 2004
-
Depth-sensing indentation tests in studying plastic instabilitiesChinh, N. Q. / Gubicza, J. / Kovács, Zs. / Lendvai, J. et al. | 2004
- 31
-
REVIEWS - Depth-sensing indentation tests in studying plastic instabilitiesChinh, N.Q. et al. | 2004
-
A survey of instrumented indentation studies on metallic glassesSchuh, C. A. / Nieh, T. G. et al. | 2004
- 46
-
REVIEWS - A survey of instrumented indentation studies on metallic glassesSchuh, C.A. et al. | 2004
- 58
-
Using multidimensional contact mechanics experiments to measure Poisson's ratioLucas, B.N. et al. | 2004
- 66
-
Deformation microstructure under microindents in single-crystal Cu using three-dimensional x-ray structural microscopyYang, Wenge et al. | 2004
- 73
-
A numerical study of indentation using indenters of different geometryMin, Li et al. | 2004
- 79
-
Mechanical characterization of secondary-hardening martensitic steel using nanoindentationOhmura, T. et al. | 2004
- 85
-
Finite element study for nanoindentation measurements on two-phase materialsDurst, Karsten et al. | 2004
- 94
-
Master curves for Hertzian indentation on coating-substrate systemsHsueh, Chun-Hway et al. | 2004
- 101
-
A new loading history for identification of viscoplastic properties by spherical indentationHuber, N. et al. | 2004
- 114
-
Three-dimensional finite element analysis of the effects of anisotropy on bone mechanical properties measured by nanoindentationFan, Z. et al. | 2004
- 124
-
Indentation-induced deformation at ultramicroscopic and macroscopic contactsThurn, Jeremy et al. | 2004
- 131
-
Polarity-induced changes in the nanoindentation response of GaAsBourhis, E.Le et al. | 2004
- 137
-
Plasticity size effects in nanoindentationBushby, A.J. et al. | 2004
- 143
-
Validated measurement of Young's modulus, Poisson ratio, and thickness for thin coatings by combining instrumented nanoindentation and acoustical measurementsJennett, N.M. et al. | 2004
- 149
-
An energy-based method for analyzing instrumented spherical indentation experimentsNi, Wangyang et al. | 2004
- 158
-
Nanoindentation testing for evaluating modulus and hardness of single-walled carbon nanotube-reinforced epoxy compositesDutta, A.K. et al. | 2004
- 165
-
Sharp probes of varying acuity: Instrumented indentation and fracture behaviorMorris, Dylan J. et al. | 2004
- 176
-
Direct observations of incipient plasticity during nanoindentation of AlMinor, A.M. et al. | 2004
- 176
-
Direct observation of incipient plasticity during nanoindentation of AlMinor, A.M. / Lilleodden, E.T. / Stach, E.A. / Morris, J.W. jun. et al. | 2004
- 183
-
Surface roughness effects on the displacement bursts observed in nanoindentationShibutani, Yoji et al. | 2004
- 189
-
Investigation of slip transmission behavior across grain boundaries in polycrystalline Ni3Al using nanoindentationWo, P.C. et al. | 2004
- 202
-
Instrumented indentation probing of laser surface-refined cast Al alloyNayak, S. et al. | 2004
- 208
-
Size effect measurement and characterization in nanoindentation testWei, Yueguang et al. | 2004
- 218
-
Hall-Petch relationship in pulsed-laser deposited nickel filmsKnapp, J.A. et al. | 2004
- 228
-
Instrumented pyramidal and spherical indentation of polycrystalline graphiteSakai, M. et al. | 2004
- 237
-
Nanoscale repetitive impact testing of polymer filmsBeake, Ben D. et al. | 2004
- 249
-
Nanoindentation of bone: Comparison of specimens tested in liquid and embedded in polymethylmethacrylateBushby, A.J. et al. | 2004
- 260
-
Depth-sensing indentation response of ordered silica foamToivola, Yvete et al. | 2004
- 273
-
A nanoindentation technique for functional evaluation of cartilage repair tissueEbenstein, Donna M. et al. | 2004
- 282
-
Measuring the strain rate sensitivity by instrumented indentation. Application to an ultra fine grain (equal channel angular-pressed) eutectic Sn-Bi alloyAlkorta, J. et al. | 2004
- 291
-
Nanoindentation and nanoscratch of a thermal oxide layer on a FeAl alloyXia, J. et al. | 2004
- 301
-
Young's modulus measurements on ultra-thin coatingsChudoba, T. et al. | 2004
- 315
-
Analyzing the mechanical behavior of thin films using nanoindentation, cantilever microbeam deflection, and finite element modelingSchwaiger, R. et al. | 2004
- 325
-
Direct measurement of indentation frame complianceVliet, Krystyn J.Van et al. | 2004
- 332
-
The R8-BC8 phases and crystal growth in monocrystalline silicon under microindentation with a spherical indenterZarudi, I. et al. | 2004
- 338
-
Mechanical properties of ion-implanted amorphous siliconFollstaedt, D.M. et al. | 2004
- 347
-
Matrix strength evaluation of ultra-fine grained steel by nanoindentationOhmura, T. et al. | 2004
- 351
-
A high-temperature displacement-sensitive indenter for studying mechanical properties of thermal barrier coatingsKim, Chang-Hoon et al. | 2004
- 357
-
Nanoindentation creep of quartz, with implications for rate- and state-variable friction laws relevant to earthquake mechanicsGoldsby, David L. et al. | 2004
- 366
-
Progress toward Systeme International d'Unites traceable force metrology for nanomechanicsPratt, J.R. / Smith, D.T. / Newell, D.B. / Kramar, J.A. / Whitenton, E. et al. | 2004
- 366
-
Progress toward Système International d'Unités traceable force metrology for nanomechanicsPratt, Jon R. et al. | 2004
- 380
-
Pop-in events induced by spherical indentation in compound semiconductorsBradby, J.E. et al. | 2004
- 387
-
Measurement of the loss tangent of a thin polymeric film using the atomic force microscopeMcGuiggan, P.M. et al. | 2004
-
IntroductionCheng, Yang-Tse / Page, Trevor / Pharr, George M. / Swain, Michael V. / Wahl, Kathryn J. et al. | 2004