Effect of machining on stress corrosion crack initiation in warm-forged type 304L stainless steel in high temperature water (English)
- New search for: Chang, Litao
- New search for: Volpe, Liberato
- New search for: Wang, Yong Liang
- New search for: Burke, M. Grace
- New search for: Maurotto, Agostino
- New search for: Tice, David
- New search for: Lozano-Perez, Sergio
- New search for: Scenini, Fabio
- New search for: Chang, Litao
- New search for: Volpe, Liberato
- New search for: Wang, Yong Liang
- New search for: Burke, M. Grace
- New search for: Maurotto, Agostino
- New search for: Tice, David
- New search for: Lozano-Perez, Sergio
- New search for: Scenini, Fabio
In:
Acta materialia
;
165
;
203-214
;
2019
-
ISSN:
- Article (Journal) / Print
-
Title:Effect of machining on stress corrosion crack initiation in warm-forged type 304L stainless steel in high temperature water
-
Contributors:Chang, Litao ( author ) / Volpe, Liberato ( author ) / Wang, Yong Liang ( author ) / Burke, M. Grace ( author ) / Maurotto, Agostino ( author ) / Tice, David ( author ) / Lozano-Perez, Sergio ( author ) / Scenini, Fabio ( author )
-
Published in:Acta materialia ; 165 ; 203-214
-
Publisher:
- New search for: Elsevier Science B.V., Amsterdam.
-
Publication date:2019-01-01
-
Size:12 pages
-
ISSN:
-
Type of media:Article (Journal)
-
Type of material:Print
-
Language:English
- New search for: 620.112
- Further information on Dewey Decimal Classification
-
Classification:
DDC: 620.112 -
Source:
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Table of contents – Volume 165
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 1
-
Effects of Mo and Mn microadditions on strengthening and over-aging resistance of nanoprecipitation-strengthened Al-Zr-Sc-Er-Si alloysDe Luca, Anthony / Seidman, David N. / Dunand, David C. et al. | 2018
- 15
-
Dewetted nanostructures of gold, silver, copper, and palladium with enhanced facetingPreston, Arin S. / Hughes, Robert A. / Demille, Trevor B. / Rey Davila, Victor M. / Neretina, Svetlana et al. | 2018
- 26
-
Nano-scale microstructure damage by neutron irradiations in a novel Boron-11 enriched TiB2 ultra-high temperature ceramicBhattacharya, A. / Parish, C.M. / Koyanagi, T. / Petrie, C.M. / King, D. / Hilmas, G. / Fahrenholtz, W.G. / Zinkle, S.J. / Katoh, Y. et al. | 2018
- 40
-
Mechanical properties of the magnetocaloric intermetallic LaFe11.2Si1.8 alloy at different length scalesGlushko, Oleksandr / Funk, Alexander / Maier-Kiener, Verena / Kraker, Philipp / Krautz, Maria / Eckert, Jürgen / Waske, Anja et al. | 2018
- 51
-
Transmutation-induced precipitation in tungsten irradiated with a mixed energy neutron spectrumHu, Xunxiang / Parish, Chad M. / Wang, Kun / Koyanagi, Takaaki / Eftink, Benjamin P. / Katoh, Yutai et al. | 2018
- 62
-
Superior energy absorption in porous magnesium: Contribution of texture development triggered by intra-granular misorientationsMayama, Tsuyoshi / Tane, Masakazu / Tadano, Yuichi et al. | 2018
- 73
-
Mechanistic understanding of the temperature dependence of crack growth rate in alloy 600 and 316 stainless steel through high-resolution characterizationShen, Zhao / Meisnar, Martina / Arioka, Koji / Lozano-Perez, Sergio et al. | 2018
- 87
-
Deformation compatibility between nanotwinned and recrystallized grains enhances resistance to interface cracking in cyclic loaded stainless steelLi, Q. / Yan, F.K. / Tao, N.R. / Ponge, D. / Raabe, D. / Lu, K. et al. | 2018
- 99
-
Time-resolved atomic-scale observations of deformation and fracture of nanoporous gold under tensionLiu, Pan / Wei, Xiao / Song, Shuangxi / Wang, Lihua / Hirata, Akihiko / Fujita, Takeshi / Han, Xiaodong / Zhang, Ze / Chen, Mingwei et al. | 2018
- 109
-
Reversible elastocaloric effect at ultra-low temperatures in nanocrystalline shape memory alloysAhadi, Aslan / Kawasaki, Takuro / Harjo, Stefanus / Ko, Won-Seok / Sun, QingPing / Tsuchiya, Koichi et al. | 2018
- 118
-
Unprecedented irradiation resistance of nanocrystalline tungsten with equiaxed nanocrystalline grains to dislocation loop accumulationEl-Atwani, O. / Esquivel, E. / Aydogan, E. / Martinez, E. / Baldwin, J.K. / Li, M. / Uberuaga, B.P. / Maloy, S.A. et al. | 2018
- 129
-
Slip band formation at free surface of lath martensite in low carbon steelInoue, Junya / Sadeghi, Alireza / Koseki, Toshihiko et al. | 2018
- 142
-
High temperature thermal and mechanical stability of high-strength nanotwinned Al alloysLi, Qiang / Cho, Jaehun / Xue, Sichuang / Sun, Xing / Zhang, Yifan / Shang, Zhongxia / Wang, Haiyan / Zhang, Xinghang et al. | 2018
- 153
-
On pinning-depinning and microkink-flow in solid state dewetting: Insights by in-situ ESEM on Al thin filmsHieke, Stefan Werner / Willinger, Marc-Georg / Wang, Zhu-Jun / Richter, Gunther / Chatain, Dominique / Dehm, Gerhard / Scheu, Christina et al. | 2018
- 164
-
Origin of the low precipitation hardening in magnesium alloysCepeda-Jiménez, C.M. / Castillo-Rodríguez, M. / Pérez-Prado, M.T. et al. | 2018
- 177
-
In situ x-ray diffraction analysis of 2D crack patterning in thin filmsFaurie, D. / Zighem, F. / Godard, P. / Parry, G. / Sadat, T. / Thiaudière, D. / Renault, P.-O. et al. | 2018
- 183
-
Unraveling the structural mechanism of Li insertion in γ′-V2O5 and its effect on cycling propertiesBaddour-Hadjean, R. / Safrany Renard, M. / Pereira-Ramos, J.P. et al. | 2018
- 192
-
Role of the slow diffusion species in the dewetting of compounds: The case of NiSi on a Si isotope multilayer studied by atom probe tomographyLuo, T. / Girardeaux, C. / Bracht, H. / Mangelinck, D. et al. | 2018
- 203
-
Effect of machining on stress corrosion crack initiation in warm-forged type 304L stainless steel in high temperature waterChang, Litao / Volpe, Liberato / Wang, Yong Liang / Burke, M. Grace / Maurotto, Agostino / Tice, David / Lozano-Perez, Sergio / Scenini, Fabio et al. | 2018
- 215
-
Formation and temporal evolution of modulated structure in high Nb-containing lamellar γ-TiAl alloyRen, Guo-dong / Dai, Cheng-ren / Mei, Wei / Sun, Jian / Lu, Song / Vitos, Levente et al. | 2018
- 228
-
Outstanding tensile properties of a precipitation-strengthened FeCoNiCrTi0.2 high-entropy alloy at room and cryogenic temperaturesTong, Y. / Chen, D. / Han, B. / Wang, J. / Feng, R. / Yang, T. / Zhao, C. / Zhao, Y.L. / Guo, W. / Shimizu, Y. et al. | 2018
- 241
-
Short crack propagation from cracked non-metallic inclusions in a Ni-based polycrystalline superalloyTexier, Damien / Stinville, Jean-Charles / Echlin, McLean P. / Pierret, Stéphane / Villechaise, Patrick / Pollock, Tresa M. / Cormier, Jonathan et al. | 2018
- 259
-
Quantitative prediction of the aged state of Ni-base superalloys using PCA and tensor regressionGorgannejad, S. / Reisi Gahrooei, M. / Paynabar, K. / Neu, R.W. et al. | 2018
- 270
-
Magnetic and magnetocaloric properties of the Co2-xMnxB system by experiment and density functional theoryEner, Semih / Fries, Maximilian / Hammerath, Franziska / Opahle, Ingo / Simon, Eszter / Fritsch, Patrizia / Wurmehl, Sabine / Zhang, Hongbin / Gutfleisch, Oliver et al. | 2018
- 278
-
Effect of carbon on strain-rate and temperature sensitivity of twinning-induced plasticity steels: Modeling and experimentsLi, Y.Z. / Luo, Z.C. / Liang, Z.Y. / Huang, M.X. et al. | 2018
- 294
-
A paradigm shift towards compositionally zero-sum binderless 3D printing of magnesium alloys via capillary-mediated bridgingSalehi, Mojtaba / Maleksaeedi, Saeed / Nai, Sharon Mui Ling / Meenashisundaram, Ganesh Kumar / Goh, Min Hao / Gupta, Manoj et al. | 2018
- 307
-
Effect of the tilt grain boundary on oxygen-ion movement in yttria-stabilized zirconia: Insights from molecular dynamicsJaipal, Methary / Chatterjee, Abhijit et al. | 2018
- 315
-
The role of Ga addition on the thermodynamics, kinetics, and tarnishing properties of the Au-Ag-Pd-Cu-Si bulk metallic glass forming systemNeuber, Nico / Gross, Oliver / Eisenbart, Miriam / Heiss, Alexander / Klotz, Ulrich E. / Best, James P. / Polyakov, Mikhail N. / Michler, Johann / Busch, Ralf / Gallino, Isabella et al. | 2018
- 327
-
Real-time observation of the thermally-induced phase transformation in GeTe and its thermal expansion propertiesTran, Xuan Quy / Hong, Min / Maeno, Hiroshi / Kawami, Youichirou / Toriyama, Takaaki / Jack, Kevin / Chen, Zhi-Gang / Zou, Jin / Matsumura, Syo / Dargusch, Matthew S. et al. | 2018
- 336
-
Multiscale mechanical fatigue damage of stainless steel investigated by neutron diffraction and X-ray microdiffractionLi, Runguang / Wang, Yan-Dong / Liu, Wenjun / Geng, Chang / Xie, Qingge / Brown, Dennis E. / An, Ke et al. | 2018
- 346
-
Spectroscopic properties and martensitic phase transition of Y4Al2O9:Ce single crystals under high pressureWang, Yongjie / Hrubiak, R. / Turczyński, S. / Pawlak, D.A. / Malinowski, M. / Włodarczyk, D. / Kosyl, K.M. / Paszkowicz, W. / Przybylińska, H. / Wittlin, A. et al. | 2018
- 362
-
Variant selection of intragranular Ni2(Mo,Cr) precipitates (γ′) in the Ni-Mo-Cr-W alloySong, Jie / Field, Robert / Clarke, Amy / Fu, Yao / Kaufman, Michael et al. | 2018
- 373
-
Development of ultra-fine grain sized SmFe12-based powders using hydrogenation disproportionation desorption recombination processDirba, I. / Sepehri-Amin, H. / Ohkubo, T. / Hono, K. et al. | 2018
- 381
-
Self-diffusion of Ti interstitial based point defects and complexes in TiCSun, Weiwei / Ehteshami, Hossein / Kent, Paul R.C. / Korzhavyi, Pavel A. et al. | 2018
- 388
-
In situ high speed imaging study and modelling of the fatigue fragmentation of dendritic structures in ultrasonic fieldsWang, S. / Kang, J. / Guo, Z. / Lee, T.L. / Zhang, X. / Wang, Q. / Deng, C. / Mi, J. et al. | 2018
- 398
-
The role of point defects and defect gradients in flash sintering of perovskite oxidesRheinheimer, Wolfgang / Phuah, Xin Li / Wang, Han / Lemke, Fabian / Hoffmann, Michael J. / Wang, Haiyan et al. | 2018
- 409
-
Anneal hardening and elevated temperature strain rate sensitivity of nanostructured metals: Their relation to intergranular dislocation accommodationRenk, O. / Maier-Kiener, V. / Issa, I. / Li, J.H. / Kiener, D. / Pippan, R. et al. | 2018
- 420
-
Enhancing strength and strain hardenability via deformation twinning in fcc-based high entropy alloys reinforced with intermetallic compoundsChoudhuri, Deep / Gwalani, Bharat / Gorsse, Stephane / Komarasamy, Mageshwari / Mantri, Srinivas A. / Srinivasan, Srivilliputhur G. / Mishra, Rajiv S. / Banerjee, Rajarshi et al. | 2018
- 431
-
Grain boundary diffusion of 59Fe in high-purity copperRibbe, Jens / Esin, Vladimir A. / Divinski, Sergiy V. et al. | 2018
- 444
-
Enhancement of strength-ductility trade-off in a high-entropy alloy through a heterogeneous structureWu, S.W. / Wang, G. / Wang, Q. / Jia, Y.D. / Yi, J. / Zhai, Q.J. / Liu, J.B. / Sun, B.A. / Chu, H.J. / Shen, J. et al. | 2018
- 459
-
Deformation induced twinning and phase transition in an interstitial intermetallic compound niobium borideJiang, Binbin / Chen, Chunjin / Wang, Xuelu / Wang, Hao / Wang, Weizhen / Ye, Hengqiang / Du, Kui et al. | 2018
- 471
-
Dislocation induced twin growth and formation of basal stacking faults in twins in pure MgWang, Fulin / Barrett, Christopher D. / McCabe, Rodney J. / El Kadiri, Haitham / Capolungo, Laurent / Agnew, Sean R. et al. | 2018
- 486
-
High-performance potassium-sodium niobate lead-free piezoelectric ceramics based on polymorphic phase boundary and crystallographic textureLi, Peng / Huan, Yu / Yang, Weiwei / Zhu, Fangyuan / Li, Xiaolong / Zhang, Xingmin / Shen, Bo / Zhai, Jiwei et al. | 2018
- 496
-
Achieving ultra-high strength and ductility in equiatomic CrCoNi with partially recrystallized microstructuresSlone, C.E. / Miao, J. / George, E.P. / Mills, M.J. et al. | 2018
- 508
-
A generalized O-element approach for analyzing interface structuresZhang, Jin-Yu / Gao, Yipeng / Wang, Yunzhi / Zhang, Wen-Zheng et al. | 2018
- 520
-
The influence of heat treatment on the microstructure and properties of HIPped Ti-6Al-4VLu, Y. / Aristizabal, M. / Wang, X. / Pang, B. / Chiu, Y.L. / Kloenne, Z.T. / Fraser, H.L. / Loretto, M.H. et al. | 2018
- 528
-
Phase-field modeling of stacking structure formation and transition of δ-hydride precipitates in zirconiumHan, G.M. / Zhao, Y.F. / Zhou, C.B. / Lin, De-Ye / Zhu, X.Y. / Zhang, J. / Hu, S.Y. / Song, H.F. et al. | 2018
- 547
-
Shock-induced two types of {102} sequential twinning in TitaniumXu, Shun / Zhou, Ping / Liu, Guisen / Xiao, Dawu / Gong, Mingyu / Wang, Jian et al. | 2018
- 561
-
Carbon and strain partitioning in a quenched and partitioned steel containing ferriteTan, Xiaodong / Ponge, Dirk / Lu, Wenjun / Xu, Yunbo / Yang, Xiaolong / Rao, Xi / Wu, Di / Raabe, Dierk et al. | 2018
- 577
-
Glass formation by severe plastic deformation of crystalline Cu|Zr nano-layersLi, Suzhi / Pastewka, Lars / Gumbsch, Peter et al. | 2018
- 587
-
Influence of topological constraints on ion damage resistance of amorphous hydrogenated silicon carbideSu, Qing / Wang, Tianyao / Gigax, Jonathan / Shao, Lin / Lanford, William A. / Nastasi, Michael / Li, Liyi / Bhattarai, Gyanendra / Paquette, Michelle M. / King, Sean W. et al. | 2018
- 603
-
Effect of Nb and Fe on damage evolution in a Zr-alloy during proton and neutron irradiationFrancis, E. / Babu, R. Prasath / Harte, A. / Martin, T.L. / Frankel, P. / Jädernäs, D. / Romero, J. / Hallstadius, L. / Bagot, P.A.J. / Moody, M.P. et al. | 2018
- 615
-
Modeling of metastable phase formation for sputtered Ti1-xAlxN thin filmsLiu, Sida / Chang, Keke / Mráz, Stanislav / Chen, Xiang / Hans, Marcus / Music, Denis / Primetzhofer, Daniel / Schneider, Jochen M. et al. | 2018
- 626
-
Deformation mechanisms and scaling relations in the mechanical response of nano-porous AuBeets, Nathan / Farkas, Diana / Corcoran, Sean et al. | 2018
- 638
-
Atomistic modelling of the diffusion of C in FeCr alloysHerschberg, Rafael / Fu, Chu-Chun / Nastar, Maylise / Soisson, Frédéric et al. | 2018
- 654
-
Probing the frequency-dependent elastic moduli of lattice materialsMukhopadhyay, T. / Adhikari, S. / Alu, A. et al. | 2018
- 666
-
Dendrite orientation transition in AlGe alloysBecker, M. / Dantzig, J.A. / Kolbe, M. / Wiese, S.T. / Kargl, F. et al. | 2018
- 678
-
The effects of heat treatment upon the shock response of a copper-beryllium alloyMillett, J.C.F. / Whiteman, G. / Park, N.T. / Case, S. / Appleby-Thomas, G. et al. | 2013
- 686
-
Hashin-Shtrikman bounds with eigenfields in terms of texture coefficients for polycrystalline materialsFernández, Mauricio / Böhlke, Thomas et al. | 2018
- 698
-
Grain boundary segregation and intermetallic precipitation in coarsening resistant nanocrystalline aluminum alloysDevaraj, A. / Wang, W. / Vemuri, R. / Kovarik, L. / Jiang, X. / Bowden, M. / Trelewicz, J.R. / Mathaudhu, S. / Rohatgi, A. et al. | 2018
- 709
-
Indentation of a plastically deforming metal crystal with a self-affine rigid surface: A dislocation dynamics studyVenugopalan, S.P. / Nicola, L. et al. | 2018
- 722
-
The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: OverviewNagumo, Michihiko / Takai, Kenichi et al. | 2018
- 734
-
Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materialsMartin, May L. / Dadfarnia, Mohsen / Nagao, Akihide / Wang, Shuai / Sofronis, Petros et al. | 2018
- 751
-
Corrigendum to “Synchrotron tomographic quantification of the influence of Zn concentration on dendritic growth in Mg-Zn alloys” [Acta Mater. 156 (2018) 287–296]Phillion, A.B. / Shuai, Sansan / Guo, Enyu / Wang, Jiang / Jing, Tao / Ren, Zhongming / Neumann-Heyme, H. / Beckermann, C. / Lee, P.D. et al. | 2018
- iii
-
Editors for Acta Materialia| 2018