High-temperature nanoindentation testing of fused silica and other materials (English)
- New search for: Beake, Ben D.
- New search for: Smith, James F.
- New search for: Beake, Ben D.
- New search for: Smith, James F.
In:
Philosophical Magazine A
;
82
, 10
;
2179-2186
;
2002
- Article (Journal) / Electronic Resource
-
Title:High-temperature nanoindentation testing of fused silica and other materials
-
Contributors:Beake, Ben D. ( author ) / Smith, James F. ( author )
-
Published in:Philosophical Magazine A ; 82, 10 ; 2179-2186
-
Publisher:
- New search for: Taylor & Francis
-
Publication date:2002-07-01
-
Size:8 pages
-
ISSN:
-
DOI:
-
Type of media:Article (Journal)
-
Type of material:Electronic Resource
-
Language:English
-
Source:
Table of contents – Volume 82, Issue 10
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 1807
-
Second international indentation workshop: Cavendish laboratory, university of cambridge, UK 15-20 July 2001Chaudhri, M. Munawar / Lim, Yong Yee et al. | 2002
- 1807
-
Second International Indentation Workshop: Cavendish Laboratory, University of Cambridge, UKChaudhri, M.Munawar et al. | 2002
- 1811
-
Why diamond is very hardGilman, John J. et al. | 2002
- 1821
-
Scaling relationships for indentation measurementsCheng, Yang-Tse / Li, Zhiyong / Cheng, Che-Min et al. | 2002
- 1831
-
A hardness equation for sharp indentation of elastic-power-law strain-hardening materialsMata, M. / Anglada, M. / Alcalá, J. et al. | 2002
- 1841
-
Time-dependent viscoelastic relation between load and penetration for an axisymmetric indenterSakai, M. et al. | 2002
- 1851
-
Nanoindentation of natural diamondSawa, T. / Tanaka, K. et al. | 2002
- 1857
-
Time-dependent characteristics of materials and micromechanisms of plastic deformation on a submicron scale by a new pulse indentation techniqueGolovin, Yu. I. / Tyurin, A. I. / Farber, B. Ya. et al. | 2002
- 1865
-
Photoplastic effects in nanoindentation experimentsWolf, Bodo / Meyer, Dirk / Belger, Andre / Paufler, Peter et al. | 2002
- 1873
-
Indentation hysteresis of glassy carbon materialsIwashita, N. / Field, J. S. / Swain, M. V. et al. | 2002
- 1883
-
Direct measurement of residual contact area and volume during the nanoindentation of coated materials as an alternative method of calculating hardnessRandall, Nicholas X. et al. | 2002
- 1893
-
Method to determine the plastic properties of bulk materials by nanoindentationXu, Zhi-Hui / Rowcliffe, David et al. | 2002
- 1903
-
Evaluation of the matrix strength of Fe-0.4 wt% C tempered martensite using nanoindentation techniquesOhmura, T. / Tsuzaki, K. / Matsuoka, S. et al. | 2002
- 1911
-
The influence of experimental parameters on hardness and Young's modulus determination using depth-sensing testingSimões, M. I. / Fernandes, J. V. / Cavaleiro, A. et al. | 2002
- 1921
-
Contact resistance and phase transformations during nanoindentation of siliconMann, A. B. / Heerden, D. van / Pethica, J. B. / Bowes, P. / Weihs, T. P. et al. | 2002
- 1931
-
Spherical indentation of compound semiconductorsBradby, J. E. / Williams, J. S. / Wong-Leung, J. / Kucheyev, S. O. / Swain, M. V. / Munroe, P. et al. | 2002
- 1941
-
Prediction of stress-strain curves of elastic-plastic materials based on the Vickers indentationMatsuda, Kenji et al. | 2002
- 1953
-
Low-load deformation of InP under contact loading; comparison with GaAsPatriarche, G. / Bourhis, E. Le et al. | 2002
- 1963
-
Deformation under nanoindents in sapphire, spinel and magnesia examined using transmission electron microscopyLloyd, S. J. / Molina-Aldareguia, J. M. / Clegg, W. J. et al. | 2002
- 1971
-
Transmission electron microscopy of amorphization and phase transformation beneath indents in SiSaka, H. / Shimatani, A. / Suganuma, M. / Suprijadi et al. | 2002
- 1983
-
Deformation structures under indentations in TiN/NbN single-crystal multilayers deposited by magnetron sputtering at different bombarding ion energiesMolina-aldareguia, J. M. / Lloyd, S. J. / Odén, M. / Joelsson, T. / Hultman, L. / Clegg, W. J. et al. | 2002
- 1993
-
Simulations of cyclic normal indentation of crystal surfaces using the bubble-raft modelvan Vliet, K. J. / Suresh, S. et al. | 2002
- 2003
-
Finite-element analysis of deformation during indentation and scratch tests on elastic-perfectly plastic materialsBucaille, J. L. / Felder, E. et al. | 2002
- 2013
-
Determination of the mechanical properties of metallic thin films and substrates from indentation testsTunvisut, K. / Busso, E. P. / O'dowd, N. P. / Brantner, H. P. et al. | 2002
- 2031
-
Quasistatic indentation and spherical particle impact studies of turbine-grade silicon nitridesYoshida, Hiro / Chaudhri, M. Munawar / Hoshi, Yoshinobu et al. | 2002
- 2041
-
The influence of sintering additives on the indentation response of liquid-phase-sintered polycrystalline aluminasGalusek, Dušan / Riley, Frank L. et al. | 2002
- 2059
-
The fatigue parameter n for subthreshold Vickers indentationsBouten, P. C. P. et al. | 2002
- 2071
-
The influence of grain size on the indentation hardness of high-purity copper and aluminiumLim, Yong Yee / Chaudhri, M. Munawar et al. | 2002
- 2081
-
Hardnesses of poly(vinylidene) fluoride and polyamide in high-pressure gas ambienceBriscoe, B. J. / Lorge, O. / Dang, P. et al. | 2002
- 2093
-
Near-surface mechanical properties of amorphous polymersMelick, Harold van / Duken, Auke van / Toonder, Jaap den / Govaert, Leon / Meijer, Han et al. | 2002
- 2103
-
Nanoindentation of polymer-bound silica agglomerate layersAkram, A. / Briscoe, B. J. / Adams, M. J. / Johnson, S. A. et al. | 2002
- 2113
-
Indentation-size effects in single-crystal MgORen, X. J. / Hooper, R. M. / Griffiths, C. / Henshall, J. L. et al. | 2002
- 2121
-
Indentation depth recovery in poly(methyl methacrylate) sheet on the microlength scaleAdams, M. J. / Gorman, D. M. / Johnson, S. A. / Briscoe, B. J. et al. | 2002
- 2133
-
How hard is fullerene-like CNx? Some observations from the nanoindentation response of a magnetron-sputtered coatingGarcia, I. Arce / Berasategui, E. G. / Bull, S. J. / Page, T. F. / Neidhardt, J. / Hultman, L. / Hellgren, N. et al. | 2002
- 2149
-
Development and application of a combined atomic force microscopy-nanoindentation system with a silicon tip and a diamond indenterMiyahara, K. / Nagashima, N. / Matsuoka, S. et al. | 2002
- 2161
-
The transition from elastic to plastic behaviour in an Al-Cu-Fe quasicrystal studied by cyclic nanoindentationDub, Sergey / Novikov, Nikolay / Milman, Yuly et al. | 2002
- 2173
-
Improvement in the nanoindentation technique for investigation of the time-dependent material propertiesGolovin, Yu. I. / Ivolgin, V. I. / Korenkov, V. V. / Korenkova, N. V. / Farber, B. Ya. et al. | 2002
- 2179
-
High-temperature nanoindentation testing of fused silica and other materialsBeake, Ben D. / Smith, James F. et al. | 2002
- 2187
-
Surface degradation of glass measured by nanoindentationSawa, T. / Tanaka, K. et al. | 2002
- 2191
-
Evaluation of the adhesion of TiN films using nanoindentation and scratch testingToparli, Mustafa / Sasaki, Shinya et al. | 2002
- 2199
-
Elasto-plastic deformation of silica glass and glassy carbons with different indentersIwashita, Norio / Swain, Michael V. et al. | 2002
- 2207
-
Thermal evolution of deformation zones around microindentations in different types of crystalGrabco, D. / Pushcash, B. / Dyntu, M. / Shikimaka, O. et al. | 2002
- 2217
-
Mechanical properties and microstructure of microcrystalline GaNZhilyaev, Iu. / Grabco, D. / Leu, D. / Botnariuc, V. / Raevskii, S. et al. | 2002
- 2223
-
A new analysis of nanoindentation load-displacement curvesZeng, Kaiyang / Shen, Lu et al. | 2002
- 2231
-
Unloading fractures in indented glassGorham, D. A. / Salman, A. D. / Tan, H. et al. | 2002