100 Dislocations in nickel-base superalloys: Formation and role in creep deformation (English)
- New search for: Link, T.
- New search for: Epishin, A.
- New search for: Klaus, M.
- New search for: Bruckner, U.
- New search for: Reznicek, A.
- New search for: Link, T.
- New search for: Epishin, A.
- New search for: Klaus, M.
- New search for: Bruckner, U.
- New search for: Reznicek, A.
In:
MATERIALS SCIENCE AND ENGINEERING A
;
405
, 1-2
;
254-265
;
2005
-
ISSN:
- Article (Journal) / Print
-
Title:100 Dislocations in nickel-base superalloys: Formation and role in creep deformation
-
Contributors:Link, T. ( author ) / Epishin, A. ( author ) / Klaus, M. ( author ) / Bruckner, U. ( author ) / Reznicek, A. ( author )
-
Published in:MATERIALS SCIENCE AND ENGINEERING A ; 405, 1-2 ; 254-265
-
Publisher:
- New search for: Elsevier Science B.V., Amsterdam.
-
Publication date:2005-01-01
-
Size:12 pages
-
ISSN:
-
Type of media:Article (Journal)
-
Type of material:Print
-
Language:English
- New search for: 620.11
- Further information on Dewey Decimal Classification
-
Classification:
DDC: 620.11 -
Source:
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Table of contents – Volume 405, Issue 1-2
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 1
-
Experimental study of structure formation in binary Al–Cu alloys at different cooling ratesEskin, D. / Du, Q. / Ruvalcaba, D. / Katgerman, L. et al. | 2005
- 1
-
Experimental study of structure formation in binary Al#8211Cu alloys at different cooling ratesEskin, D. et al. | 2005
- 11
-
Effect of nitrogen on short-range atomic order in the feritic #948 phase of a duplex steelBliznuk, T. et al. | 2005
- 11
-
Effect of nitrogen on short-range atomic order in the feritic delta phase of a duplex steelBliznuk, T. / Mola, M. / Polshin, E. / Pohl, M. / Gavriljuk, V. et al. | 2005
- 11
-
Effect of nitrogen on short-range atomic order in the feritic d phase of a duplex steelBliznuk, T. / Mola, M. / Polshin, E. / Pohl, M. / Gavriljuk, V. et al. | 2005
- 11
-
Effect of nitrogen on short-range atomic order in the feritic δ phase of a duplex steelBliznuk, T. / Mola, M. / Polshin, E. / Pohl, M. / Gavriljuk, V. et al. | 2005
- 18
-
Lattice strain partitioning in a two-phase alloy and its redistribution upon yieldingHan, Tong-Seok / Dawson, Paul R. et al. | 2005
- 34
-
Thermal processing of polycrystalline NiTi shape memory alloysFrick, Carl P. / Ortega, Alicia M. / Tyber, Jeffrey / Maksound, A.El.M. / Maier, Hans J. / Liu, Yinong / Gall, Ken et al. | 2005
- 50
-
Analysis of failure of nanobelt-coated copper-based leadframe/epoxy-based molding compound systems after pull-out testLee, Ho-Young / Park, Young-Bae / Jeon, Insu / Kim, Yong-Hyup / Chang, Young-Keun et al. | 2005
- 65
-
Age hardening of a sintered Al–Cu–Mg–Si–(Sn) alloyKent, D. / Schaffer, G.B. / Drennan, J. et al. | 2005
- 65
-
Age hardening of a sintered Al#8211Cu#8211Mg#8211Si#8211(Sn) alloyKent, D. et al. | 2005
- 74
-
Influence of long term annealing on grain boundary character distributions in nickelLee, Siu-Lun / Richards, N.L. et al. | 2005
- 86
-
Primary recrystallization modelling for interstitial free steelsChoi, Shi-Hoon / Cho, Jae Hyung et al. | 2005
- 102
-
Gaseous corrosion resistance of Fe–Al based alloys containing Cr additionsRegina, J.R. / DuPont, J.N. / Marder, A.R. et al. | 2005
- 102
-
Gaseous corrosion resistance of Fe#8211Al based alloys containing Cr additionsRegina, J.R. et al. | 2005
- 102
-
Gaseous corrosion resistance of Fe-Al based alloys containing Cr additions. Part II. Scale morphologyRegina, J.R. / DuPont, J.N. / Marder, A.R. et al. | 2005
- 111
-
An investigation of the effects of microstructure on dwell fatigue crack growth in Ti-6242McBagonluri, F. / Akpan, E. / Mercer, C. / Shen, W. / Soboyejo, W.O. et al. | 2005
- 135
-
On iron contamination in mechanically alloyed Cr–Si powdersFernandes, Bruno B. / Rodrigues, Geovani / Coelho, Gilberto C. / Ramos, Alfeu S. et al. | 2005
- 135
-
On iron contamination in mechanically alloyed Cr#8211Si powdersFernandes, Bruno B. et al. | 2005
- 140
-
Mechanochemical synthesis of Cu–Al2O3 nanocompositesHwang, Seung J. / Lee, Jin-hyung et al. | 2005
- 140
-
Mechanochemical synthesis of Cu#8211Al2O3 nanocompositesHwang, Seung J. et al. | 2005
- 147
-
The effect of the carbon and nitrogen contents on the fracture toughness of Type 347 austenitic stainless steelsYoo, One / Oh, Yong-Jun / Lee, Bong-Sang / Nam, Soo Woo et al. | 2005
- 158
-
Microstructure of reaction-bonded silicon nitride fabricated under static nitrogen pressurePark, Dong-soo / Kim, Hai-doo / Lim, Kwon taek / Bang, Kook-soo / Park, Chan et al. | 2005
- 163
-
Correlation of microstructure with hardness and wear resistance in Cr3C2/stainless steel surface composites fabricated by high-energy electron beam irradiationYun, Eunsub / Lee, Sunghak et al. | 2005
- 173
-
Alpha-case formation mechanism on titanium investment castingsSung, Si-Young / Kim, Young-Jig et al. | 2005
- 178
-
On enhanced impact strength of calcium carbonate-reinforced high-density polyethylene compositesTanniru, M. / Misra, R.D.K. et al. | 2005
- 194
-
Characterization of rupture and fatigue resistance of TBC superalloy for combustion linersRay, A.K. / Das, D.K. / Venkataraman, B. / Roy, P.K. / Goswami, B. / Roy, N. / Das, S.K. / Parida, N. / Tarafder, S. / Chaudhuri, S. et al. | 2005
- 201
-
Anisotropic plasticity and cavity growth during upset forging of Ti–6Al–4VBieler, Tom / Goetz, R.L. / Semiatin, S.L. et al. | 2005
- 201
-
Anisotropic plasticity and cavity growth during upset forging of Ti#82116Al#82114VBieler, Tom et al. | 2005
- 214
-
Effect of service exposure on the mechanical properties of 2.25Cr#82111Mo pressure vessel steel in a hot-wall hydrofining reactorTan, Jinzhu et al. | 2005
- 214
-
Effect of service exposure on the mechanical properties of 2.25Cr–1Mo pressure vessel steel in a hot-wall hydrofining reactorTan, Jinzhu / Chao, Yuh J. et al. | 2005
- 221
-
Dislocation structures and crystal orientations of copper single crystals deformed by equal-channel angular pressingMiyamoto, H. / Fushimi, J. / Mimaki, T. / Vinogradov, A. / Hashimoto, S. et al. | 2005
- 233
-
Preparation of zirconia–mullite composites by an infiltration routePark, H.C. / Yang, T.Y. / Yoon, S.Y. / Stevens, R. et al. | 2005
- 233
-
Preparation of zirconia#8211mullite composites by an infiltration routePark, H.C. et al. | 2005
- 239
-
Cyclic deformation behavior in pure Cu with growth-in twinsGuo, X.L. / Lu, L. / Li, S.X. et al. | 2005
- 246
-
Testing and evaluation on the thermal and mechanical properties of carbon nano fiber reinforced SC-15 epoxyPervin, Farhana / Zhou, Yuanxin / Rangari, Vijaya K. / Jeelani, Shaik et al. | 2005
- 254
-
<1 0 0> Dislocations in nickel-base superalloys: Formation and role in creep deformationLink, Thomas / Epishin, A. / Klaus, M. / Bruckner, U. / Reznicek, A. et al. | 2005
- 254
-
〈100〉 Dislocations in nickel-base superalloys: Formation and role in creep deformationLink, T. / Epishin, A. / Klaus, M. / Brückner, U. / Reznicek, A. et al. | 2005
- 254
-
#9001100#9002 Dislocations in nickel-base superalloys: Formation and role in creep deformationLink, T. et al. | 2005
- 266
-
A non-linear viscoelastic model developed for semi-crystalline polymer deformed at small strains with loading and unloading pathsLai, Dawei / Yakimets, Iryna / Guigon, Michèle et al. | 2005
- 272
-
A new thermal-shock-resistance model for ceramics: Establishment and validationZhou, Zehua / Ding, Peidao / Tan, Shouhong / Lan, Junsi et al. | 2005
- 277
-
Microstructure evolution during FSW/FSP of high strength aluminum alloysSu, Jian-Qing / Nelson, Tracy W. / Sterling, Colin J. et al. | 2005
- 287
-
Effects of particle arrangement on stress concentrations in compositesSun, C.J. / Saffari, P. / Sadeghipour, K. / Baran, G. et al. | 2005
- 296
-
Aging response of coarse- and fine-grained β titanium alloysIvasishin, O.M. / Markovsky, P.E. / Semiatin, S.L. / Ward, C.H. et al. | 2005
- 296
-
Aging response of coarse- and fine-grained b titanium alloysIvasishin, O. M. / Markovsky, P. E. / Semiatin, S. L. / Ward, C. H. et al. | 2005
- 296
-
Aging response of coarse- and fine-grained #946 titanium alloysIvasishin, O.M. et al. | 2005
- 296
-
Aging response of coarse- and fine-grained beta titanium alloysIvasishin, O.M. / Markovsky, P.E. / Semiatin, S.L. / Ward, C.H. et al. | 2005
- 306
-
Influence of high-intensity ultrasound on grain refining performance of Al–5Ti–1B master alloy on aluminiumHan, Yanfeng / Li, Ke / Wang, Jun / Shu, Da / Sun, Baode et al. | 2005
- 306
-
Influence of high-intensity ultrasound on grain refining performance of Al#82115Ti#82111B master alloy on aluminiumHan, Yanfeng et al. | 2005
- 313
-
Thick ceramic thermal barrier coatings with high durability deposited using solution-precursor plasma sprayJadhav, Amol / Padture, Nitin P. / Wu, Fang / Jordan, Eric H. / Gell, Maurice et al. | 2005
- 321
-
Crystallization behavior and magnetic properties of amorphous B-rich NdFeB alloy in presence of an external electric fieldLi, Shandong / Tang, Jiancheng / Lü, Liya / Zou, Wenqin / Huang, Zhigao / Lai, Heng / Du, Youwei et al. | 2005
- 325
-
Synthesis and consolidation of nanostructured W#821110#821140wt.% Cu powdersHong, Seong-Hyeon et al. | 2005
- 325
-
Synthesis and consolidation of nanostructured W–10–40wt.% Cu powdersHong, Seong-Hyeon / Kim, Byoung-Kee / Munir, Zuhair A. et al. | 2005
- 333
-
Characteristics of the kissing-bond in friction stir welded Al alloy 1050Sato, Yutaka S. / Takauchi, Hideaki / Park, Seung Hwan C. / Kokawa, Hiroyuki et al. | 2005
- 339
-
Application of the EBSD technique for the characterisation of deformation zones in metal cuttingM'Saoubi, R. / Ryde, L. et al. | 2005
- 350
-
Corrigendum to “Study of texture in a TiTaNb alloy using electron back scattered diffraction technique” [Mater. Sci. Eng. A 393 (1–2) (2005) 294–302]Karthikeyan, T. / Dasgupta, Arup / Khan, A.J. / Saroja, S. / Vijayalakshmi, M. / Bhattacharjee, D. / Raghunathan, V.S. et al. | 2005
- 350
-
Corrigendum to #8220Study of texture in a TiTaNb alloy using electron back scattered diffraction technique#8221 (Mater. Sci. Eng. A 393 (1#82112) (2005) 294#8211302)Karthikeyan, T. et al. | 2005
- 352
-
Author Index| 2005
- 354
-
Subject Index| 2005
- CO2
-
Inside Front Cover: Editorial Board| 2005