The chloride stress-corrosion cracking behavior of stainless steels under different test methods (English)
- New search for: Jin, L. Z.
- New search for: Jin, L. Z.
In:
Journal of Materials Engineering and Performance
;
3
, 6
; 734-739
;
1994
-
ISSN:
- Article (Journal) / Print
-
Title:The chloride stress-corrosion cracking behavior of stainless steels under different test methods
-
Contributors:Jin, L. Z. ( author )
-
Published in:Journal of Materials Engineering and Performance ; 3, 6 ; 734-739
-
Publisher:
- New search for: Springer US
- New search for: Springer
-
Place of publication:[New York, NY]
-
Publication date:1994
-
ISSN:
-
ZDBID:
-
DOI:
-
Type of media:Article (Journal)
-
Type of material:Print
-
Language:English
- New search for: 51.00 / 52.00
- Further information on Basic classification
- New search for: 770/5100
-
Keywords:
-
Classification:
-
Source:
Table of contents – Volume 3, Issue 6
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 679
-
EditorialOgren, John R. et al. | 1994
- 681
-
News| 1994
- 693
-
HotSpot| 1994
- 694
-
Environment| 1994
- 698
-
Events| 1994
- 699
-
Mechanism of improved corrosion resistance of type 304l stainless steel, nitric acid grade, in nitric acid environmentsKain, V. / Shinde, S. S. / Gadiyar, H. S. et al. | 1994
- 706
-
Microstructures and magnetic properties of heatproof domain-refined grain-oriented silicon steel sheetsKosuge, K. / Hirose, K. / Kuroki, K. et al. | 1994
- 712
-
Finite element modeling of segmental chip formation in high-speed orthogonal cuttingHashemi, J. / Tseng, A. A. / Chou, P. C. et al. | 1994
- 722
-
Reproducibility of small-strain creep tests of Ti 6242SiDelos-Reyes, M. A. / Kassner, M. E. et al. | 1994
- 726
-
The effect of hole drilling on fatigue and residual stress properties of shot-peened aluminum panelsChaudhuri, J. / Donley, B. S. / Gondhalekar, V. / Patni, K. M. et al. | 1994
- 734
-
The chloride stress-corrosion cracking behavior of stainless steels under different test methodsJin, L. Z. et al. | 1994
- 740
-
Prevention of hydrogen degradation in titanium by deposition of TiN thin filmLee, S. C. / Ho, W. Y. / Chen, T. M. et al. | 1994
- 744
-
In vitro electrochemical investigations of advanced stainless steels for applications as orthopaedic implantsSivakumar, M. / Mudali, U. Kamachi / Rajeswari, S. et al. | 1994
- 754
-
Mechanical properties of haynes alloy 188 after 22,500 hours of exposure to LiF-22CaF2 and vacuum at 1093 KWhittenberger, J. D. et al. | 1994
- 763
-
Tensile properties of haynes alloy 230 and inconel 617 after long exposures to LiF-22CaF2 and vacuum at 1093 KWhittenberger, J. D. et al. | 1994