Morphology characterisation of pitting corrosion on sensitized austenitic stainless steel by digital image analysis (English)
- New search for: Ribeiro, R.B.
- New search for: Silva, J.W.J.
- New search for: Hein, L.R.O.
- New search for: Pereira, M.C.
- New search for: Codaro, E.N.
- New search for: Matias, N.T.
- New search for: Bereket, G.
- New search for: Caporali, S.
- New search for: Salghi, R.
- New search for: Ribeiro, R.B.
- New search for: Silva, J.W.J.
- New search for: Hein, L.R.O.
- New search for: Pereira, M.C.
- New search for: Codaro, E.N.
- New search for: Matias, N.T.
- New search for: Bereket, G.
- New search for: Caporali, S.
- New search for: Salghi, R.
In:
ISRN Corrosion
;
2013
;
1-7
;
2013
-
ISSN:
- Article (Journal) / Print
-
Title:Morphology characterisation of pitting corrosion on sensitized austenitic stainless steel by digital image analysis
-
Contributors:Ribeiro, R.B. ( author ) / Silva, J.W.J. ( author ) / Hein, L.R.O. ( author ) / Pereira, M.C. ( author ) / Codaro, E.N. ( author ) / Matias, N.T. ( author ) / Bereket, G. ( author ) / Caporali, S. ( author ) / Salghi, R. ( author )
-
Published in:ISRN Corrosion ; 2013 ; 1-7
-
Publisher:
-
Publication date:2013
-
Size:7 Seiten, 21 Quellen
-
ISSN:
-
DOI:
-
Type of media:Article (Journal)
-
Type of material:Print
-
Language:English
-
Keywords:
-
Source:
Table of contents – Volume 2013
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 1
-
One-step anodization/sol-gel deposition of Ce3+-doped silica-zirconia self-healing coating on aluminumKumar, N. / Jyothirmayi, A. / Raju, K.R.C.Soma / Uma, V. / Subasri, R. / Aparicio, M. / Bereket, G. / Sakairi, M. et al. | 2013
- 1
-
Evaluation of corrosion growth on SS304 based on textural and color features from image analysisPidaparti, Ramana M. / Hinderliter, Brian / Maskey, Darshan / Fürbeth, W. / Salghi, R. et al. | 2013
- 1
-
Corrosion behaviour of Ti-6Al-4V alloy with nitride coatings in simulated body fluids at 36 °C and 40 °CPohrelyuk, I.M. / Tkachuk, O.V. / Proskurnyak, R.V. / Bereket, G. / Hsu, C.H. / Wang, R. et al. | 2013
- 1
-
The corrosion resistance of nickel electrocomposite coating containing BaFe12O19 particlesAruna, S.T. / Savitha, G. / Shedthi, Jyothi / William Grips, V.K. / El Mahdy, G. / Gu, C. / Miao, H. / Valentini, C. et al. | 2013
- 1
-
Corrosion inhibition of Cu-Ni (90/10) alloy in seawater and sulphide-polluted seawater environments by 1,2,3-benzotriazoleBoyapati, Venkata Appa Rao / Kanukula, Chaitanya Kumar / Fuerbeth, W. / Lee, S.J. et al. | 2013
- 1
-
Corrosion of WC-VC-Co hardmetal in neutral chloride containing mediaMachio, C.N. / Konadu, D.S. / Potgieter, J.H. / Potgieter-Vermaak, S. / Van der Merwe, J. / Marginean, G. / Wang, R. et al. | 2013
- 1
-
Effect of serine and methionine on electrochemical behavior of the corrosion of mild steel in aqueous solutionsRahuma, Mohamed N. / El Sabbah, Mohamed B. / Hamad, Imperiyka M. / Boshkov, N. / Qu, Q. et al. | 2013
- 1
-
Corrosion study of powder-coated galvanised steelBhadu, Manish Kumar / Guin, Akshya Kumar / Singh, Veena / Choudhary, Shyam K. / Hsu, C.H. / Umoren, S. et al. | 2013
- 1
-
Microstructural characteristics and mechanical properties of nanostructured and conventional TiAlN and AlCrN coatings on ASTM-SA210 Grade A-1 boiler steelChawla, Vikas / Lee, S.J. / Qu, Q. / Solmaz, R. et al. | 2013
- 1
-
Morphology characterisation of pitting corrosion on sensitized austenitic stainless steel by digital image analysisRibeiro, R.B. / Silva, J.W.J. / Hein, L.R.O. / Pereira, M.C. / Codaro, E.N. / Matias, N.T. / Bereket, G. / Caporali, S. / Salghi, R. et al. | 2013
- 1
-
Corrosion inhibition and adsorption properties of ethanolic extract of Calotropis for corrosion of aluminium in acidic mediaKumar, Sudesh / Mathur, Suraj Prakash / Boshkov, N. / Gervasi, C. / Qu, Q. et al. | 2013