Microfractographic aspects of stress corrosion cracking of Inconel 600 in a pressurized water reactor environment (English)
- New search for: Magnin, T.
- New search for: Magnin, T.
- New search for: Noel, D.
- New search for: Rios, R.
In:
Materials science and engineering / A
;
177
, 1-2
; L11
;
1994
-
ISSN:
- Article (Journal) / Print
-
Title:Microfractographic aspects of stress corrosion cracking of Inconel 600 in a pressurized water reactor environment
-
Contributors:
-
Published in:Materials science and engineering / A ; 177, 1-2 ; L11
-
Publisher:
- New search for: Elsevier
-
Place of publication:Amsterdam [u.a.]
-
Publication date:1994
-
ISSN:
-
ZDBID:
-
Type of media:Article (Journal)
-
Type of material:Print
-
Language:English
- New search for: 51.00
- Further information on Basic classification
- New search for: 535/5100
-
Keywords:
-
Classification:
-
Source:
Table of contents – Volume 177, Issue 1-2
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 1
-
Effects of strain rate and temperature on deformation behaviour of IN 718 during high temperature deformationZhou, L.X. et al. | 1994
- 11
-
Degradation of the strength of glass after light contact with other materialsAl-Amri, A. et al. | 1994
- 19
-
Effect of reinforcement on age hardening of cast 6061 Al-SiC and 6061 Al-Al2O3 particulate compositesSalvo, L. et al. | 1994
- 29
-
Cyclic stress-strain response of polycrystalline nickelMorrison, D.J. et al. | 1994
- 43
-
Effect of environment on the rupture behavior of alloys 909 and 718Hayes, R.W. et al. | 1994
- 55
-
Experimental and theoretical investigation of the residual stress distribution in brazed ceramic-steel componentsPintschovius, L. et al. | 1994
- 63
-
Effects of aging on the tensile and fatigue behaviour of the near- Ti-1100 at room temperature and 593CMadsen, A. / Ghonem, H. et al. | 1994
- 63
-
Effects of aging on the tensile and fatigue behaviour of the near- a Ti-1100 at room temperature and 593(degree)CMadsen, A. et al. | 1994
- 63
-
Effects of aging on the tensile and fatigue behavior of the near-alpha Ti-1100 at room temperature and 593 deg CMadsen, A. / Ghonem, H. et al. | 1994
- 75
-
An investigation of creep behaviour of a low carbon 18Cr-12Ni (304L type) stainless steel at 873-1173 KSustek, V. et al. | 1994
- 83
-
Strengthening of discontinuous reinforced NiAl compositesWang, L. et al. | 1994
- 89
-
Creep behavior of molybdenum and a molybdenum-hafnium carbide alloy from 1600 to 2100 KLuo, A. et al. | 1994
- 95
-
Tensile damage development in fiber-reinforced ceramic matrix compositesDannemann, K.A. et al. | 1994
- 115
-
Evaluation of stresses in Ni-NiO and Cr-Cr2O3 during high temperature oxidation by in-situ X-ray diffractionGeodjen, J.G. et al. | 1994
- 125
-
An interactive simulation technique to determine the internal stress states in fiber reinforced metal matrix compositesGhonem, H. et al. | 1994
- 135
-
On the formation of Al2O3-Al composite by directed oxidation of molten metalsTang, W. et al. | 1994
- 143
-
Processing maps for hot working of commercial grade wrought staineless steel type AISI 304Venugopal, S. / Mannan, S.L. / Prasad, Y.V.R.K. et al. | 1994
- 143
-
Processing maps for hot working of commercial grade wrought stainless steel type AISI 304Venugopal, S. et al. | 1994
- 151
-
Microstructure and fracture behavior of SiC-platelet-reinforced Si3N4 matrix compositesLee, B.T. et al. | 1994
- 161
-
Analysis of hydrogen atom transport in a two-phase alloyTurnbull, A. et al. | 1994
- 173
-
Interfacial reactions and age hardening in Al-Mg-Si metal matrix composites reinforced with SiC particlesSalvo, L. et al. | 1994
- 185
-
Processing of an -2 aluminide alloy, Ti-24Al-11NbSagar, P. K. / Banerjee, D. / Prasad, Y. V. R. K. et al. | 1994
- 185
-
Processing of an alpha-2 aluminide alloy, Ti-24Al-11NbSagar, P.K. / Banerjee, D. / Prasad, Y.V.R.K. et al. | 1994
- 185
-
Processing of an a-2 aluminide alloy, Ti-24Al-11NbSagar, P.K. et al. | 1994
- 199
-
Thermal stability of dispersoids in ferritic oxide-dispersion- strengthened alloysKrautwasser, P. et al. | 1994
- 209
-
Temperature-induced phase development in titanium-implanted silicon carbideVardiman, R.G. et al. | 1994
- 217
-
Atomic short-range ordering in Au-Fe alloys: a resistometric studyMigschitz, M. et al. | 1994
- 227
-
Thermal cyclic response of laser-glazed plasma-sprayed ZrO2- 19.5wt.%Y2O3-Ni-22Cr-10Al-1Y thermal barrier coatingsTsai, H.L. et al. | 1994
- 233
-
Embedded-atom-Monte Carlo study of short-range order in nitrogen strengthened Fe-Ni-Cr austeniteGrujicic, M. et al. | 1994
- 243
-
Nitrogen in pressure-diffused powder iron alloysRawers, J.C. et al. | 1994
- 253
-
Correlation of microstructure variability and local stress field in two-phase materialsPyrz, R. et al. | 1994
- 261
-
Ultrasonic and neutron diffraction characterization of texture in an inhomogeneously rolled titanium plateThompson, R.B. et al. | 1994
- 269
-
Whisker alignment by slip extrusionFarkash, M. et al. | 1994
- 277
-
SiC-whisker-reinforced ceramics with modulated microstructuresFarkash, M. et al. | 1994
- 283
-
AUTHOR INDEX| 1994
- 285
-
SUBJECT INDEX| 1994
-
Investigation of fractal dimensions of hydrogen-induced brittle fracture of titanium aluminideZhang, Y. et al. | 1994
-
Microfractographic aspects of stress corrosion cracking of Inconel 600 in a pressurized water reactor environmentMagnin, T. et al. | 1994
-
Evaluation of fracture toughness of duplex microstructures by an indentation techniqueEbrahimi, F. et al. | 1994