The effect of cycling on the stress corrosion cracking mechanisms of an 8090 Al-Li-Cu alloy (English)
- New search for: Magnin, T.
- New search for: Chieragatti, R.
- New search for: Magnin, T.
- New search for: Chieragatti, R.
In:
Materials Science and Engineering, Part A (Structural Materials: Properties, Microstructure and Processing)
;
A154
, 1
;
L5-L7
;
1992
-
ISSN:
- Article (Journal) / Print
-
Title:The effect of cycling on the stress corrosion cracking mechanisms of an 8090 Al-Li-Cu alloy
-
Additional title:Der Einfluß zyklischer Belastung auf die Mechanismen der Spannungsrißkorrosion bei der Al-Li-Cu-Legierung 8090
-
Contributors:Magnin, T. ( author ) / Chieragatti, R. ( author )
-
Published in:
-
Publisher:
-
Publication date:1992
-
Size:3 Seiten, 5 Bilder, 6 Quellen
-
ISSN:
-
DOI:
-
Type of media:Article (Journal)
-
Type of material:Print
-
Language:English
-
Keywords:ALUMINIUMLEGIERUNG , CHEMISCHE ZUSAMMENSETZUNG , BLECH , STRANGPRESSEN (METALL) , LOESUNGSGLUEHEN , GLUEHTEMPERATUR , WASSERABSCHRECKEN , RECKALTERUNG , UMFORMGRAD , TEMPERATUR , HALTEDAUER , KORROSIONSERMUEDUNG , SPANNUNGSRISSKORROSION , LUFT (GASFOERMIGER STOFF) , NATRIUMCHLORID , WAESSRIGE LOESUNG , DEHNGESCHWINDIGKEITSEMPFINDLICHKEIT , MIKRORISS
-
Source:
Table of contents – Volume A154, Issue 1
The tables of contents are generated automatically and are based on the data records of the individual contributions available in the index of the TIB portal. The display of the Tables of Contents may therefore be incomplete.
- 1
-
Comparison of saturation behavior of thermal shock damage in a variety of brittle materialsWon Jae Lee / Case, E.D. et al. | 1992
- 11
-
Fracture mechanisms of fiber-reinforced titanium alloy matrix composites. V: Fatigue crack propagationJeng, S.M. / Alassoeur, P. / Yang, J.M. et al. | 1992
- 21
-
Intergranular crack tip oxidation mechanism in a nickel-based superalloyAndrieu, E. / Molins, R. / Ghonem, H. / Pineau, A. et al. | 1992
- 29
-
Plastic deformation and decay of dislocation in quasi-crystalsOvidko, I.A. et al. | 1992
- 35
-
Micromechanical fracture process of SiC-particle-reinforced aluminium alloy 6061-T6 metal matrix compositesKim, H.J. / Kobayashi, T. / Yoon, H.S. / Yoon, E.P. et al. | 1992
- 43
-
Effects of chemical composition, rolling and cooling conditions on the amount of martensite/austenite (M/A) constituent formation in low carbon bainitic steelsXhyi-Cing Wang / Jer-Ren Yang et al. | 1992
- 59
-
Influence of solution treatment on the microstructure of a 9 wt.%Cr-1 wt%Mo-0.07 wt.%C steelSaroja, S. / Vijayalakshmi, M. / Raghunathan, V.S. et al. | 1992
- 69
-
Flow transient during strain rate jump tests in a titanium-modified austenitic stainless steelVenkadesan, S. / Rodriguez, P. / Padmanabhan, K.A. / Sivaprasad, P.V. / Phaniraj, C. et al. | 1992
- 75
-
Design of Ti-Al-V beta phase for transformation toughening of gamma-titanium aluminideMica Grujicic et al. | 1992
- 79
-
Ferromagnetic icosahedral Al-Cu-Mn-Ge alloy by mechanical alloyingBahadur, D. / Singh, K. / Roy, M. et al. | 1992
- 85
-
A study of solidification crack susceptibility using the solidification cycle hot-tension testSun, Z. et al. | 1992
- 93
-
Temperature rise of rapidly solidified deposit layers of Al-Si alloys during low pressure plasma spraying and its effect on their structures and mechanical propertiesKanji Murakami / Naoki Takuno / Taira Okamoto / Yoshinari Miyamoto et al. | 1992
- 103
-
Effect of boron nitride coating on the tensile strength of Nextel 480Fernando, J.A. / Chawla, K.K. / Ferber, M.K. / Coffey, D. et al. | 1992
- L1
-
Tensile properties and shape memory effect of chromium-varied Fe-30Mn-5Si-Cr shape memory alloysYang, Jung P. / Kim, Young G. et al. | 1992
- L5
-
The effect of cycling on the stress corrosion cracking mechanisms of an 8090 Al-Li-Cu alloyMagnin, T. / Chieragatti, R. et al. | 1992
- L9
-
On the rotational effect on shock-loaded metalsGutkin, M.Y. / Ovidko, I.A. et al. | 1992