Dislocation dynamics in a nickel-based superalloy via in-situ transmission scanning electron microscopy (English)
- New search for: Stinville, J.C.
- New search for: Yao, Eric R.
- New search for: Callahan, Patrick G.
- New search for: Shin, Jungho
- New search for: Wang, Fulin
- Further information on Wang, Fulin:
- https://orcid.org/0000-0002-4684-3121
- New search for: Echlin, McLean P.
- New search for: Pollock, Tresa M.
- New search for: Gianola, Daniel S.
- Further information on Gianola, Daniel S.:
- https://orcid.org/0000-0003-4660-0805
- New search for: Stinville, J.C.
- New search for: Yao, Eric R.
- New search for: Callahan, Patrick G.
- New search for: Shin, Jungho
- New search for: Wang, Fulin
- Further information on Wang, Fulin:
- https://orcid.org/0000-0002-4684-3121
- New search for: Echlin, McLean P.
- New search for: Pollock, Tresa M.
- New search for: Gianola, Daniel S.
- Further information on Gianola, Daniel S.:
- https://orcid.org/0000-0003-4660-0805
In:
Acta Materialia
;
168
;
152-166
;
2018
-
ISSN:
- Article (Journal) / Electronic Resource
-
Title:Dislocation dynamics in a nickel-based superalloy via in-situ transmission scanning electron microscopy
-
Contributors:Stinville, J.C. ( author ) / Yao, Eric R. ( author ) / Callahan, Patrick G. ( author ) / Shin, Jungho ( author ) / Wang, Fulin ( author ) / Echlin, McLean P. ( author ) / Pollock, Tresa M. ( author ) / Gianola, Daniel S. ( author )
-
Published in:Acta Materialia ; 168 ; 152-166
-
Publisher:
- New search for: Acta Materialia Inc.
-
Publication date:2018-12-11
-
Size:15 pages
-
ISSN:
-
DOI:
-
Type of media:Article (Journal)
-
Type of material:Electronic Resource
-
Language:English
-
Keywords:
-
Source:
Table of contents – Volume 168
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 1
-
The role of elastic and plastic anisotropy in intergranular spall failureNguyen, Thao / Luscher, D.J. / Wilkerson, J.W. et al. | 2019
- 13
-
Particle deformation and microstructure evolution during cold spray of individual Al-Cu alloy powder particlesLiu, Tian / Leazer, Jeremy D. / Brewer, Luke N. et al. | 2019
- 24
-
Tuning the microstructure and metastability of β-Ti for simultaneous enhancement of strength and ductility of Ti-based bulk metallic glass compositesZhang, L. / Narayan, R.L. / Fu, H.M. / Ramamurty, U. / Li, W.R. / Li, Y.D. / Zhang, H.F. et al. | 2019
- 37
-
On the effect of Re addition on microstructural evolution of a CoNi-based superalloyPandey, P. / Sawant, A.K. / Nithin, B. / Peng, Z. / Makineni, S.K. / Gault, B. / Chattopadhyay, K. et al. | 2019
- 52
-
Revealing the factors influencing grain boundary segregation of P, As in Si: Insights from first-principlesZhao, Dongdong / Li, Yanjun et al. | 2019
- 63
-
Morphological evolution of transformation products and eutectoid transformation(s) in a hyper-eutectoid Ti-12 at% Cu alloyDonthula, Harish / Vishwanadh, B. / Alam, T. / Borkar, T. / Contieri, R.J. / Caram, R. / Banerjee, R. / Tewari, R. / Dey, G.K. / Banerjee, S. et al. | 2019
- 76
-
Boundary micro-cracking in metastable Fe45Mn35Co10Cr10 high-entropy alloysWei, Shaolou / Kim, Jinwoo / Tasan, Cemal Cem et al. | 2019
- 87
-
Comparison between stress-strain plots obtained from indentation plastometry, based on residual indent profiles, and from uniaxial testingCampbell, J.E. / Thompson, R.P. / Dean, J. / Clyne, T.W. et al. | 2019
- 100
-
Structure-property relationships in the lead-free piezoceramic system K0.5Bi0.5TiO3 - BiMg0.5Ti0.5O3Zeb, Aurang / Hall, David A. / Aslam, Zabeada / Forrester, Jennifer / Li, Jing-Feng / Li, Yizhe / Tang, Chiu C. / Wang, Ge / Zhu, Fangyuan / Milne, Steven J. et al. | 2019
- 109
-
Thermodynamics of grain boundary segregation, interfacial spinodal and their relevance for nucleation during solid-solid phase transitionsKwiatkowski da Silva, A. / Kamachali, R. Darvishi / Ponge, D. / Gault, B. / Neugebauer, J. / Raabe, D. et al. | 2019
- 121
-
Origin of an unusual systematic variation in the heteroepitaxy of Ag on Ni – The roles of twinning and step alignmentWynblatt, P. / Chatain, D. / Rollett, A.D. / Dahmen, U. et al. | 2019
- 133
-
Simultaneous enhancement of stress- and strain-controlled fatigue properties in 316L stainless steel with gradient nanostructureLei, Y.B. / Wang, Z.B. / Xu, J.L. / Lu, K. et al. | 2019
- 143
-
New tessellation-based procedure to design perfectly hyperuniform disordered dispersions for materials discoveryKim, J. / Torquato, S. et al. | 2019
- 152
-
Dislocation dynamics in a nickel-based superalloy via in-situ transmission scanning electron microscopyStinville, J.C. / Yao, Eric R. / Callahan, Patrick G. / Shin, Jungho / Wang, Fulin / Echlin, McLean P. / Pollock, Tresa M. / Gianola, Daniel S. et al. | 2018
- 167
-
Quantitative phase field modeling of solute trapping and continuous growth kinetics in quasi-rapid solidificationPinomaa, Tatu / Provatas, Nikolas et al. | 2019
- 178
-
Linking microstructure and local mechanical properties in SiC-SiC fiber composite using micromechanical testingZayachuk, Yevhen / Karamched, Phani / Deck, Christian / Hosemann, Peter / Armstrong, David E.J. et al. | 2019
- 190
-
Crystallographic orientation dependent maximum layer thickness of cubic AlN in CrN/AlN multilayersChen, Zhuo / Holec, David / Bartosik, Matthias / Mayrhofer, Paul H. / Zhang, Zaoli et al. | 2019
- 203
-
Local non-equilibrium effect on the growth kinetics of crystalsGalenko, P.K. / Ankudinov, V. et al. | 2019
- 210
-
Long term evolution of microstructure and stress around tin whiskers investigated using scanning Laue microdiffractionHektor, Johan / Micha, Jean-Sébastien / Hall, Stephen A. / Iyengar, Srinivasan / Ristinmaa, Matti et al. | 2019
- 222
-
Modeling solution hardening in BCC refractory complex concentrated alloys: NbTiZr, Nb1.5TiZr0.5 and Nb0.5TiZr1.5Rao, S.I. / Akdim, B. / Antillon, E. / Woodward, C. / Parthasarathy, T.A. / Senkov, O.N. et al. | 2019
- 237
-
Grain growth and solid-state dewetting of Bi-Crystal Ni-Fe thin films on sapphireSharma, Amit / Kumar, Aakash / Gazit, Nimrod / Srolovitz, David J. / Rabkin, Eugen et al. | 2019
- 250
-
Tilt strain glass in Sr and Nb co-doped LaAlO3 ceramicsJi, Yuanchao / Zhang, Pei / He, Liqiang / Wang, Dong / Luo, Hanyu / Otsuka, Kazuhiro / Wang, Yunzhi / Ren, Xiaobing et al. | 2019
- 261
-
Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturingBermingham, M.J. / StJohn, D.H. / Krynen, J. / Tedman-Jones, S. / Dargusch, M.S. et al. | 2019
- 275
-
The effects of solid solution and oxide dispersion alloying on the viscoelastic behavior of Au alloy thin filmsMongkolsuttirat, K. / Smyth, J.R. / McLean, M. / Brown, W.L. / Vinci, R.P. et al. | 2019
- 287
-
Formation mechanism of abnormally large grains in a polycrystalline nickel-based superalloy during heat treatment processingWang, Xin / Huang, Zaiwang / Cai, Biao / Zhou, Ning / Magdysyuk, Oxana / Gao, Yanfei / Srivatsa, Shesh / Tan, Liming / Jiang, Liang et al. | 2019
- 299
-
Directional and oscillating residual stress on the mesoscale in additively manufactured Ti-6Al-4VStrantza, M. / Vrancken, B. / Prime, M.B. / Truman, C.E. / Rombouts, M. / Brown, D.W. / Guillaume, P. / Van Hemelrijck, D. et al. | 2019
- 309
-
Fracture of notched ductile bulk metallic glass bars subjected to tension-torsion: Experiments and simulationsRaut, Devaraj / Narayan, R.L. / Yokoyama, Yoshihiko / Tandaiya, Parag / Ramamurty, Upadrasta et al. | 2019
- 321
-
Modern data analytics approach to predict creep of high-temperature alloysShin, D. / Yamamoto, Y. / Brady, M.P. / Lee, S. / Haynes, J.A. et al. | 2019
- 331
-
Mechanism of hardening and damage initiation in oxygen embrittlement of body-centred-cubic niobiumYang, Ping-Jiong / Li, Qing-Jie / Tsuru, Tomohito / Ogata, Shigenobu / Zhang, Jie-Wen / Sheng, Hong-Wei / Shan, Zhi-Wei / Sha, Gang / Han, Wei-Zhong / Li, Ju et al. | 2019
- 343
-
Stress-induced formation of TCP phases during high temperature low cycle fatigue loading of the single-crystal Ni-base superalloy ERBO/1Meid, Carla / Eggeler, Mario / Watermeyer, Philipp / Kostka, Aleksander / Hammerschmidt, Thomas / Drautz, Ralf / Eggeler, Gunther / Bartsch, Marion et al. | 2019
- 353
-
Role of local stresses on co-zone twin-twin junction formation in HCP magnesiumArul Kumar, M. / Gong, M. / Beyerlein, I.J. / Wang, J. / Tomé, C.N. et al. | 2019
- 362
-
In situ investigation of stress-induced martensitic transformation in granular shape memory ceramic packingsRauch, Hunter A. / Chen, Yan / An, Ke / Yu, Hang Z. et al. | 2019
- 376
-
In-situ and ex-situ synchrotron X-ray diffraction studies of microstructural length scale controlled dealloyingSong, T. / Yan, M. / Webster, N.A.S. / Styles, M.J. / Kimpton, J.A. / Qian, M. et al. | 2019
- 393
-
Influence of microstructural features on the plastic deformation behavior of metallic nanoglassesAdjaoud, Omar / Albe, Karsten et al. | 2019
- 401
-
Multiscale structure of super insulation nano-fumed silicas studied by SAXS, tomography and porosimetryBenane, Belynda / Baeza, Guilhem P. / Chal, Bruno / Roiban, Lucian / Meille, Sylvain / Olagnon, Christian / Yrieix, Bernard / Foray, Geneviève et al. | 2019
- 411
-
In-situ XRD study of actuation mechanisms in BiFeO3-K0.5Bi0.5TiO3-PbTiO3 ceramicsLi, Yizhe / Chen, Ying / Zhang, Zhenbo / Kleppe, Annette / Hall, David A. et al. | 2019
- 426
-
Mobility of dislocations in Aluminum: Faceting and asymmetry during nanoscale dislocation shear loop expansionDang, Khanh / Bamney, Darshan / Bootsita, Kanis / Capolungo, Laurent / Spearot, Douglas E. et al. | 2019
- 436
-
Atomistic modeling of dislocation cross-slip in nickel using free-end nudged elastic band methodChen, Dengke / Costello, Luke L. / Geller, Clint B. / Zhu, Ting / McDowell, David L. et al. | 2019
- 448
-
Interplay between the effects of deformation mechanisms and dynamic recrystallization on the failure of Mg-3Al-1ZnVaughan, M.W. / Nasim, W. / Dogan, E. / Herrington, J.S. / Proust, G. / Benzerga, A.A. / Karaman, I. et al. | 2019
- 473
-
Materials informatics: From the atomic-level to the continuumRickman, J.M. / Lookman, T. / Kalinin, S.V. et al. | 2019
- 511
-
Corrigendum to “Crystal orientation dependence of the stress-induced martensitic transformation in zirconia-based shape memory ceramics” [Acta Mater. 116 (2016) 124–135]Zeng, Xiao Mei / Lai, Alan / Gan, Chee Lip / Schuh, Christopher A. et al. | 2019
- 513
-
Corrigendum to “Relationship between electromechanical properties and phase diagram in the Ba(Zr0.2Ti0.8)O3–x(Ba0.7Ca0.3)TiO3 lead-free piezoceramic” [Acta Mater. 80 (2014) 48–55]Acosta, Matias / Novak, Nikola / Jo, Wook / Rödel, Jürgen et al. | 2019
- iii
-
Editors for Acta Materialia| 2018