Cyclic nanoindentation and Raman microspectroscopy study of phase transformations in semiconductors (English)
- New search for: Gogotsi, Yury G.
- New search for: Domnich, Vladislav
- New search for: Dub, Sergey N.
- New search for: Kailer, Andreas
- New search for: Nickel, Klaus G.
- New search for: Gogotsi, Yury G.
- New search for: Domnich, Vladislav
- New search for: Dub, Sergey N.
- New search for: Kailer, Andreas
- New search for: Nickel, Klaus G.
In:
Journal of Materials Research
;
15
, 4
; 871-879
;
2000
-
ISSN:
- Article (Journal) / Print
-
Title:Cyclic nanoindentation and Raman microspectroscopy study of phase transformations in semiconductors
-
Contributors:Gogotsi, Yury G. ( author ) / Domnich, Vladislav ( author ) / Dub, Sergey N. ( author ) / Kailer, Andreas ( author ) / Nickel, Klaus G. ( author )
-
Published in:Journal of Materials Research ; 15, 4 ; 871-879
-
Publisher:
- New search for: Springer International Publishing
- New search for: Materials Research Society
-
Place of publication:Warrendale, Pa.
-
Publication date:2000
-
ISSN:
-
ZDBID:
-
DOI:
-
Type of media:Article (Journal)
-
Type of material:Print
-
Language:English
- New search for: 770/5000
- New search for: 51.00
- Further information on Basic classification
-
Keywords:
-
Classification:
-
Source:
Table of contents – Volume 15, Issue 4
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 835
-
RAPID COMMUNICATIONS - Microstructure and Hall-Petch behavior of Fe-Co-based Hiperco(C) alloysShang, Chang-He et al. | 2000
- 835
-
Microstructure and Hall-Petch behavior of Fe-Co-based Hiperco© alloysShang, Chang-He / Cammarata, R. C. / Weihs, T. P. / Chien, C. L. et al. | 2000
- 838
-
RAPID COMMUNICATIONS - Nanoscale mechanical properties of polymer composites: Changes in elastic modulus and measurement of ion penetration depth due to a-radiationChien, Allen T. et al. | 2000
- 838
-
Nanoscale mechanical properties of polymer composites: Changes in elastic modulus and measurement of ion penetration depth due to alpha-radiationChien, A.T. / Felter, T. / LeMay, J.D. / Balooch, M. et al. | 2000
- 838
-
Nanoscale mechanical properties of polymer composites: Changes in elastic modulus and measurement of ion penetration depth due to α-radiationChien, Allen T. / Felter, Tom / LeMay, James D. / Balooch, Mehdi et al. | 2000
- 842
-
RAPID COMMUNICATIONS - Sol-gel-derived magnesium oxide precursor for thin-film fabricationChoi, Hyungsoo et al. | 2000
- 842
-
Sol-gel-derived magnesium oxide precursor for thin-film fabricationChoi, Hyungsoo / Hwang, Soontaik et al. | 2000
- 846
-
Epitaxial growth of anisotropically shaped, single-crystal particles of cubic $ SrTiO_{3} $Watari, Koji / Brahmaroutu, Bhaskar / Messing, Gary L. / Trolier-McKinstry, Susan / Cheng, Shang-Cong et al. | 2000
- 846
-
RAPID COMMUNICATIONS - Epitaxial growth of anisotropically shaped, single-crystal particles of cubic SrTiO3Watari, Koji et al. | 2000
- 850
-
Microwave-assisted Al-substituted tobermorite synthesisMiyake, Michihiro / Niiya, Shigeto / Matsuda, Motohide et al. | 2000
- 850
-
RAPID COMMUNICATIONS - Microwave-assisted Al-substituted tobermorite synthesisMiyake, Michihiro et al. | 2000
- 854
-
REVIEW - Materials aspects of the high-temperature superconductors in the system Bi2O3-SrO-CaO-CuOMajewski, Peter et al. | 2000
- 854
-
Materials aspects of the high-temperature superconductors in the system $ Bi_{2} $$ O_{3} $-SrO-CaO-CuOMajewski, Peter et al. | 2000
- 871
-
ARTICLES - Cyclic nanoindentation and Raman microspectroscopy study of phase transformations in semiconductorsGogotsi, Yury G. et al. | 2000
- 871
-
Cyclic nanoindentation and Raman microspectroscopy study of phase transformations in semiconductorsGogotsi, Yury G. / Domnich, Vladislav / Dub, Sergey N. / Kailer, Andreas / Nickel, Klaus G. et al. | 2000
- 880
-
ARTICLES - Photoluminescence spectra of Zn1-xCdxAl2Se4 single crystalsHyun, Seung-Cheol et al. | 2000
- 880
-
Photoluminescence spectra of $ Zn_{1−x} $$ Cd_{x} $$ Al_{2} $$ Se_{4} $ single crystalsHyun, Seung-Cheol / Kim, Chang-Dae / Park, Tae-Young / Kim, Hyung-Gon / Jin, Moon-Seog / Lee, Choong-Il / Goh, Jae-Mo / Kim, Wha-Tek et al. | 2000
- 884
-
Heat resistance of Sn-9Zn solder/Cu interface with or without coatingSuganuma, Katsuaki / Murata, Toshikazu / Noguchi, Hiroji / Toyoda, Yoshitaka et al. | 2000
- 884
-
ARTICLES - Heat resistance of Sn-9Zn solder-Cu interface with or without coatingSuganuma, Katsuaki et al. | 2000
- 892
-
Stability and phase transformations of icosahedral phase in a 41.5Zr41.5Ti17Ni alloyYi, S. / Kim, D. H. et al. | 2000
- 892
-
ARTICLES - Stability and phase transformations of icosahedral phase in a 41.5Zr41.5Ti17Ni alloyYi, S. et al. | 2000
- 898
-
Stereophotogrammetric investigation of overload and cyclic fatigue fracture surface morphologies in a Zr-Ti-Ni-Cu-Be bulk metallic glassTatschl, A. / Gilbert, C. J. / Schroeder, V. / Pippan, R. / Ritchie, R. O. et al. | 2000
- 898
-
ARTICLES - Stereophotogrammetric investigation of overload and cyclic fatigue fracture surface morphologies in a Zr-Ti-Ni-Cu-Be bulk metallic glassTatschl, A. et al. | 2000
- 904
-
Nanophase Fe alloys consolidated to full density from mechanically milled powdersHe, L. / Allard, L. F. / Breder, K. / Ma, E. et al. | 2000
- 904
-
ARTICLES - Nanophase Fe alloys consolidated to full density from mechanically milled powdersHe, L. et al. | 2000
- 913
-
Nano-scratch behavior of a bulk Zr-10Al-5Ti-17.9Cu-14.6Ni amorphous alloyWang, J. G. / Choi, B. W. / Nieh, T. G. / Liu, C. T. et al. | 2000
- 913
-
ARTICLES - Nano-scratch behavior of a bulk Zr-10Al-5Ti-17.9Cu-14.6Ni amorphous alloyWang, J.G. et al. | 2000
- 923
-
Aligned diamond nanowhiskersBaik, Eun-Song / Baik, Young-Joon / Jeon, Dongryul et al. | 2000
- 923
-
ARTICLES - Aligned diamond nanowhiskersBaik, Eun-Song et al. | 2000
- 927
-
ARTICLES - Nanocrystalline tungsten oxide thin film: Preparation, microstructure, and photochromic behaviorSun, Mu et al. | 2000
- 927
-
Nanocrystalline tungsten oxide thin film: Preparation, microstructure, and photochromic behaviorSun, Mu / Xu, Ning / Cao, Y. W. / Yao, J. N. / Wang, E. G. et al. | 2000
- 934
-
Preferred orientation of copper phthalocyanine thin films evaporated on amorphous substratesResel, R. / Ottmar, M. / Hanack, M. / Keckes, J. / Leising, G. et al. | 2000
- 934
-
ARTICLES - Preferred orientation of copper phthalocyanine thin films evaporated on amorphous substratesResel, R. et al. | 2000
- 940
-
ARTICLES - Electrical conductivity of discontinuous filament-reinforced unidirectional compositesTing, Jyh-Ming et al. | 2000
- 940
-
Electrical conductivity of discontinuous filament-reinforced unidirectional compositesTing, Jyh-Ming / Chen, Kuo-Wei et al. | 2000
- 944
-
Reaction pathways at the iron-microspherical silica interface: Mechanistic aspects of the formation of target iron oxide phasesRamesh, Sivarajan / Felner, Israel / Koltypin, Yuri / Gedanken, Aharon et al. | 2000
- 944
-
ARTICLES - Reaction pathways at the iron-microspherical silica interface: Mechanistic aspects of the formation of target iron oxide phasesRamesh, Sivarajan et al. | 2000
- 951
-
Temperature dependence of in situ constituent properties of polymer-infiltration-pyrolysis-processes Nicalon SiC fiber-reinforced SiC matrix compositeGuo, S. / Kagawa, Y. et al. | 2000
- 951
-
Temperature dependence of in situ constituent properties of polymer-infiltration-pyrolysis-processed Nicalon™ SiC fiber-reinforced SiC matrix compositeGuo, Shuqi / Kagawa, Yutaka et al. | 2000
- 951
-
ARTICLES - Temperature dependence of in situ constituent properties of polymer-infiltration-pyrolysis-processed NicalonTM SiC fiber-reinforced SiC matrix compositeGuo, Shuqi et al. | 2000
- 961
-
Oxygen stoichiometry in $ PdO_{x} $and $ PdO_{x} $/Pt electrode layers during processing of ferroelectric and high-epsilon perovskitesSaenger, K. L. / Cabral, C. / Duncombe, P. R. / Grill, A. / Neumayer, D. A. et al. | 2000
- 961
-
ARTICLES - Oxygen stoichiometry in PdOx and PdOx-Pt electrode layers during processing of ferroelectric and high-epsilon perovskitesSaenger, K.L. et al. | 2000
- 967
-
Preparation and nonstoichiometric property of wide compositional Fe(III)-doped $ TiO_{2} $ (anatase)Uekawa, N. / Kurashima, Y. / Kakegawa, K. / Sasaki, Y. et al. | 2000
- 967
-
ARTICLES - Preparation and nonstoichiometric property of wide compositional Fe(III)-doped TiO2 (anatase)Uekawa, N. et al. | 2000
- 974
-
Novel synthesis of nitride powders by microwave-assisted combustionVaidhyanathan, B. / Agrawal, D. K. / Roy, R. et al. | 2000
- 974
-
ARTICLES - Novel synthesis of nitride powders by microwave-assisted combustionVaidhyanathan, B. et al. | 2000
- 982
-
Densification of $ Al_{2} $$ O_{3} $ powder using spark plasma sinteringWang, S. W. / Chen, L. D. / Hirai, T. et al. | 2000
- 982
-
ARTICLES - Densification of Al2O3 powder using spark plasma sinteringWang, S.W. et al. | 2000
- 988
-
ARTICLES - Sintering of nanopowders of amorphous silicon nitride under ultrahigh pressureLi, Ya-Li et al. | 2000
- 988
-
Sintering of nanopowders of amorphous silicon nitride under ultrahigh pressureLi, Ya-Li / Liang, Yong / Zheng, Fen / Ma, Xian-Feng / Cui, Suo-Jing et al. | 2000
- 995
-
Structural properties of strontium vanadate glassesSen, S. / Ghosh, A. et al. | 2000
- 995
-
ARTICLES - Structural properties of strontium vanadate glassesSen, S. et al. | 2000
- 1000
-
A method for determining crystallization kinetic parameters from one nonisothermal calorimetric experimentZhang, Haoyue / Mitchell, Brian S. et al. | 2000
- 1000
-
ARTICLES - A method for determining crystallization kinetic parameters from one nonisothermal calorimetric experimentZhang, Haoyue et al. | 2000
- 1008
-
Controlled planar interface synthesis by ultrahigh vacuum diffusion bonding/depositionKim, M. J. / Carpenter, R. W. / Cox, M. J. / Xu, J. et al. | 2000
- 1008
-
ARTICLES - Controlled planar interface synthesis by ultrahigh vacuum diffusion bonding-depositionKim, M.J. et al. | 2000
- 1017
-
Role of adhesive interlayer in transverse fracture of brittle layer structuresChai, Herzl / Lawn, Brian et al. | 2000
- 1017
-
ARTICLES - Role of adhesive interlayer in transverse fracture of brittle layer structuresChai, Herzl et al. | 2000
- 1025
-
ARTICLES - A transmission electron microscope study of hardness Indentations in MoSi2Boldt, P.H. et al. | 2000
- 1025
-
A transmission electron microscope study of hardness indentations in $ MoSi_{2} $Boldt, P. H. / Weatherly, G. C. / Embury, J. D. et al. | 2000