Effects of welding defects on reducing lifetimes of first stage nozzles of a 123MW gas turbine made of FSX-414 alloy (Unknown)
- New search for: Jahangiri, M.R.
- New search for: Jahangiri, M.R.
- New search for: Fallah, A.A.
In:
Materials and design
;
32
, 1
; 424-433
;
2011
-
ISSN:
- Article (Journal) / Print
-
Title:Effects of welding defects on reducing lifetimes of first stage nozzles of a 123MW gas turbine made of FSX-414 alloy
-
Contributors:Jahangiri, M.R. ( author ) / Fallah, A.A.
-
Published in:Materials and design ; 32, 1 ; 424-433
-
Publisher:
- New search for: Elsevier Science
-
Place of publication:Oxford
-
Publication date:2011
-
ISSN:
-
ZDBID:
-
Type of media:Article (Journal)
-
Type of material:Print
-
Language:Unknown
- New search for: 51.00 / 51.00 / 51.32 / 51.32
- Further information on Basic classification
-
Classification:
-
Source:
Table of contents – Volume 32, Issue 1
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 1
-
Effect of tool rotational speed and probe length on lap joint quality of a friction stir welded magnesium alloyCao, X. et al. | 2011
- 12
-
Effects of industrial scale production on the chemical composition of novel coupling agents and its relationship to the mechanical properties of chopped glass fibre mat reinforced thermoset compositesVarga, Cs. et al. | 2011
- 21
-
Comparison of the microstructures in continuous-cooled and quench-tempered pre-hardened mould steelsHoseiny, H. et al. | 2011
- 29
-
Isothermal oxidation behavior of reactive hot-pressed TiN–TiB2 ceramics at elevated temperaturesYang, Zhen-Lin et al. | 2011
- 36
-
Influence of pores on the thermal insulation behavior of thermal barrier coatings prepared by atmospheric plasma sprayWang, L. et al. | 2011
- 48
-
Parameter identification of an elasto-plastic behaviour using artificial neural networks–genetic algorithm methodAguir, Hamdi et al. | 2011
- 54
-
Effect of different whiskers on the physical and tribological properties of non-metallic friction materialsZhu, Zhencai et al. | 2011
- 62
-
Electrical, mechanical and thermal properties of polyvinyl chloride composites filled with aluminum powderBishay, I.K. et al. | 2011
- 69
-
Theoretical and experimental studies of the instantaneous folding force of the polyurethane foam-filled square honeycombsNiknejad, Abbas et al. | 2011
- 76
-
Bond strength evaluation of roll bonded bi-layer copper alloy strips in different rolling conditionsHosseini, S.A. et al. | 2011
- 82
-
Microstructural evolution during friction surfacing of tool steel H13Rafi, H. Khalid et al. | 2011
- 88
-
Analysis of the S–N curves of welded joints enhanced by ultrasonic peening treatmentZhao, Xiaohui et al. | 2011
- 97
-
Fracture mechanisms of aluminium alloy AA7075-T651 under various loading conditionsPedersen, Ketill O. et al. | 2011
- 108
-
Optimisation of process parameters in flanging operation in order to minimise stresses and Lemaitre’s damageBahloul, Riadh et al. | 2011
- 121
-
The influence of Strontium addition on wear properties of Al–20wt% Si alloys under dry reciprocating sliding conditionLiu, Gang et al. | 2011
- 127
-
Design of laser micromachined single crystal 6H–SiC diaphragms for high-temperature micro-electro-mechanical-system pressure sensorsGupta, Saurabh et al. | 2011
- 133
-
Corrosion resistance enhancement of Ni–P electroless coatings by incorporation of nano-SiO2 particlesRabizadeh, Taher et al. | 2011
- 139
-
Crack and wear behavior of SiC particulate reinforced aluminium based metal matrix composite fabricated by direct metal laser sintering processGhosh, Subrata Kumar et al. | 2011
- 146
-
Processing of porous Ti and Ti5Mn foams by spark plasma sinteringIbrahim, Ahmed et al. | 2011
- 154
-
Ductility of thin copper films on rough polymer substratesXu, W. et al. | 2011
- 162
-
Influence of lustrous carbon defects on the fatigue life of ductile iron castings using lost foam processChakherlou, T.N. et al. | 2011
- 170
-
Utilization of new micronized and nano-CoO·MgO/kaolin mixed pigments in improving the properties of styrene–butadiene rubber compositesAhmed, N.M. et al. | 2011
- 183
-
Fatigue life prediction under variable loading based on a new damage modelAid, A. et al. | 2011
- 192
-
Contribution of Ti addition to characteristics of extruded Cu40Zn brass alloy prepared by powder metallurgyLi, Shufeng et al. | 2011
- 198
-
The size effect on micro deformation behaviour in micro-scale plastic deformationChan, W.L. et al. | 2011
- 207
-
Microstructure evolution and oxidation behaviour of Tif/TiAl3 compositesYang, W.S. et al. | 2011
- 217
-
Selection and experimental evaluation of low-cost porous materials for regenerator applications in thermoacoustic enginesAbduljalil, Abdulrahman S. et al. | 2011
- 229
-
Dissimilar welding of WC–Co cemented carbide to Ni42Fe50.9C0.6Mn3.5Nb3 invar alloy by laser–tungsten inert gas hybrid weldingXu, P.Q. et al. | 2011
- 238
-
Polyfuran, polythiophene and their blend as novel antioxidants for styrene- butadiene rubber vulcanizatesAbdelwahab, N.A. et al. | 2011
- 246
-
Characterization of raw materials and manufactured binderless particleboard from oil palm biomassHashim, Rokiah et al. | 2011
- 255
-
Study of the characteristics of duplex stainless steel activated tungsten inert gas weldsChern, Tsann-Shyi et al. | 2011
- 264
-
Powder material parameters establishment through warm forming routeRahman, M.M. et al. | 2011
- 272
-
An experimental study on the comparative assessment of hydraulic bulge test analysis methodsKoç, Muammer et al. | 2011
- 282
-
Stress distribution in dental implant with elastomeric stress barrierAchour, T. et al. | 2011
- 291
-
The role of impressions on users’ tactile interaction with product materials: An analysis of associative concept networksNagai, Yukari et al. | 2011
- 303
-
The influence of hybrid phosphate–alumina pigments on properties of Ethylene-propylene-diene rubber compositesAhmed, Nivin M. et al. | 2011
- 322
-
The fatigue damage development in a cast Al–Si–Cu alloyDietrich, Lech et al. | 2011
- 330
-
The effect of sigma phases formation depending on Cr/Ni equivalent ratio in AISI 316L weldmentsKim, Y.H. et al. | 2011
- 337
-
Basalt woven fiber reinforced vinylester composites: Flexural and electrical propertiesCarmisciano, Salvatore et al. | 2011
- 343
-
Ultrasonic assisted fabrication of particle reinforced bonds joining aluminum metal matrix compositesYan, Jiuchun et al. | 2011
- 348
-
Effect of grain refinement on the mechanical properties of Cu–Al–Be–B shape memory alloyZhang, Ping et al. | 2011
- 353
-
Simulation of effects of particle size and volume fraction on Al alloy strength, elongation, and toughness by using strain gradient plasticity conceptZhou, Li et al. | 2011
- 361
-
Precipitation and its effect on age-hardening behavior of as-cast Mg–Gd–Y alloyLiang, Shuquan et al. | 2011
- 365
-
Superelastic behavior of aged and thermomechanical treated NiTi alloy at Af+10degreeCShahmir, H. / Nili-Ahmadabadi, M. / Naghdi, F. et al. | 2011
- 365
-
Superelastic behavior of aged and thermomechanical treated NiTi alloy at Af +10°CShahmir, H. et al. | 2011
- 371
-
Effect of Cr/Ni equivalent ratio on ductility-dip cracking in AISI 316L weld metalsJang, A.Y. et al. | 2011
- 377
-
Radiative properties characterization of ZrB2–SiC-based ultrahigh temperature ceramic at high temperatureMeng, Songhe et al. | 2011
- 382
-
Interfacial microstructure and mechanical properties of joining electroless nickel plated quartz fibers reinforced silica composite to InvarLei, Zhao et al. | 2011
- 388
-
Effect of vacuum heat treatment on microstructure and microhardness of cold-sprayed TiN particle-reinforced Al alloy-based compositesLi, Wen-Ya et al. | 2011
- 395
-
Microstructures and mechanical properties of directionally solidified Ti–45Al–8Nb–(W, B, Y) alloysDing, X.F. et al. | 2011
- 401
-
Effect of BN grain size on microstructure and mechanical properties of the ZrB2–SiC–BN compositesLi, Gang et al. | 2011
- 406
-
Hot tensile properties and microstructural evolution of as cast NiTi and NiTiCu shape memory alloysMorakabati, M. et al. | 2011
- 414
-
Optimization of injection molding process parameters using sequential simplex algorithmFarshi, Behrooz et al. | 2011
- 424
-
Effects of welding defects on reducing lifetimes of first stage nozzles of a 123MW gas turbine made of FSX-414 alloyJahangiri, M.R. et al. | 2011
- 433
-
Mechanical and corrosion behavior of plain low carbon dual-phase steelsBhagavathi, Lakshmana Rao et al. | 2011
- 441
-
Compatibility study of high density polyethylene with bioethanol–gasoline blendsBerlanga-Labari, C. et al. | 2011
- 447
-
Investigation on the effect of lubrication and forming parameters to the green compact generated from iron powder through warm forming routeRahman, M.M. et al. | 2011
- 453
-
Microstructural, physico-chemical and mechanical characterisation of Sansevieria cylindrica fibres – An exploratory investigationSreenivasan, V.S. et al. | 2011
- 462
-
Prediction of tensile strength of friction stir welded aluminium matrix TiCp particulate reinforced compositeGopalakrishnan, S. et al. | 2011
-
Inside Front Cover (Editorial Board)| 2011