Effect of oxygen on near-neutral pH stress corrosion crack initiation under a simulated tape coating disbondment (English)
- New search for: Eslami, A.
- New search for: Eadie, R.
- New search for: Chen, W.
- New search for: Eslami, A.
- New search for: Eadie, R.
- New search for: Chen, W.
In:
Canadian Metallurgical Quarterly
;
55
, 2
;
177-185
;
2016
- Article (Journal) / Electronic Resource
-
Title:Effect of oxygen on near-neutral pH stress corrosion crack initiation under a simulated tape coating disbondment
-
Contributors:
-
Published in:Canadian Metallurgical Quarterly ; 55, 2 ; 177-185
-
Publisher:
- New search for: Taylor & Francis
-
Publication date:2016-04-02
-
Size:9 pages
-
ISSN:
-
DOI:
-
Type of media:Article (Journal)
-
Type of material:Electronic Resource
-
Language:English
-
Keywords:
-
Source:
Table of contents – Volume 55, Issue 2
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 131
-
Microstructure and mechanical properties of Al-alloyed ductile iron upon casting and austemperingMourad, M. M. / El-Hadad, S. / Ibrahim, M. M. / Nofal, A. A. et al. | 2016
- 138
-
The effects of Ni3Al binder content on the electrochemical response of melt-infiltration processed TiC–Ni3Al cermetsHolmes, M. B. / Ibrahim, A. / Kipouros, G. J. / Farhat, Z. N. / Plucknett, K. P. et al. | 2016
- 147
-
Simultaneous co-deposition of SiC and CNT into the Ni coatingMosallanejad, M. H. / Shafyei, A. / Akhavan, S. et al. | 2016
- 156
-
Effects of ternary elements on the ductility of TiAlShu, S.-L. / Tong, C.-Z. / Qiu, F. / Zou, Q. / Jiang, Q.-C. et al. | 2016
- 161
-
Thermodynamics and kinetics analyses of ZrB2 formation in molten aluminium alloysKhaliq, A. / Rhamdhani, M. A. / Brooks, G. A. / Grandfield, J. et al. | 2016
- 173
-
Synthesis of TiC–TiB–TiB2 composite powders by solid reaction of powdersWu, S. / Wang, Y. / Fei, Y. / Yang, Y. / Guo, Q. et al. | 2016
- 177
-
Effect of oxygen on near-neutral pH stress corrosion crack initiation under a simulated tape coating disbondmentEslami, A. / Eadie, R. / Chen, W. et al. | 2016
- 186
-
Influence of MgO, Al2O3 and CaO/SiO2 on the viscosity of blast furnace type slag with high Al2O3 and 5 wt-% TiO2Yan, Z. / Lv, X. / Zhang, J. / Qin, Y. / Bai, C. et al. | 2016
- 195
-
Pyrite oxidation kinetics in an oxygen–nitrogen atmosphere at temperatures from 400 to 500°CAracena, A. / Jerez, O. / Ortiz, R. / Morales, J. et al. | 2016
- 202
-
Solubility and activity of oxygen in liquid bismuthJacob, K. T. / Mansoor, A. K. et al. | 2016
- 210
-
Kinetic study on the metallothermic reduction of chromite ore using magnesium scrapOchoa, R. / Flores, A. / Torres, J. / Guía, J. / Muñiz, R. et al. | 2016
- 221
-
Study on electrical conductivity of FexO–CaO–SiO2–Al2O3 slagsLiu, J.-H. / Zhang, G.-H. / Wu, Y.-D. / Chou, K.-C. et al. | 2016
- 226
-
High-temperature phase equilibria of Cu–O–Al2O3 system in airHellstén, N. / Hamuyuni, J. / Taskinen, P. et al. | 2016
- 234
-
Distribution equilibria and slag chemistry of DON smeltingStrengell, D. / Avarmaa, K. / Johto, H. / Taskinen, P. et al. | 2016
- 243
-
Phase equilibria of the Na2O–SiO2 system between 1173 and 1873 KSantoso, I. / Taskinen, P. et al. | 2016
- 251
-
Numerical simulation of copper recovery from converter slags by the utilisation of spent potlining (SPL) from aluminium electrolytic cellsYu, D. / Chattopadhyay, K. et al. | 2016